Mitsubishi Chemical Novaduran Pbt Gf30 Hb 5010g30

Mitsubishi Chemical Novaduran™ PBT+GF30%-HB 5010G30

    • Product Name: Mitsubishi Chemical Novaduran™ PBT+GF30%-HB 5010G30
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 925886
    Manufacturer Mitsubishi Chemical
    Product Name Novaduran™ PBT+GF30%-HB 5010G30
    Polymer Type Polybutylene terephthalate (PBT)
    Reinforcement Glass fiber
    Glass Fiber Content 30%
    Flame Rating UL 94 HB
    Density 1.53 g/cm³
    Tensile Strength 135 MPa
    Flexural Modulus 8500 MPa
    Elongation At Break 2.5%
    Notched Charpy Impact Strength 8 kJ/m²
    Heat Deflection Temperature At 1 82 Mpa 205 °C
    Melting Point 224 °C
    Water Absorption 0.08%
    Molding Shrinkage 0.3–0.8%
    Processing Method Injection molding

    As an accredited Mitsubishi Chemical Novaduran™ PBT+GF30%-HB 5010G30 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg moisture-proof paper bags, palletized, containing Mitsubishi Chemical Novaduran™ PBT+GF30%-HB 5010G30 resin pellets.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Mitsubishi Chemical Novaduran™ PBT+GF30%-HB 5010G30 loaded in 25 kg bags, palletized and secured for export shipment.
    Shipping Mitsubishi Chemical Novaduran™ PBT+GF30%-HB 5010G30 is supplied as glass-fiber-reinforced PBT pellets. It is generally not classified as dangerous goods for transport (ADR/IMDG/IATA) and ships in moisture-barrier bags or octabins on pallets. Keep dry, avoid heat and direct sunlight; follow the SDS and local regulations.
    Storage Store Mitsubishi Chemical Novaduran™ PBT+GF30%-HB 5010G30 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and moisture. Keep material in original, tightly sealed packaging on pallets; avoid opening until use. Protect from humidity, dust, and contamination, do not stack excessively, and follow first-in, first-out stock rotation. Dry as required before processing.
    Shelf Life Shelf life is typically 24 months from manufacture when stored dry, cool, and protected from moisture in unopened original packaging.
    Free Quote

    Competitive Mitsubishi Chemical Novaduran™ PBT+GF30%-HB 5010G30 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The Mitsubishi Chemical Novaduran™ PBT+GF30%-HB 5010G30 is a 30% glass-fiber-reinforced polybutylene terephthalate injection-molding compound. The matrix is a semi-crystalline aromatic polyester with rapid crystallization kinetics; the short-glass reinforcement is melt-compounded to raise rigidity, heat deflection, and molded-part dimensional stability. The “HB” suffix identifies a horizontal-burn classification under UL 94, not a vertical V-0 self-extinguishing rating. Representative density is 1.53 g/cm³ under ISO 1183-1; tensile strength at break is typically 130–140 MPa under ISO 527-2; flexural modulus is near 9.0 GPa under ISO 178; notched Charpy impact at 23°C is near 8 kJ/m² under ISO 179-1/1eA; heat deflection temperature under 1.8 MPa is near 205°C under ISO 75-2/A. The PBT melting point is near 225°C, and melt volume-flow rate at 250°C and 2.16 kg is typically 15–25 cm³/10 min under ISO 1133-1. These values are single-point resin measurements and do not replace part-specific validation for warpage, weld-line strength, or long-term creep.

    Representative physical and mechanical values for Novaduran™ PBT+GF30%-HB 5010G30
    PropertyValueTest method
    Density1.53 g/cm³ISO 1183-1
    Tensile strength at break130–140 MPaISO 527-2
    Tensile modulus9.5–10.5 GPaISO 527-2
    Flexural modulus8.5–9.5 GPaISO 178
    Charpy notched impact, 23°C7.5–9.0 kJ/m²ISO 179-1/1eA
    Heat deflection temperature, 1.8 MPa200–210°CISO 75-2/A
    Mold shrinkage, parallel to flow0.3–0.9%ISO 294-4

    Incoming resin should be checked for glass content by ashing at 600°C for 2 h under ISO 3451-1; batch-to-batch filler variation of ±2 wt% is possible and influences mold shrinkage and flow-front behavior. Water absorption after immersion at 23°C for 24 h is generally below 0.08% under ISO 62, which is lower than a polyamide 66 GF30 comparator. The unfilled PBT phase has a glass transition temperature near 50–60°C; above this range modulus is fiber-dominated, while below this range the polymer matrix controls impact and surface strain.

    Why Does Moisture and Residence Time Control Melt-Quality Reliability?

    Processing on a production injection molding line requires drying to residual moisture below 0.02 wt%. Desiccant drying at 120°C for 4–6 h is the standard condition for fresh material; vacuum drying at 100–110°C for 4–8 h is acceptable when dryer capacity is limited. Silo conveyors operating above 60% relative humidity must use dry process air with a pressure dew point at or below -40°C because GF30 PBT reabsorbs surface moisture rapidly. At 23°C and 50% RH, dried PBT can regain approximately 0.01 wt% moisture within 30 min if exposed to plant air; closed hopper dryers are therefore required for continuous runs. In plant trials on a 20:1 L/D hardened reciprocating screw, loss of dry-air blanketing produced shot-mass variation of 3–5% over 45 min and splay localized at the fiber-rich flow front. The hydrolysis mechanism involves ester cleavage in the polymer backbone; moisture acts as a chain scission catalyst under melt conditions. A moisture content of 0.05 wt% can reduce melt viscosity by roughly one-third over a typical residence-time distribution.

    Barrel zone temperatures are typically set from 240°C at the feed section to 260°C at the nozzle; melt temperature measured at the cushion should remain between 250°C and 270°C. Residence time above 5 min at 270°C accelerates hydrolysis and thermal yellowing; the material should not be held in a hot barrel during tool changes or line shutdowns. Mold temperature is generally set to 80–100°C for structural parts and 60–80°C for thin-wall short-cycle parts; mold temperatures below 60°C reduce crystallinity and lower the effective HDT of the part. Injection pressure typically lies between 60 MPa and 120 MPa, with hold pressure 40–70 MPa applied for 2–4 s/mm wall thickness. Screw and barrel wear must be monitored because glass fiber abrasion removes metal from unprotected feedscrews; hardfaced screw flight lands and hardened barrel liners are required for sustained production, particularly when the screw L/D exceeds 22.

    Melt viscosity at 250°C and 1000 s⁻¹ is commonly between 150 Pa·s and 250 Pa·s for GF30 PBT; the glass fiber raises shear thinning and reduces flow length. Gate diameter for GF30 PBT should be 0.8–1.5 mm for thin-wall parts; edge gates below 0.8 mm may freeze prematurely and cause hesitation marks. Runner systems should use a shot volume between 30% and 70% of barrel capacity, with cushion maintained at 3–6 mm to control melt plastication consistency. On a multi-cavity tool, cavity-to-cavity mold temperature variation above ±5°C increases part-mass variation and differential shrinkage; conformal cooling or heated mold inserts are required for high-tolerance structural components.

    When 5010G30 Replaces Unfilled PBT, GF15, or GF45

    In direct substitution of unfilled Novaduran PBT, the 30% glass reinforcement reduces linear mold shrinkage from approximately 1.7–2.0% to 0.3–0.9% parallel to flow under ISO 294-4. Transverse shrinkage can be 0.5–0.7% higher than flow-direction shrinkage; this anisotropy is the primary source of out-of-plane warp in flat or partly ribbed parts. Existing tools designed for unfilled PBT must be re-evaluated for gate size because the higher melt viscosity of GF30 reduces flow length. In comparison with GF15, 5010G30 raises flexural modulus and heat deflection but lowers spiral-flow length and increases screw/barrel wear. In comparison with GF45, the 30% loading preserves lower melt viscosity and less tool abrasion while sacrificing flexural modulus and HDT. If a structural bracket currently uses a GF45 compound, replacement with 5010G30 requires a rigidity and creep check under ISO 899-2; published data for long-term creep of this exact configuration is limited, so component validation is required.

    Compared with a polyamide 66 GF30 product, 5010G30 exhibits lower moisture uptake and therefore more stable electrical properties under humid conditions, but lower notched Charpy impact and lower continuous-use heat resistance above 150°C. The product is not an exact drop-in for unfilled PBT or PC/PBT blends because the fiber network alters weld-line strength, surface appearance, and gate-freeze behaviour. Weld-line tensile retention of GF30 PBT is commonly 40–60% of the main-path tensile value; the ratio depends on meld angle, venting, and fiber orientation. Weld-line positions should be identified by short-shot study on the target reciprocating screw with L/D 18–22 and non-return valve rather than assumed from unfilled resin data.

    Fiber orientation is controlled by melt velocity, cavity thickness, and fill time. Fast injection velocity aligns glass fibers in the skin, increasing flow-direction tensile modulus while reducing strength at weld lines. Fiber breakage during melt recirculation reduces fiber length and tensile modulus; regrind levels above 20% can increase impact variability and should be validated for each part geometry. Regrind must be dried and free of fines because glass fines can segregate in drying hoppers and alter bulk density. The material should not be regrind-blended with flame-retarded PBT batches unless compatibility of the flame-retardant package is confirmed; some acidic or brominated FR systems accelerate polyester hydrolysis during reprocessing.

    Because the grade carries an HB designation under UL 94, it is suitable only for final assemblies whose standards permit horizontal-burn classification at the relevant wall thickness. Applications requiring vertical V-0 or V-2 under IEC 60695-11-10 or glow-wire ignition resistance under IEC 60695-2-11 should use a flame-retarded Novaduran grade instead. The HB rating is thickness-dependent; color concentrates, regrind content, and gate design can shift flammability performance, so candidate-part flame tests are required after tooling changes. For electrical connector frames, relay bases, and sensor carriers, dimensional stability is often assessed by molded-part gaging after thermal cycling; evaluation should include tensile creep under ISO 899-2 because glass-fiber PBT can show stress-dependent creep above 80°C. The compound is not formulated for food-contact use; any FDA 21 CFR status must be established at the final article level because fiber surface-sizing agents and processing aids are present.

    Chemical resistance is controlled by the polyester backbone. Strong acids, high-pH cleaners, and hot water above 85°C hydrolyze the ester linkages; in continuous exposure to hot coolant or alkaline wash baths, tensile strength can degrade by more than 30% after 1,000 h. Published data for this specific configuration under every exposure condition is limited, so component validation under ISO 175 should be completed for underhood or industrial fluid contact. For dry-air structural applications below 140°C, the compound can be used in high-stiffness brackets, fan impellers, pump housings, connector frames, and relay bases where UL 94 HB is acceptable and where the fiber-induced anisotropy is controlled by gate placement and cooling design.

    Top