| HS Code | 905859 |
| Density | 1.36 g/cm³ |
| Melting Point | 250-270 °C |
| Glass Transition Temperature | 120-155 °C |
| Water Absorption | 0.30% |
| Molding Shrinkage | 0.2-0.6% |
| Tensile Strength | 55-75 MPa |
| Tensile Modulus | 2.2-2.8 GPa |
| Elongation At Break | 10-50% |
| Flexural Modulus | 2.2-2.8 GPa |
| Heat Deflection Temperature | 85-100 °C at 1.82 MPa |
| Dielectric Constant | 3.0-3.2 at 1 MHz |
| Dissipation Factor | 0.002-0.005 at 1 MHz |
| Dielectric Strength | 20-30 kV/mm |
| Processing Temperature | 280-300 °C |
As an accredited Mitsubishi Chemical PEN Resin Generic PEN factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Mitsubishi Chemical PEN Resin Generic PEN is supplied in 25 kg moisture-barrier bags, palletized for industrial handling and storage. |
| Container Loading (20′ FCL) | Generic PEN resin is loaded into a 20-foot FCL dry container, palletized or bagged, and secured for ambient ocean transport. |
| Shipping | Shipping description: Mitsubishi Chemical PEN Resin Generic PEN is supplied as solid resin pellets in moisture-barrier bags, drums, or octabins. It is generally not classified as dangerous goods for transport. Ship in dry, ventilated conditions, avoiding heat, sunlight, and moisture; standard cargo handling applies. |
| Storage | Store Mitsubishi Chemical PEN Resin Generic PEN in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep containers tightly closed to prevent moisture, dust, and contamination. Avoid static buildup and contact with strong oxidizers or incompatible materials. Follow the manufacturer’s SDS, labeling, and local storage regulations. |
| Shelf Life | Store in original sealed packaging in a dry, cool place away from sunlight; typical shelf life is 12 months. |
Competitive Mitsubishi Chemical PEN Resin Generic PEN prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
The product designated Mitsubishi Chemical PEN Resin Generic PEN is an unfilled thermoplastic polyester derived from ethylene glycol and 2,6-naphthalenedicarboxylic acid. The naphthalene ring in the main chain increases chain stiffness and packing density relative to poly(ethylene terephthalate) and poly(butylene terephthalate), producing a resin grade intended for injection moulding, extrusion, and compounding where elevated thermal stability and reduced gas permeation are required. The generic designation indicates a non-application-specific pellet product; specific lot certifications for intrinsic viscosity, carboxyl end-group concentration, and colour coordinates should be obtained from the supplier before process qualification. Representative neat PEN homopolymer values measured according to ISO 1183 place solid density at approximately 1.36 g/cm³. The glass transition measured by ISO 11357-2 typically occurs near 120 °C, while the crystalline melting endotherm appears near 265 °C. These thermal transitions are approximately 45 °C and 10–15 °C higher than corresponding transitions in bottle-grade PET, which directly expands the upper service temperature in structural applications. Melt viscosity is shear-sensitive; published data for the Mitsubishi Chemical generic grade is limited, but unfilled PEN grades commonly exhibit an MVR of 10–30 cm³/10 min at 300 °C under 1.2 kg load when tested to ISO 1133-1:2022.
Pre-drying with a closed-loop desiccant dryer to a dew point of −40 °C or lower is required for typical melt-processing operations. Residual moisture content below 50 ppm is the accepted threshold to limit hydrolytic chain scission during plastication; above 80 ppm, measurable reductions in intrinsic viscosity and increases in acetaldehyde generation become apparent on production-scale injection lines. Drying at 150 °C for 4–6 h using a hopper dryer with a regenerated desiccant bed is standard. When ambient relative humidity exceeds 60 %, residence time should be extended to 6–8 h, and the hopper should remain under positive dry-air purge. Machine hoppers with unheated conical sections have been observed to permit moisture regain in high-humidity plants, causing intermittent nozzle drool and loss of shot-to-shot consistency on machines with 100–150 t clamp force running thin-wall connectors.
Substitution of the naphthalene-2,6-dicarboxylate for terephthalate increases mesomeric conjugation along the polymer backbone and reduces free volume. The resulting polymer has a higher cohesive energy density, which lowers oxygen and carbon dioxide transmission relative to PET by a factor of approximately 4–5× when measured at 23 °C and 50 % RH by ASTM D3985. Water vapour barrier is improved but to a lesser extent; typical PEN homopolymer films exhibit roughly 2–3× lower water vapour transmission than PET at equivalent thickness under ASTM F1249. The naphthalate ring also shifts the ultraviolet absorption edge to longer wavelengths, which is functional for UV-blocking packaging and optical components but creates a slight yellow tint in thick sections. Compared with PBT, the generic PEN grade has lower aliphatic flexibility and therefore lower elongation at break but higher dimensional stability under load and lower creep at temperatures near 100 °C.
| Property | Test Method | PEN | PET | PBT |
|---|---|---|---|---|
| Solid density | ISO 1183 | 1.36 g/cm³ | 1.34 g/cm³ | 1.31 g/cm³ |
| Glass transition | ISO 11357-2 | 120 °C | 78 °C | 45 °C |
| Melting point | ISO 11357-3 | 265 °C | 255 °C | 225 °C |
| Tensile modulus | ISO 527-2 | 2.4–2.7 GPa | 2.0–2.2 GPa | 2.5–2.8 GPa |
| Oxygen barrier factor | ASTM D3985 | 4–5× lower than PET | reference | poorer than PET |
Melt processing on a reciprocating screw injection moulding machine with a low-compression barrier screw is recommended. A screw L/D of 20:1–24:1 and compression ratio of 2.5:1–3.0:1 provide sufficient melting without excessive shear heating. Barrel temperature profiles are typically set from 280 °C at the rear zone to 310–320 °C at the nozzle, with the melt temperature measured at the nozzle held between 300 °C and 315 °C. Exceeding 320 °C for more than 5 min residence time promotes thermal degradation, visible as yellowing and a drop in melt viscosity. Production lines with hot-runner systems should use externally heated manifolds with minimum dead spots; internally heated systems have shown higher pressure drop and uneven filling when processing unfilled PEN at melt temperatures below 295 °C. Clamp force requirements are similar to PET, but injection pressures are generally 10–20 % higher due to the higher melt viscosity at equivalent temperatures. Mould temperatures between 120 °C and 150 °C are required to achieve sufficient crystallinity for dimensional stability in demoulded parts. In thin-wall moulding below 1.0 mm wall thickness, filling analysis should assume a solidification layer that develops more rapidly than PET at mould temperatures below 110 °C.
For extrusion compounding, a co-rotating twin-screw extruder with L/D 36:1–44:1 and vacuum venting at −0.08 MPa gauge is appropriate. The higher melting point requires zone settings 20–30 °C above PET to avoid unmelted granules in the side feeder zone. Torque per unit throughput typically increases relative to PET by 15–25 % at the same screw speed, which should be accounted for in gearbox sizing. Strand pelletizing is preferred over water-ring pelletizing because rapid quenching can produce amorphous pellets with excessive fines and irregular shape. Published data for this specific Mitsubishi Chemical grade is limited; these are representative processing windows for unfilled PEN homopolymer.
Where ultraviolet blocking and reduced birefringence are required, the naphthalate structure provides intrinsic UV absorption below 380 nm without the use of low-molecular-weight UV stabilizers. This is relevant for optical pick-up bases, solar cell junction boxes, and sensor housings where additive migration to the surface can degrade reflectivity or electrical contact resistance. Moulded plaques of 2 mm thickness show increased yellowness index compared with PET; colour tolerances should be specified against ASTM D1003 and ASTM E313 prior to tooling release. Surface gloss is influenced by mould temperature and polishing direction; hot-tool moulding at 140 °C reduces internal haze but can replicate micro-scratches from an inadequately vented cavity. Applications requiring high optical clarity are not recommended for thick sections above 3 mm because the intrinsic absorption edge produces perceptible yellow tint under D65 illumination.
Regrind strategies for the generic PEN grade must account for thermal and hydrolytic degradation accumulated during first-pass processing. Up to 30 wt% clean regrind of the same resin is commonly acceptable in non-critical parts if the regrind has been dried to below 50 ppm moisture and the flake size distribution is controlled to prevent bridging in the throat. Above 30 wt%, increases in carboxyl end-group concentration and decreases in intrinsic viscosity may shift melt viscosity below the lower control limit for thin-wall filling. Capillary rheometry at 300 °C and a shear rate of 1000 s⁻¹ provides a practical incoming lot check; a viscosity drop greater than 10 % relative to virgin pellets indicates excessive degradation. On injection lines producing SMT-compatible connectors, regrind above 40 wt% has been associated with short shots in ribs below 0.4 mm width and with intermittent gate blush on hot-runner drops. For applications requiring JEDEC moisture-sensitivity level rating, regrind content should be specified because additional heat history alters moisture uptake and desorption kinetics under J-STD-020 reflow profiles.
Hydrolysis of the ester linkages proceeds autocatalytically when the melt contains free water or acidic species. The apparent activation energy for hydrolytic chain scission in PEN is close to that of PET, but the lower processing moisture tolerance of PEN arises from the higher melt temperature required. At a melt temperature of 310 °C, each 10 ppm increase in residual moisture above 50 ppm can reduce intrinsic viscosity measurably within a single average residence time of 2–4 min. The practical consequence is that even brief exposure of dried pellets to ambient air in a transfer line can reintroduce sufficient moisture to produce viscosity drift. Therefore, machine feed throats should be blanketed with dried air at a dew point below −30 °C. Chemical incompatibilities include unneutralized primary amines, strong alkali solutions above 60 °C, and chlorinated solvents such as methylene chloride, which can induce environmental stress cracking in moulded parts under residual stress. Aliphatic hydrocarbons, mineral oils, dilute acids at ambient temperature, and alcohol-based cleaners generally show acceptable compatibility under short-term contact. Long-term exposure to hot water above 80 °C is not recommended for load-bearing components because hydrolysis of the amorphous phase reduces tensile strength at welded joints.
For regulatory submissions, the neat resin is typically assessed under the European Union REACH regulation and the RoHS Directive. No intentionally added substances of very high concern are expected above 0.1 wt% in the homogeneous resin under Regulation (EC) No 1907/2006, Article 33. RoHS compliance under Directive 2011/65/EU as amended by (EU) 2015/863 applies only to electrical and electronic equipment; the neat resin does not contain the restricted heavy metals or phthalate plasticizers above the maximum concentration values. Food-contact status for the generic grade is not self-certified and must be confirmed against a specific supplier compliance letter, because migration limits under Regulation (EU) No 10/2011 are grade and application dependent. The following checklist is used for initial compliance screening.
| Regulatory Area | Standard or Regulation | Typical Status for Neat Generic PEN |
|---|---|---|
| REACH SVHC | Regulation (EC) No 1907/2006 Article 33 | No intentionally added SVHC above 0.1 wt% |
| RoHS restricted substances | Directive 2011/65/EU (EU) 2015/863 | Below maximum concentration values for homogeneous material |
| Food-contact migration | Regulation (EU) No 10/2011 | Supplier-specific compliance letter required |
| Moisture sensitivity classification | J-STD-020 | Application and regrind dependent; no universal level |