Mitsubishi Chemical Novaduran Pbt Gf30 Fr V0 5010gn1 30

Mitsubishi Chemical Novaduran™ PBT+GF30%-FR-V0 5010GN1-30

    • Product Name: Mitsubishi Chemical Novaduran™ PBT+GF30%-FR-V0 5010GN1-30
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 252656
    Polymer Type Polybutylene terephthalate (PBT)
    Glass Fiber Content 30%
    Flame Retardancy Yes
    Ul94 Rating V-0
    Density 1.65 g/cm³
    Tensile Strength 135 MPa
    Tensile Modulus 10000 MPa
    Elongation At Break 2.5%
    Flexural Modulus 9000 MPa
    Flexural Strength 200 MPa
    Charpy Notched Impact Strength 9 kJ/m²
    Hdt At 1 82 Mpa 205 °C
    Melting Temperature 225 °C
    Molding Shrinkage 0.3-0.7%
    Water Absorption 0.08%
    Volume Resistivity 1E16 Ω·cm
    Dielectric Strength 20 kV/mm

    As an accredited Mitsubishi Chemical Novaduran™ PBT+GF30%-FR-V0 5010GN1-30 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaging: 25 kg moisture-barrier bags, 40 bags per pallet, labeled Mitsubishi Chemical Novaduran™ PBT+GF30%-FR-V0 5010GN1-30 for safe storage and transport.
    Container Loading (20′ FCL) 20′ FCL container loaded with Mitsubishi Chemical Novaduran™ PBT+GF30%-FR-V0 5010GN1-30 in 25 kg bags, palletized and secured.
    Shipping Mitsubishi Chemical Novaduran™ PBT+GF30%-FR-V0 5010GN1-30 is shipped as non-hazardous thermoplastic pellets in sealed moisture-barrier bags or octabins, palletized. Protect from moisture, heat, and direct sunlight. Store dry and ventilated; observe normal industrial hygiene. Handle carefully to avoid packaging damage. No special dangerous-goods transport classification applies.
    Storage Store in a cool, dry, well-ventilated area, away from direct sunlight, heat, moisture, and ignition sources. Keep in original, sealed packaging and prevent contact with incompatible substances. Avoid dust generation and static buildup. Do not store outdoors or near oxidizing materials. Maintain inventory rotation and follow the manufacturer’s safety data sheet and local regulations for safe storage and handling.
    Shelf Life Typically 12 months from manufacture when stored dry, sealed, and protected from moisture, heat, and direct sunlight.
    Free Quote

    Competitive Mitsubishi Chemical Novaduran™ PBT+GF30%-FR-V0 5010GN1-30 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The Mitsubishi Chemical Novaduran™ PBT+GF30%-FR-V0 5010GN1-30 grade is a polybutylene terephthalate compound incorporating a nominal 30% by mass glass-fibre reinforcement and a flame-retardant package that achieves UL 94 V-0 classification at a nominal 0.75 mm test plaque thickness. The material is designated under ISO 11469 as PBT-GF30 FR and is intended for injection-moulded electrical and electronic components requiring elevated flexural modulus and defined flammability performance. Measured density in accordance with ISO 1183-1 typically falls within 1.60–1.68 g/cm³, depending on pigment and flame-retardant lot variation. After plastication, the glass-fibre length distribution is bimodal with a mean fibre length commonly between 200 µm and 400 µm in moulded parts, contributing to the orientation-dependent mechanical response described below. Melt volume-flow rate determined by ISO 1133-1 is generally in the 10–25 cm³/10 min range at 250 °C/2.16 kg for this class of 30% glass-filled flame-retardant PBT. Published data for the specific 5010GN1-30 configuration should be confirmed against the current Mitsubishi Chemical technical datasheet; the ranges quoted herein represent the product class and are not a substitute for lot-specific certificate-of-analysis values. The compound is supplied as cylindrical pellets with a nominal bulk density of 700–850 kg/m³, which affects silo inventory calculation and hopper level detection.

    Why Is Drying Control the First Processing Gate for 5010GN1-30?

    Hydrolysis of the PBT ester linkage is the dominant melt-degradation mechanism for this grade, particularly in high-humidity production aisles. Bulk or hopper drying at 120 °C for 4–6 hours using a desiccant dryer with a dew point of -30 °C or lower is required to reduce residual moisture below 0.02% by mass. At moisture levels above 0.05%, melt viscosity drops measurably, and the flame-retardant package can undergo hydrolytic attack, producing surface splay and reduced UL 94 V-0 reproducibility. On production-scale equipment, a single 200 kg drying hopper operated with intermittent withdrawal can develop moisture stratification; the lower cone region should be sampled after 2 hours of residence and verified by Karl Fischer titration or a calibrated moisture analyser before start-up. In plants where ambient relative humidity exceeds 60%, pre-drying of unopened sacks and use of closed conveying lines from dryer to feed throat are recommended. These controls are not optional when regrind is introduced, because regrind from rejected mouldings typically absorbs moisture faster than virgin pellets due to increased surface area and residual heat history. Batch-to-batch variance in moisture uptake is observable on open mezzanine storage mezzanines where sacks remain unsealed; a shift of only 0.01–0.02% moisture has been associated with gate-area delamination in hot-runner tools.

    When Melt Temperature Exceeds 270°C in Hot-Runner Moulds

    In hot-runner tools with multiple drops and internally heated manifolds, the melt must be maintained between 245 °C and 265 °C; excursions above 270 °C for more than 5 minutes are associated with accelerated degradation of the flame-retardant system and amber discoloration at gate vestiges. The compound is processed on reciprocating-screw injection-moulding machines with an L/D ratio of 20:1 to 24:1 and a screw compression ratio of 2.0:1 to 3.0:1. Backpressure should be held between 0.3 MPa and 0.7 MPa to avoid fibre over-grinding, while injection speed is typically set at 80–120 mm/s for wall sections of 1.5–3.0 mm. Mould temperature control at 80–100 °C is required to obtain the intended crystallinity and low post-mould shrinkage; lower mould temperatures reduce cycle time but increase amorphous skin thickness and long-term dimension drift. Clamp force requirement is derived from cavity pressure; for a 80 MPa cavity-pressure assumption and a projected part area of 100 cm², 800 kN clamp force is needed, excluding runner projection. Accumulator-equipped moulding machines are preferred for thin-wall parts because the material exhibits a steep viscosity-shear-rate relationship; a fill time exceeding 0.8 s for a 1.0 mm nominal wall in a multi-cavity connector tool can create short-shot boundaries and weld-line weakness. Use of hot-runner valve-gate sequencing changes shear heating locally by 5–15 °C, and thermocouple placement at the gate tip is required to prevent local residence zones from exceeding the 270 °C ceiling.

    Mechanical evaluation of 5010GN1-30 according to ISO 527-2 yields tensile stress at break commonly in the range 110–140 MPa and tensile modulus of 9,000–11,000 MPa when tested parallel to mould flow. Flexural strength determined by ISO 178 is generally between 180 MPa and 220 MPa, with flexural modulus of 8,000–10,000 MPa. Notched Charpy impact per ISO 179-1/1eA is typically 6–10 kJ/m² at 23 °C, falling to 4–7 kJ/m² at -30 °C; this low-temperature reduction is characteristic of glass-filled PBT and must be considered for outdoor charging infrastructure in cold climates. Heat deflection temperature under 1.8 MPa load measured by ISO 75-2 method A is generally in the 200–220 °C range, while the continuous service temperature in air without mechanical load should not exceed 130–140 °C for intermittent operation. The coefficient of linear thermal expansion parallel to flow is approximately 25–35 µm/(m·K) between -30 °C and 100 °C, whereas transverse values can be 70–90 µm/(m·K). These anisotropic thermal-expansion values drive warpage in planar parts and must be paired with mouldflow simulation using orientation tensors rather than isotropic assumptions. Creep behaviour under sustained load in electrical-connector contact retention features is dependent on crystallinity; parts moulded at 80–100 °C tool temperature show lower creep than parts moulded at 60 °C because of higher crystalline fraction and reduced amorphous phase mobility.

    Flammability, Comparative Tracking Indices, and Ignition Resistance Metrics

    The flame-retardant designation V-0 is evaluated in accordance with IEC 60695-11-10, with total afterflame time for a set of five specimens typically below 50 s and no specimen exceeding 10 s after second flame application. The vertical burning test uses 125 mm × 13 mm specimens conditioned at 23 °C/50% RH for 48 hours before testing. Glow-wire ignition temperature under IEC 60695-2-13 is typically 775 °C or higher; glow-wire flammability index under IEC 60695-2-12 is typically 960 °C for a 1.0 mm plaque, but exact values require lot-specific certification. Comparative tracking index measured by IEC 60112 is generally between 250 V and 350 V, placing the grade in the PLC 1 to PLC 2 range under UL 746A. This CTI window is an important differentiator for high-voltage creepage design: connectors specified under IEC 60664-1 may require larger creepage distances if CTI falls below 400 V. The glass-fibre reinforcement reduces resistance to surface tracking relative to unfilled flame-retardant PBT, so leakage-current-sensitive designs should not assume the unfilled-grade CTI. Flammability performance must be re-confirmed after colouring; pigment loading above 0.5% can alter UL 94 V-0 behaviour through changes in dripping and char formation.

    Compared with an unfilled flame-retardant PBT compound, 5010GN1-30 provides higher flexural modulus and improved dimensional stability under clamp load, but it sacrifices elongation at break and introduces fibre-orientation-dependent mechanical properties. Against a standard non-flame-retardant 30% glass-filled PBT, the V-0 package in 5010GN1-30 typically reduces tensile strength by 5–15% and lowers notched Charpy impact by 10–25% depending on the specific flame-retardant chemistry. The trade-off is most visible at weld lines, where strength retention in a V-0 glass-filled PBT can be 40–55% of the base resin, compared with 55–70% for a non-FR GF30 PBT. The table below summarises indicative property-class comparisons using standardised test methods.

    Property and method 5010GN1-30 FR V-0 GF30 Unfilled FR V-0 PBT Non-FR GF30 PBT Halogenated GF30 FR V-0
    Density, ISO 1183-1 1.60–1.68 g/cm³ 1.40–1.50 g/cm³ 1.50–1.60 g/cm³ 1.60–1.70 g/cm³
    Tensile stress at break, ISO 527-2 110–140 MPa 50–70 MPa 120–150 MPa 100–130 MPa
    Flexural modulus, ISO 178 8,000–10,000 MPa 2,400–2,800 MPa 9,000–11,000 MPa 8,000–9,500 MPa
    Notched Charpy, ISO 179-1/1eA 6–10 kJ/m² 3–5 kJ/m² 9–12 kJ/m² 6–9 kJ/m²
    HDT-A, ISO 75-2 200–220 °C 60–80 °C 205–225 °C 195–215 °C
    CTI, IEC 60112 250–350 V 250–400 V 400–600 V 250–350 V
    UL 94, IEC 60695-11-10 V-0 at 0.75 mm V-0 at 0.75 mm HB V-0 at 0.75 mm

    Assessing Shrinkage Anisotropy and Warpage in Thin-Wall Connectors

    Mould shrinkage parallel to fibre orientation is typically 0.2–0.4%, while transverse shrinkage ranges from 0.8–1.2%. This disparity, measured on flat plaques moulded at 80–100 °C tool temperature, is the primary cause of post-mould warpage in rectangular connector housings with wall sections below 1.2 mm. Multiple end-gated geometries create knit lines where glass fibres align perpendicular to flow, reducing local tensile strength to 55–70 MPa; placement of the gate at the longest flow path and use of sequential valve-gate control can reduce warp-by-edge lift claims on production assembly lines. Tool designers should specify mould-temperature uniformity of ±5 °C across the cavity surface, because uneven crystallisation in PBT produces differential shrinkage that cannot be corrected by packing pressure alone. Packing pressure of 60–80 MPa with a holding time of 0.2–0.5 s/mm nominal wall is commonly used, followed by a screw speed of 60–100 rpm during recovery to minimise fibre-length attrition. These parameters are starting points; validation via short-shot studies and pressure-transducer curves is required because local hot-runner balance shifts as the flame-retardant additive package degrades over extended residence.

    Application records for this grade centre on electrical connectors, relay sockets, circuit-breaker housings, motor end caps, capacitor enclosures, and charging-interface components where UL 94 V-0 at relatively thin walls is a purchase specification. In EV charging inlet bodies, the material supports IEC 62196 dimensional interfaces, but the design must account for reduced CTI and the need for creepage distances defined by IEC 60664-1 pollution degree 3. For components exposed to mineral oil or grease-laden air, the PBT matrix has good resistance to aliphatic hydrocarbons at ambient temperature, but prolonged contact with hot water above 60 °C degrades the ester linkage; steam sterilisation is not recommended. The flame-retardant package is generally incompatible with amine-based lubricants and strong alkaline mould-release agents, which can migrate to the surface and reduce UL 94 V-0 reproducibility. Hot-runner purging compounds containing fluoropolymer processing aids should be tested for compatibility before use, because certain fluorinated additives alter surface energy and can promote gate deposit formation on long production runs. Published data for the specific interaction of 5010GN1-30 with all possible additive combinations is limited; when a new masterbatch or regrind stream is introduced, a lot-specific flammability and tensile test per ISO 527-2 and IEC 60695-11-10 is advised.

    Top