Lyondellbasell Polyblak 4669 Premium Conductive 35 Carbon Black Concentrate Based In Lldpe

LyondellBasell POLYBLAK™ 4669 Premium Conductive 35% Carbon Black Concentrate Based In LLDPE

    • Product Name: LyondellBasell POLYBLAK™ 4669 Premium Conductive 35% Carbon Black Concentrate Based In LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 120363
    Productname LyondellBasell POLYBLAK™ 4669 Premium Conductive 35% Carbon Black Concentrate Based In LLDPE
    Manufacturer LyondellBasell
    Grade POLYBLAK 4669
    Producttype Carbon Black Concentrate
    Carrierresin LLDPE
    Carbonblackcontent 35%
    Form Pellets
    Color Black
    Density 1.17 g/cm³
    Meltflowrate 20 g/10 min (190°C/2.16 kg)
    Moisturecontent <0.10%
    Bulkdensity 0.60 g/cm³
    Pelletsize 2-3 mm
    Volatiles <0.5%
    Conductivity Conductive
    Thermalstability >250°C
    Odor Mild
    Recommendedletdownratio 1:1 to 1:2 (concentrate:base)

    As an accredited LyondellBasell POLYBLAK™ 4669 Premium Conductive 35% Carbon Black Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell POLYBLAK 4669 comes in 25 kg polyethylene bags, palletized and stretch-wrapped, with 1,000 kg bulk bags available.
    Container Loading (20′ FCL) Container Loading (20′ FCL): LyondellBasell POLYBLAK™ 4669 Premium 35% conductive carbon black concentrate in LLDPE; palletized, dry, securely stowed for shipment.
    Shipping LyondellBasell POLYBLAK™ 4669 ships as non-hazardous solid pellets, typically in 25 kg moisture-barrier bags, octabins, or bulk bags on pallets. Standard truck, rail, or sea freight applies; no special DOT/IMDG/ADR classification. Keep dry, cool, and away from direct sunlight or ignition sources.
    Storage Store LyondellBasell POLYBLAK™ 4669 indoors in a cool, dry, well-ventilated area in tightly closed original containers. Keep away from direct sunlight, heat, ignition sources, moisture, and contaminants. Place on pallets, not directly on floors. Avoid dust generation and static discharge. Ensure containers are labeled, inspected, and protected from damage. Follow FIFO, observe shelf-life, and maintain good housekeeping.
    Shelf Life Shelf life: 12 months from manufacture when stored unopened in original packaging at room temperature, dry, away from direct sunlight.
    Application of LyondellBasell POLYBLAK™ 4669 Premium Conductive 35% Carbon Black Concentrate Based In LLDPE
    The blown-film conversion of electrostatic discharge (ESD) protective outer packaging for moisture-barrier-laminated semiconductor component bags proceeds by gravimetric dosing of POLYBLAK™ 4669 Premium Conductive 35% Carbon Black Concentrate Based In LLDPE into clean-slate linear low-density polyethylene (LLDPE) having melt flow index between 1.0 g/10 min and 2.3 g/10 min determined under ISO 1133-1:2022 at 190°C with 2.16 kg load. Three-layer coextrusion blown film lines fitted with grooved-barrier feed screws of L/D 30:1 to 36:1, spiral mandrel dies having annular die gaps from 1.8 mm to 2.4 mm, and dual-lip air rings operating at blow-up ratios between 2.5:1 and 3.5:1 are deployed for this application. The masterbatch is introduced exclusively into the two skin layers via side-feeder gravimetric stations at letdown ratios of 25-35 wt%, generating carbon black loading of 8.75-12.25 wt% within those layers and 5.25-7.00 wt% across the aggregate three-layer structure. Surface resistivity of the resulting 50-100 μm films measured per ASTM D257-14(2021) at 23 ± 2°C and 12 ± 3% RH with electrode and sample preconditioning per ANSI/ESD STM11.11-2021 is specified within 10³-10⁵ Ω/sq. Pre-drying of the masterbatch in dehumidified-air hopper dryers at 80°C for 2-4 hours with dew point below -40°C is mandatory when ambient relative humidity exceeds 60%; carbon black-bound moisture exceeding 0.15 wt% produces surface porosity and interfacial delamination at the film laminate bond line during downstream barrier-lamination stages.The wicketed films emerging from the collapsing frame and haul-off nip undergo secondary lamination with 12 μm aluminium foil and 12 μm polyester barrier layers on a solventless adhesive laminator operating at line speeds between 150 m/min and 220 m/min. Peel strength at the conductive PE sealant-to-foil interface tested per ASTM F904-16 must typically exceed 4.5 N/15 mm to qualify the lamination for vacuum pouch fabrication. Process conflict data from production lines reveals that attempts to raise melt temperature above 230°C in the die zone to improve adhesion trigger thermo-oxidative degradation of the carbon black surface, producing polar oxygen-containing functional groups that disrupt particle-particle contact resistance and cause surface resistivity drift of up to two orders of magnitude over 14-day ambient shelf ageing. End products manufactured under this configuration include ESD barrier bags for PCB array packaging, side-gusseted Faraday cage pouches for disk drive components, and pallet-top shrouds tested for charge decay per IEC 61340-5-1 clause 5.3.3 with initial 1000 V charge decaying to less than 100 V within 2 seconds measured at 12% RH. The formulation gradient table below consolidates representative letdown-to-resistivity relationships reported in manufacturer technical bulletins for 35% carbon black masterbatches compounded into LLDPE carriers.
    Masterbatch letdown (wt%)Final carbon black loading (wt%)Surface resistivity range (Ω/sq) per ASTM D257-14(2021)Application classification
    155.2510⁷-10⁹Static dissipative
    258.7510⁴-10⁶Conductive ESD
    3512.2510²-10⁴Low-resistivity conductive
    4515.7510¹-10³Highly conductive

    When Non-Metallic Intermediate Bulk Containers Are Deployed in Flammable Solvent Transfer Duty

    Non-metallic intermediate bulk containers (IBCs) and liner inserts deployed for transfer of flammable solvents with flash points below 23°C must satisfy surface resistance limits specified in IEC 60079-0 clause 26.13, which mandates a measured value not exceeding 10⁹ Ω at 50 ± 5% RH when the part is intended for installation within Group II explosive atmosphere equipment categories. Injection molding of conductive LLDPE IBC inner bottles using the masterbatch at letdown ratios between 30 wt% and 40 wt% produces final carbon black concentrations of 10.5-14.0 wt%, yielding surface resistivity values of 10²-10⁵ Ω/sq under ASTM D257-14(2021) at 23°C and 50% RH. The molding operation employs reciprocating-screw injection machines with clamp force between 1200 kN and 2500 kN, volumetric dosing of the masterbatch via throat-mounted auger feeders, and melt temperatures maintained between 210°C and 225°C measured at the nozzle. The critical process constraint in this application is flow-length conductivity decay: at effective melt travel distances exceeding 300 mm from the gate, regions of the container wall frequently exhibit surface resistivity elevated by two to three orders of magnitude relative to the near-gate zone owing to orientation-induced interruption of the carbon black conductive network along the frozen skin layer.Compensation strategies implemented on production lines include increasing nominal wall thickness from 2.5 mm to 3.5 mm, reducing injection velocity in the final 12% of volumetric fill to permit conductive network reformation during the packing phase, and relocating gates to shorten the longest flow path to below 220 mm. Thickness increases above 4.0 mm are generally avoided because the elevated thermal conductivity of carbon black compounds accelerates heat removal uniformity but prolongs cycle time to the extent that per-unit energy cost exceeds acceptable thresholds for commodity IBC production. The compliance testing programme for finished containers includes surface resistance measurement per IEC 60079-0 clause 26.13 with concentric ring electrode configuration per IEC 60079-32-2, volume resistivity measurement per ASTM D4496-21, and charge decay evaluation per IEC 61340-5-1 Annex B using ±1000 V applied potential with decay time threshold below 2 seconds. Service lifetime is constrained by conductive network fatigue under repeated flexural loading; containers subjected to more than 500 flex cycles may exhibit localised resistive hot spots at stress concentration points where the conductive carbon black network fractures irreversibly. End products include conductive inner bottles for composite IBCs, 210 L drum inserts, and flammable liquid jerry cans where the material is additionally evaluated for chemical compatibility under EN 14479 with representative solvent classes including ketones, esters, and aromatic hydrocarbons.

    What Injection Gate Configuration Prevents Conductivity Collapse in Long-Flow-Length Molded Trays?

    Injection-molded ESD trays for semiconductor component handling in cleanroom-compatible packaging require isotropic surface resistance across the entire part geometry to avoid static charge accumulation at the tray extremities during robotic extraction sequences. The masterbatch is let down at 25-30 wt% into a high-flow LLDPE base resin having melt flow index of 20-30 g/10 min under ISO 1133-1:2022, producing final carbon black loadings of 8.75-10.5 wt%. Molded trays of approximately 450 mm × 320 mm envelope with 1.8 mm nominal wall thickness are produced on electric injection machines with clamp force between 650 kN and 900 kN using either single-point edge gating or twin-fan gating systems. Production-line observations document surface resistivity differentials of up to 10² Ω/sq between the near-gate zone and the far-end corner at effective flow lengths exceeding 250 mm with single-point gating, while twin-fan gating reduces the maximum differential to below 10¹ Ω/sq at the cost of two additional weld lines across the tray floor. The weld lines themselves act as conductive network discontinuities, exhibiting surface resistivity values at least one order of magnitude higher than adjacent bulk material under ASTM D257 measurement; carbon black concentration at the weld-line interface is diluted by the fountain-flow effect, which preferentially deposits the carrier polymer rather than the agglomerated black particles at the advancing melt front during cavity filling.Productivity trade-offs govern this application: twin-fan gating requires higher packing pressure of 6-8 MPa (hydraulic) to close additional weld-line porosity, extending the holding phase by 25-35% relative to single-point gate operation. Mold temperature is maintained at 35-45°C with water circulation to avoid excessive cooling-induced shrinkage that would accentuate conductive path interruption at the frozen skin/core boundary. Tray flatness per ASTM D955-08(2024) is maintained within ±0.5 mm across the diagonal to ensure stable stack alignment in automated component handling stations. Compliance evaluation includes surface resistance per ANSI/ESD STM11.11-2021 at 23 ± 2°C and 12 ± 3% RH with values between 10³ Ω and 10⁶ Ω qualifying for ESD-protective handling, plus outgassing screening per ASTM E595-15(2021) where total mass loss below 0.10% and collected volatile condensable material below 0.01% are required for cleanroom deployment. End products include wafer shipping trays, chip carrier trays for quad flat pack packages, DIP shipping rails, and component storage bins compatible with IEC 61340-5-1 protected area requirements.Underground coal extraction operations in methane-laden atmospheres require non-metallic ventilation ducts that satisfy surface resistance limits under EN 14973:2015 for ducting used in potentially explosive atmospheres, where the measured value may not exceed 3×10⁸ Ω when tested per EN ISO 8030:2014 at 23 ± 2°C and 50 ± 5% RH. The masterbatch is compounded at letdown ratios of 20-28 wt% with a flame-retardant LLDPE/EVA carrier blend containing magnesium hydroxide or ammonium polyphosphate FR systems, producing carbon black loading of 7.0-9.8 wt% in the final compound. Extrusion of corrugated flexible ducting is performed on single-screw extruders of L/D 24:1 to 30:1 with grooved feed sections and barrier mixing pins, followed by spiral-wound corrugator molds operating at haul-off speeds between 3 m/min and 8 m/min depending on duct bore diameter (typically 300-800 mm). The primary process conflict in this application concerns the interaction between the flame-retardant filler and the conductive carbon black network: mineral FR loadings above 45 wt% in the compound act as conductive path diluents, raising surface resistivity by one to two orders of magnitude relative to unfilled compounds at identical carbon black concentration. Compensation requires either increasing masterbatch letdown to the upper end of the specified range (28 wt%) or accepting reduced flame-retardant filler loading, which then must be defended under the flammability testing regime of EN 14973:2015 clause 5.The compounding sequence exerts a documented influence on final electrical performance based on dispersion quality measurements from twin-screw extrusion lines. A two-pass compounding protocol, in which the masterbatch is first dispersion-compounded with the base resin on a co-rotating twin-screw extruder of L/D 40:1 at specific energy input between 0.18 kWh/kg and 0.25 kWh/kg, then subsequently blended with the flame-retardant filler in a second low-shear pass, produces surface resistivity values one to two orders of magnitude lower than single-pass compounding all components simultaneously. Published data for this specific two-pass configuration with flame-retardant co-fillers is limited; the described improvement is based on production line records rather than peer-reviewed experimental series. The enhanced dispersion of the carbon black in the first pass establishes a more continuous conductive network before the FR filler is introduced, minimising the particle-particle interruption effect of the mineral platelets. Pre-drying of the masterbatch and the FR filler at 80°C for 3 hours using dehumidified air at dew point below -30°C is standard practice; residual moisture above 0.12 wt% in the combined feedstock produces steam-induced surface defects in the extrudate. The compliance checklist below consolidates the governing standards across the industrial domains relevant to this masterbatch.
    Application domainGoverning standardReference clause / test methodCompliance threshold
    ESD packaging filmsANSI/ESD S20.20STM11.11-202110³-10⁵ Ω/sq
    ATEX containersIEC 60079-0Clause 26.13≤ 10⁹ Ω at 50% RH
    Electronics traysANSI/ESD S20.20 / ASTM E595STM11.11-202110³-10⁶ Ω/sq; TML 0.10%
    Mining ductingEN 14973:2015EN ISO 8030:2014≤ 3×10⁸ Ω
    Automotive fuel systemsSAE J1645:2019Surface resistivity evaluation< 10⁹ Ω/sq
    Cable conduitASTM D4496-21Volume resistivity after ageing≤ 10⁴ Ω·cm
    In the United States, MSHA 30 CFR Part 18 governs permissible equipment for underground coal mines and mandates surface resistance limits and flame-resistance certification for non-metallic ducting. The static dissipation requirement is non-negotiable in this application domain because the minimum ignition energy of methane-air mixtures at stoichiometric concentration is approximately 0.28 mJ, and the energy stored on a charged polymer surface can exceed this threshold at applied potentials well below human perception. Compliance testing for underground mining deployment in the European Union additionally includes the full EN 14973:2015 evaluation chain: longitudinal tensile strength ≥ 18 MPa per ASTM D638-14, tear propagation resistance per ISO 34-1, surface resistance per EN ISO 8030:2014, and flammability classification per EN 14973:2015 Annex A. End products include flexible ventilation ducts, dust extraction hoses, and air-curtain plenum sections used in continuous miner sections, where flame-retardant qualification and surface resistance compliance must both be certified before underground installation is permitted.

    Fuel Filler Neck Compounds and SAE J1645 Electrostatic Charge Dissipation Requirements

    Multilayer coextrusion of conductive fuel filler necks and vapor return line components for automotive fuel systems mandates surface resistivity below 10⁹ Ω/sq per SAE J1645:2019 when measured at 23 ± 2°C and 50% RH to prevent electrostatic discharge ignition of fuel vapours during refuelling operations. The masterbatch is let down at 30-35 wt% into a LLDPE base resin with melt flow index of 0.5-1.0 g/10 min under ISO 1133-1:2022 to achieve carbon black loading of 10.5-12.25 wt% in the conductive inner layer. The extrusion process utilises co-extrusion blow molding machines with accumulator heads and multiple extruder stations, where the conductive inner layer of 0.3-0.5 mm thickness within the multilayer wall is coextruded with a high-density polyethylene structural middle layer and a polyamide or EVOH barrier outer layer. Melt temperature for the conductive layer is held at 200-220°C to avoid VOC emissions from carbon black surface chemistry that can occur above 230°C. The primary controlled variable is the purge protocol between colour changes on the conductive-layer extruder; carbon black carry-over contamination into the barrier layer must be prevented because it compromises fuel permeation resistance measured per ASTM F1249-20 at 40°C with permeation maintained below 2 g·mm/m²·day for the barrier layer. End products include fuel filler necks, carbon canister vapor return lines, and fuel tank access flange covers, all validated for the vehicle platform under ECE R110 homologation testing.

    Underground Cable Duct Stock Exhibits Volume Resistivity ≤ 10⁴ Ω·cm After 85°C/85% RH Ageing

    Polyethylene cable duct stock for underground power distribution and telecommunications cable protection requires volume resistivity not exceeding 10⁴ Ω·cm per ASTM D4496-21 after conditioning at 85°C and 85% RH for 1000 hours to ensure long-term leakage current dissipation along the duct bore without reliance on migratory antistatic additives that leach out under wet underground conditions. The masterbatch is let down at 25-30 wt% into medium-density LLDPE having melt flow index of 0.7-1.5 g/10 min under ISO 1133-1:2022, producing final carbon black loading of 8.75-10.5 wt%. The extrusion process uses single-screw grooved-feed extruders with L/D 30:1, screen packs of 60/80/60 mesh, and annular dies for smooth-wall duct of 50 mm to 160 mm outer diameter. Corrugated duct variants are formed by post-extrusion blow molding into corrugator molds with vacuum assist, operating at haul-off speeds of 2-5 m/min. The key limitation in this application is the trade-off between carbon black loading and elongation at break: compounds at the upper end of the letdown range (> 30 wt% masterbatch) exhibit tensile elongation reduction from typical 600-700% for unfilled LLDPE to below 300% per ASTM D638-14, which restricts deployment in installations requiring significant flexibility such as directional drilling pull-throughs. Compliance testing also includes ring stiffness per ISO 9969, impact resistance at -20°C per EN 744, and weathering evaluation under ASTM G154-23 cycle 1 for above-ground riser sections. End products include plain and corrugated cable ducts, cable protection sleeves for fiber optic installation, and slotted conduit sections for cable management trays in ESD-protected server rooms.
    Free Quote

    Competitive LyondellBasell POLYBLAK™ 4669 Premium Conductive 35% Carbon Black Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell POLYBLAK™ 4669 Premium Conductive 35% Carbon Black Concentrate Based in LLDPE is a pelletized masterbatch containing 35 wt% conductive carbon black dispersed in a linear low-density polyethylene carrier resin. The material is intended for dilution with LLDPE or LDPE in blown film, cast film, sheet, and injection moulding processes where electrostatic discharge protection or static dissipation is required. It is a conductive masterbatch rather than a conventional color concentrate; the carbon black grade is selected for high structure and electrical conductivity, not primarily for jetness.

    The carrier is an olefinic linear low-density polyethylene. It is therefore most compatible with polyolefin matrices. Polyamide, PET, polystyrene, and PVC may not form a uniform conductive network because the polyethylene phase can remain isolated, and compatibility testing is required before use in such polymers. Incoming inspection should confirm carbon black loading by thermogravimetric analysis under nitrogen, melt mass-flow rate by ISO 1133-1:2022 at 190 °C and 2.16 kg, and dispersion assessment by ISO 18553. Density can be measured according to ISO 1183-1:2019; product-specific density values should be taken from the lot-specific certificate of analysis. Published data specific to this configuration is limited for absolute melt flow rate values because carbon black aggregate geometry, loading, and carrier molecular weight distribution jointly influence flow.

    What Twin-Screw Compounding Conditions Promote Uniform Carbon Black Dispersion?

    On co-rotating twin-screw extruders with an L/D ratio of 28:1 to 36:1, the concentrate can be added after the main polyolefin pellets have begun to melt. This sequencing lowers the viscosity mismatch and helps wet the carbon black aggregates. If the concentrate and neat resin are dry-blended and starve-fed, pellet segregation may occur because the concentrate pellets have higher density than unfilled LLDPE. Loss-in-weight gravimetric feeders with vertical agitators should maintain feed accuracy within ±0.5% of setpoint; this is necessary because conductive carbon black systems exhibit a narrow percolation window. A shift in final carbon black content from 5 wt% to 7 wt% can alter surface resistivity by several orders of magnitude depending on dispersion quality.

    Conductive carbon black used in this class of masterbatch typically has a primary particle size below 50 nm, but the primary particles are fused into aggregates with high structure. High-structure grades can be characterized by dibutyl phthalate absorption under ASTM D2414-21; higher values generally indicate better conductivity at lower loadings but also higher melt viscosity. The percolation threshold is therefore not a single weight percentage but a dispersion-dependent window. Poor dispersion creates locally insulating regions even when the average final carbon black content is above the threshold. Production-scale twin-screw extruders with side feeders and sequential kneading sections provide more reproducible dispersion than short single-screw extruders. Screw configuration should contain two or three kneading blocks with wide discs, followed by distributive mixing elements before the vacuum vent. Melt temperature in the mixing zone should be kept below 220 °C because excessive shear raises localized temperature and may initiate chain scission in the LLDPE carrier. The vacuum vent should be maintained below -0.08 MPa gauge to remove moisture and low-molecular-weight volatiles that would otherwise create surface defects in film or sheet.

    The relationship between screw speed and dispersion is non-monotonic. High screw speed can improve filler breakdown but may also shorten residence time and elevate melt temperature; low screw speed may not generate enough shear stress to break agglomerates. Dispersive mixing should be targeted rather than excessive distributive mixing alone, because carbon black agglomerates require high shear stress to fragment.

    In blown film extrusion of the diluted concentrate, bubble stability and screen-pack pressure are the primary process constraints. Carbon black increases melt extensional viscosity, and the frost line may exhibit shark-skin or visible pitting if dispersion is incomplete. Back pressure across a 60/80/100 mesh screen pack should be monitored at start-up and after each production hour; a rapid rise can indicate carbon black agglomerates or degraded gel particles accumulating at the screen. Melt temperature should not exceed 240 °C because carbon black surfaces can accelerate thermo-oxidative degradation of polyethylene. Tensile properties of the final film are measured by ASTM D882-18, Elmendorf tear by ASTM D1922-15, and dart impact by ASTM D1709-16; these values should be evaluated at each final carbon black content because increasing filler loading generally reduces elongation at break and tear resistance while raising modulus.

    Calculated final carbon black content after gravimetric dilution of a 35 wt% concentrate
    Concentrate parts by weightNeat LLDPE parts by weightNominal final carbon black content
    10903.5 wt%
    15855.25 wt%
    20807.0 wt%
    25758.75 wt%
    307010.5 wt%

    Melt Rheology Shifts Away from Unfilled LLDPE Once Carbon Black Networks Percolate

    In low-shear regimes, carbon black aggregates form a solid-like network that elevates shear viscosity and storage modulus. Capillary rheometry under ISO 11443:2021 or small-amplitude oscillatory shear under ISO 6721-10:2015 can identify the percolation threshold by measuring the frequency dependence of storage modulus. Unfilled LLDPE shows terminal flow at low frequencies, but conductive composites often exhibit a plateau in storage modulus when carbon black content exceeds percolation. That plateau may be used as a quality control indicator: if the plateau is absent at the expected final loading, dispersion is likely inadequate. Because the concentrate contains 35 wt% carbon black, the final diluted compound percolates at a lower carbon black content than the concentrate itself; published data for this specific concentrate is limited concerning exact rheological curves. The manufacturing site should generate shear viscosity versus shear rate curves at processing temperature because these curves determine pressure drop through flat-film dies and injection mould runners.

    At high shear rates, pseudoplastic behavior reduces viscosity; injection moulding and film extrusion can therefore operate at lower apparent viscosity than predicted from low-shear measurements. However, carbon black fillers also increase thermal conductivity, which can accelerate surface skin formation in film and produce flow marks if die temperature is non-uniform. Die lip temperature differences larger than ±2 °C can cause gauge bands and varying surface resistivity across the web. Die temperature uniformity should be verified with an infrared pyrometer before full production is attempted.

    Surface Resistivity Targets and Electrostatic Discharge Packaging Compliance

    Electrically conductive films and thermoformed trays produced from the diluted concentrate are commonly evaluated for surface resistivity using ASTM D257-14 with a concentric ring electrode at 23 ± 2 °C and 50 ± 10% relative humidity. Static dissipative packaging materials are defined by IEC 61340-5-1 as having a surface resistivity from 1 × 10^4 Ω to 1 × 10^11 Ω; conductive materials fall below 1 × 10^4 Ω. The precise final reading depends on final carbon black content, dispersion quality, film thickness, surface roughness, and conditioning time. Published data for this specific concentrate at film gauges below 50 µm is limited; users should establish their own correlation between let-down ratio and surface resistivity on production-scale equipment.

    Surface resistivity measured by ASTM D257-14 is electrode-geometry-specific. The result cannot be directly equated with resistance point-to-point measurements described in IEC 61340-4-4 or with packaged-device discharge tests under ANSI/ESD S541-2019. When compliance is required, the final article should be evaluated under the exact conditioning and electrode configuration of the end-user specification.

    Compliance and test methodology matrix for conductive polyolefin articles
    Regulation or standardScope
    EU 2011/65/EURoHS restriction of hazardous substances in electrical and electronic equipment
    EU 1907/2006REACH registration, evaluation, authorisation, and restriction of chemicals
    ASTM D257-14DC resistance or conductance of insulating materials
    IEC 61340-5-1Protection of electronic devices from electrostatic phenomena
    ANSI/ESD S541-2019Packaging materials for ESD-sensitive items
    ISO 1133-1:2022Melt mass-flow rate of thermoplastics
    ISO 18553Assessment of pigment or carbon black dispersion in polyolefins
    ISO 1183-1:2019Density of non-cellular plastics
    ASTM D2414-21Carbon black oil absorption number

    Differences from lower-loading conductive concentrates are most evident in let-down ratio and rheology. A 35 wt% carbon black concentrate reduces the amount of masterbatch needed to reach a given final carbon black content compared with 15 wt% or 20 wt% products. However, the higher filler level increases melt viscosity and may reduce throughput in shallow-flighted extruders or require higher melt temperatures. Compared with EVA-based conductive masterbatches, the LLDPE carrier of POLYBLAK™ 4669 provides closer melt rheology to LLDPE blown film, but it may have a higher heat-seal initiation temperature and a narrower seal window on high-speed form-fill-seal lines. Seal strength should be evaluated by ASTM F88/F88M-21; seal initiation temperature should be determined on the final film at production speed.

    Compared with a polypropylene-based conductive masterbatch, an LLDPE carrier is less likely to disrupt polyethylene heat sealing, but it is softer and may require lower conveying temperatures to avoid pellet softening during long hopper residence. In comparison with direct carbon black powder addition, the pelletized concentrate reduces dusting and improves housekeeping. Direct powder handling often requires local exhaust ventilation and operator exposure controls; the concentrate can be fed through closed gravimetric systems with less carbon black dust release. However, concentrates require distributive mixing, and unacceptable dilution zones can remain in low-shear single-screw extruders with short L/D ratios.

    When POLYBLAK™ 4669 Replaces Powdered Acetylene Black in Injection Moulded Conductive Trays

    Injection moulding of the diluted concentrate into conductive handling bins or trays requires attention to flow length, gate configuration, and anisotropic resistivity. LLDPE-based conductive compounds generally process at melt temperatures of 180 °C to 230 °C and mould temperatures of 20–40 °C. Thin-wall sections below 2 mm may experience short shots if the gate diameter is below 1.5 mm. Vent depth should be 0.02–0.05 mm to avoid gas burn marks caused by volatile release from the carrier. Carbon black aggregates can orient during flow; injection moulded plaques may therefore show lower resistivity in the flow direction than in the transverse direction. Surface resistivity measurements on moulded parts should be taken in both orientations and at multiple gate distances.

    Weld lines in carbon black-filled polyolefins often show higher surface resistivity because discontinuous flow fronts disrupt the conductive network. Multiple gates may improve conductivity across the part but introduce additional weld lines; gate location should be selected so that final flow fronts meet outside critical ESD performance regions. Tensile properties can be measured by ASTM D638-14 or ISO 527-1:2019. At high final carbon black loadings, elongation at break can fall below 10%, although the actual value depends on carrier molecular weight, filler dispersion, and test speed.

    Operational boundaries include closed storage at ambient conditions. If packaging is left open at relative humidity above 60%, moisture uptake can cause feeding surging and surface defects. Pre-drying at 70–80 °C for 2–4 h in a desiccant dryer is advisable when open-bag exposure has occurred. Avoid combining the concentrate with amine-based flame retardants or amine-functionalized processing aids that can react with carbon black surfaces and alter the conductive network. Extended residence time above 250 °C should be avoided because carbon black may accelerate degradation of the LLDPE matrix, producing gel particles and discoloration.

    Top