| HS Code | 652828 |
| Polymer Type | PBT |
| Glass Fiber Content | 15% |
| Flame Retardancy | UL 94 V-0 |
| Low Warpage | Yes |
| Density | 1.50 g/cm³ |
| Tensile Modulus | 6000 MPa |
| Tensile Strength | 95 MPa |
| Elongation At Break | 2.5% |
| Flexural Modulus | 5500 MPa |
| Flexural Strength | 145 MPa |
| Charpy Notched Impact Strength | 5 kJ/m² |
| Charpy Unnotched Impact Strength | 25 kJ/m² |
| Heat Deflection Temperature At 1 8 Mpa | 195 °C |
| Melting Temperature | 225 °C |
| Mold Shrinkage | 0.2–0.6% |
| Water Absorption | 0.1% |
As an accredited Mitsubishi Chemical Novaduran™ PBT+GF15%-LW-V0-LW 5810GN2-15 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Mitsubishi Chemical Novaduran™ PBT+GF15%-LW-V0-LW 5810GN2-15 is supplied in 25 kg moisture-barrier bags, palletized and securely wrapped for industrial handling. |
| Container Loading (20′ FCL) | 20′ FCL container loading of Mitsubishi Chemical Novaduran™ PBT+GF15%-LW-V0-LW 5810GN2-15 in standard packaging, securely stowed for safe transport. |
| Shipping | Mitsubishi Chemical Novaduran™ PBT+GF15%-LW-V0-LW 5810GN2-15 is shipped as non-hazardous plastic resin pellets in moisture-barrier bags, sacks, or octabins. It is classified as non-dangerous goods; no UN number, proper shipping name, hazard class, or packing group applies for transport. Store dry, away from heat, using normal industrial hygiene. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and open flames. Keep in original sealed packaging to prevent moisture absorption and contamination. Avoid contact with strong oxidizers. Maintain normal warehouse temperature and humidity; use desiccants if required. Follow the SDS and handle with appropriate PPE. |
| Shelf Life | Shelf life is typically 12 months from production when stored dry, in original sealed packaging, away from moisture, heat, and sunlight. |
Competitive Mitsubishi Chemical Novaduran™ PBT+GF15%-LW-V0-LW 5810GN2-15 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Mitsubishi Chemical Novaduran™ 5810GN2-15 is identified by the designation PBT+GF15%-LW-V0-LW as a polybutylene terephthalate moulding compound containing 15% glass fibre reinforcement, a low-warpage additive package, and a flame-retardant system that provides a UL 94 V-0 classification at a thickness specified on the manufacturer’s UL Yellow Card. The material belongs to the semi-crystalline polyester family and is processed by injection moulding. The glass fibre content raises tensile modulus and heat deflection temperature relative to unfilled PBT, while the low-warpage modification is intended to reduce anisotropic shrinkage and out-of-plane distortion in flat electrical components. Published data for the specific 5810GN2-15 configuration is limited; grade-specific values should be obtained from the supplier datasheet before design freeze.
Melt flow-related data for this product class are commonly measured under ISO 1133-1:2022 at 250 °C with a 2.16 kg load. For a 15% glass fibre flame-retarded PBT, melt volume-flow rates are generally lower than unfilled PBT because of fibre packing and flame-retardant solids. The exact value for 5810GN2-15 must be verified from the manufacturer’s certificate. The product designation should be read as a resin-family identifier, not as a complete material specification. The grade is intended for electrical and electronic housings, connectors, relay bases, sensor mounts, and power-distribution components where dimensional precision and flammability requirements are combined.
Low-warpage behaviour in reinforced PBT is not achieved by glass fibre loading alone. In a conventional 15% glass fibre PBT, shear-induced fibre orientation creates a layered morphology with different longitudinal and transverse shrinkage. When measured on 60 mm × 60 mm × 2 mm plaques moulded according to ISO 294-4:2018, standard grades can exhibit out-of-flatness that exceeds connector seating tolerances. The “LW” portion of the designation indicates that the compound has been modified—typically through low-aspect-ratio glass, mineral fillers, or flow modifiers—to reduce the difference between parallel and perpendicular shrinkage. The resulting moulded residual stress remains anisotropic; the designation does not guarantee perfectly isotropic behaviour. Tool design still requires balanced gating, uniform wall thickness, and adequate mould-cooling circuits. Dimensional stability after moulding is further influenced by crystallinity distribution. Parts should be conditioned for 24 h at 23±2 °C and 50±10% relative humidity before metrology under ISO 291:2008.
Pre-drying is mandatory. The ester linkage in PBT is hydrolytically sensitive at melt processing temperatures. Moisture above 0.02% produces molecular weight reduction, silver streaking, and loss of mechanical strength. Desiccant drying to a dew point of −30 °C or lower, with inlet air at 120 °C for 4–6 h, is a standard starting condition for flame-retarded glass-filled PBT compounds. A residual moisture analyser should be used where available; visual inspection of granules is insufficient. Flame-retarded PBT can be thermally sensitive at high shear. Barrel temperatures should be profiled from 230 °C at the feed section to 260 °C at the nozzle, with an absolute melt temperature not exceeding 270 °C. Mould temperatures between 60 °C and 100 °C are used to balance crystallinity, cycle time, and part glazing. Shutdowns longer than 10 min at processing temperature require purging to avoid black specks and flame-retardant decomposition residues. Avoid contamination with polyamide residues or other amine-bearing polymers in the screw, hot runner, or drying system because transesterification and degradation can occur at PBT processing temperatures.
The V-0 portion of the designation refers to vertical-burn testing under UL 94. The pass/fail criteria include flame time after first and second flame application, afterglow time, and cotton ignition. The achievable V-0 thickness depends on the flame-retardant system and is declared in the UL Yellow Card. Common thicknesses for flame-retarded PBT grades are 0.75 mm, 1.5 mm, and 3.0 mm. For 5810GN2-15, the manufacturer’s certification should be consulted before designing below 1.0 mm wall stock. Electrical insulation suitability is not fully defined by UL 94 alone. Tracking resistance is evaluated under IEC 60112, glow-wire ignition under IEC 60695-2-10 and IEC 60695-2-11, and glow-wire flammability under IEC 60695-2-12. Glass reinforcement can reduce comparative tracking index relative to unfilled flame-retarded PBT because fibres can concentrate electric field stress at the surface. Unfilled flame-retarded PBT systems may have CTI values above 500 V, whereas glass-filled versions can fall into the 250–400 V range. Therefore, creepage and clearance distances should be designed using the actual CTI value for 5810GN2-15, not a generic PBT assumption.
Relative to an unfilled flame-retarded PBT, the 15% glass content raises flexural modulus and reduces the coefficient of linear thermal expansion. Unfilled flame-retarded PBT may exhibit tensile elongation at break above 20%, whereas GF15 FR compounds normally exhibit elongation below 5% under ISO 527-1/2:2012. The trade-off is reduced ductility and greater notch sensitivity at sharp corners or press-fit inserts. Compared with a 30% glass fibre flame-retarded PBT, the 15% grade lowers melt viscosity, improves thin-wall filling, reduces screw and barrel wear, and produces lower density. The density of a GF15 PBT FR grade is often between 1.50 g/cm³ and 1.60 g/cm³ measured by ISO 1183-1:2019, while a GF30 PBT FR analogue may exceed 1.65 g/cm³. Heat deflection temperature under ISO 75-1/2:2013 at 1.8 MPa for the GF15 class is generally lower than GF30; GF30 PBT FR grades can approach 200–220 °C, whereas GF15 versions typically fall in the 180–205 °C range. Published data for this specific configuration is limited and should not replace supplier-certified values for structural simulation.
Thin-wall relay housings, battery-management-system connectors, and high-density PCB connectors often have nominal wall sections from 0.5 mm to 1.2 mm. At these sections, the flow resistance of a 30% glass fibre flame-retarded PBT can exceed the practical injection pressure of many electric injection moulding machines. The 15% glass loading of 5810GN2-15 lowers filling pressure and permits longer flow lengths before jetting. The low-warpage modification is most useful in multi-cavity tools where flatness tolerance across a connector body must remain within 0.05 mm over a 40 mm length; part flatness is also governed by gate placement and holding pressure. In production trials, cavity-to-cavity pressure variation should be held below ±5% to avoid differential shrinkage. Weld lines should be relocated to low-stress ribs rather than snap-fit flexure elements. Venting in the parting line and ejector pins is required because flame-retardant PBT can emit low-level decomposition volatiles at processing temperatures; inadequate venting produces burn marks and gas marks. Published case-study data for 5810GN2-15 is limited.
For component compliance, the following standards are frequently requested in electrical and electronic applications. The table presents the standard framework rather than supplier-specific certified values. Material certifications should be retrieved from the manufacturer for each production batch.
| Assessment | Standard or regulation | Condition or status |
|---|---|---|
| Flammability | UL 94 V-0 | Thickness-dependent; per UL Yellow Card |
| Comparative tracking index | IEC 60112 | Verify grade-specific voltage |
| Glow-wire flammability index | IEC 60695-2-12 | Common for unattended appliance enclosures |
| Restriction of hazardous substances | RoHS Directive 2011/65/EU, IEC 63000 | Supplier declaration required |
| REACH SVHC communication | Regulation (EC) No 1907/2006 | Article 33 communication if applicable |
Injection moulding machines with general-purpose screws of 20:1 to 24:1 length-to-diameter ratio and a compression ratio of 2.5:1 to 3.0:1 are typically suitable for glass-filled PBT. A free-flow nozzle is preferred; if drooling occurs because of the melt viscosity of a flame-retarded formulation, a shut-off nozzle may be used. The feed throat must be cooled to prevent granule sticking. Regrind levels above 25% are not recommended without testing because repeated heat history can degrade the flame-retardant system and the PBT matrix. Hot-runner manifold temperatures should be set at the lower end of the melt-temperature range and should not exceed 270 °C. Screw recovery speed should be controlled to avoid excessive shear heating; melt-temperature increases of more than 10 °C above the nozzle setpoint indicate excessive screw speed or backpressure. The low-warpage character does not eliminate the need for stable mould-temperature control; oil or pressurised-water mould heating circuits with a variation below ±2 °C are used to achieve repeatable shrinkage.