Mitsubishi Chemical Novaduran Pbt Gf40 Gwit V0 5830gn6 40

Mitsubishi Chemical Novaduran™ PBT+GF40%-GWIT-V0 5830GN6-40

    • Product Name: Mitsubishi Chemical Novaduran™ PBT+GF40%-GWIT-V0 5830GN6-40
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 445167
    Product Mitsubishi Chemical Novaduran™ PBT+GF40%-GWIT-V0 5830GN6-40
    Polymer Base Polybutylene terephthalate (PBT)
    Reinforcement 40% glass fiber
    Flame Retardant Yes
    Ul94 Rating V-0
    Glow Wire Ignition Temperature Gwit 775 °C
    Density 1.65 g/cm³
    Molding Shrinkage 0.2-0.8 %
    Tensile Strength 125 MPa
    Tensile Modulus 13000 MPa
    Elongation At Break 2.0 %
    Flexural Modulus 12000 MPa
    Flexural Strength 190 MPa
    Charpy Notched Impact Strength 8 kJ/m²
    Hdt At 1 8 Mpa 205 °C
    Melting Point 225 °C
    Comparative Tracking Index Cti 600 V
    Volume Resistivity 1E15 Ω·cm
    Dielectric Strength 20 kV/mm

    As an accredited Mitsubishi Chemical Novaduran™ PBT+GF40%-GWIT-V0 5830GN6-40 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Mitsubishi Chemical Novaduran™ PBT+GF40%-GWIT-V0 5830GN6-40 is supplied in 25 kg sealed moisture-proof bags, palletized for shipment.
    Container Loading (20′ FCL) Mitsubishi Chemical Novaduran™ PBT+GF40%-GWIT-V0 5830GN6-40 loaded in a 20′ FCL container: palletized 25 kg bags, shrink-wrapped and secured for export.
    Shipping Mitsubishi Chemical Novaduran™ PBT+GF40%-GWIT-V0 5830GN6-40 ships as non-hazardous, flame-retardant, 40% glass-fiber-reinforced PBT pellets in sealed moisture-barrier bags or octabins on pallets. Transport and store dry at ambient temperature, away from direct sunlight, heat, moisture, and contamination; follow normal industrial hygiene practices.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and moisture. Keep original packaging sealed and palletized; protect from dust and physical damage. Avoid prolonged exposure to high humidity and UV. Use first-in, first-out stock rotation; dry material per supplier recommendations before processing if moisture pickup is suspected.
    Shelf Life Shelf life is typically 2 years in original sealed packaging, stored dry and cool, protected from moisture, heat, and direct sunlight.
    Free Quote

    Competitive Mitsubishi Chemical Novaduran™ PBT+GF40%-GWIT-V0 5830GN6-40 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    In injection moulding operations producing IEC 60695-2-13 compliant appliance enclosures, Mitsubishi Chemical Novaduran™ PBT+GF40%-GWIT-V0 5830GN6-40 is specified where a 40 wt% glass-fibre-reinforced polybutylene terephthalate must combine UL 94 V-0 classification with glow-wire ignition temperature performance. The compound is supplied as cylindrical pellets and processed as a polyester engineering thermoplastic. The designation 5830GN6-40 identifies the base resin, glass-fibre content and flame-retardant technology; the suffix GWIT-V0 positions the material for applications in which end-product glow-wire testing under IEC 60695-2-13 is the acceptance criterion, not only small-flame UL 94 vertical burning. Representative manufacturer-published property ranges are listed below; they are not specification limits. Lot-specific certificates of analysis can vary within the supplier’s release tolerance.

    PropertyTest methodRepresentative range
    DensityISO 11831.68–1.72 g/cm³
    Glass fibre contentISO 3451-140 wt% nominal
    Tensile strengthISO 527-2120–140 MPa
    Tensile elongation at breakISO 527-21.8–2.2 %
    Flexural modulusISO 17812 000–14 000 MPa
    Flexural strengthISO 178180–210 MPa
    Charpy notched impact strength, +23 °CISO 179-1/1eA8–10 kJ/m²
    Heat deflection temperature, 1.80 MPaISO 75-2/A200–210 °C
    Flammability classificationUL 94V-0 at 0.75 mm
    Glow-wire ignition temperatureIEC 60695-2-13775 °C at 1.5 mm
    Comparative tracking indexIEC 60112600 V
    Volume resistivityIEC 62631-3-11.0 × 1015 Ω·cm

    Why Does 5830GN6-40 Differ from Conventional PBT-GF40 Compounds?

    The distinguishing feature is the combination of 40% glass loading with a non-halogen flame-retardant system that maintains a UL 94 V-0 classification without reliance on brominated or chlorinated additives. In conventional PBT-GF40 grades, the glass fibre increases tensile strength and heat deflection, but the base polymer remains flammable and can produce flaming drips in vertical burn testing. In 5830GN6-40, the flame-retardant package modifies decomposition behaviour and reduces the probability of ignition under a hot wire. The grade is formulated to pass glow-wire ignition temperature testing at 775 °C at 1.5 mm, a value relevant to unattended appliance circuits. The trade-off is higher melt viscosity and a narrower processing window than non-FR PBT-GF40. The 40% glass content also produces anisotropic shrinkage; mould design must compensate for flow-direction and transverse shrinkage differences. Compared with 30% glass-filled V-0 PBT grades, 5830GN6-40 provides higher flexural modulus, lower thermal expansion and greater creep resistance under sustained load, but reduced notched impact and higher injection pressure requirements. The grade is therefore assigned to structurally stiff electrical and electronic parts rather than thin-wall snap-fit geometries.

    Controlling Hydrolytic Degradation and Glass-Fibre Attrition in the Melt

    Before melt processing, pellet moisture must be reduced below 0.02% to prevent hydrolytic chain scission. Desiccant drying at 120–130 °C for 4–6 h is typical; a dew point of −40 °C at the dryer outlet is required when ambient relative humidity exceeds 60%. If regrind is used above 20%, drying time is extended and the regrind fraction is blended with virgin pellets by gravimetric metering. Melt temperatures are maintained within 250–270 °C at the nozzle; barrel zone profiles of 240/250/260/260 °C are typical for a 20:1–24:1 L/D three-zone screw. Residence time at the upper melt-temperature limit should not exceed 8 minutes to limit polyester degradation and flame-retardant volatilisation. A compression ratio of 2.5:1–3.0:1 and a low-shear screw design preserve glass-fibre length; high-compression or high-shear screws can reduce fibre length and lower tensile strength. The melt is sensitive to shear heating in hot-runner systems; hot-runner manifolds must be externally heated and designed without dead spots, because stagnant melt can blacken and produce intermittent burning marks. Injection speed is set medium to high to fill quickly without jetting; cavity thickness below 1 mm commonly requires injection pressures above 100 MPa. Back pressure is kept at 0.3–0.7 MPa to avoid unnecessary glass-fibre breakage.

    In multi-cavity tools for this compound, gate dimensions are normally set to 50–75% of the nominal wall thickness, and gate land lengths are kept below 1.0 mm. Sprue and runner channels are tapered and highly polished; cold slug wells are used to prevent glass-rich solidified material from entering the cavity. Ejection systems must account for a flexural modulus near 13 000 MPa; ejector pin contact areas are enlarged to prevent surface stress whitening. Because mould shrinkage is anisotropic, with flow-direction values near 0.2–0.4% and transverse values near 0.6–0.9%, steel-safe shrinkage allowances are biased according to the dominant orientation pattern in the part. Venting depth of 0.015–0.030 mm is used along the parting line to prevent burn marks at flow-front convergence.

    When Glow-Wire Ignition Temperature Compliance Must Be Verified at Final Part Thickness

    End-product standards such as IEC 60335-1 require glow-wire testing on the final appliance enclosure or support part, not only on the raw material plaque. In such cases, 5830GN6-40 is selected because its published glow-wire ignition temperature at 1.5 mm is 775 °C under IEC 60695-2-13. This covers many household appliance applications in which unattended operation with currents above 0.2 A requires glow-wire testing at 750 °C or 850 °C depending on the product standard. The material’s UL 94 V-0 classification at 0.75 mm provides a baseline small-flame resistance, but glow-wire performance is the stricter criterion for components retaining live parts after thermal stress. Tests should be conducted at the minimum part wall thickness, at the most unfavourable location such as a boss, weld line or gate. Published data for this specific configuration is limited where part thickness falls below 1.0 mm or where moulded-in inserts act as heat sinks; end-product verification is mandatory. The flame-retardant system is formulated to reduce ignition probability under a hot wire and to minimise flaming drip, but any machining of the moulded part that removes the resin-rich surface can alter glow-wire results.

    Miniature circuit breaker housings and terminal blocks moulded in 5830GN6-40 are typically evaluated for dimensional stability after exposure to heat and humidity cycling. The glass-fibre network lowers linear thermal expansion and retains creep resistance under screw torque. The comparative tracking index of 600 V under IEC 60112 supports creepage distances in power distribution assemblies, but final certification remains subject to the clearance and creepage requirements of IEC 60947-1 for the specific overvoltage category. In multi-pole terminal blocks, the high mould shrinkage anisotropy of a 40% glass-filled PBT can cause pin-to-pin pitch error; cavity pressure monitoring and post-mould fixture cooling are used to hold critical dimensions. For parts with living hinges or high snap-in deflection, the grade is not recommended because the 40% glass content reduces elongation at break to approximately 2.0%.

    In electric vehicle power distribution units and photovoltaic inverter housings, the material is considered when a thermoplastic is required to support busbars and connector insulators. The compound’s volume resistivity in the dry as-moulded state is approximately 1.0 × 1015 Ω·cm; under humid conditions, PBT absorbs less moisture than polyamide, which supports better retention of surface resistivity. Moulded parts are nonetheless tested for dielectric strength and insulation resistance after conditioning at 85 °C/85% RH for 168 h. The material’s high crystallinity provides a heat deflection temperature near 205 °C at 1.80 MPa, but continuous-use temperature is lower than that of PPS or high-temperature polyamides. Where service temperatures exceed 140 °C for extended periods, 5830GN6-40 is outside its long-term thermal-oxidative stability boundary.

    Comparative Property Benchmarks Against Alternative FR Thermoplastics

    Against a non-FR PBT-GF40, 5830GN6-40 has a higher density, typically around 1.70 g/cm³ versus approximately 1.60–1.65 g/cm³ for non-FR PBT-GF40, and slightly lower tensile strength because flame-retardant additives dilute the glass-matrix interface. Against a PBT-GF30 V-0 compound, the 40% glass grade raises flexural modulus from roughly 9 000–10 000 MPa to roughly 12 000–14 000 MPa and reduces notched impact. Compared with a halogen-free PA66-GF30 FR, the PBT grade provides better dimensional stability in humid environments and lower moisture absorption, but lower notched impact and lower continuous-use temperature. Compared with PBT/PET blends, 5830GN6-40 retains faster crystallisation and can be moulded at lower mould temperatures, typically 60–100 °C, which reduces cooling time in thick sections. It is not a direct replacement for PPS or PPA in soldering-temperature applications; heat deflection temperature at 1.80 MPa near 205 °C does not imply resistance to reflow soldering above 260 °C.

    In photovoltaic inverter housings and power distribution modules, 5830GN6-40 is evaluated for busbar support insulators and connector housings. The material is processed on 100–350 t injection moulding machines with shot sizes kept below 70% of barrel capacity to limit residence time. Moulded parts are annealed at 120 °C for 2 h in some production lines to stabilise crystallinity and reduce post-mould dimensional drift. If the part is used in contact with alkaline cleaning agents, compatibility must be confirmed; hot alkaline solutions can accelerate polyester surface hydrolysis. For direct exposure to automotive underhood temperatures above 140 °C, published data for this specific configuration is limited; the grade is not substituted for PPS or PPA without long-term heat-aging validation.

    Top