Mitsubishi Chemical Novaduran Pbt Gf15 Hb 5010g15

Mitsubishi Chemical Novaduran™ PBT+GF15%-HB 5010G15

    • Product Name: Mitsubishi Chemical Novaduran™ PBT+GF15%-HB 5010G15
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 437245
    Polymer Type PBT
    Glass Fiber Reinforcement Yes
    Glass Fiber Content 15%
    Flame Retardancy UL 94 HB
    Density 1.41 g/cm3
    Tensile Strength 90 MPa
    Elongation At Break 2.5%
    Flexural Modulus 5500 MPa
    Notched Charpy Impact Strength 4 kJ/m2
    Heat Deflection Temperature At 1 82 Mpa 190 °C
    Water Absorption At 24 H 0.07%
    Molding Shrinkage 0.4-0.7%
    Processing Method Injection molding

    As an accredited Mitsubishi Chemical Novaduran™ PBT+GF15%-HB 5010G15 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaging: 25 kg moisture-proof bags, palletized and clearly labeled with product name, grade, batch number, and handling information.
    Container Loading (20′ FCL) 20′ FCL loaded with Mitsubishi Chemical Novaduran™ PBT+GF15%-HB 5010G15 in standard export packaging, evenly distributed and secured for transport.
    Shipping Shipping description: Mitsubishi Chemical Novaduran™ PBT+GF15%-HB 5010G15, glass-fiber reinforced PBT pellets, non-hazardous and not regulated for transport. Supplied in 25 kg moisture-barrier bags on pallets; keep dry and protect from heat, sunlight, and contamination during normal commercial freight.
    Storage Store Mitsubishi Chemical Novaduran™ PBT+GF15%-HB 5010G15 in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and open flames. Keep containers tightly closed to prevent moisture absorption and contamination. Avoid high humidity and incompatible chemicals, maintain stock rotation, use appropriate PPE, and follow the manufacturer’s SDS and local regulations.
    Shelf Life Typically 12 months when stored in original sealed packaging in a dry, cool place, protected from moisture and direct sunlight.
    Free Quote

    Competitive Mitsubishi Chemical Novaduran™ PBT+GF15%-HB 5010G15 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Grade 5010G15 in the Mitsubishi Chemical Novaduran™ range is a glass-fibre-reinforced polybutylene terephthalate injection moulding compound. The designation encodes a 15% mass fraction of E-glass reinforcement in the Novaduran 5010 polyester base, with an HB suffix denoting a horizontal burn classification under UL94. The grade is supplied as free-flowing pellets and is intended for melt processing on conventional reciprocating-screw injection moulding machines. The matrix polymer is a semicrystalline aromatic polyester synthesised from 1,4-butanediol and dimethyl terephthalate or terephthalic acid. The reinforcement is a silane-sized short glass fibre with nominal filament diameter of 10–13 µm; the silane size promotes fibre-matrix adhesion. Published datasheet values place the density at 1.40 g/cm³ under ISO 1183-1. Melt volume-flow rate is characterised at 250°C with a 2.16 kg load using ISO 1133-1; nominal melt volume-flow rate is 19 cm³/10 min for standard lot control.

    PropertyTest methodNominal valueUnit
    DensityISO 1183-11.40g/cm³
    Tensile strength at breakISO 527-2/1A100MPa
    Tensile elongation at breakISO 527-2/1A3%
    Tensile modulusISO 527-2/1A4,700MPa
    Flexural strengthISO 178155MPa
    Flexural modulusISO 1784,700MPa
    Charpy notched impact strength, 23°CISO 179-1/1eA5.0kJ/m²
    Deflection temperature under load, 1.80 MPaISO 75-2/A195°C
    Melt volume-flow rate, 250°C/2.16 kgISO 1133-119cm³/10 min
    Mould shrinkage, flow directionISO 294-40.4%
    Mould shrinkage, normal directionISO 294-40.8%
    Moisture absorption, 23°C, 24 hISO 620.07%
    Flammability classUL94HB—

    Mechanical property data are generated on dry-as-moulded specimens conforming to ISO 20753 type 1A geometry. Tensile strength is measured at 5 mm/min; flexural properties are measured at 2 mm/min under ISO 178. The 15% reinforcement produces anisotropic properties in injection moulded parts because fibre orientation follows the flow front. Tensile modulus in the flow direction is generally higher than in the transverse direction. Weld-line tensile strength is lower than bulk strength, but published data for this specific configuration is limited. Weld-line-specific values should be measured on prototype tooling because gate placement and knit-line location change local fibre orientation and packing behaviour.

    Glass fibre loading is fixed at 15% by mass for balanced stiffness and mouldability

    At 15% glass content, 5010G15 occupies a middle range in the Novaduran 5010 family. The tensile modulus is approximately 4,700 MPa under ISO 527-2/1A. This is roughly 2.3–2.5 times the modulus of unfilled 5010, while the notched Charpy impact strength remains higher than many 30% glass-reinforced grades because lower fibre packing reduces brittle crack propagation. Mould shrinkage is lower than unfilled PBT because the rigid glass network restrains crystallite volume contraction. The in-flow shrinkage of 0.4% and cross-flow shrinkage of 0.8% under ISO 294-4 produce an anisotropy ratio of 0.5, which is significant for flat rectangular parts. This anisotropy causes corner-to-corner warpage when the mould surface temperature is too low; mould temperatures near 80°C reduce under-cooling and allow more uniform crystallisation.

    Compared with unfilled 5010, direct substitution of 5010G15 in an existing tool usually changes demoulding shrinkage enough that ejection clearances and gate dimensions require re-cutting. Compared with 5010G30, the 15% reinforcement reduces screw torque and melt pressure, but it also lowers flexural modulus. The lower fibre packing typically reduces the severity of exposed surface fibres on moulded parts, although surface gloss remains lower than unfilled PBT.

    Because PBT hydrolyses in the melt, pre-drying is the primary operational boundary for 5010G15. The pellets are dried in desiccant-bed dryers with closed-loop regeneration and a dew point of -30°C or below. Drying at 120°C for 4–6 h reduces residual moisture to below 0.02% as determined by ISO 15512 method B. Higher humidity or storage in open hoppers produces silver streaking, screw deposit formation and a measurable reduction in tensile elongation due to hydrolytic cleavage of ester bonds. The hydrolysis reaction is pseudo-first-order in moisture concentration and becomes significant above 0.02% at melt temperatures above 250°C. Melt residence times above 10 min are not recommended. On production-scale equipment with oversized barrels or long standby periods, molecular weight loss accelerates and black specks appear. If the moulding cycle is interrupted, barrel temperatures should be reduced to 230°C during standby and the screw should be retracted.

    Moulding parameterUnitSet range or requirement
    Pre-drying temperature°C120
    Pre-drying time, virgin pelletsh4–6
    Residual moisture, maximum%<0.02
    Desiccant dryer dew point°C≤ -30
    Barrel rear zone°C240–250
    Barrel middle zone°C250–260
    Barrel front zone°C250–270
    Melt temperature°C250–270
    Nozzle temperature°C250–260
    Mould temperature°C60–80
    Injection pressureMPa60–100
    Holding pressure% of injection pressure50–70
    Back pressureMPa0.3–0.7
    Screw speedmin⁻¹80–120
    Maximum melt residence timemin<10

    What moulding parameters govern hydrolytic stability during melt processing?

    Hydrolytic stability during melt processing is governed by the interaction of residual moisture, melt temperature and residence time. Water consumes ester linkages in the PBT backbone, generating carboxylic acid and hydroxyl end groups. The resulting molecular weight reduction lowers melt viscosity and mechanical strength. The hydrolysis reaction becomes progressively faster as temperature rises from 250°C to 270°C; operation at the upper end of the melt-temperature window therefore requires stricter moisture control and shorter residence time. Published data for this specific configuration is limited for the exact kinetic constant, but industrial practice treats 0.02% residual moisture as the maximum safe level for ordinary cycles of 5–10 min. Mould temperature does not hydrolyse the melt, but higher mould temperatures in the 60–80°C range improve crystallisation and dimensional consistency. The practical equipment requirement is a desiccant-bed dryer with closed-loop regeneration, not a hot-air dryer. Hot-air drying alone cannot reach the required dew point and leaves sufficient moisture to degrade the melt.

    Connector and relay housing requirements in injection moulding

    Typical application areas include multi-pin connector bodies, sensor housings, relay bases, ignition coil bobbins, pump impellers and gear trims. In connector bodies, the property of interest is retention of terminal normal force after thermal cycling; the coefficient of linear thermal expansion is determined by ISO 11359-2. Terminal retention is usually validated under the relevant appliance standard, such as IEC 60512 for electrical connectors, rather than by tensile data alone. For relay bases, the 0.4% in-flow mould shrinkage improves pin-position accuracy after demoulding. In pump housings, short glass fibres improve creep resistance under clamp load, but immersion in hot alkaline cleaners above 85°C can hydrolyse the polyester; suitability should be confirmed under ISO 22088-2 or end-use media testing. The material is not intended for continuous load-bearing service above its deflection temperature under load. The UL94 HB rating is not equivalent to a flame-retardant barrier; components requiring vertical burn resistance should use a V-0 grade or additional shielding.

    When 5010G15 is compared with other products in the Novaduran range, the trade-off is between flow length, stiffness, surface quality and toughness. Unfilled 5010 has better melt flow and surface gloss but lower tensile modulus and much higher mould shrinkage. 5010G30 has higher tensile and flexural modulus, but lower melt flow and higher screw torque. For components with wall thickness below 1.2 mm, the 15% grade flows better than 30% glass-filled PBT, but maximum flow length is still lower than unfilled PBT. Published data for this specific configuration is limited for weld-line strength and multi-axial impact; these properties should be measured on prototype tools before production. The HB designation also differentiates 5010G15 from flame-retardant Novaduran grades that contain halogenated or phosphorus-based additive packages and that are used for electrical enclosures requiring V-0 performance.

    When replacing zinc or aluminium die castings, joint relaxation and thermal expansion mismatch require reappraisal

    When 5010G15 is used to replace zinc or aluminium die-cast housings, the tensile modulus of the polymer is significantly lower than the metal values, which changes load transfer in clamped joints. Moulded bosses must be designed with larger thread engagement and, if necessary, inserted metal bushings. Differential thermal expansion between the polymer and metal inserts creates residual stress; the coefficient of linear thermal expansion is approximately 5.0 × 10⁻⁵ K⁻¹ under ISO 11359-2, whereas aluminium is approximately 2.3 × 10⁻⁵ K⁻¹. This mismatch is accommodated by slotted holes or oversize clearances. Creep under clamp load is slower than unfilled PBT, but it remains finite; creep modulus values under ISO 899-2 should be requested for critical bolted joints. No galvanic corrosion occurs because the material is non-conductive; that removes the need for isolating washers used in metal-to-metal assemblies.

    Regulatory declarations are available from Mitsubishi Chemical. The grade can be supplied with a declaration that, to the manufacturer’s knowledge, the commercial product conforms to the substance restrictions in EU Regulation (EC) No 1907/2006 and the recast 2011/65/EU RoHS directive when used as supplied. A separate IEC 62474 declaration should be obtained for import documentation. No food-contact compliance under FDA 21 CFR or EU 10/2011 should be presumed from the HB classification. The material should be stored away from high-humidity environments; prior to moulding, any bag opened for more than 2 h should be returned to a desiccant dryer because PBT absorbs moisture rapidly at relative humidity above 60%.

    Top