Lyondellbasell Polyblak 4692 Premium Black Color Concentrate 35 Carbon Black Based In Lldpe

LyondellBasell POLYBLAK™ 4692 Premium Black Color Concentrate, 35% Carbon Black Based In LLDPE

    • Product Name: LyondellBasell POLYBLAK™ 4692 Premium Black Color Concentrate, 35% Carbon Black Based In LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 982317
    Product Name LyondellBasell POLYBLAK™ 4692 Premium Black Color Concentrate
    Manufacturer LyondellBasell
    Product Code POLYBLAK™ 4692
    Carbon Black Content 35%
    Carrier Resin LLDPE
    Form Pellets
    Color Black
    Density 1.10 g/cm³ (typical)
    Melt Flow Rate 20 g/10 min (190°C/2.16 kg, typical)
    Moisture Content <0.20% (typical)
    Let Down Ratio 2-5% (typical, application dependent)
    Compatibility Polyolefins
    Processing Methods Extrusion, injection molding, blow molding, film
    Carbon Black Dispersion Premium/Excellent
    Uv Protection Yes
    Thermal Stability Good

    As an accredited LyondellBasell POLYBLAK™ 4692 Premium Black Color Concentrate, 35% Carbon Black Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell POLYBLAK™ 4692 Premium Black Color Concentrate, 35% Carbon Black in LLDPE, supplied in 25 kg polyethylene bags.
    Container Loading (20′ FCL) 20′ FCL container loading: LyondellBasell POLYBLAK™ 4692 Premium Black Color Concentrate, 35% carbon black based in LLDPE, palletized for shipment.
    Shipping POLYBLAK™ 4692 ships as solid, non-hazardous LLDPE pellets in 25 kg bags or 1,000 kg bulk bags, palletized and stretch-wrapped. No special transport classification is required. Store dry, away from excessive heat, and handle using standard industrial hygiene. Follow the SDS and local regulations.
    Storage Store in a cool, dry, well-ventilated area in original, tightly closed containers. Protect from direct sunlight, moisture, heat, and ignition sources. Keep away from incompatible materials such as strong oxidizers. Avoid dust generation and contamination. Maintain good housekeeping; follow manufacturer’s SDS and local regulations. Use first-in, first-out stock rotation. Do not store near food, drink, or animal feed. Ensure containers are labeled.
    Shelf Life Shelf life is 24 months from manufacture when stored unopened in original packaging in a cool, dry area below 50°C.
    Application of LyondellBasell POLYBLAK™ 4692 Premium Black Color Concentrate, 35% Carbon Black Based In LLDPE

    In LLDPE blown film towers producing black agricultural mulch and silage wrap at thicknesses from 12 µm to 40 µm, POLYBLAK™ 4692 is introduced through gravimetric dosing at the feed throat. The product is a 35 wt% carbon black concentrate based in LLDPE. The typical let-down range for full opacity in a 25 µm film is 4.0 wt% to 6.0 wt%, which produces final carbon black content of 1.40 wt% to 2.10 wt%. Extrusion is maintained at melt temperatures of 190°C to 230°C, with die gap set between 1.5 mm and 2.2 mm. Blow-up ratio is held at 2.0:1 to 3.5:1. Carbon black modifies bubble thermal behaviour because the dark film absorbs more radiant heat from the die and surrounding air; frost line height must therefore be stabilised within a narrow band to avoid moving the bubble expansion zone into a region of higher crystallinity. A wandering frost line on black LLDPE film produces gauge bands, tear anisotropy in the machine direction, and inconsistent dart impact values. Screen pack pressure should be logged after each shift. A rise above 15 MPa at constant screw speed indicates carbon black agglomerate accumulation on the screen pack rather than polymer degradation, because the LLDPE carrier has a relatively narrow melt-viscosity shift across normal processing temperatures. Luminous transmittance of black agricultural film is verified by ASTM D1003 when a specification below 5% is required, while tensile properties are measured by ISO 527-3. Outdoor weathering acceptance is generally based on exposure protocols such as ISO 4892-2 or ASTM G154, not on carbon black content alone.

    Let-down ratios for POLYBLAK™ 4692 based on 35 wt% carbon black content
    Concentrate additionFinal carbon black contentTypical application category
    2.0 wt%0.70 wt%Injection-moulded dark grey articles with moderate UV demand
    3.0 wt%1.05 wt%Cast film, cable jacketing, and industrial wrap
    4.0 wt%1.40 wt%Black packaging film and thin containers
    5.7 wt%2.00 wt%Minimum carbon black loading for exposed polyethylene pipe
    6.0 wt%2.10 wt%Agricultural mulch and LLDPE geomembrane
    8.6 wt%3.01 wt%Maximum outdoor UV stabilisation in exposed sheet or pipe

    What limits let-down consistency in injection-moulded rigid packaging?

    When POLYBLAK™ 4692 is metered into LLDPE injection-moulded crates, bins, and non-food caps, the primary processing risk is not thermal degradation but gravimetric dosing error. Let-down below 2.0 wt% magnifies feeder variance. A 0.1 wt% deviation in concentrate addition translates into 0.035 wt% carbon black variation because the concentrate is only 35 wt% carbon black. Barrel temperatures on a reciprocating screw machine are set from 180°C to 230°C, with the nozzle held below 240°C to prevent black speck formation from degraded LLDPE. If storage ambient relative humidity exceeds 60%, pellets should be dried for 2 h at 75°C before processing. Moisture adsorbed on carbon black surfaces can produce splay streaks on black moulded surfaces, particularly near the gate. Screw back-pressure is held at 5–10 MPa and cushion is maintained at 5–10 mm; a short cushion transfers partially dispersed concentrate into the cavity and creates dark weld lines. Carbon black agglomerates above 10 µm remain visible as grey specks on textured tool surfaces, so dispersion must be checked on microtomed sections under transmitted light. Mechanical acceptance is based on ISO 527-2 tensile yield and ISO 180 notched impact at 23°C, but the required values are set by the article specification and not by the masterbatch alone. Food-contact use requires separate compliance review of the final moulded article under FDA 21 CFR 177.1520 for the olefin polymer base and, where applicable, FDA 21 CFR 178.3297 for colourant use. Published data for this specific concentrate in injection-moulded article qualification is limited, so laboratory confirmation of dispersion, mechanical retention, and migration is required before production release.

    When the concentrate is run on single-screw pipe extrusion lines with barrier screws of 30:1 L/D for LLDPE drip irrigation laterals and flexible black conduit, melt temperature should be held between 200°C and 220°C. Final carbon black content for outdoor UV stabilisation in exposed polyethylene pipe is generally 2.0 wt% to 3.0 wt%, requiring concentrate let-downs of 5.7 wt% to 8.6 wt%. Carbon black dispersion is assessed on microtomed sections according to ISO 18553 or the classification method in ASTM D3350-21. Agglomerate populations above the specified rating reduce dart impact resistance and may shorten slow crack growth life in pressurised piping. Die-head pressure at constant screw speed should be recorded; a steady increase greater than 10% across an 8 h batch signals screen pack plugging by carbon black agglomerates. A melt pump is preferred to isolate die flow from screw pressure surges, especially when thin-wall tubing is pulled at high line speed. Thermal stabiliser demand in carbon black pipe compounds is non-linear. The black particles can adsorb phenolic and phosphite stabilisers from the LLDPE matrix, altering oxidative induction time measured by ISO 11357-6 or ASTM D3895. The processor should verify that the final diluted compound retains the OIT required by the pipe specification after masterbatch addition. If final OIT falls below target, the base resin stabiliser package must be increased before adding black concentrate; increasing the let-down ratio alone will not restore oxidative stability.

    When carbon black content enters the 2.0–3.0 wt% window in LLDPE geomembrane sheet

    In LLDPE geomembrane sheet extruded through flat dies at thicknesses from 1.0 mm to 2.5 mm, POLYBLAK™ 4692 can be let down to achieve carbon black content within the 2.0–3.0 wt% envelope referenced by GRI-GM17. Direct addition on a single-screw flat-die sheet line requires a screw mixing section with sufficient dispersive shear; low-shear designs produce black streaks oriented in the machine direction because the 35 wt% concentrate is not fully redispersed. Melt temperature is set at 210°C to 240°C. Sheet opacity is not a substitute for dispersion rating. A microtomed sample must be examined under transmitted light at 100× and rated against the ISO 18553 procedure. Agglomerates larger than 25 µm are a visual defect in geomembrane because they can act as local stress concentrations during tensile elongation per ISO 527-3. Carbon black content in the final sheet can be confirmed by ASTM D1603 or thermogravimetric analysis. Oxidative induction time is the critical formulation boundary. Carbon black concentrates can reduce OIT by adsorbing phenolic and phosphite stabilisers from the LLDPE base polymer, so the final blend should be tested per ISO 11357-6 at 200°C in oxygen. If OIT drops below the geomembrane engineering specification, the resin stabiliser package must be increased before adding black concentrate. Recycled content in black geomembrane has been associated with wider OIT scatter and higher agglomerate counts, so incoming regrind and flake should be screened for metal contamination before blending with masterbatch.

    Dry pre-treatment of the concentrate becomes critical when transfer lines feed black LLDPE cable jacketing compounds into a crosshead extrusion line. Pellets exposed to humid air above 60% RH should be dried at 75°C for 2 h to 4 h, because moisture desorbed from carbon black surfaces creates micro-voids at the conductor interface during crosshead extrusion. In low-voltage outdoor cable sheathing, the concentrate is added at 3.0 wt% to 6.0 wt%, giving final carbon black contents of 1.05 wt% to 2.10 wt%. This range is selected for weathering resistance rather than electrical conductivity; the concentrate is not formulated as a semiconductive carbon black compound. Melt temperature is restricted to 190°C to 220°C to avoid thermal decomposition of the LLDPE carrier. Pressure at the breaker plate is monitored because poorly dispersed carbon black concentrates increase filtration pressure and alter melt flow distribution in the crosshead, producing uneven wall thickness. Jacketing compounds are tested for tensile properties per IEC 60811-501 and for oxidative ageing per IEC 60811-401; these standards apply to the complete compound after let-down and not to the masterbatch alone. If a cable jacket is intended for RoHS-registered markets, the compound must be evaluated under 2011/65/EU for restricted substances in the final jacket formulation, although carbon black itself is not a restricted substance.

    Cast film edge instability and masterbatch let-down control

    On high-output cast film lines making black stretch film and industrial overwrap, POLYBLAK™ 4692 is fed into an LLDPE matrix at let-downs of 3.0 wt% to 5.0 wt%. Melt temperature at the flat die is set at 220°C to 240°C. Edge thickening and draw resonance are more pronounced with carbon black concentrates because the filled melt has lower melt strength and higher extensional viscosity than natural LLDPE; edge pinning settings must be adjusted as let-down increases. Chill-roll temperature is held at 20°C to 30°C, and melt draw distance is kept below 25 mm to reduce neck-in. Carbon black particles in thin cast film can form die lip deposits after prolonged runs, so die lip cleaning intervals should be tied to optical quality inspection rather than fixed calendar hours. Film haze and transmittance are measured per ASTM D1003. A final carbon black content of 1.0 wt% to 1.75 wt% is typical for opaque industrial films, but exact values depend on film thickness and product specification. The cast film pile retains more heat when black film is wound at high tension; winding tension should be reduced by 10–15% relative to natural LLDPE to prevent blocking and roll telescoping.

    Free Quote

    Competitive LyondellBasell POLYBLAK™ 4692 Premium Black Color Concentrate, 35% Carbon Black Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell POLYBLAK™ 4692 Premium Black Color Concentrate, 35% Carbon Black Based In LLDPE, is identified as a high-loading black masterbatch consisting of a nominal 35% by weight carbon black content dispersed in a linear low-density polyethylene carrier resin. The product is intended for polyolefin conversion processes in which the concentrate is metered into natural or pre-compounded polyolefin at a controlled ratio. The LLDPE carrier is a defining formulation variable because it influences melt-viscosity matching, seal performance, and dilution effects in LLDPE-rich film, extrusion coating, and injection moulding applications. Product-specific and lot-specific numerical data are not reproduced here; the manufacturer’s technical data sheet should be consulted for measured values. The present text identifies the test methods, processing boundaries, and comparative factors relevant to this class of carbon black concentrate.

    What limits practical addition rates for a 35% carbon black concentrate in blown film extrusion?

    In blown film extrusion, the practical let-down ratio is controlled by target optical density, film gauge, and the concentrate’s viscosity relative to the base resin. General industrial practice for carbon black concentrates in LLDPE spans addition rates of 2% to 6% by weight, but published data for POLYBLAK™ 4692 in a specific film structure is limited. At low addition rates, colour strength may be insufficient for light-blocking or weathering-critical applications. At high addition rates, the carrier resin contributes to the total melt stream and can alter crystallisation kinetics, tear properties, and sealing behaviour of the finished film. After each let-down change, simultaneous monitoring of melt temperature, die pressure, film appearance, and optical density is required.

    The higher melt viscosity of a 35% carbon black concentrate relative to neat LLDPE is a significant processing constraint. Capillary rheometry per ISO 11443 or melt mass-flow rate testing per ASTM D1238/ISO 1133-1 is used to characterise the carrier and compound, but single-point laboratory data do not fully predict shear-thinning behaviour in a grooved-feed extruder. Dispersion quality should not be judged visually alone; filter pressure value testing according to EN 13900-3 or a laboratory pressure-rise test provides a more objective indication of carbon black agglomerate loading and screen pack blocking tendency.

    On production-scale blown film lines with single-screw extruders of 25:1 to 30:1 L/D and general-purpose polyolefin screws, batches with equivalent carbon black loading can show measurable differences in filter pressure value because of carbon black grade selection and pellet geometry. Pellet geometry is not captured by melt flow rate but affects feed throat stability. If pellets are metered through a side-port blender into a hopper, inconsistent pellet size distribution can create short-term let-down ratio variation, observed as oscillating opacity in thin film. The condition is corrected by sieve analysis or by use of positive-displacement pellet feeders rather than purely volumetric auger metering. In injection moulding, clamp force is not usually the limiting factor with this concentrate class, but plasticising rate, melt cushion stability, and surface appearance require adjustment after masterbatch addition. Moulders commonly evaluate these parameters when adding masterbatch at 2% to 4% by weight; supplier-specific guidance for POLYBLAK™ 4692 may be required for a given part and machine combination.

    Dispersion Mechanisms, Carbon Black Aggregate Morphology, and Test Method Selection

    The term premium black color concentrate refers to a combination of carbon black grade, dispersion quality, and lot-to-lot consistency rather than to a single physical property. Carbon black aggregates in a 35% loaded LLDPE carrier are subjected to dispersive and distributive mixing in the melt. High-shear twin-screw compounding achieves primary dispersion based on specific energy input and residence time distribution. In downstream single-screw processing, the objective is to preserve existing dispersion rather than to perform primary dispersion. Carbon black loading of 35% by weight is high enough that the masterbatch itself is not optically evaluable without dilution; meaningful colour and opacity measurements are made after let-down into a defined base resin.

    Dispersion quality may be evaluated by optical microscopy on pressed films according to ISO 18553, by filter pressure value according to EN 13900-3, or by surface roughness measurement after extrusion. A low filter pressure value generally indicates fewer large agglomerates, but absolute values are equipment-specific. Mesh size, extruder diameter, throughput, and test temperature must be specified before comparing filter pressure values between laboratories. A specification sheet for POLYBLAK™ 4692 should therefore state the test method version and screening conditions rather than reporting a single unqualified number.

    Carbon black influences optical properties through both absorption and scattering. For black masterbatch intended for film, relevant post let-down measurements include total luminous transmittance per ISO 13468, blackness coordinates L*, a*, b* per ISO 7724-2, and contrast ratio when evaluated over white and black substrates. For weathering-critical applications, the contribution of carbon black to UV absorption is not equivalent to a stabiliser package; polyolefin formulations may still require hindered amine light stabilisers and phenolic antioxidants. The LLDPE carrier can also affect seal initiation temperature and hot-tack behaviour when the concentrate is used at elevated addition levels. Comparative testing using ASTM F1921 for hot tack and ASTM F88/F88M for seal strength is necessary when the base resin is an LLDPE-rich formulation. Carbon black concentrates based in LLDPE generally show better compatibility with octene- or hexene-based LLDPE than with LDPE in terms of melt-viscosity match, but this compatibility statement is not a substitute for matching melt-flow and shear-thinning behaviour between concentrate and base resin.

    When Carrier Resin Choice Causes Property Trade-Offs in LLDPE-Dominated Articles

    If the base resin is an LLDPE with a density below 0.925 g/cm³, addition of a 35% carbon black LLDPE concentrate may produce a smaller viscosity mismatch than a concentrate based on LDPE or EVA. The degree of mismatch is evaluated by comparing melt flow ratios or by capillary rheometry across the shear rate range of the target process. In cast film extrusion, shear rates may exceed 1000 s-1; in blow moulding, shear rates are considerably lower. A masterbatch that disperses well at low shear may exhibit die-lip build-up or micro-gels in high-shear processes if the carrier resin has insufficient thermal stabilisation. Conversely, a concentrate with a low-viscosity carrier may lower melt pressure but can produce striping or poor colour uniformity in single-screw extrusion because it reduces the shear available for dispersion.

    The selection of POLYBLAK™ 4692 over a commodity black concentrate is generally based on lot-to-lot consistency, carbon black grade, and dispersion characteristics, not on carbon black loading alone. The difference between a premium concentrate and a general-purpose concentrate is frequently detected only through filter pressure value, spectrophotometric blackness after a standardised let-down, or film appearance rating after a fixed extrusion time. A specification of 35% carbon black loading does not by itself guarantee optical jetness or dispersion. Two concentrates with identical nominal loading can differ in aggregate size distribution, volatile content, and surface treatment.

    Potential process conflicts arise when the masterbatch is combined with resins containing high levels of slip or antiblock additives. Carbon black can adsorb some processing additives and alter the coefficient of friction of the finished film. Coefficient of friction should be re-evaluated per ASTM D1894 or ISO 8295 after the concentrate is added at the intended let-down ratio. The interaction is concentration-dependent and may not be detectable at 2% addition but may become significant above 4%.

    Storage of carbon black concentrates in LLDPE requires attention to moisture uptake and contamination. Carbon black can adsorb moisture and volatile organic compounds; the LLDPE carrier is not highly hygroscopic, but condensation on cold pellets during warehouse-to-plant transfer can produce surface moisture. In film extrusion, surface moisture may cause bubbles, die lines, or optical defects. Pre-drying is often unnecessary when packaging remains sealed, but if bags are opened in relative humidity above 60%, a drying step may be required before processing. The exact drying temperature and duration for POLYBLAK™ 4692 should be obtained from the supplier’s handling instructions rather than from generic LLDPE guidelines, because carbon black surfaces can retain moisture and affect moisture analysis by ISO 15512. The product should be stored in a clean, dry area away from direct sunlight. Carbon black is a combustible dust; facilities should observe the relevant housekeeping and grounding practices under NFPA 652 when handling bulk material.

    Compliance reference Applicability Limitation or required confirmation
    REACH Regulation 1907/2006 Carbon black registration and mixture communication obligations SDS and end-use restrictions must be confirmed with the supplier
    EU RoHS Directive 2011/65/EU Electrical and electronic equipment materials Product-level compliance with Annex II substance limits should be confirmed
    FDA 21 CFR 178.3290 Colourants for polymers used in food-contact articles Not a blanket approval; applicable only within specified conditions and end uses
    EU 10/2011 Plastics intended for food contact Overall migration and specific migration limits require material-specific certification
    ISO 9001:2015 Quality management system Indicates manufacturing consistency, not product performance

    Melt Temperature, Shear Heating, and Screen Pack Selection Govern Concentrate Performance

    The concentrate should be metered into the main feed throat rather than into a downstream side port unless the system is specifically designed to incorporate pre-melted masterbatch into the main melt. Feed-throat addition maximises residence time for distributive mixing. The barrel temperature profile should match the melting behaviour of the carrier and base resin; for LLDPE-based systems, typical flat profiles are in the range of 190 °C to 230 °C for blown film and 200 °C to 250 °C for injection moulding, but these values are machine-dependent. Processing above 260 °C can accelerate polyethylene degradation and increase the risk of crosslinked gels, particularly in long residence time sections.

    Screen pack and breaker plate selection is important because carbon black concentrates may contain agglomerates or incidental contaminants. Melt filtration with mesh sizes from 80 to 250 µm is common in film extrusion. Finer mesh can cause rapid pressure increases if the concentrate has a high filter pressure value. In cast film and sheet, continuous screen changers are preferred because they allow operation at higher contamination levels without frequent shutdowns. Monitoring pressure differential across the screen pack provides early indication of carbon black agglomerate accumulation. A gradual pressure rise is normal; a sudden pressure increase typically indicates a broken screen or a foreign contaminant rather than normal masterbatch behaviour.

    Compared with a 40% carbon black masterbatch in LDPE, a 35% loading in LLDPE generally requires a slightly higher let-down ratio to reach the same visual opacity, but the LLDPE carrier may introduce less modification of the base resin mechanics in LLDPE-rich formulations. Compared with a 25% carbon black concentrate in LLDPE, the 35% grade offers higher pigment concentration and may reduce total carrier resin addition, but it also demands greater shear energy for dispersion and may be more sensitive to screen pack blockage. Electrical conductivity is not an intended property of this concentrate; if antistatic or conductive performance is required, surface resistivity per ASTM D257 or IEC 62631-3-2 must be evaluated before use.

    Top