| HS Code | 838239 |
| Polymerbase | PBT |
| Glassfibercontent | 15% |
| Lowwarpmodification | Yes |
| Flameretardant | Yes |
| Density | 1.54 g/cm³ |
| Moldingshrinkage | 0.3–0.7% |
| Waterabsorption | 0.08% |
| Tensilestrength | 100 MPa |
| Flexuralmodulus | 6000 MPa |
| Elongationatbreak | 2.0% |
| Charpynotchedimpactstrength | 5 kJ/m² |
| Hdtat1 8mpa | 195 °C |
| Ul94flamerating | V-0 |
| Volumeresistivity | 1×10^16 Ω·cm |
| Dielectricstrength | 20 kV/mm |
| Melttemperature | 250–270 °C |
| Moldtemperature | 60–100 °C |
| Dryingconditions | 120 °C for 3–4 h |
As an accredited Mitsubishi Chemical Novaduran™ PBT+GF15%-LW-V0 5710GN6-15 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaged in 25 kg moisture-resistant, polyethylene-lined bags, palletized at 1,000 kg per pallet for Mitsubishi Chemical Novaduran™ PBT+GF15%-LW-V0 5710GN6-15. |
| Container Loading (20′ FCL) | 20′ FCL loading of Mitsubishi Chemical Novaduran™ PBT+GF15%-LW-V0 5710GN6-15, packaged per supplier specification, palletized, and securely stowed for export. |
| Shipping | Mitsubishi Chemical Novaduran™ PBT+GF15%-LW-V0 5710GN6-15 is shipped as thermoplastic resin pellets in moisture-barrier bags, 25 kg bags, octabins, or bulk containers. Keep dry, cool, and ventilated; avoid moisture, ignition sources, and direct sunlight. Follow SDS, packaging, labeling, and local transport regulations. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and moisture. Keep containers tightly closed and palletized; avoid dust generation and static discharge. Segregate from oxidizers and strong acids. Use first-in, first-out inventory, retain original labels, and consult the SDS/supplier for specific temperature and drying requirements. |
| Shelf Life | Shelf life is typically indefinite when stored dry in sealed original packaging; avoid moisture, heat, and direct sunlight. |
Competitive Mitsubishi Chemical Novaduran™ PBT+GF15%-LW-V0 5710GN6-15 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Mitsubishi Chemical Novaduran™ PBT+GF15%-LW-V0 5710GN6-15 is a polybutylene terephthalate injection molding compound reinforced with 15% by weight glass fiber and formulated to achieve a V-0 flammability classification under UL 94. The LW suffix identifies a low-warpage modification that distinguishes the grade from standard glass-filled flame-retardant PBT compounds. The product is specified through ISO 1183-1 for density, ISO 527-2 for tensile strength and elongation, ISO 178 for flexural modulus, ISO 179-1/1eA for notched Charpy impact, ISO 75-1/-2 for heat deflection temperature, and ISO 1133-1 for melt volume-flow rate. Numerical values must be taken from the manufacturer-controlled datasheet; published data for this specific configuration outside that datasheet is limited. The grade is positioned for thin-wall electrical and electronic housings, connectors, relay bases, and sensor mounts in which flame retardancy and flatness control are simultaneous requirements.
The compound is hydrolytically sensitive and must be pre-dried before melt processing. A desiccant dryer producing a dew point of −30 °C or lower and a hopper temperature of 120 °C for 4 h is a standard starting condition. Residual moisture above 0.02% can cause splay, reduction of melt strength, and hydrolytic degradation during processing. Residual moisture is commonly verified by Karl Fischer titration or a calibrated moisture balance. Production-scale molding lines for glass-filled PBT require hardened screw flights, bimetallic barrel surfaces, and closed-loop dry-air conveying to prevent moisture regain between dryer and feed throat. Three-zone screws with 20:1 to 25:1 L/D ratio and compression ratio from 2.0:1 to 2.5:1 are typical. Barrel temperatures of 250 °C to 270 °C and mold temperatures of 60 °C to 90 °C are representative process windows for glass-filled flame-retardant PBT compounds; back pressure between 0.3 MPa and 0.7 MPa assists glass dispersion without excessive fiber breakage.
Melt residence time above 10 min at processing temperature is not recommended because the flame-retardant system may degrade and the molten stock may discolor. The nozzle should be of a shut-off design to prevent drooling and fiber-rich stringing. Hot-runner systems should use balanced valve-gated drops to reduce fiber orientation streaks and gate freeze-off. Specific hot-runner performance data for 5710GN6-15 is not widely published, so tool trials are required for mold approval. The presence of glass fiber accelerates screw and check-ring wear; consistent screw-diameter tolerance and periodic check-ring replacement are necessary to maintain a stable melt cushion and shot weight. On production presses, the shot size is normally maintained between 30% and 70% of barrel capacity to limit residence time and thermal history.
The combination of 15% glass fiber and flame-retardant additives lowers melt flow relative to unfilled PBT. For sections below 1.0 mm, shear viscosity data from capillary rheometry according to ISO 11443 is more useful than a single melt volume-flow rate value because it captures shear-rate dependence. Mold filling simulations require shear viscosity, thermal conductivity, and pvT inputs; published data for this specific configuration outside the controlled datasheet is limited, so simulation inputs should be measured or obtained from the material supplier. In connectors with wall thickness below 0.8 mm, injection velocity, gate diameter, and cavity venting are controlling variables. Short-shot studies on the production tool should validate gate dimensions; gates below 0.8 mm can cause glass fiber accumulation and premature freeze-off. Cavity pressure sensors document the fill-pressure threshold and detect lot-to-lot viscosity shifts before dimensional rejects occur.
Weld lines in multi-gated tools reduce local tensile strength compared with flow-aligned bulk material. Weld-line strength is measured with tensile specimens according to ISO 527-2 and should be evaluated at the minimum service wall thickness. Processing windows that favor high mold temperatures improve weld-line healing but may increase cycle time. In thin-wall applications, mold temperature uniformity is more significant than the selection of a single setpoint; differential cooling in the tool can override the low-warpage benefits of the formulation. Gas venting is also necessary because flame-retardant compounds can generate volatile by-products at the upper end of the melt-temperature range. Vent depths should follow standard tooling practice for filled PBT, typically 0.02 mm to 0.03 mm for side vents, with periodic cleaning to prevent blocking.
Flatness and terminal alignment in electrical enclosures, relay bases, and sensor housings depend on mold shrinkage anisotropy. Differential shrinkage is evaluated according to ISO 294-4. In glass-filled PBT, fiber orientation usually produces higher transverse shrinkage than flow-direction shrinkage; the low-warpage formulation is intended to reduce that spread. The benefit is most visible in large flat parts with nonuniform wall thickness and in ribbed geometries. Mold temperature uniformity within ± 2 °C and balanced coolant circuits at bosses and rib roots preserve the warpage benefit in production. Gate location remains a primary determinant of fiber orientation; low-warpage additives do not fully compensate for unfavorable gate placement or unbalanced filling.
Low warpage does not remove post-mold dimensional movement caused by moisture uptake. Specimens conditioned at 23 °C and 50% relative humidity should be included in dimensional capability studies. In circular or tubular parts, roundness measurements after moisture conditioning may be more relevant than flatness values. Published data for extended thermal aging of 5710GN6-15 is limited; long-term dimensional stability should be confirmed on production-representative parts under the intended service environment. The material is not suited for direct exposure to hot aqueous media above the expected continuous service temperature because PBT can undergo hydrolysis and progressive loss of mechanical properties.
Compared with an unfilled flame-retardant PBT grade, 5710GN6-15 produces higher flexural modulus, tensile strength, and heat deflection temperature and a lower coefficient of linear thermal expansion. Elongation at break and notched impact toughness are lower, which must be considered in snap-fit geometries. Compared with a GF30 V-0 grade, the 15% glass loading provides lower density, lower melt viscosity, and reduced screw and barrel wear, but the flexural modulus and tensile strength are lower. The principal difference from a standard GF15 V-0 grade is the LW low-warpage technology, which targets shrinkage anisotropy rather than absolute stiffness.
| Configuration | Flexural modulus ISO 178 | Mold shrinkage anisotropy ISO 294-4 | Thin-wall fill tendency | Density ISO 1183-1 |
|---|---|---|---|---|
| Unfilled FR V-0 | Lowest | Low | Highest | Lowest |
| Standard GF15 FR V-0 | Moderate | High | Moderate | Moderate |
| 5710GN6-15 LW-V0 | Moderate | Reduced | Moderate | Moderate |
| GF30 FR V-0 | Highest | High | Lowest | Highest |
These directional comparisons are not substitutes for datasheet values. They identify the product’s intended operating zone: a middle glass content with reduced warpage and flame retardancy. The material is therefore specified where unfilled V-0 has insufficient stiffness and GF30 V-0 creates excessive density, flow loss, or abrasive wear in fine-pitch tooling. The grade may also replace standard GF15 V-0 when post-molding distortion is a recurring production reject mode.
The V-0 classification under UL 94 is thickness-dependent. The minimum thickness recorded on the UL Yellow Card for 5710GN6-15 controls flame-barrier design; the rating is not automatically valid for thinner sections or nonstandard colors. For unattended electrical equipment, glow-wire testing according to IEC 60695-2-12 and comparative tracking index according to IEC 60112 are required because flame-retardant additives can change surface tracking behavior. Dielectric strength may be evaluated according to IEC 60243-1, and volume resistivity according to IEC 62631-3-1. These electrical values are grade-specific and should be confirmed for the thickness and conditioning state used in service.
| Area | Standard designation | Boundary condition for 5710GN6-15 |
|---|---|---|
| Flammability | UL 94 | V-0 at thickness on UL Yellow Card |
| Glow-wire flammability | IEC 60695-2-12 | End product standard determines required temperature |
| Comparative tracking index | IEC 60112 | Value reported on supplier datasheet; design margin required |
| RoHS | Directive 2011/65/EU as amended by (EU) 2015/863 | Lot-level declaration required |
| REACH | Regulation (EC) No 1907/2006 | Candidate list review required |
| Melt volume-flow rate | ISO 1133-1 | Process control parameter, not a primary specification |
In power distribution terminal blocks and connector bodies, the low-warpage feature is applied to maintain terminal pitch after molding. Coordinate measuring machine inspection according to ISO 1101 is used for flatness and positional tolerances. Lot acceptance for production parts includes notched Charpy impact tested to ISO 179-1/1eA and flammability coupons molded at the minimum UL thickness. Regrind levels above 30% should trigger re-qualification of impact strength and flame retardancy. The material should not be processed after moisture regain above 0.02%, and tooling should be vented adequately to prevent gas marks from the flame-retardant system.