| HS Code | 970351 |
| Density | 1.60 g/cm³ |
| Glass Fiber Content | 30% |
| Molding Shrinkage Flow | 0.2–0.4% |
| Molding Shrinkage Transverse | 0.6–0.8% |
| Tensile Strength | 120 MPa |
| Tensile Elongation At Break | 2.5% |
| Flexural Modulus | 8.5 GPa |
| Flexural Strength | 180 MPa |
| Charpy Notched Impact Strength 23c | 7 kJ/m² |
| Hdt 1 82mpa | 200 °C |
| Melting Temperature | 224 °C |
| Volume Resistivity | 1E16 Ω·cm |
| Dielectric Strength | 20 kV/mm |
| Comparative Tracking Index | 600 V |
| Ul94 Flammability | V-0 |
As an accredited Mitsubishi Chemical Novaduran™ PBT+GF30%-Track 5010GN6-30TS factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Mitsubishi Chemical Novaduran™ PBT+GF30%-Track 5010GN6-30TS is supplied in 25 kg moisture-resistant bags, 40 bags per pallet. |
| Container Loading (20′ FCL) | Container loading: 20′ FCL loaded with palletized bags of Mitsubishi Chemical Novaduran™ PBT+GF30%-Track 5010GN6-30TS, secured and moisture-protected for export. |
| Shipping | Mitsubishi Chemical Novaduran™ PBT+GF30%-Track 5010GN6-30TS is shipped as non-hazardous, moisture-sensitive thermoplastic pellets in sealed 25 kg bags, palletized and stretch-wrapped. Store dry at ambient temperature, away from heat, sunlight, and contamination. Use standard covered freight; avoid punctures or broken seals during handling. |
| Storage | Store in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed to prevent moisture pickup and contamination. Avoid contact with strong oxidizers. Prevent dust generation and accumulation, and use local exhaust ventilation where needed. Store separately from food and drink, and follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Typical shelf life is 12 months when stored in original unopened packaging, dry, cool, and away from direct sunlight. |
Competitive Mitsubishi Chemical Novaduran™ PBT+GF30%-Track 5010GN6-30TS prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Mitsubishi Chemical Novaduran™ PBT+GF30%-Track 5010GN6-30TS is an injection-molding-grade polybutylene terephthalate compound modified with 30% by weight short-glass-fiber reinforcement, a flame-retardant package, and a tracking-resistant additive system. The grade designation places the material within the high-CTI Novaduran flame-retardant portfolio; the “30” suffix identifies glass-fiber content, and “TS” identifies tracking-resistant stabilization. The product is supplied as pelletized feedstock sized for dehumidified hopper dryers and screw plasticating injection-molding machines. Electrical-insulation coordination is the primary design driver because the supplier lists a comparative tracking index of 600 V under IEC 60112, placing the material in material group I under IEC 60664-1. The polymer matrix is semi-crystalline PBT with a melting peak near 224 °C by ISO 11357-3 differential scanning calorimetry; the glass fibers are melt-incorporated during compounding, not dry-blended, and therefore the final part exhibits anisotropic shrinkage and weld-line strength dominated by fiber orientation. Regulatory compliance for RoHS 2011/65/EU and REACH 1907/2006 should be confirmed against the current producer declaration, because lot-specific additive systems may change.
General-purpose 30% glass-reinforced PBT without a tracking-resistant flame-retardant package often falls below 250 V CTI under IEC 60112, and many flame-retardant PBT-GF30 grades occupy material group II or IIIa. The 5010GN6-30TS formulation changes the surface failure mechanism under electrical stress; its 600 V CTI allows closer conductor spacing when the design is assessed under IEC 60664-1 pollution degree 2 conditions. Compared with standard PBT-GF30, this grade has higher melt density—typically 1.62–1.64 g/cm³ by ISO 1183—and lower tensile elongation, with a representative value of 2.0% by ISO 527-1/-2. The flame-retardant and tracking-resistant additives increase melt viscosity at low shear rates; pressure drop through hot-runner drops and thin-wall flow length are therefore inferior to non-flame-retardant PBT-GF30, and gate freeze occurs earlier for a given wall thickness. The glass-fiber reinforcement provides flexural modulus near 9.5 GPa by ISO 178, but notched impact and knit-line strength are lower than those of unfilled PBT. The material is not a direct substitute for non-FR PBT-GF30 in geometries with long, thin ribs below 0.8 mm unless injection-pressure limits and tool venting are rechecked by mold-filling simulation.
Residual moisture must be reduced below 0.020 wt% by Karl Fischer titration before melt processing. The recommended drying configuration is a closed-loop dehumidifying desiccant dryer with a dew point of −40 °C or lower and an air-flow rate of approximately 3.6 m³/h per kg/h throughput. A baseline schedule of 120 °C for 4–6 h is typical; hoppers should be sized so dried pellets are held at temperature for no longer than 8 h. At moisture levels near 0.030 wt%, hydrolysis during plastication releases gas and creates silver streaks, and tensile strength measured by ISO 527-1/-2 can drop measurably before visual defects appear. The melt/nozzle temperature is maintained at 250–270 °C, with rear-zone settings of 230–245 °C and front-zone settings of 255–265 °C. Mold temperature is controlled from 60 °C to 90 °C; temperatures below 40 °C reduce crystallinity and lower heat deflection behavior below the 205 °C at 1.80 MPa value obtained under ISO 75-1/-2. In hot-runner systems, manifold set-points above 280 °C or residence time beyond 10 min degrade the flame-retardant package and darken the melt. Production lines typically use valve-gate shutoff and longer screw-recovery delay rather than elevated barrel temperatures to manage stringing. Screw geometry is a medium-shear PBT or general-purpose screw with L/D 18:1 to 22:1 and compression ratio 2.2:1 to 2.8:1. Back pressure is limited to 0.3–0.7 MPa; higher settings produce frictional heating and fiber attrition. Regrind content is capped at 25 wt% for thin-wall electrical parts because repeated screw recovery shortens fibers and moves notched Charpy impact below the typical virgin range of 7–9 kJ/m² under ISO 179/1eA.
Representative dry-as-molded property values for 5010GN6-30TS are shown in the following table from publicly available supplier literature and standard test designations. Lot-specific certificates of analysis govern production acceptance, and the values should not be treated as design minima without component-level validation.
| Property | Test method | Representative value |
|---|---|---|
| Density | ISO 1183 | 1.63 g/cm³ |
| Tensile stress at break | ISO 527-1/-2 | 130 MPa |
| Tensile strain at break | ISO 527-1/-2 | 2.0% |
| Flexural stress at conventional deflection | ISO 178 | 200 MPa |
| Flexural modulus | ISO 178 | 9.5 GPa |
| Charpy notched impact strength, 23 °C | ISO 179/1eA | 8 kJ/m² |
| Heat deflection temperature, 1.80 MPa | ISO 75-1/-2 | 205 °C |
| Comparative tracking index | IEC 60112 | 600 V |
| Flame retardancy | UL 94 | V-0 at 0.75 mm |
| Volume resistivity | IEC 62631-3-1 | 1 × 1015 Ω·cm |
| Surface resistivity | IEC 62631-3-2 | 1 × 1014 Ω |
Continuous-use temperature is not defined by the heat deflection temperature. The UL Yellow Card for this grade assigns relative temperature index values based on long-term oven aging under UL 746B; designers should use the RTI mechanical or electrical value rather than the 205 °C HDT/A for continuous thermal load. The high CTI rating is not a guarantee against arc tracking in heavily contaminated systems; conductive dust and humidity reduce the effective tracking resistance of any polymer surface. In outdoor charging-inlet applications, sealing, conformal coating, or increased creepage may be required.
Hydrolytic stability is a service boundary, not a single-point property. In connectors exposed to condensation or salt mist, the glass-fiber–matrix interface is attacked before bulk PBT matrix degradation is visible. Components molded from this grade and exposed to 85 °C and 85% relative humidity under IEC 60068-2-78 can develop surface blisters and exposed fiber ends after several hundred hours when high molded-in stress and fiber-rich surfaces are present. Published long-term data for this specific high-CTI flame-retardant configuration under combined thermal cycling and salt-mist exposure are limited; end-product qualification should therefore include component-level IEC 60068-2-14 temperature cycling followed by dielectric withstand or partial-discharge measurement. Post-mold annealing at 120 °C for 2 h reduces residual stress but changes dimensions and may lower impact strength. Continuous contact with strong aqueous ammonia, aliphatic amines, or hot concentrated acids is outside the recommended operational envelope because PBT undergoes ester hydrolysis and chain scission; tensile strength can fall below design thresholds before gross cracking appears. For underhood connectors with glycol-contaminated humidity, a hydrolysis-stabilized PBT or PBT/PET copolymer may provide lower strength loss because of a more resistant ester-linkage environment near humid interfaces.
Insulation coordination under IEC 60664-1 uses CTI as the basis for solid-insulation material grouping. A 600 V CTI under IEC 60112 places 5010GN6-30TS in material group I, which permits reduced creepage distances relative to material group II or IIIa polymers at the same working voltage and pollution degree. This advantage drives the product into compact power-distribution parts: AC/DC charging connectors, inverter busbar supports, relay bases, terminal blocks, miniature circuit-breaker housings, and sensor enclosures. The 30% glass reinforcement contributes flexural modulus and creep resistance under clamp loads, but also introduces anisotropic shrinkage: flow-direction linear mold shrinkage is generally 0.2–0.5%, while transverse shrinkage is 0.8–1.2% when measured on plaques under ISO 294-4. Large flat components warp from differential fiber orientation and mold-temperature gradients; gate location and wall-thickness transitions should be evaluated with fiber-orientation-calibrated mold-filling simulation rather than isotropic shrinkage factors. Thin walls below 0.8 mm increase fiber orientation in the flow direction and raise pressure drop; injection-pressure requirements can exceed machine limits in multi-cavity tools. Mold venting must be sufficient at flow fronts to avoid diesel burns, particularly because flame-retardant decomposition gases evolve more readily than in non-FR PBT-GF30 at the upper end of the melt-temperature window.
On production-scale injection machines with clamping force from 80 t to 150 t, the most frequent deviations are silver streaking from incomplete drying, brown streaks from hot-runner dead spots, and short shots in ribs below 0.8 mm. Mold deposit formation from volatile flame-retardant decomposition products is observed at high barrel temperatures and long residence time; preventive purging with a compatible purging compound after every 8 h of continuous operation reduces accumulation. The glass fibers develop a shell-core orientation structure in thin walls; when two melt fronts meet, a knit line behaves as a notch-like weak plane. A knit-line tensile specimen with an opposing gate configuration under ISO 527-1/-2 may retain only 40–60% of the bulk tensile stress at break. Load-bearing bosses and snap-fit features should therefore be relocated away from knit lines or locally thickened. Cushion is maintained at 3–5 mm and decompression at 3–7 mm to prevent drool without drawing air into the melt. Lot-to-lot rheology is tracked by melt volume-flow rate under ISO 1133-1 on the certificate of analysis; processors use this value to adjust cushion and injection velocity before long production campaigns. The material is not intended for continuous immersion in hot water or for high-voltage components where partial-discharge inception voltage is the governing criterion; for those applications, unfilled high-CTI grades or other insulating polymers may be more suitable.