| HS Code | 614189 |
| Material Type | Polybutylene terephthalate (PBT) |
| Filler Reinforcement | 15% glass fiber |
| Density | 1.42 g/cm³ |
| Tensile Strength | 90 MPa |
| Tensile Elongation At Break | 3.0% |
| Flexural Modulus | 5500 MPa |
| Charpy Notched Impact Strength | 5 kJ/m² |
| Heat Deflection Temperature At 1 82 Mpa | 195 °C |
| Melting Point | 225 °C |
| Water Absorption 24 H | 0.05% |
| Volume Resistivity | 1E15 Ω·cm |
| Dielectric Strength | 20 kV/mm |
| Comparative Tracking Index Cti | 600 V |
| Flammability Rating | UL94 V-0 |
| Molding Shrinkage Flow | 0.4% |
| Processing Melt Temperature | 250-270 °C |
As an accredited Mitsubishi Chemical Novaduran™ PBT+GF15%-Track 5010GN6-15TS factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Mitsubishi Chemical Novaduran™ PBT+GF15%-Track 5010GN6-15TS is supplied in 25 kg moisture-barrier bags, palletized for secure handling. |
| Container Loading (20′ FCL) | Novaduran PBT+GF15% loaded in 20′ FCL: palletized 25 kg bags, dry container, secured, approx. 17–18 MT net per container. |
| Shipping | Shipping description: Mitsubishi Chemical Novaduran™ PBT+GF15%-Track 5010GN6-15TS is a non-hazardous thermoplastic polyester compound, not regulated as dangerous goods for transport. Ship in sealed moisture-barrier bags or 25 kg sacks, palletized. Keep dry, avoid direct sunlight, and store at ambient temperature; observe standard industrial handling. |
| Storage | Store Mitsubishi Chemical Novaduran™ PBT+GF15%-Track 5010GN6-15TS in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and moisture. Keep in original sealed packaging on pallets, protected from dust, dirt, and contamination. Avoid prolonged high humidity and temperature extremes that may affect processing. Store at moderate ambient temperature. Do not stack excessively. Follow first-in, first-out inventory and supplier SDS recommendations. |
| Shelf Life | Shelf life is typically 2 years (24 months) when stored cool, dry, and in unopened original packaging. |
Competitive Mitsubishi Chemical Novaduran™ PBT+GF15%-Track 5010GN6-15TS prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Mitsubishi Chemical Novaduran™ PBT+GF15%-Track 5010GN6-15TS is designated in supplier documentation as a polybutylene terephthalate injection-molding grade with a nominal 15% glass-fiber mass fraction and a flame-retardant package. Under ISO 1043-1, the base material is commonly classed as PBT-GF15; the full commercial code 5010GN6-15TS carries grade-specific suffix information for lot traceability and product differentiation. The compound is supplied as cylindrical pellets in moisture-barrier packaging and is intended for electrical connectors, automotive sensor housings, relay bases, switch components, and appliance harness parts where stiffness, dimensional stability, and flammability performance are specified. Published data for this exact suffix is limited in some public distributor databases; processing boundaries below are therefore drawn from the broader Novaduran™ PBT-GF15 flame-retardant product class and should be verified against the manufacturer’s lot-specific datasheet and certificate of analysis.
The 15% glass-fiber mass fraction places the compound in a semi-structural range between unfilled PBT and 30% glass-fiber PBT. Glass filaments shorten during compounding and molding to a typical number-average fiber length of 200–400 µm, but the fiber network raises tensile strength into the 90–110 MPa band when tested to ISO 527-1/-2. Flexural modulus measured to ISO 178 generally lies between 4000 MPa and 5500 MPa, roughly double the stiffness of unfilled PBT. Charpy notched impact strength measured to ISO 179-1/1eA is expected in the 4–6 kJ/m² range, similar to unfilled PBT; the glass reinforcement increases modulus but does not automatically improve notched impact toughness. Tensile elongation at break falls to 2.5–4.0%, limiting local yielding around mounting bosses. Mold shrinkage measured by ISO 294-4 is reduced to 0.4–0.7% parallel-to-flow, while cross-flow values commonly reach 0.8–1.2%, creating planar anisotropy that must be controlled through gate placement. Heat deflection temperature under 1.80 MPa load measured to ISO 75-1/-2 method A rises to approximately 195–205°C for dry-as-molded specimens. These values are representative industrial data bands for flame-retardant PBT-GF15 grades and are not lot-acceptance criteria.
In injection molding, the recommended barrel-temperature profile for 5010GN6-15TS spans 240–260°C from feed throat to metering zone, with a nozzle set point of 250–260°C and a mold surface temperature of 70–90°C. Mold temperatures below 60°C suppress skin-layer crystallinity, which can increase sink marks and accelerate post-mold dimensional drift. A general-purpose three-zone screw with a compression ratio of 2.2:1–2.5:1 and an L/D of 18:1–22:1 is adequate; high-shear barrier screws are not required and may fracture glass fibers. Back pressure is maintained at 2–5 MPa to limit fiber-length loss. Holding pressure from 60–100 MPa is applied through gate-seal, particularly in bosses and ribs with wall thickness above 2 mm. On machines with clamp force below 500 kN, flow paths longer than 120 mm with a 1.0 mm gate have shown gas splay and gate blush; tooling corrections such as a 1.5–2.0 mm gate diameter or a fan gate are preferred over raising melt temperature above 270°C. Melt residence time at 260°C or higher should remain under 5 min because polybutylene terephthalate undergoes hydrolytic chain scission and generates oligomeric deposits. Shot volume should be 40–70% of barrel capacity to limit hot residence time.
Polybutylene terephthalate undergoes hydrolytic chain scission at processing temperature when moisture content exceeds approximately 0.02%. Glass fiber does not absorb water significantly, so the uptake rate is governed by the PBT matrix and pellet surface area. Material stored in open containers at relative humidity above 60% can approach the critical moisture level after 4–6 h, but the adsorbed layer on cold pellet surfaces often produces gas splay before bulk moisture is measurable. Pre-drying in a desiccant-bed dryer with a supply-air dew point of -40°C or lower, an air temperature of 120°C, and a residence time of 4–6 h is required for virgin material. Hopper drying for less than 3 h is insufficient for pellet core equilibration; residual moisture should be measured by Karl Fischer titration to ISO 15512 rather than by a simple loss-on-drying balance. A known production-scale failure mode is hopper short-circuiting, in which wet pellets slide down the cone wall and enter the feed throat while dry pellets remain in the center. The return-air dew point should therefore be monitored, and hopper fill level should not fall below 50% during automatic operation.
On a co-rotating twin-screw compounding line, glass fiber is introduced after the PBT melt seal through a side-stuffer positioned at approximately 40% of total barrel length. This placement preserves fiber length and avoids excessive screw wear before the polymer is molten. A machine with L/D 40:1, screw diameter 40–75 mm, and screw speed 300–450 rpm typically operates in a specific energy input window of 0.25–0.35 kWh/kg for this product class. Energy input above that boundary reduces fiber length and lowers notched impact performance; energy input below the lower boundary leaves incompletely wetted fiber bundles that appear as dull streaks or raised roughness on molded surfaces. The flame-retardant package can restrict stabilizer selection: amine-based antioxidant systems should not be substituted without supplier approval because basic nitrogen species may interact with halogenated or antimony-based flame retardants and shift UL94 classification during long melt residence. Vacuum venting should be set at -80 kPa gauge pressure or lower to remove volatile by-products from the melt before pelletizing.
Flame-retardant PBT grades generate volatile by-products during molding, especially when melt temperature or screw speed is elevated. In high-speed injection of thin-wall connectors with fill times below 0.5 s, the advancing flow front compresses air and volatiles; without adequate venting, trapped gas creates surface splay that cannot be polished out. Vent depths of 0.02–0.03 mm are typical for PBT-GF15, and vents should be placed at end-of-fill regions and around blind pockets. Full-perimeter venting is preferred over interlocks for multi-cavity tools because gas evacuation must occur before the flow front reaches the vent land. Mold deposit from flame-retardant decomposition appears as a brown-white film on the cavity surface and increases cleaning frequency; reducing melt temperature from 260°C to 250°C and shortening melt residence time are more effective than increasing mold release use. Tool steel should be high-chromium or hard-plated in areas where the deposit forms most heavily, and cleaning agents must not leave alkaline residues that catalyze PBT hydrolysis on the cavity surface.
Warpage in 15% glass-fiber PBT often reflects fiber-orientation gradients created during mold filling. If a flash-molded connector body grows by more than 0.1 mm along its longitudinal axis after 48 h at 23°C and 50% relative humidity, the primary suspects are low mold surface temperature, insufficient holding time, or gate geometry that produces jetting. The corrective procedure is to raise mold temperature to 80–90°C, set a holding-pressure profile indexed to part thickness, and reposition the gate so that a continuous flow front fills the cavity without free-jet turbulence. A holding time of 0.5 s per mm wall thickness is a practical lower boundary for parts with flatness requirements. Post-mold shrinkage measurements should be made according to ISO 294-4 after 24 h and 48 h; values recorded 1 h after demolding understate final movement. In production trials, flash-molded parts measured only at the press often pass initial gauging but fail later in assembly due to slow crystallization and relaxation of frozen-in fiber orientation.
The semi-structural position of the 15% glass-fiber grade becomes visible in comparison to unfilled PBT and a 30% glass-fiber PBT. The data below are representative industrial ranges for injection-molding grades; the test methods identify the standard used to generate each band.
| Property | Test method | Unfilled PBT | PBT-GF15 FR | PBT-GF30 |
|---|---|---|---|---|
| Density | ISO 1183-1 | 1.30–1.32 g/cm³ | 1.42–1.50 g/cm³ | 1.50–1.58 g/cm³ |
| Tensile strength | ISO 527-1/-2 | 50–60 MPa | 90–110 MPa | 125–140 MPa |
| Tensile elongation at break | ISO 527-1/-2 | 20–30% | 2.5–4.0% | 1.5–2.5% |
| Flexural modulus | ISO 178 | 2200–2600 MPa | 4000–5500 MPa | 7500–8500 MPa |
| Charpy notched impact | ISO 179-1/1eA | 3–5 kJ/m² | 4–6 kJ/m² | 5–7 kJ/m² |
| HDT/A 1.80 MPa | ISO 75-1/-2 | 55–65°C | 195–205°C | 200–210°C |
| Melt volume-flow rate | ISO 1133-1 | 20–30 cm³/10 min | 10–20 cm³/10 min | 5–12 cm³/10 min |
| UL94 classification | IEC 60695-11-10 | HB | V-0 at 0.75–1.5 mm | V-0 at 0.75–1.5 mm |
The first 15% of glass fiber produces a larger relative gain in tensile strength and flexural modulus than the additional shift from 15% to 30%. At the same time, the 15% grade retains lower melt viscosity and less cross-flow shrinkage anisotropy than PBT-GF30, which is an advantage in thin-wall relay bases and multi-cavity connectors. Selection of 5010GN6-15TS over a 30% glass-fiber grade should therefore be made when dimensional control and filling pressure are limiting constraints, not when absolute stiffness is the primary requirement.
Regulatory documentation for 5010GN6-15TS should be requested from the supplier, but the relevant framework for electrical and appliance applications includes REACH Regulation (EC) No 1907/2006, RoHS Directive 2011/65/EU with delegated amendments, and IEC 60695-11-10 for flammability classification. When claiming a UL94 V-0 listing, batch traceability documents should identify the flame-retardant package and the minimum tested wall thickness, typically 0.75 mm to 1.5 mm. For connectors subjected to high-voltage tracking, comparative tracking index should be measured according to IEC 60112; the suffix “Track” in the commercial name may suggest a grade intended for tracking-sensitive environments, but the actual CTI value and test conditions must be taken from the supplier datasheet rather than inferred from nomenclature.
Connectors molded from 5010GN6-15TS are used where unfilled PBT cannot provide sufficient flatness or where a 30% glass-fiber grade would create excessive warpage and flow resistance. Reduced shrinkage along the flow axis allows tighter pin spacing, but gate location must still account for glass-fiber orientation because connector bodies are often gated at one end, creating longitudinal orientation and anisotropic thermal expansion. For relay housings, stiffness at the mounting feet is critical; the flexural modulus band of 4000–5500 MPa is sufficient to prevent cracking around snap-fit features when nominal wall thickness is maintained above 1.5 mm. In appliance power-entry modules, the compound’s UL94 V-0 rating at the tested wall thickness is used to support IEC 60335-1 end-product requirements. Weld-line strength remains a limiting factor: when multiple gates fill around large core pins, the weld line may retain only 50–70% of base tensile strength. For components with mechanically loaded weld lines, a gating study with short-shot analysis and tensile testing of weld-line plaques to ISO 527-1/-2 is recommended before tool approval.
Operational boundaries for this compound include a maximum recommended melt temperature of 270°C and a maximum hot residence time of 5 min. Regrind from sprues and runners may be added at 20% or less, provided the regrind has been dried and has not experienced multiple heat histories; each additional heat history reduces molecular weight and can lower impact strength. Contact with strong alkaline chemicals and hot water at 80°C or above should be assessed independently because PBT hydrolyzes in high-moisture, high-temperature environments even in the solid state. Incompatible additives include amine-based blowing agents, some polyester color concentrates with basic carriers, and unapproved lubricants that can plate out on the mold and interfere with ultrasonic welding. Published data for this specific configuration is limited for long-term hot-oil exposure and continuous outdoor UV aging; applications requiring those exposures should be qualified with the supplier using long-term heat-ageing and weathering programs such as ISO 4892-2.