| HS Code | 757494 |
| Carbonblackcontent | 50% |
| Carrierresin | LLDPE |
| Color | Black |
| Form | Pellets |
| Density | 1.15 g/cm³ |
| Meltflowrate | 1.5 g/10 min (190°C/2.16 kg) |
| Moisturecontent | <0.2% |
| Ashcontent | 50% |
| Pelletsize | 3 mm |
| Bulkdensity | 0.65 g/cm³ |
| Volatiles | <0.5% |
| Dispersion | <15 µm |
| Lightfastness | 8 |
| Uvstabilization | Yes |
| Thermalstability | >250°C |
| Recommendedadditionlevel | 2-6% |
| Processingtemperature | 180-260°C |
| Compatiblepolymers | Polyolefins |
As an accredited LyondellBasell POLYBLAK™ 4676 Black Color Concentrate, 50% Carbon Black Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell POLYBLAK™ 4676 Black Color Concentrate is packaged in 25 kg polyethylene bags, with 40 bags per pallet (1,000 kg). |
| Container Loading (20′ FCL) | 20′ FCL: LyondellBasell POLYBLAK™ 4676 Black Color Concentrate, 50% carbon black in LLDPE, palletized, shrink-wrapped, securely loaded for ocean transport. |
| Shipping | POLYBLAK™ 4676 Black Color Concentrate is shipped as non-hazardous solid pellets in moisture-resistant bags, boxes, or octabins on pallets. It is not classified as dangerous goods for transport. Store dry, cool, and protected from UV/contamination. Handle with standard industrial hygiene; avoid dust. Follow applicable local and international regulations. |
| Storage | Store at ambient temperature in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep original containers tightly closed to prevent moisture pickup and contamination. Stack pallets securely and avoid excessive loads. Maintain good housekeeping to minimize dust. Keep separate from strong oxidizers. Follow local regulations and the manufacturer’s SDS for safe handling and storage. |
| Shelf Life | Shelf life is typically two years when stored unopened in original packaging under cool, dry conditions, away from direct sunlight. |
In high-UV agricultural mulch and silage cover film extrusion, LyondellBasell POLYBLAK™ 4676, a 50% carbon black color concentrate in an LLDPE carrier, is metered into LLDPE or LDPE at a let-down ratio of 3 wt% to 6 wt%, producing a final carbon black mass fraction of 1.5 wt% to 3.0 wt% and the opacity required to suppress weed germination. Compliance for this segment is assessed against EN 13206 for agricultural film mechanical properties and weathering durability, while carbon black dispersion is verified by ASTM D5596; a rating of 3 or better is commonly specified to prevent UV-shielding weak spots. The production route on a single-layer or coextruded blown film line uses a barrier screw with L/D of 30:1 and a die gap of 1.8 mm to 2.4 mm; the carbon black concentrate is introduced through a gravimetric hopper feeder after the main resin feed throat, and melt temperatures are held within 190 °C to 230 °C to limit thermal degradation of the LLDPE carrier while maintaining bubble stability. When the concentrate is fed without side-stream mixing, carbon black agglomerates appear as fisheyes and reduce dart impact strength at thinner gauges. Terminated products include black mulch films, silage cover films, and light-deprivation greenhouse films.
The dispersion rating of carbon black in a finished geomembrane is not a cosmetic property; it controls heat-wedge and hot-air weld continuity at the overlap. The concentrate is added at 4 wt% to 6 wt% to yield 2.0 wt% to 3.0 wt% carbon black in the sheet, a range consistent with GRI-GM13 specification for HDPE geomembrane and the dispersion evaluation methods ASTM D5596 and ISO 18553. In flat die extrusion, the base LLDPE or MDPE is combined with the concentrate in a compounding screw or coextrusion feed block, processed through a melt pump at 220 °C to 250 °C, and pulled from a 2.0 mm to 3.0 mm polished roll nip. Poorly dispersed agglomerates above rating 3 create local carbon-rich domains that resist fusion during wedge welding, producing channel leaks detectable only by vacuum box or spark testing per ASTM D6392. Because the concentrate contains 50% carbon black, a feeder calibration error of 1 wt% changes final carbon black content by 0.5 wt%, sufficient to shift the sheet from specification into a rejected lot. Sheet thickness variation across the die width directly influences wedge-weld heat transfer; line operators monitor roll nip gap and die bolt adjustment to keep gauge uniform. Terminal products include landfill liner, pond liner, and secondary containment sheets.
Pressure pipe compounders running PE80 and PE100 grades must reconcile two opposing constraints: the final carbon black mass fraction must remain within 2.0 wt% to 2.5 wt% as required by ISO 4427-1 and EN 12201-1, while the addition of an LLDPE carrier must not create an unacceptable shift in slow crack growth resistance. A let-down ratio of 4 wt% to 5 wt% of the 50% carbon black concentrate delivers the target carbon black loading; carbon black content is verified by ISO 6964, and dispersion is rated by ISO 18553 or ASTM D5596. On a grooved-feed single-screw pipe extruder with L/D of 36:1, the carbon black concentrate is pre-blended with natural PE100 granules in a gravimetric batch mixer before entering the feed throat, then melt filtered through a screen pack of 80 mesh and shaped through a spiral mandrel die. Screen pack pressure increases when carbon black agglomerates accumulate, forcing more frequent filter changes than the same natural pipe compound. Routine incoming resin quality checks include melt flow rate comparison per ISO 1133-1 between natural PE100 and the carbon black concentrate to detect carrier-related rheological drift that could alter pipe wall thickness control. Terminal products are water distribution mains, gas distribution pipe, and mining slurry lines where outdoor storage demands UV stabilization.
| Application sector | Standard or test method | Numeric requirement relevant to 50% carbon black concentrate |
|---|---|---|
| Agricultural film | EN 13206; ASTM D5596 | Final carbon black 1.5–3.0 wt%; dispersion rating ≤ 3 |
| Geomembrane | GRI-GM13; ASTM D5596; ISO 18553 | Final carbon black 2.0–3.0 wt%; dispersion rating ≤ 3 |
| Pressure pipe | ISO 4427-1; EN 12201-1; ISO 6964 | Final carbon black 2.0–2.5 wt%; dispersion grade per ISO 18553 |
| Injection moulding | EU No 10/2011; FDA 21 CFR 178.3290; RoHS 2011/65/EU | Migration limits per food-contact category; heavy metals below RoHS thresholds |
| Rotomoulding | FDA 21 CFR 177.1520; EN 13575 | Final carbon black 1.5–2.5 wt%; wall thickness tolerance per EN 13575 |
| Cable jacket | IEC 60502-1; UL 1581; ASTM D1248 | Final carbon black 1.0–2.5 wt% for UV; insulation resistance retained |
On high-clamp-force injection moulding cells producing nestable logistics crates and pallet boxes, the concentrate is metered at 2 wt% to 4 wt%, giving 1.0 wt% to 2.0 wt% carbon black in the moulded part. This lower loading is sufficient for opacity and uniform surface color but not for long-term outdoor UV resistance, so exterior exposure specifications must be verified separately. Food-contact moulded articles fall under EU No 10/2011 and FDA 21 CFR 178.3290 for colorants in polymers, while electrical/electronic enclosures require conformity to RoHS 2011/65/EU heavy-metal limits. The injection moulding process on a machine with clamp force from 2,000 kN to 6,000 kN uses barrel temperatures of 200 °C to 240 °C and a back pressure of 0.5 MPa to 1.0 MPa to disperse the carbon black without oxidizing the LLDPE carrier; the moulded products are stackable crates, industrial waste containers, and black closures for chemical pails.
Low-shear rotational moulding exposes the same concentrate to a completely different mixing environment than a twin-screw compounding extruder. The recommended addition is 3 wt% to 5 wt%, yielding 1.5 wt% to 2.5 wt% carbon black in a roto-grade LLDPE or MDPE wall. Compliance for potable water and chemical storage tanks draws on FDA 21 CFR 177.1520 for the olefin polymer wall and EN 13575 for thermoplastic tanks above-ground storage. Production uses a biaxial rotational moulding machine with a peak internal air temperature of 190 °C to 210 °C and a mould rotation ratio of 4:1; the carbon black concentrate is dry-blended with 35-mesh pulverized base resin because melt mixing is absent, and any agglomerate that survives as a visible speck larger than 50 μm becomes a potential moisture path or surface defect in the tank wall. The density difference between the 50% concentrate and pulverized base resin can cause segregation during mould charging; a high-intensity paddle mixer is used immediately before filling to reduce batch-to-batch color variation. Published data for POLYBLAK™ 4676 in roto-grade LLDPE are limited; validation on the specific pulverized base resin is required before production release. Finished types include vertical water storage tanks, underground cisterns, and acid-neutralizing sump tanks.
In thermoplastic polyethylene cable jackets, carbon black loading is specified for ultraviolet resistance, not aesthetic color depth. The concentrate is added at 2 wt% to 5 wt%, resulting in 1.0 wt% to 2.5 wt% carbon black in the outer sheath; this range protects against embrittlement in sunlight while retaining the insulation resistance values required by IEC 60502-1 and the mechanical and flame tests of UL 1581. The production process on a single-screw extruder with a crosshead die imposes higher melt viscosity than blown film, so the LLDPE carrier is processed at 180 °C to 220 °C and the carbon black concentrate is fed through a gravimetric loss-in-weight feeder at the feed throat to avoid carbon black accumulation on the screw root. For crosslinked polyethylene jackets, the concentrate should be reviewed for peroxide compatibility because carbon black can adsorb organic peroxide, shifting crosslink density; ASTM D1248 material classification for wire and cable polyethylene provides the baseline for finished compound validation. On high-speed sheathing lines, online spark testing per IEC 60502-1 detects jacket faults caused by carbon black agglomerates, and insulation resistance tests are repeated on finished cable lengths to confirm that the carbon black does not create leakage paths. Terminal products include medium-voltage cable outer sheaths, telecommunications duct, and outdoor low-voltage aerial cable jackets.
Competitive LyondellBasell POLYBLAK™ 4676 Black Color Concentrate, 50% Carbon Black Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell POLYBLAK™ 4676 is a black color concentrate compounded with a nominal carbon black loading of 50% by mass in a linear low-density polyethylene carrier. The formulation is supplied as pelletized concentrate intended for metered dilution into natural polyethylene streams; it is not a ready-to-use moulding compound. The LLDPE carrier selection reduces melt-index mismatch when the concentrate is let down into LLDPE-based blown film, cast film, or extrusion coating lines. A final carbon black concentration of 1.0% by mass is achieved by adding 2.0 kg of concentrate per 100 kg of total blend. The mass-balance calculation assumes all carbon black is contained in the concentrate and that no carbon black is lost through feeder spillage or purge. Incoming lot verification for carbon black content may be performed by ASTM D1603, while melt flow rate is typically determined under ASTM D1238 or ISO 1133-1:2022 using a 2.16 kg load at 190 °C. Certificate-of-analysis values for moisture, ash, and bulk density should be consulted for lot-specific limits because these values vary with carbon black morphology and pelletizing conditions. No anti-block, slip, or ultraviolet-stabilizer additive package is implied by the product designation; additive compatibility must be confirmed before combining POLYBLAK™ 4676 with additive masterbatches containing amine-based stabilisers, which may interact with carbon black surfaces at elevated processing temperatures.
Carbon black dispersion failure in thin-gauge LLDPE film made with a 50% concentrate typically appears as visible specks, pinholes, or gel-like defects. The concentration of carbon black in the carrier is high enough that the masterbatch itself should not be added directly to the throat of a low-shear single-screw extruder without a mixing section. Blown film lines running at die gaps below 0.8 mm are especially sensitive to undispersed agglomerates because film draw-down amplifies particle dimensions. ISO 18553:2002, Method A, provides a microscopic rating system for pigment dispersion in polyolefin compounds; a rating of ≤3 is commonly used as an internal acceptance limit for film converters, although the exact limit depends on the final film optical density and surface quality specification. Filtration pressure rise across a screen pack can provide an inline indication of agglomerate loading. A screen pack of 60/120/60 mesh is often installed at the breaker plate, but the pressure-drop limit depends on the extruder thrust bearing and clamp design. On lines where screen pack pressure exceeding 25 MPa forces premature screen changes, a more open screen pack or a continuous melt filter should be considered. Melt temperature upstream of the die should remain within the supplier-specified range for the LLDPE carrier; typical LLDPE extrusion temperatures fall between 190 °C and 240 °C. Temperatures above 250 °C can initiate oxidation of the carrier and increase the risk of carbon black reagglomeration at long residence times.
On a single-screw extruder with a barrel length-to-diameter ratio of at least 24:1, the concentrate should be metered downstream of the main resin feed but upstream of the compression zone. A Maddock or barrier mixing section can improve dispersion if the melt seals are not overfilled; excessive mixing-section length can raise melt temperature through frictional work and reduce output. Gravimetric feeders are preferred for addition rates below 2% because volumetric screw feeders can lose accuracy with low bulk density and pellet geometry variations. Feeder calibration should use the actual dry bulk density of the concentrate rather than the bulk density of natural resin. The screw speed range of the feeder should be selected so that the target addition rate falls between 20% and 80% of the maximum screw speed; operation below 20% can produce pulsating feed and inconsistent dilution. Blown film processors may preblend POLYBLAK™ 4676 with natural LLDPE using tumble or gravimetric blenders; if tumble blending is used, pellet segregation can occur because the concentrate pellets have a higher bulk density than natural LLDPE pellets due to carbon black loading. Periodic blend uniformity checks by carbon black content or melt flow rate are recommended on production lots.
Direct replacement of a 25% or 40% carbon black concentrate with POLYBLAK™ 4676 changes the letdown ratio and the amount of carrier resin introduced into the final compound. For a fixed final carbon black loading of 0.5%, a 25% concentrate requires 2.0 kg per 100 kg total blend; a 50% concentrate requires only 1.0 kg. The reduction in carrier resin can be advantageous when minimising rheological alteration of the base resin, but it also means that the mixing volume available to distribute carbon black is smaller. In practice, this places greater dispersion demand on the mixing sections of the main extruder, particularly at final loadings above 1.5%. The following mass-balance comparison may be used for production set-up.
| Final carbon black target (wt%) | POLYBLAK™ 4676 addition (kg per 100 kg blend) | 25% concentrate addition (kg per 100 kg blend) |
|---|---|---|
| 0.5 | 1.0 | 2.0 |
| 1.0 | 2.0 | 4.0 |
| 1.5 | 3.0 | 6.0 |
| 2.0 | 4.0 | 8.0 |
Because feeder turn-down ratios and screw diameter determine minimum flow accuracy, a change from 2.0 kg to 1.0 kg per 100 kg may move the feeder too near its lower authority if the feeder was sized for a low-loading concentrate. A loss-in-weight feeder with an accuracy of ±0.25% of full scale is generally specified for these duty points. The higher carbon black concentration also influences pellet hardness and abrasion; pellet dust generated during pneumatic conveying may accumulate in filters and can create carbon black build-up on hopper loaders. When comparing products, users should note that the LLDPE carrier in POLYBLAK™ 4676 distinguishes it from LDPE-carrier black concentrates of similar loading. An LDPE carrier may be preferred where broader compatibility with HDPE and LLDPE is desired, but LLDPE carrier provides greater melt elongation compatibility in LLDPE film structures and may reduce the incidence of carrier-induced gel particles in high-strength film lines.
Quality control on the diluted compound should include melt flow rate according to ASTM D1238 or ISO 1133-1:2022, tensile testing according to ASTM D638 or ASTM D882 as appropriate for the article, and carbon black dispersion evaluation according to ISO 18553. For food-contact packaging, compliance is not automatically conferred by the use of a specific masterbatch; the final article must meet the applicable positive-list and migration requirements of 21 CFR 178.3297 or Commission Regulation (EU) 10/2011. In electrical and electronic applications, the pigment and carrier matrix must be evaluated against the RoHS Directive 2011/65/EU restricted substances. The following test method matrix is used for routine batch release documentation.
| Property | Standard designation |
|---|---|
| Carbon black content | ASTM D1603 |
| Melt flow rate | ASTM D1238 / ISO 1133-1:2022 |
| Density | ASTM D1505 / ISO 1183-1:2019 |
| Moisture content | ASTM D6869 / ISO 15512 |
| Pigment dispersion | ISO 18553 |
Viscosity mismatch between POLYBLAK™ 4676 and the base resin can influence screw plastication and melt temperature. LLDPE carriers have lower zero-shear viscosity than HDPE carriers at equivalent melt index; this property generally favours compatibility with LLDPE film resins but may require line adjustments when the concentrate is used at addition levels above 5% in extrusion coating grades. The carbon black aggregates increase the storage modulus and low-shear viscosity of the melt. In screen pack filtration studies on resin systems with high carbon black loading, the pressure drop across a 100 mesh screen can show a nonlinear increase as the melt flow rate decreases. Processors should record screen pack pressure at the start of the run and after each screw-speed change. A pressure rise of more than 1.0 MPa per hour at constant throughput often indicates excessive agglomerate loading or fines accumulation. Regrind from black film that contains POLYBLAK™ 4676 can be re-extruded into LLDPE film, but regrind levels above 20% may require re-evaluation of tensile properties and film gauge uniformity depending on the number of heat histories. The reused carbon black-containing regrind should be evaluated for oxidation induction time or melt flow drift because the carbon black surface can adsorb stabilisers and alter long-term heat aging behaviour. When comparing carrier systems, a PP-carrier black concentrate is not recommended for use in LLDPE-rich film where PP gel particles would be visible; an EVA-carrier concentrate may be selected for polar seal layers or adhesive applications, but it can introduce vinyl acetate-dependent odour and melt stability limits.
Processors qualifying POLYBLAK™ 4676 for agricultural film, geomembrane, stretch wrap, or opaque packaging should validate final film performance with ASTM D882 for tensile properties, ASTM D1709 for dart impact, and ASTM D1003 for optical haze if the film is not intentionally opaque. The concentrate is not represented as a conductive compound; surface resistivity under ASTM D257 should not be assumed unless a specific conductive grade is specified in the certificate of analysis. Store the concentrate in unopened packaging at temperatures below 50 °C and protected from direct sunlight. If condensate forms on the pellet surface, dry at 70 °C to 80 °C for 2 h to 4 h in a desiccant dryer before processing.