| HS Code | 429638 |
| Density | ≈1.62 g/cm³ |
| Glass Fiber Content | 40 wt% |
| Tensile Strength | 125 MPa |
| Tensile Elongation At Break | 2.0% |
| Flexural Modulus | 10,500 MPa |
| Flexural Strength | 180 MPa |
| Charpy Notched Impact Strength At 23 C | 8 kJ/m² |
| Izod Notched Impact Strength At 23 C | 75 J/m |
| Heat Deflection Temperature At 1 82 Mpa | 205°C |
| Melting Point | 224°C |
| Water Absorption After 24 H | 0.06% |
| Molding Shrinkage In Flow Direction | 0.3% |
| Molding Shrinkage In Cross Flow Direction | 0.6% |
| Volume Resistivity | 1×10^16 Ω·cm |
| Dielectric Strength | 20 kV/mm |
| Arc Resistance | 120 s |
| Flammability Rating | HB |
As an accredited Mitsubishi Chemical Novaduran™ PBT+GF40%-LW 5810G40 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaged in 25 kg moisture-resistant bags, Mitsubishi Chemical Novaduran™ PBT+GF40%-LW 5810G40 is palletized for safe transport and storage. |
| Container Loading (20′ FCL) | 20′ FCL loaded with Mitsubishi Chemical Novaduran™ PBT+GF40%-LW 5810G40, palletized 25 kg bags, securely braced for ocean transport. |
| Shipping | Mitsubishi Chemical Novaduran™ PBT+GF40%-LW 5810G40, non-hazardous glass-fiber-reinforced PBT pellets; not regulated for transport under DOT/IMDG/IATA. Ship in sealed moisture-barrier bags or boxes, protect from moisture, contamination, and direct sunlight; store at ambient temperature. |
| Storage | Store Mitsubishi Chemical Novaduran™ PBT+GF40%-LW 5810G40 in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, flames, and ignition sources. Maintain original sealed packaging on pallets to prevent moisture absorption, dust, and contamination. Avoid high humidity and prolonged elevated temperatures. Practice first-in/first-out stock rotation, inspect packaging regularly, and follow the SDS and local storage regulations. |
| Shelf Life | Typically 12 months when stored dry, cool, and in unopened original packaging per manufacturer guidance. |
Competitive Mitsubishi Chemical Novaduran™ PBT+GF40%-LW 5810G40 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Mitsubishi Chemical Novaduran™ PBT+GF40%-LW 5810G40 is a 40% glass-fiber-reinforced polybutylene terephthalate injection-moulding grade classified within the Novaduran family as a low-warpage material. The grade designation identifies the base polymer as PBT, the reinforcement as glass fibre at 40% by mass, and the low-warpage modification as a formulation and morphology-control strategy intended to reduce post-moulding out-of-plane distortion. The filled mass fraction can be verified by ash content according to ISO 3451-1. Published data for this specific configuration is limited outside manufacturer-controlled technical documentation, so all grade-specific values for density, melt volume-flow rate, tensile modulus, and shrinkage must be confirmed against the Mitsubishi Chemical lot release certificate for 5810G40.
Mechanical evaluation of moulded specimens from this material is normally performed using a suite of ISO-defined test methods. Tensile strength and elongation are measured under ISO 527-2 at 23°C. Flexural strength and flexural modulus are measured under ISO 178. Notched Charpy impact is reported according to ISO 179-1/1eA, and heat deflection temperature is reported under ISO 75-2 Method A at 1.8 MPa. Moulding shrinkage is tested on plaques using ISO 294-4. For electrical and electronic applications, comparative tracking index is tested under IEC 60112, and dielectric strength may be measured according to IEC 60243-1. The 40% glass loading places the compound in the high-stiffness segment of PBT materials, but the primary difference from standard PBT+GF40 grades is not total glass content; it is the reduction in differential shrinkage between flow and transverse directions.
At elevated temperature, 40% glass-filled PBT retains substantial stiffness because the reinforcement suppresses creep and dimensional relaxation, but the PBT matrix softens as temperature approaches the crystalline melting region near 225°C. Heat deflection temperature for 40% glass-filled PBT under ISO 75-2 Method A is commonly in the range 200°C to 215°C. Continuous service temperature must be lower due to thermal-oxidative ageing and creep. For load-bearing structural brackets used above 80°C, creep modulus under ISO 899-1 and fatigue data under ISO 13003 should be requested. These ranges are representative of 40% glass-filled PBT material families and do not replace grade-specific 5810G40 datasheet values.
In electrical and electronic applications, comparative tracking index for glass-filled PBT commonly falls between 400 V and 600 V under IEC 60112, though glass fibres can promote surface tracking relative to unfilled PBT. Dielectric strength under IEC 60243-1 is thickness-dependent and cannot be extrapolated across wall sections. Flammability classification under UL 94 is also thickness-dependent; many glass-filled PBT grades are tested at 0.75 mm and 1.5 mm. A V-0 classification must not be assumed for this grade unless the supplier has listed the exact colour and thickness range on the UL Yellow Card. The low-warpage additive system is not generally designed to improve electrical properties; those properties remain governed by matrix purity, glass content, and moisture condition.
Standard PBT+GF40 compounds frequently show pronounced orientation-induced shrinkage anisotropy because glass fibres align in the flow direction during injection moulding. Flow-direction shrinkage can be much lower than transverse-direction shrinkage, and the resulting internal stress appears as bow or twist in flat parts. Low-warpage grades such as 5810G40 are formulated to reduce that differential, not necessarily to lower absolute shrinkage uniformly. The mechanisms include control of glass-fibre length distribution, modification of the PBT crystallisation rate, and additive packages that moderate fibre orientation near the surface. The comparative matrix below summarises generally observed differences between low-warpage 40% glass-filled PBT grades and conventional 40% glass-filled PBT grades. It is not a substitute for the manufacturer’s datasheet.
| Property | Reference method | Standard PBT+GF40 | Low-Warpage PBT+GF40 5810G40 |
|---|---|---|---|
| Glass-fibre content | ISO 3451-1 | 40% by mass | 40% by mass |
| Moulding shrinkage, flow | ISO 294-4 | 0.3% to 0.6% typical | lower end of typical PBT+GF40 range; grade-specific data required |
| Moulding shrinkage, transverse | ISO 294-4 | 0.8% to 1.2% typical | reduced toward flow-direction value; grade-specific data required |
| Warpage tendency in flat plaques | internal tooling data | may exceed 1.0 mm out-of-plane on 60 mm × 60 mm × 2 mm plaques | lower than standard PBT+GF40; component-geometry dependent |
Users with held flatness tolerances below 0.1 mm must conduct tool-specific moulding trials because gate location, part thickness, and cooling-channel layout affect warpage more than the nominal material classification. A low-warpage grade does not correct a badly designed gate or an unbalanced cooling circuit; it reduces the material-side contribution to distortion.
Drying before injection moulding is required for 5810G40. Residual moisture above 0.02% by mass can hydrolyse the ester backbone at melt temperatures, reducing molecular weight and notched Charpy impact. Dehumidified-air drying at 120°C for 4 h to 6 h is a standard starting condition for material from sealed packaging. The dryer return-air dew point should remain below −30°C. When ambient relative humidity exceeds 60%, exposure of open material to shop air should be limited to 30 min unless a sealed hopper dryer is used. Regrind of sprues and short shots may be incorporated at no more than 15% by mass; the regrind must be free of oil, mould release, and mixed resin. Hot-air dryers are not preferred for this material because they may not achieve the low dew point required to reduce moisture below 0.02% under humid plant conditions. The stated conditions are conventional for hydrolysis-sensitive glass-filled PBT processing; no drying data specific to this grade is published outside the technical datasheet.
Typical nozzle melt temperatures for glass-filled PBT injection moulding lie between 250°C and 270°C. Barrel temperatures from feed to nozzle should follow a flat or slightly descending profile to avoid overheating the glass-filled melt; the rear zone is usually kept below 250°C to prevent bridging of the feedstock. Mould temperatures between 60°C and 100°C are used, with the higher end favouring crystallinity and lower post-moulding shrinkage but also increasing cycle time. For low-warpage behaviour, the mould temperature must be uniform within ±5°C across the cavity surface; a differential above this range can induce distortion even when nominal shrinkage values are low. General-purpose screws with L/D 20:1 to 25:1 and screw speeds of 50 rpm to 150 rpm are acceptable starting parameters. Back pressure is maintained between 2 bar and 5 bar to improve homogenisation without excessive fibre breakage. Injection speed is selected to prevent jetting and to keep shear rate at the gate below 50,000 s⁻¹; this limiting shear rate is a processing rule for glass-filled PBT and is not a grade-specific value for 5810G40. Residence time should not exceed 5 min at 270°C; otherwise thermal degradation can increase melt flow and reduce impact strength. During machine stoppages, the barrel should be purged with a commercial purging compound or a polyolefin to minimize residence time at temperature.
Tooling design for low-warpage PBT+GF40 components uses balanced multi-gating in flat parts instead of a single edge gate. A single edge gate creates highly directional glass-fibre orientation and a residual stress gradient through the thickness, producing out-of-plane bow even when the measured moulding shrinkage is within specification. Balanced multiple gates reduce the distance between injection points and lower orientation-induced distortion. Conformal cooling channels or high-turbulence cooling circuits with Reynolds numbers above 10,000 are preferred for complex geometries, because cavity temperature variation affects crystallisation rate and local shrinkage. In some tools, pre-distortion of the cavity is machined to compensate for the expected warp direction; this approach is used when flatness tolerances are tighter than 0.2% of the characteristic part length. Weld lines in glass-filled PBT can retain only 50% to 70% of the unnotched tensile strength of the bulk material; gate placement should therefore avoid positioning weld lines in load-bearing or sealing areas.
The 40% glass loading of 5810G40 increases tensile and flexural modulus compared with unfilled PBT and PBT+GF30. That stiffness is accompanied by reduced elongation at break and generally lower notched impact strength because the glass fibres reduce the energy absorbed by the PBT matrix. Compared with a standard PBT+GF40, the low-warpage version targets flatter parts after ejection and cooling; however, the same glass content means that the material is not a direct substitute for PBT+GF30 in snap-fit designs that require high ultimate elongation. For electronic connectors, relay bases, sensor housings, and power-tool housings, dimensional stability under ambient humidity is evaluated according to ISO 62 and moulding shrinkage according to ISO 294-4. In automotive underhood components, resistance to hydrocarbon fluids can be assessed using ISO 1817 or OEM-specific immersion protocols. PBT generally resists aliphatic hydrocarbons, automotive coolants, and many solvents, but esters, ketones, and strong alkaline solutions can attack the ester groups. Continuous contact with hot water above 80°C or alkaline media above pH 9 is not recommended because hydrolysis and surface degradation become significant.
The low-warpage modification for 5810G40 is not compatible with certain additives that accelerate PBT hydrolysis. Amine-based stabilizers or amine-functional flame retardants should be avoided unless verified through thermal ageing and melt-flow stability testing; these can cause premature chain scission and plate-out during moulding. Halogenated flame-retardant masterbatches may affect warpage and moulding shrinkage and must be evaluated for mould deposit formation. When colour masterbatches are added, the carrier resin and pigment crystallinity effects can shift shrinkage locally; a masterbatch content above 2% by mass requires a new shrinkage and warpage trial because pigments can nucleate PBT crystallisation. Published data for these specific interactions with 5810G40 is limited.
Processing 40% glass-filled PBT can increase screw and barrel wear compared with unfilled PBT. Bimetallic barrels and hardened screws are used on production machines with long campaigns. A general-purpose nitrided screw may show excessive wear after processing several hundred tonnes of glass-filled PBT; published data for this specific configuration is limited. For parts requiring adhesive bonding or painting, mould releases based on silicones or fatty acid esters can leave surfaces that interfere with adhesion. Surface activation by plasma or corona and adhesive selection should be tested using lap-shear methods such as ISO 4587 or DIN EN 1465. Silicone mould release is not recommended for parts that are subsequently coated.
Regulatory compliance for finished components is application-specific. Under REACH Article 33, communication duties for substances of very high concern above 0.1% by mass in the article must be confirmed through the supplier’s safety data sheet. For electrical and electronic equipment sold in the EU, the final component must satisfy the restrictions of Directive 2011/65/EU as amended by (EU) 2015/863. For food-contact applications, migration testing according to EU Regulation 10/2011 or FDA 21 CFR must be performed on the finished article; no food-contact approval should be inferred for this glass-filled grade. Recycling of process scrap is limited to 15% by mass of clean, moisture-controlled regrind and must be re-evaluated for impact and warpage performance.