Mitsubishi Chemical Novaduran Unreinforced Soft Pbt 5510r

Mitsubishi Chemical Novaduran™ Unreinforced-Soft PBT 5510R

    • Product Name: Mitsubishi Chemical Novaduran™ Unreinforced-Soft PBT 5510R
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 868179
    Density 1.21 g/cm³
    Moldshrinkage 1.5-2.0 %
    Waterabsorption 0.08 %
    Tensilestrength 45 MPa
    Tensileelongationatbreak 150 %
    Flexuralmodulus 1,700 MPa
    Flexuralstrength 65 MPa
    Charpynotchedimpactstrength 15 kJ/m²
    Hdt 1 82mpa 65 °C
    Hdt 0 45mpa 150 °C
    Meltingpoint 224 °C
    Ul94flammability HB

    As an accredited Mitsubishi Chemical Novaduran™ Unreinforced-Soft PBT 5510R factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Typically supplied in 25 kg moisture-proof bags, Mitsubishi Chemical Novaduran™ Unreinforced-Soft PBT 5510R packaging supports safe storage and handling.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Mitsubishi Chemical Novaduran™ Unreinforced-Soft PBT 5510R, 25 kg bags palletized, shrink-wrapped and secured for sea transport.
    Shipping Mitsubishi Chemical Novaduran™ Unreinforced-Soft PBT 5510R ships as non-hazardous thermoplastic pellets in sealed, moisture-barrier bags or containers under normal freight conditions. Keep packaging intact and labeled; store dry, away from heat and sunlight. No special dangerous-goods handling is required unless local regulations specify otherwise.
    Storage Mitsubishi Chemical Novaduran™ Unreinforced-Soft PBT 5510R should be stored in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and moisture. Keep containers tightly closed when not in use to prevent contamination and moisture uptake. Avoid contact with strong oxidizers, acids, and bases. Follow local regulations and use proper labeling and inventory rotation.
    Shelf Life Mitsubishi Chemical Novaduran™ Unreinforced-Soft PBT 5510R typically has a 24-month shelf life when stored dry, cool, and in sealed original packaging.
    Free Quote

    Competitive Mitsubishi Chemical Novaduran™ Unreinforced-Soft PBT 5510R prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Novaduran™ Unreinforced-Soft PBT 5510R is a Mitsubishi Chemical polybutylene terephthalate injection-moulding grade supplied without glass-fibre reinforcement and with a reduced stiffness profile compared with standard unfilled PBT. The grade is intended for parts requiring repeated assembly deflection, including snap-fit closures, cable clamps, grommets, seals, plug housings, and strain-relief components. Its specification framework references ISO 1183-1 for density, ISO 1133-1 melt volume-flow rate at 250 °C with a 2.16 kg piston load, ISO 527-1/-2 for tensile modulus, stress, and strain, ISO 178 for flexural modulus, ISO 868 for Shore D hardness, ISO 179/1eA for Charpy notched impact, ISO 180/1A for Izod notched impact, ISO 75-1/-2 for heat deflection temperature, and ISO 294-4 for mould shrinkage. Because lot-specific numerical values depend on formulation and process history, the manufacturer certificate of analysis is the controlling release document. Published numerical data for this exact configuration in open literature is limited; the supplier technical datasheet should be treated as authoritative for design inputs.

    Material handling for 5510R is governed by the hydrolysis sensitivity of the polybutylene terephthalate backbone. The resin is dried in a desiccant-bed dryer with supply air dew point at or below -40 °C, typically at 120 °C for 4 h. When storage has exceeded 60% relative humidity, drying is extended to 6 h or the temperature raised to 130 °C. Target moisture content is below 0.02 wt% before the feed throat. Conveyance from dryer to machine throat uses dried air. Open hopper residence at 23 °C and 50% RH should remain below 30 min. Surface splay and a sharp drop in melt viscosity are the primary visual and rheological indicators of moisture reuptake. On a 40 mm screw with L/D between 20:1 and 24:1, rear-to-nozzle barrel settings of 240/245/250/255 °C and a nozzle melt temperature of 250–260 °C are typical. Tool temperature is held at 60–80 °C to balance crystallinity, chemical resistance, and post-mould dimensional stability.

    What separates the 5510R material from standard unfilled and glass-filled Novaduran grades?

    The primary separation is in stiffness and deflection response. A 30% glass-filled PBT commonly exhibits flexural modulus in the range of 8–10 GPa under ISO 178, while an unreinforced soft PBT is generally positioned below 2 GPa. This reduction lowers insertion force in snap-fit assembly and reduces stress concentration at sharp root radii, but it also reduces load-bearing capacity and bolt-boss pull-out strength. Compared with standard unfilled Novaduran 5010R, the 5510R grade typically exhibits lower Shore D hardness under ISO 868 and higher nominal strain at break under ISO 527-1/-2. Compared with thermoplastic polyester elastomers, 5510R retains the polyester continuous phase and therefore remains higher in modulus, harder, and more creep-resistant at room temperature under ISO 899-2, while giving up some low-temperature notched impact under ISO 180/1A. The substitution boundary is therefore set by creep modulus, notched impact, and clamping or sealing force requirements, not by melt temperature alone.

    Flow and tooling behaviour permit thin-wall filling, but gate and hot-runner control is required. For a 2 mm wall, screw-tip injection pressure is typically 60–100 MPa; hold pressure is usually 50–70% of peak fill pressure. Vent depth is maintained between 0.015 mm and 0.025 mm, because deeper vents may flash in unfilled soft PBT during packing. Gate thickness is normally 50–70% of the wall thickness and gate land is held below 1 mm to prevent premature freeze and high gate stress. In hot-runner systems, valve gates are preferred over open tips because unfilled soft PBT can drool, and dead-stop regions can cause discolouration after residence times exceeding 8–10 min at 260 °C. Shot size should use 30–70% of barrel capacity to limit residence-time effects and maintain melt homogeneity.

    When 5510R is evaluated for snap-fit closures and low-cycle hinge functions

    For snap-fit closures, lower flexural modulus under ISO 178 reduces outer-fibre strain at a given deflection. Design calculations compare allowable strain with the tensile stress/strain curve under ISO 527-1/-2. The reduced stiffness can increase repeated-assembly tolerance, but semi-crystalline PBT is not an ideal living-hinge material; the hinge line may develop stress whitening and fracture after repeated flexure. The grade should be limited to one-time assembly deflection or low-cycle flexing unless prototype flex-fatigue data at application frequency confirm survival. Weld-line strength measured on double-gate tensile specimens per ISO 527-1/-2 is lower than parent-material strength. Gate locations should keep weld lines away from snap-beam roots, pin-retention bosses, and sealing lips. Force-inserted metal pins in moulded bosses should be checked for hoop stress against tensile yield stress from ISO 527-1/-2; insertion force is reduced because the soft grade has lower hardness under ISO 868 than glass-filled PBT, but boss wall thickness must be validated to avoid splitting at low temperature.

    In electrical connector bodies, cable clamps, and grommets, 5510R is often qualified by thermal cycling from -40 °C to 85 °C, followed by notched impact under ISO 180/1A at low temperature and at room temperature. Unfilled PBT shows lower notched impact at -30 °C than at 23 °C, so gate blush and ejector marks should not lie in notch-sensitive stress paths. Long-term clamp retention is assessed by flexural creep or stress relaxation under ISO 899-2. Grommets and plugs benefit from the lower Shore D hardness under ISO 868, which reduces lip sealing force. The material is not a direct replacement for thermoset elastomers in high-temperature vibration isolation because its dynamic modulus and damping profile under dynamic mechanical analysis are different. In cable strain relief, cyclic flexure endurance should be evaluated with a defined bend radius and temperature, because PBT will not match the high-cycle flex-fatigue of a suitably compounded thermoplastic elastomer.

    Regrind incorporation is permissible after drying. Clean sprues and runners are commonly re-used at 20% by weight in unfilled PBT injection moulding. Higher regrind ratios lower notched impact under ISO 179/1eA and increase hydrolysis sensitivity because prior heat history has shortened average chain length. Regrind stored in open containers at 50% RH is re-dried at 120 °C for at least 4 h. Melt volume-flow rate should be checked after 3 regrind cycles against the supplier specification to prevent nonconforming parts. Virgin and regrind pellets are tumbled in a sealed container to counter demixing caused by bulk-density differences between irregular regrind particles and cylindrical virgin pellets.

    Chemical resistance and end-use compliance operate within defined boundaries.

    PBT resists aliphatic hydrocarbons, greases, and many automotive fluids at room temperature. The 5510R grade inherits the chemical resistance of PBT, but the soft-segment package and unfilled matrix impose limits. Continuous exposure to aqueous media above 60 °C accelerates hydrolysis. Strong alkaline solutions and acidic oxidising agents degrade the ester linkage and can attack the soft-segment package. Under mechanical load, chemical attack can be evaluated by environmental stress cracking tests such as ISO 22088-3; the unfilled soft grade has lower residual moulded-in stress than glass-filled PBT but remains susceptible to stressed-crack promotion in strong solvents. For electrical insulation, unfilled PBT often carries a UL 94 HB classification, but the current Yellow Card must be confirmed for the exact colour and wall thickness. Glow-wire ignition behaviour may be tested under IEC 60695-2-11. No food-contact status is implied; where relevant, compliance should be verified against FDA 21 CFR 177 and the applicable migration test method for the target polymer.

    In multi-cavity tools, balancing for this grade is validated by shot-weight variance below 2% across cavities. Runner and hot-runner channels are sized so that runner pressure drop does not dominate cavity pressure drop. When a long-flow component is transferred from a 30% glass-filled PBT, the same tool often requires higher injection speed and lower pack pressure. Weld lines in unfilled soft PBT may be less visible than in glass-filled PBT, but mechanical weakness remains. Sequential valve gating is commonly specified for large connector housings to move the weld line away from structural features. During process commissioning, in-mould cavity pressure measurements should be used to confirm that hold pressure transfers consistently to the last-filling cavity, because cavity-to-cavity imbalance will alter shrinkage under ISO 294-4 and can compromise snap-fit geometry.

    Lot acceptance, specification framework, and standards matrix

    PropertyStandard designationTypical reporting unit
    DensityISO 1183-1g/cm³
    Melt volume-flow rateISO 1133-1 at 250 °C, 2.16 kgcm³/10 min
    Tensile modulus, stress, strainISO 527-1/-2MPa, %
    Flexural modulus, strengthISO 178MPa
    Charpy notched impactISO 179/1eAkJ/m²
    Izod notched impactISO 180/1AkJ/m²
    Shore D hardnessISO 868Shore D
    Heat deflection temperatureISO 75-1/-2°C
    Mould shrinkageISO 294-4%

    The matrix is not a release limit; lot-specific certificate-of-analysis values control acceptance. For dimensional validation, mould shrinkage is measured after 48 h at 23 °C under ISO 294-4 and normally falls within 1.5–2.0% parallel to flow and can be 0.2–0.5% lower in the transverse direction, depending on gate location and packing pressure. Soft PBT has a greater tendency to creep under sustained load than glass-filled PBT; tight tolerances should be verified under ISO 291 conditioning and, where relevant, ISO 62 water absorption after exposure. Because the unfilled matrix is not constrained by glass fibres, anisotropic shrinkage can occur at thin-to-thick transitions. Tooling design should include cold slug wells and flow channels sized to prevent premature freeze at the fill end.

    Top