| HS Code | 447352 |
| Manufacturer | Mitsubishi Chemical Corporation |
| Product Family | Novaduran |
| Grade | SEF-515T |
| Base Polymer | Polybutylene terephthalate (PBT) |
| Glass Fiber Content | 15% |
| Flame Retardant System | Non-halogen, tracking-resistant |
| Density | approx. 1.45 g/cm³ |
| Tensile Strength | approx. 100 MPa |
| Elongation At Break | approx. 2-3% |
| Flexural Modulus | approx. 5,500 MPa |
| Notched Charpy Impact Strength | approx. 5-7 kJ/m² |
| Heat Deflection Temperature At 1 82 Mpa | approx. 195-205 °C |
| Melting Temperature | approx. 225 °C |
| Water Absorption | approx. 0.05-0.1% |
| Mold Shrinkage | approx. 0.3-0.6% |
| Flammability Rating | UL94 V-0 (typical) |
| Comparative Tracking Index Cti | >=600 V (typical) |
| Volume Resistivity | >=1E16 Ω·cm |
| Dielectric Strength | approx. 20 kV/mm |
As an accredited Mitsubishi Chemical Novaduran™ PBT+GF15%-NF-Track SEF-515T factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaged in 25 kg moisture-resistant bags, palletized with 40 bags per pallet (1,000 kg net) for industrial storage and transport. |
| Container Loading (20′ FCL) | Container loading for 20′ FCL shipment of Mitsubishi Chemical Novaduran™ PBT+GF15%-NF-Track SEF-515T, securely packed and stowed for ocean transport. |
| Shipping | Mitsubishi Chemical Novaduran™ PBT+GF15%-NF-Track SEF-515T is supplied as moisture-sensitive thermoplastic pellets in sealed bags or boxes. Ship in dry, clean containers at ambient temperature, protected from sunlight and moisture. Typically not classified as dangerous goods; follow the SDS and local regulations. |
| Storage | Store Mitsubishi Chemical Novaduran™ PBT+GF15%-NF-Track SEF-515T in a cool, dry, well-ventilated area away from direct sunlight, heat, and moisture. Keep original packaging tightly sealed to prevent contamination and humidity pickup; use first-in, first-out rotation. Avoid strong oxidizers and incompatible chemicals, and follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Typically 12 months from manufacture when stored dry, cool, and in original sealed packaging, protected from sunlight and moisture. |
Competitive Mitsubishi Chemical Novaduran™ PBT+GF15%-NF-Track SEF-515T prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Mitsubishi Chemical Novaduran™ PBT+GF15%-NF-Track SEF-515T is a glass-fiber-reinforced polybutylene terephthalate injection-molding compound with a nominal glass-fiber content of 15% by mass. The designation places it between unfilled PBT and higher-glass Novaduran grades, and the suffix SEF-515T identifies the specific melt and additive package within the Mitsubishi Chemical portfolio. The material is supplied in pellet form for injection molding of dimensionally stable components where a non-flame-retardant polyester with moderate reinforcement is acceptable. Because publicly available datasheets for this specific suffix are limited, values cited below are given as typical published ranges for PBT+15% glass-fiber compounds or as standard test conditions; the manufacturer’s current technical datasheet and lot-specific certificate of analysis remain the controlling documents for tooling release.
Drying is non-negotiable. PBT undergoes hydrolytic chain scission at melt temperature if residual moisture exceeds approximately 0.02%. A desiccant dryer with supply-air dew point no higher than -40 °C should be operated at 110 °C to 120 °C for 4 to 6 hours. Storage in humid air above 60% relative humidity for more than 24 hours requires extending drying to 8 hours at 120 °C. Dried pellets should be conveyed in closed lines and consumed within 2 hours of drying; in humid conditions, open-hopper residence can reintroduce surface moisture within 30 minutes.
Melt temperature at the nozzle is normally kept between 250 °C and 270 °C. Above 280 °C, thermal degradation accelerates and produces volatile decomposition products, discoloration, and loss of tensile strength. A typical barrel profile uses rear-zone 240 °C, center-zone 250 °C, and front-zone 260 °C, but direct melt-temperature measurement should govern. Total barrel residence time should not exceed 8 minutes; for stops longer than 15 minutes, barrel temperatures should be reduced to 180 °C or the unit purged.
Moisture-related splay at the gate appears as a fan-shaped silver streak. It is corrected by reducing ambient exposure of dried pellets and checking the desiccant bed dew point, not by raising mold temperature. If splay persists after drying, purge with fiber-free PBT and inspect for dead spots in the feed throat or hot-runner manifold.
For continuous injection cycles on machines of 80 to 120 t clamp force producing multi-cavity electronic housings, shot-to-shot stability requires a melt cushion of 3 to 6 mm. Screw recovery is typically set between 1.5 and 3.0 times the cooling time. Back pressure is maintained at 0.3 to 0.7 MPa to limit fiber breakage while ensuring color and glass dispersion. Injection velocities of 100 to 250 mm/s are common for wall thicknesses from 1.5 to 3.0 mm. Holding pressure is usually 50% to 70% of peak injection pressure; gate freeze time for a 2 mm wall at 80 °C mold temperature can range from 3 to 6 seconds.
Regrind use should be limited to 20% by mass in virgin material unless downstream impact tests demonstrate acceptable retention. Regrind containing fines smaller than 0.5 mm increases fiber-length distribution variability and can reduce notched Izod impact by 15% to 25%. Sieving or dust removal is recommended for high-volume production.
The PBT matrix melting peak is approximately 223 °C according to differential scanning calorimetry performed under ISO 11357. The glass transition is near 45 °C to 55 °C. Heat deflection temperature at 1.8 MPa, tested to ISO 75-1/-2, shifts from roughly 60 °C–70 °C for unfilled PBT to 190 °C–205 °C for a 15% glass-fiber compound. This allows short-term dimensional stability in wave-soldering or paint-bake operations, provided the part is supported and not under continuous load.
Weld-line strength is governed by fiber orientation at the flow front. Fibers align parallel to the weld plane and may reduce local tensile strength by 30% to 50% compared with the bulk. Gate placement that moves the weld line into low-stress regions is preferred over increasing fiber content, and sequential valve gating or overflow wells can be used when weld lines occur near mounting bosses or snap hooks.
Published property ranges for PBT with 15% glass fiber position it between unfilled PBT and 30% glass-fiber compounds. The following summary is not a certified SEF-515T lot property table but represents typical values from public polymer databases and supplier literature.
| Property | Test method | PBT unfilled | PBT+GF15 typical | PBT+GF30 typical |
|---|---|---|---|---|
| Density | ISO 1183 | 1.31 g/cm3 | 1.42 g/cm3 | 1.53 g/cm3 |
| Tensile strength | ISO 527-1/-2 | 55 MPa | 95–110 MPa | 125–140 MPa |
| Flexural modulus | ISO 178 | 2.5 GPa | 5.0–6.0 GPa | 8.5–9.5 GPa |
| HDT at 1.8 MPa | ISO 75-1/-2 | 60–70 °C | 190–205 °C | 200–215 °C |
| Mold shrinkage flow direction | ISO 294-4 | 1.5%–2.0% | 0.4%–0.8% | 0.2%–0.6% |
| Notched Izod impact | ISO 180 | 4 kJ/m2 | 6–8 kJ/m2 | 8–10 kJ/m2 |
Where North American specifications are used, tensile properties may be reported according to ASTM D638-14, and heat deflection temperature according to ASTM D648-16; values are not directly interchangeable with ISO determinations. Shrinkage anisotropy is more important than total shrinkage in tool design. Unfilled PBT exhibits comparatively isotropic but high shrinkage; 30% glass-fiber compounds exhibit lower average shrinkage but greater flow-direction to cross-flow difference. A 15% glass loading reduces warpage in flat lids and connector bodies while providing enough stiffness for snap-fit retention. In multi-cavity tools, cavity-to-cavity mass variance above 0.5% signals runner imbalance or gate-freeze differential, and should be corrected through runner profiling rather than by increasing barrel temperature.
Replacement of unfilled PBT with SEF-515T is driven by creep resistance and stiffness. Flexural modulus rises from approximately 2.5 GPa to 5.0–6.0 GPa, enabling wall-thickness reduction in housings while maintaining deflection limits. Snap-fit retention under repeated insertion is improved if the snap beam is oriented perpendicular to flow-induced fiber orientation; if the beam lies parallel to fiber orientation, surface strain can cause microcracking earlier than expected.
Compared with 30% glass-fiber PBT, SEF-515T has lower melt viscosity and reduced abrasive wear. Screw and barrel wear in production runs above 100,000 cycles is reduced because the lower filler volume fraction reduces glass contact with metal surfaces; wear-resistant screw flights and nitrided barrels remain standard specification. The trade-off is reduced modulus and higher shrinkage. If a tool designed for GF30 is processed with SEF-515T without adjusted packing, flow-direction dimensions may exceed tolerance by 0.2% to 0.5%; increased hold pressure and longer gate seal can reduce but not fully eliminate this difference.
In humid environments, PBT+GF15 provides greater dimensional consistency than glass-reinforced polyamide 66. Water absorption after 24 h immersion at 23 °C is generally near 0.2% for PBT according to ISO 62, whereas PA66 can absorb several times that amount at saturation. This property makes the material suitable for tightly toleranced connectors and sensor housings exposed to brief condensation, but not for continuous hot-water service above 60 °C, where the PBT ester linkage undergoes progressive hydrolysis.
Tool feed systems for SEF-515T should use round or trapezoidal cold runners and gate diameters not less than 0.8 to 1.0 mm for parts with wall thickness below 2 mm. Gate diameters that are too small produce high shear, fiber breakage, and surface roughening near the gate. Hot-runner drops should be individually controlled and maintained below 260 °C; residence time in the manifold should not exceed 5 minutes to avoid discoloration and loss of mechanical properties.
Holding pressure and gate freeze determine sink and shrinkage. For a 2 mm wall, a gate freeze time of 3 to 6 seconds at 80 °C mold temperature is typical. Shorter hold times produce sink over ribs and larger flow-direction shrinkage; longer hold times can pack the part but also increase molded-in stress. Mold temperatures from 60 °C to 100 °C are acceptable; higher mold temperatures improve surface finish and dimensional stability at the expense of cycle time.
In electromechanical terminal blocks and connector shells, dimensional stability under heat is combined with moderate comparative tracking index. The material class is evaluated for CTI according to IEC 60112. Glass fibers at the surface may reduce CTI relative to unfilled PBT; SEF-515T is therefore likely to be used where fiber-reinforced stiffness and creep resistance are more important than maximum surface tracking performance. Chemical resistance should be reviewed: PBT is resistant to many mineral oils, aliphatic hydrocarbons, and alcohols at ambient temperature, but not recommended for continuous hot-water contact above 60 °C or for strong alkaline solutions, which attack the ester group. Strong alkaline additives or amine-based processing aids should be avoided because they can catalyze hydrolysis of the PBT ester linkage during melt processing. Stressed parts may also show environmental stress cracking in contact with aromatic solvents or ketones.
No single regulatory classification covers all regions. The base PBT+15% glass-fiber compound is typically assessed for RoHS compliance under Directive 2011/65/EU including amendment 2015/863, and for REACH SVHC content under Regulation EC 1907/2006. UL 94 flammability class, comparative tracking index, and relative thermal index are grade-specific data requiring a valid UL Yellow Card; published data for this specific SEF-515T configuration is limited and must be confirmed with the current manufacturer document. In food-contact or medical applications, SEF-515T should not be assumed to comply with FDA 21 CFR or EU 10/2011 unless explicitly stated in supplier certification. If the suffix “NF” is intended to indicate a non-flame-retardant grade as is common in some supplier naming systems, then the product is not intended for applications requiring UL 94 V-0 performance; this interpretation must be verified against the commercial datasheet.
On production-scale equipment with hot-runner manifolds, thermal history in the manifold is the dominant cause of lot-to-lot color shift and impact loss. If a production line sees melt-pressure fluctuation above 5% during screw recovery, feed throat bridging or glass segregation should be suspected. The material can be processed on general-purpose screws with L/D 20:1 to 22:1 and moderate compression ratio 2.5:1 to 3.0:1; high-compression screws increase fiber attrition and reduce notched impact.
Melt flow rate determined at 250 °C under 2.16 kg load according to ISO 1133-1 is often in the range 15 to 25 g/10 min for this class, but glass fiber makes MFR an incomplete lot-to-lot viscosity control. Capillary rheometry or in-line melt-pressure monitoring is more useful for critical components. A melt-pressure variation above 5% during screw recovery indicates feeding variation, fiber segregation, or inadequate drying consistency.
Surface roughness and fiber prominence in molded parts are influenced by mold temperature and injection speed. Higher mold temperature in the 80 °C to 100 °C range produces a resin-rich surface and improves gloss, while lower mold temperatures increase fiber pattern visibility. For parts requiring adhesive bonding or pad printing, surface activation with plasma or organosilane primer may be needed to raise surface energy above 40 mN/m. This is an operational boundary that is not visible in standard mechanical property tables.
Compared with a 10% glass-fiber compound, SEF-515T provides higher flexural modulus and lower mold shrinkage but lower impact resistance. Compared with a 20% glass-fiber compound, it flows more readily and may fill thin-wall sections with lower injection pressure; the modulus difference is moderate and may be acceptable in many housings. The selection is therefore not simply based on filler content but on the interaction of tool geometry, gate location, and performance requirements.