| HS Code | 514420 |
| Density | 1.53 g/cm³ |
| Glass Fiber Content | 30% |
| Tensile Strength | 120 MPa |
| Tensile Elongation At Break | 2.0% |
| Flexural Modulus | 8500 MPa |
| Flexural Strength | 180 MPa |
| Charpy Notched Impact Strength | 8 kJ/m² |
| Izod Notched Impact Strength | 70 J/m |
| Hdt At 1 82 Mpa | 200 °C |
| Melting Point | 224 °C |
| Water Absorption | 0.07% |
| Mold Shrinkage | 0.2–0.6% |
As an accredited Mitsubishi Chemical Novaduran™ PBT+GF30%-LW 5810G30 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Mitsubishi Chemical Novaduran™ PBT+GF30%-LW 5810G30 is supplied in 25 kg moisture-barrier bags, palletized for industrial handling and storage. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with palletized 25 kg bags of Mitsubishi Chemical Novaduran™ PBT+GF30%-LW 5810G30, shrink-wrapped and secured for ocean transport. |
| Shipping | Mitsubishi Chemical Novaduran™ PBT+GF30%-LW 5810G30 is shipped as non-hazardous, glass-fiber-reinforced PBT resin pellets. It is not regulated as dangerous goods. Use moisture-barrier bags or containers, keep dry, avoid direct sunlight and excessive heat, and follow the SDS and local transport regulations. |
| Storage | Store Mitsubishi Chemical Novaduran™ PBT+GF30%-LW 5810G30 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and oxidizing agents. Keep in original sealed packaging or tightly closed containers to prevent moisture pickup and contamination. Avoid dust generation and humid air. Use first-in, first-out rotation, and dry per processing guidelines before use. |
| Shelf Life | Shelf life is typically 24 months in original unopened packaging, stored dry, below 30°C, away from direct sunlight and moisture. |
Competitive Mitsubishi Chemical Novaduran™ PBT+GF30%-LW 5810G30 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Mitsubishi Chemical Novaduran™ PBT+GF30%-LW 5810G30 is an injection-molding-grade polybutylene terephthalate compound containing a nominal glass-fiber mass fraction of 30% and a low-warpage modification package. The grade is supplied in pellet form for use on reciprocating-screw injection-molding machines and, where thin-wall filling permits, high-speed electric molding machines. The product designation separates the base polymer, the 30% glass reinforcement, and the LW modifier system; 5810G30 is the specific low-warpage grade within the Novaduran PBT family.
Representative physical data determined under ISO 1183-1 place density in the range of 1.52 g/cm³ to 1.54 g/cm³. Tensile properties are evaluated on multipurpose test specimens under ISO 527-1/-2 at 23 °C; tensile strength typically lies between 115 MPa and 130 MPa, and tensile elongation at break is generally 2.0% to 3.0%. Flexural modulus under ISO 178 is reported from 8.0 GPa to 9.5 GPa. Notched Charpy impact energy under ISO 179-1/1eA at 23 °C is normally 6 kJ/m² to 9 kJ/m². Heat deflection temperature under ISO 75-1/-2 at 1.80 MPa is typically 195 °C to 205 °C. Melt volume-flow rate under ISO 1133-1 at 250 °C with 10 kg load is generally 12 cm³/10 min to 25 cm³/10 min, though glass-fiber attrition during machine plasticating can shift the measured value. Because single-point values vary with lot and test laboratory, production-lot certificates of analysis should be consulted for specification compliance.
Standard 30% glass-reinforced PBT compounds often show a pronounced difference between flow-direction and transverse-direction mold shrinkage. On ISO 294-4 plaques, standard GF30 PBT frequently shows flow shrinkage of 0.3% to 0.6% and transverse shrinkage of 0.7% to 1.2%. The 5810G30 low-warpage formulation narrows this differential to approximately 0.2% to 0.4% in the flow direction and 0.5% to 0.7% in the transverse direction. The reduction is achieved by filler and matrix modification rather than by lowering glass content; the nominal glass fraction remains 30%. This behavior is relevant in rectangular connectors, coil-form flanges, and power-module housings where post-ejection distortion is governed by the difference in principal shrinkage strains across the part.
| Property | Test standard | Unit | 5810G30 LW typical range | Standard GF30 PBT typical range |
|---|---|---|---|---|
| Density | ISO 1183-1 | g/cm³ | 1.52–1.54 | 1.52–1.55 |
| Tensile strength at 23 °C | ISO 527-1/-2 | MPa | 115–130 | 125–140 |
| Flexural modulus | ISO 178 | MPa | 8000–9500 | 8500–10000 |
| Notched Charpy impact at 23 °C | ISO 179-1/1eA | kJ/m² | 6–9 | 7–10 |
| Heat deflection temperature at 1.80 MPa | ISO 75-1/-2 | °C | 195–205 | 195–210 |
| Mold shrinkage, flow | ISO 294-4 | % | 0.2–0.4 | 0.3–0.6 |
| Mold shrinkage, transverse | ISO 294-4 | % | 0.5–0.7 | 0.7–1.2 |
Compared with unfilled PBT, the 5810G30 grade has lower isotropic shrinkage and higher stiffness, but lower elongation. Unfilled PBT mold shrinkage is typically 1.5% to 2.5%, with tensile modulus below 3 GPa; the glass-reinforced low-warpage compound therefore permits closer tolerances under DIN ISO 2768-1 or equivalent part-drawing specifications. Compared with impact-modified GF30 PBT, the LW grade may show lower notched impact, especially at −40 °C. Snap-fit designs must be recalculated using datasheet flexural modulus and strain at break, because direct substitution from a standard GF30 PBT grade without re-evaluation can produce weld-line or root-radius failures. Weld-line strength should be measured directly by tensile testing under ISO 527-1/-2 on specimens with a central weld line, since glass orientation at the meeting line controls the result. For applications requiring UL 94 V-0, a flame-retardant variant must be specified separately; the non-flame-retardant 5810G30 is generally UL 94 HB at the manufacturer’s listed thickness.
Before melt processing, desiccant-bed drying is required. Hot-air circulation alone is insufficient. Residual moisture must be reduced below 0.020% before plastication. Dryer settings of 120 °C for 4 h to 6 h are typical; when ambient relative humidity exceeds 60%, drying time should be extended to 6 h or more. The dryer dew point should be −40 °C or lower. Moisture content can be verified by ISO 15512 or an equivalent Karl Fischer method. Wet pellets entering the melt stream undergo hydrolytic degradation, reducing molecular weight, melt viscosity, and molded-part toughness. The same hydrolysis boundary restricts continuous service in hot water above approximately 80 °C; long-term exposure to hot aqueous media should be validated on molded parts, not inferred from dry as-molded properties.
Barrel temperature settings on a typical three-zone machine are 240 °C to 250 °C in the rear zone, 250 °C to 260 °C in the center zone, and 260 °C to 270 °C in the front zone, with the nozzle at 250 °C to 260 °C. Melt temperature measured by an inserted pyrometer should remain in the 250 °C to 270 °C range. Residence time at melt temperature should not exceed 8 min; above 280 °C or after 15 min stagnation, accelerated degradation may produce gas, discoloration, and loss of mechanical properties. Screw recovery should use back pressure of 0.5 MPa to 2.0 MPa and screw speed of 50 min⁻¹ to 150 min⁻¹. Excessive back pressure above 2.0 MPa increases glass-fiber attrition and can lower tensile strength. The screw should have an L/D ratio of 20:1 to 24:1, and the non-return valve should be a free-flow type suitable for glass-reinforced compounds. Shot size should use 40% to 70% of barrel capacity to avoid excessive residence time. Hot-runner systems should avoid dead spots and should use internally heated manifolds; valve gates are preferred where gate freeze must be controlled.
Mold wall temperature is the dominant process variable controlling crystallinity and post-molding dimensional movement. At mold temperatures below 60 °C, the surface layer freezes before complete crystallization, leaving a higher amorphous fraction. When the part later sees service temperatures from 80 °C to 120 °C, secondary crystallization can produce additional local contraction. The recommended mold temperature for 5810G30 is 80 °C to 120 °C, with 90 °C to 100 °C typical for close-tolerance parts. A heated mold also lowers the in-plane shrinkage differential and improves flatness. Packing pressure should be held until gate freeze; typical packing levels are 40 MPa to 80 MPa, with hold time determined by gate geometry and wall thickness. If hold time is shorter than gate-seal time, sink marks and voiding occur. Post-mold fixturing can constrain warpage during cooling, but it cannot correct a large internal stress gradient. If a part is subsequently annealed at 150 °C to 160 °C, additional dimensional change may occur; annealing studies should use the final part geometry and not a generic test plaque.
In automotive electrical distribution systems, the 5810G30 grade is used for connector housings, relay bases, sensor bodies, and power-module frames where terminal alignment and pin retention are affected by warpage. The low-warpage filler system reduces cavity-to-cavity positional error in multi-cavity connectors. Validation for such applications commonly includes USCAR-2 for electrical connector performance, IEC 60664-1 for insulation coordination, and IEC 60112 for comparative tracking index. The comparative tracking index of GF30 PBT formulations is often measured between 200 V and 275 V, but the specific value for the production lot must be confirmed from the compounder’s certificate. Thermal endurance data are generated under ISO 60216 or UL 746B relative thermal index protocols; GF30 PBT grades are generally assigned RTI values near 140 °C electrical and 130 °C mechanical, though the exact rating depends on grade and specimen thickness. Under-hood continuous use at 130 °C to 150 °C is common for this class, with short-term excursions to 180 °C. In reflow-soldered modules, the 1.80 MPa heat deflection temperature near 200 °C and the PBT melting point near 225 °C define the thermal ceiling.
In motor commutators, bobbins, relay bases, and circuit-breaker housings, dimensional flatness and thermal creep are central acceptance criteria. Volume resistivity is measured under IEC 62631-3-1, with typical values for glass-reinforced PBT from 1 × 10¹⁵ Ω·m to 1 × 10¹⁶ Ω·m. Surface resistivity is measured under IEC 62631-3-2. Dielectric strength under IEC 60243-1 is typically 18 kV/mm to 24 kV/mm at 3 mm thickness, although thickness and electrode geometry alter the result. In high-voltage designs above 600 V, creepage distances must be calculated under IEC 60664-1; the presence of glass fibers can initiate surface tracking, so the insulation system must be validated on the final molded part rather than on pellet tests alone. Published data for this specific configuration in high-voltage assemblies is limited; component-level dielectric testing is therefore required. The material is not intended for direct food-contact applications, and UL 94 V-0 classifications require a flame-retardant Novaduran variant rather than the unreinforced or standard HB grade.