| HS Code | 175982 |
| Polymer Type | PBT |
| Glass Fiber Content | 30% |
| Hydrolysis Resistance | Hydrolytic stabilized |
| Low Warpage | Yes |
| Density | 1.53 g/cm³ |
| Tensile Strength | 140 MPa |
| Tensile Modulus | 9500 MPa |
| Elongation At Break | 2.5% |
| Flexural Modulus | 9000 MPa |
| Charpy Notched Impact Strength | 8 kJ/m² |
| Heat Deflection Temperature At 1 8 Mpa | 205 °C |
| Melting Point | 225 °C |
| Mold Shrinkage | 0.2-0.8% |
| Water Absorption | 0.1% |
| Flammability Ul94 | HB |
As an accredited Mitsubishi Chemical Novaduran™ PBT+GF30%-LW-Hydrolytic 5810G30X4 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Mitsubishi Chemical Novaduran™ PBT+GF30%-LW-Hydrolytic 5810G30X4: sealed 25 kg moisture-barrier bags, 40 bags (1,000 kg) per pallet. |
| Container Loading (20′ FCL) | 20′ FCL containing Mitsubishi Chemical Novaduran™ PBT+GF30%-LW-Hydrolytic 5810G30X4, packed in 25 kg bags on pallets, shrink-wrapped and secured for export. |
| Shipping | Mitsubishi Chemical Novaduran™ PBT+GF30%-LW-Hydrolytic 5810G30X4 is shipped as a non-hazardous solid in moisture-barrier bags, packed in cartons or on pallets. Transport and store cool, dry, ventilated, protected from humidity, heat, sunlight, and contamination; handle according to the SDS and local regulations. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep containers or bags tightly sealed to prevent moisture pickup and contamination. Avoid prolonged exposure to high humidity; use desiccant if recommended. Do not store near incompatible chemicals. Maintain good housekeeping to control dust, protect from physical damage, and follow the supplier’s SDS and local regulations. |
| Shelf Life | Shelf life is typically 24 months when stored in original unopened packaging, dry, cool, and protected from moisture and sunlight. |
Competitive Mitsubishi Chemical Novaduran™ PBT+GF30%-LW-Hydrolytic 5810G30X4 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Mitsubishi Chemical Novaduran™ PBT+GF30%-LW-Hydrolytic 5810G30X4 is a 30 wt% short-glass-fiber-reinforced polybutylene terephthalate injection-molding compound carrying a hydrolytic stabilization package and a low-warpage modification. The product designation identifies three simultaneous requirements: the stiffness and creep resistance of 30% glass reinforcement, reduced flow/cross-flow shrinkage differential for flat part geometry, and extended property retention after hot-moisture exposure. The grade is not moisture-tolerant; predrying to ≤0.02 wt% by ISO 15512:2019 method B is required before plastication. Typical melt processing uses barrel settings of 250–270°C and mold surface temperatures of 80–100°C. Outside this window, glass-reinforced PBT can exhibit surface delamination, jetting, non-uniform crystallization, or hydrolytic molecular weight loss in the barrel.
| Property | Test method | Expected range | Test condition / specimen |
|---|---|---|---|
| Glass fiber content | ISO 3451-1 method A | 30 ± 2 wt% | calcination at 600°C |
| Density | ISO 1183-1:2019 | 1.51–1.56 g/cm³ | method A, 23°C |
| Tensile strength at break | ISO 527-1/-2 | 120–140 MPa | 5 mm/min, type 1A |
| Tensile elongation at break | ISO 527-1/-2 | 2.0–4.0% | 5 mm/min, type 1A |
| Flexural modulus | ISO 178:2019 | 8,000–10,000 MPa | 2 mm/min, 80 × 10 × 4 mm specimen |
| Flexural strength | ISO 178:2019 | 180–220 MPa | 2 mm/min |
| Charpy notched impact | ISO 179-1/1eA | 6–10 kJ/m² | edgewise, 23°C |
| Heat deflection temperature | ISO 75-1/-2 | 195–210°C | 1.8 MPa, flatwise |
| Melt volume-flow rate | ISO 1133-1:2022 | 8–20 cm³/10 min | 250°C, 2.16 kg |
| Water absorption | ISO 62:2008 | 0.05–0.10 wt% | 23°C, 24 h |
| Molding shrinkage | ISO 294-4:2018 | flow 0.2–0.5%; cross-flow 0.6–1.0% | end-gated plaque |
These ranges are not grade-specific certificate values. They define the general class of PBT GF30 low-warpage hydrolysis-resistant compounds; the manufacturer’s lot certificate for 5810G30X4 must be consulted for actual tensile, flexural, and impact data. Datasheet comparisons are typically reported in the ISO 10350-1:2017 single-point format, with specimens prepared according to ISO 294-1 and conditioned to the specified moisture state. Fiber orientation, weld-line location, specimen thickness, and regrind content can shift the measured values more than the difference between adjacent commercial grades.
PBT is a semicrystalline polyester whose melting peak is near 223°C and whose glass transition is approximately 45–60°C. The ester linkage in the polymer backbone is susceptible to hydrolysis, and the carboxylic acid end-groups released by chain scission autocatalyze further degradation. A 30 wt% glass-fiber phase increases the number of interfacial pathways for moisture transport; hydrolytic stability must therefore be evaluated on the composite, not on the unfilled matrix. The standard acceleration test for underhood and electrical housings is exposure at 85°C/85%RH according to IEC 60068-2-78, with tensile property retention measured after 500 h and 1,000 h intervals using ISO 527-1/-2 type 1A specimens. The hydrolytic additive package retards molecular weight loss, but it does not reduce equilibrium water absorption to zero. Water absorption after 24 h immersion at 23°C per ISO 62:2008 remains in the 0.05–0.10 wt% range for the GF30 class.
Pre-drying of 5810G30X4 is mandatory. The target moisture content before melt processing is ≤0.02 wt%; verification by ISO 15512:2019 method B is preferred over loss-on-drying because the latter can overstate or understate volatiles when silane coupling agents are present in the glass sizing. A closed desiccant-bed dryer with outlet air dew point ≤ -40°C, inlet air temperature of 120–130°C, and airflow of at least 1.85 m³/h per kg/h throughput is typical. Drying time from cold pellets is 3–5 h; hopper residence beyond 8 h at temperature can cause oxidative yellowing and should be avoided. If a machine stop exceeds 30 min, the barrel should be purged with a PBT-compatible purge and the feed throat kept dry. Melt-state hydrolysis at barrel temperatures above 270°C proceeds rapidly when moisture is present; silver streaks, foaming, and loss of Charpy impact are the usual consequences.
Glass fiber orientation in a filling cavity is non-uniform: the frozen surface layer has high in-plane orientation, the core can become transverse depending on gate location, and weld lines act as local fiber-depleted or fiber-rich regions. Flow-direction mold shrinkage measured by ISO 294-4:2018 on end-gated plaques is generally 0.2–0.5%, while cross-flow shrinkage is 0.6–1.0%; the resulting differential is the main source of saddle warp in standard glass-reinforced PBT. The low-warpage modification in 5810G30X4 is intended to narrow this gap. Tooling compensation should not use uniform scaling; cavity dimensions should be corrected independently for flow and cross-flow directions. Gate placement should locate weld lines in low-stress, flat areas, and valve-gated hot runners should be evaluated because frozen cold-runner slugs increase pressure loss and can disrupt fiber orientation.
Weld lines in glass-reinforced PBT are fiber-depleted and generally exhibit lower tensile and impact strength than the bulk material. Charpy notched impact at a weld line can be 30–60% lower than the bulk value under ISO 179-1/1eA. When a low-warpage grade is used in flat connector bodies with multiple subgates, weld-line locations must be moved to non-stressed regions or the gate count reduced to increase the melt meeting angle. Mold-filling simulation with fiber orientation tensors is useful, but its accuracy depends on the interaction coefficient and wall-slip assumptions. Physical short-shots and cross-polarized microscopy on sectioned parts are therefore required for tool validation.
Rheological characterization at 250°C and shear rate 1000 s⁻¹ shows pronounced shear thinning for PBT GF30. Production-scale filling of thin ribs below 1.2 mm therefore benefits from high injection velocities in the 180–300 mm/s flow-front range and gate thickness of 50–80% of the nominal wall. On electric injection molding machines with 20–22:1 L/D screws and clamp force between 800 kN and 1,800 kN, the grade is suited for connectors, relay bases, sensor brackets, and housing covers. Large-area power-distribution covers may require 3,000–5,000 kN clamp force when projected area exceeds 300 cm² and injection pressure approaches 120 MPa. Hot-runner manifolds should be designed without dead spots; resin stagnation above 270°C for more than 10 min total melt residence can generate black specks, acetaldehyde odor, and reduced Charpy notched impact. Screw recovery speed should be limited to 50–100 rpm because aggressive fiber breakage in the compression zone lowers impact strength.
The principal differentiation is the simultaneous presence of three attributes. Unfilled PBT exhibits elongation at break above 10% and flexural modulus often below 2,600 MPa, but it lacks the stiffness and heat-distortion resistance needed for large thin-wall housings. Standard PBT GF30 increases flexural modulus to the 8,000–10,000 MPa range but retains strong flow/cross-flow shrinkage anisotropy and is not hydrolysis-stabilized. A hydrolysis-resistant PBT GF30 grade improves hot-moisture tensile retention but can still produce excessive warpage if the part is dimensionally flat. A low-warpage PBT GF30 grade without the hydrolytic package addresses warpage but may lose tensile and impact properties faster in coolant splash or 85°C/85%RH environments. The 5810G30X4 grade occupies the intersection of these three property sets; the trade-off typically appears as a slight reduction in Charpy notched impact compared with a standard GF30 grade because low-warpage additives can reduce plastic flow at the notch tip. Users should compare Charpy notched impact values from ISO 179-1/1eA rather than Izod values when selecting for impact-sensitive clips.
Compared with polyamide 66 GF30, this PBT grade absorbs less moisture under ISO 62:2008 and therefore exhibits lower hygroscopic dimensional change. However, PA66 GF30 generally offers higher long-term thermal resistance and often better toughness at low temperatures. Selection between PBT and PA66 should be made with ISO 1110 accelerated moisture conditioning for PA66 and ISO 62 for PBT. For high-temperature automotive environments above 140°C, PBT may soften or warp under load, and the actual thermal load must be evaluated before replacing a heat-resistant polyamide or polyphenylene sulfide.
Connector and power-distribution housings exposed to warm humidity, road salt splash, or glycol/water coolant are typical application zones when dimensional flatness and hydrolytic retention must be specified simultaneously. Qualification should include tensile tests after 500 h and 1,000 h at 85°C/85%RH per IEC 60068-2-78, Charpy impact on specimens cut from gate and end-of-fill regions, and warp measured with a coordinate measuring machine after 24 h post-mold conditioning at 23°C/50%RH. If the part is used near stressed snap-fits, creep-rupture testing under 80°C and dry/wet cycling is more relevant than short-term tensile. The material is not inherently flame-retardant; if UL 94 V-0, 5VA, or V-2 is required at a specific thickness, the UL Yellow Card and specific FR grade must be checked. Chemical compatibility with glycol/water coolant, road salt, and cleaning solvents should be tested at the actual concentration and temperature. PBT is generally resistant to aliphatic hydrocarbons, but hot concentrated alkalis and strong oxidizing acids cause surface attack and stress-cracking. RoHS Directive 2011/65/EU and REACH EC 1907/2006 apply to the finished article, and the final compliance position requires extraction testing on the molded component because color concentrates, regrind, mold release, and assembly adhesives can alter the chemical inventory. Published data for 5810G30X4 in this specific configuration is limited outside the manufacturer’s datasheet; the ranges above are not a substitute for lot-specific certification.