| HS Code | 937459 |
| Density | 1.42 g/cm³ |
| Glassfibercontent | 15 % |
| Waterabsorption | 0.07 % |
| Moldshrinkage | 0.2-0.6 % |
| Tensilestrength | 100 MPa |
| Elongationatbreak | 2.5 % |
| Flexuralmodulus | 5.6 GPa |
| Flexuralstrength | 150 MPa |
| Charpynotchedimpactstrength | 5 kJ/m² |
| Hdtat1 82mpa | 190 °C |
| Meltingpoint | 224 °C |
| Volumeresistivity | 1e16 Ω·cm |
| Dielectricstrength | 20 kV/mm |
| Dielectricconstant | 3.5 |
| Flammability | HB |
As an accredited Mitsubishi Chemical Novaduran™ PBT+GF15%-LW 5810G15 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packed in 25 kg moisture-barrier bags, Mitsubishi Chemical Novaduran™ PBT+GF15%-LW 5810G15 resin is supplied on pallets for industrial handling. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with palletized Mitsubishi Chemical Novaduran™ PBT+GF15%-LW 5810G15 in sealed moisture-barrier bags, safely secured for ocean shipment. |
| Shipping | Mitsubishi Chemical Novaduran™ PBT+GF15%-LW 5810G15 is typically shipped as non-hazardous plastic pellets in moisture-barrier bags or octabins, palletized and protected from moisture, UV, and contamination. Normal road, sea, or air freight applies; store cool and dry. Keep packaging sealed until use. Confirm SDS and transport classification before shipment. |
| Storage | Store Mitsubishi Chemical Novaduran™ PBT+GF15%-LW 5810G15 in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and oxidizing agents. Keep original packaging sealed to prevent moisture absorption; use desiccant in humid conditions. Avoid dust generation, contamination, and ignition sources. Stack pallets securely, rotate stock, and follow the manufacturer’s SDS and local storage regulations. |
| Shelf Life | Typically 24 months when stored unopened in original packaging in a dry, cool, well-ventilated area away from direct sunlight. |
Competitive Mitsubishi Chemical Novaduran™ PBT+GF15%-LW 5810G15 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Designated within the Mitsubishi Chemical Novaduran™ thermoplastic polyester portfolio as PBT+GF15%-LW 5810G15, this compound is a semi-crystalline polybutylene terephthalate injection-moulding grade containing a nominal 15 wt% glass-fibre reinforcement and a low-warpage additive package. The LW suffix indicates a formulation intended to reduce differential flow-to-transverse shrinkage relative to conventional glass-filled PBT. The base PBT matrix is produced from 1,4-butanediol and terephthalic acid; differential scanning calorimetry under ISO 11357-3 typically records a melting endotherm between 220 °C and 225 °C. The glass transition of the unfilled matrix, measured under ISO 11357-2, is generally reported in the 45–60 °C range. Ash content per ISO 3451-1 is the accepted method for verifying the nominal 15% fibre loading. Density determined under ISO 1183-1 is typically in the 1.39–1.44 g/cm³ range for this class of glass-reinforced PBT.
At 15 wt% glass loading, the fibre network increases modulus and strength but reduces elongation to break. The tensile modulus is typically 4500–5500 MPa, approximately two to three times the modulus of unfilled PBT. The notch sensitivity of glass-reinforced PBT is the principal trade-off: notched Charpy impact values commonly remain below 6 kJ/m² under ISO 179-1/1eA, whereas unfilled PBT can exceed 10 kJ/m² in unnotched configurations. The low-warp modification does not eliminate notch sensitivity, but it improves flatness through more balanced shrinkage between the flow and transverse directions. Representative property ranges for this glass-fibre loading class are given below; purchase-specification values must be verified against the current manufacturer datasheet.
| Property | Test method | Representative range |
|---|---|---|
| Density | ISO 1183-1 | 1.39–1.44 g/cm³ |
| Glass-fibre content | ISO 3451-1 | 15% by weight nominal |
| Tensile strength at break | ISO 527-1/-2 | 85–105 MPa |
| Tensile elongation at break | ISO 527-1/-2 | 2–4% |
| Flexural modulus | ISO 178 | 4.0–5.5 GPa |
| Flexural strength | ISO 178 | 130–150 MPa |
| Charpy notched impact strength | ISO 179-1/1eA | 3.5–6.0 kJ/m² |
| Charpy unnotched impact strength | ISO 179-1/1eU | 25–40 kJ/m² |
| Heat deflection temperature at 1.80 MPa | ISO 75-1/-2 | 175–200 °C |
| Melt volume-flow rate at 250 °C/2.16 kg | ISO 1133-1:2022 | 15–30 cm³/10 min |
| Mould shrinkage, parallel | ISO 294-4 | 0.4–0.7% |
| Mould shrinkage, transverse | ISO 294-4 | 0.7–1.1% |
Moisture control is the principal pre-processing constraint for 5810G15. Pellets should be dried in a desiccant-bed dryer with a dew point no higher than −30 °C at 120 °C for 4–6 h. Residual moisture above 0.02 wt%, determined by Karl Fischer titration, leads to hydrolytic chain scission at the PBT ester linkages when melt temperature exceeds 250 °C. The resulting molecular weight loss produces silver streaking and a measurable reduction in notched Charpy impact under ISO 179-1/1eA. Hopper residence time at temperature should not exceed 2 h without sealed feeding, and regrind content should be limited to the percentage specified by the end-use qualification plan to avoid fibre-length reduction.
The melt-volume flow rate under ISO 1133-1:2022 at 250 °C and 2.16 kg is commonly between 15 cm³/10 min and 30 cm³/10 min for glass-reinforced PBT of this loading. The fibre content raises shear viscosity relative to unfilled PBT and produces pronounced pseudoplastic flow; injection moulders observe pressure loss concentrated in small gates and thin runners. Gate diameters below 0.8 mm should be evaluated for glass-fibre jamming and high shear heating. On production-scale hydraulic machines with 25–30 mm screw diameter and 80–120 t clamp force, screw speed is typically held below 100 min⁻¹ to limit fibre attrition. Back pressure is set between 0.3 MPa and 0.5 MPa to maintain a homogeneous melt without excessive residence time. Nozzle melt temperature is commonly profiled from 240 °C at the feed zone to 260 °C at the nozzle, with a maximum melt temperature of 270 °C. Operation above 270 °C accelerates thermal degradation of the PBT ester linkage; operation below 240 °C can freeze off gates prematurely and produce short shots. The practical melt-temperature window is therefore approximately ±5 °C around the mid-set temperature for a given tool, making barrel thermocouple calibration and residence-time control critical.
Flatness-critical applications are the primary use case for the LW suffix. The material is specified for electronic housings, sensor brackets, relay bases, and other thin-wall components where post-mould distortion must remain within narrow assembly tolerances. The low-warpage additive package reduces the difference between parallel and transverse mould shrinkage, but the final flatness result depends heavily on gate location, packing pressure, and mould-temperature uniformity. Tool trials should therefore use a full factorial design with melt temperature, mould temperature, and hold pressure as factors, not a single conservative parameter set.
When flatness tolerance falls below 0.2 mm across a 150 mm flow path, the dominant variables shift from material selection to tooling and packing. Mould temperature is held between 60 °C and 80 °C to control post-mould crystallization and to shift shrinkage toward the tool dimension. Higher mould temperatures reduce freeze-in orientation but create longer cycle times. Packing pressure should be set to maintain gate-seal time slightly beyond the point of as-built volume fill; pressures commonly range from 40 MPa to 70 MPa depending on wall thickness and gate geometry. Published third-party comparative data for the exact 5810G15 grade under these tolerance conditions is limited; therefore, cavity-pressure sensors and response-surface trials are recommended before transferring a tool to production. The low-warp property should not be interpreted as a guarantee of zero distortion, but as a reduction in the anisotropic shrinkage component that otherwise dominates flatness error.
Differences from unfilled PBT and from 30% glass-fibre PBT are defined by stiffness, ductility, and shrinkage anisotropy. Unfilled PBT provides elongation at break typically above 100% but flexural modulus below 3000 MPa; 5810G15 moves into a structural range at the expense of ductility. Relative to a 30% glass-fibre PBT, the 15% reinforcement retains lower modulus and lower warpage potential, making it more suitable for thin-wall parts where over-stiffening can amplify internal stress. The low-warpage package should not be assumed to improve chemical resistance; PBT remains susceptible to hydrolysis in hot water above 80 °C, and continuous exposure to strong alkalis or hot glycols should be avoided. If a specific comparative tracking index is required for electrical applications, the product certificate under IEC 60112 should be obtained from the supplier rather than inferred from generic PBT data.