| HS Code | 630015 |
| Productname | LyondellBasell POLYBATCH™ Yellow 20232U Concentrate Based In LLDPE |
| Productcode | 20232U |
| Carrierresin | LLDPE |
| Color | Yellow |
| Form | Pellets |
| Pigmentcontent | 50% |
| Density | 1.05 g/cm³ |
| Meltflowrate | 20 g/10 min (190°C/2.16 kg) |
| Moisturecontent | ≤0.2% |
| Bulkdensity | 0.60 g/cm³ |
| Pelletsize | 2-3 mm |
| Recommendedletdownratio | 2-5% |
| Processingtemperature | 180-230°C |
| Lightfastness | 7 (Blue Wool Scale) |
| Heatstability | 250°C |
| Compatibility | Polyolefins |
As an accredited LyondellBasell POLYBATCH™ Yellow 20232U Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell POLYBATCH™ Yellow 20232U Concentrate Based In LLDPE: 25 kg polyethylene bags, palletized and stretch-wrapped, 40 bags (1,000 kg) per pallet. |
| Container Loading (20′ FCL) | 20′ FCL loading of LyondellBasell POLYBATCH™ Yellow 20232U Concentrate Based In LLDPE: palletized bags, shrink-wrapped, safely secured for ocean transport. |
| Shipping | POLYBATCH™ Yellow 20232U is a non-hazardous, solid LLDPE-based color concentrate supplied as pellets in sealed bags, boxes, or octabins on pallets. It is not regulated as dangerous goods for transport. Store cool, dry, away from direct sunlight and ignition sources. |
| Storage | Store in original, closed containers in a cool, dry, well-ventilated area. Protect from direct sunlight, heat, moisture, and contamination. Keep away from ignition sources and incompatible materials. Avoid excessive stacking or prolonged high-temperature exposure. Use first-in, first-out stock rotation. Inspect containers regularly for damage or leakage. Consult the Safety Data Sheet and local regulations for specific storage requirements. |
| Shelf Life | Shelf life is 12 months from manufacture when stored unopened in original packaging, dry, below 30°C, protected from direct sunlight. |
Competitive LyondellBasell POLYBATCH™ Yellow 20232U Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell POLYBATCH™ Yellow 20232U Concentrate Based In LLDPE is a yellow colorant preparation carried in a linear low-density polyethylene matrix. The public designation identifies the colour family, carrier resin, and concentrate form; it does not specify pigment loading, melt flow rate, density, or heavy-metal content. Those parameters are batch-controlled and must be read from the certificate of analysis. Published data for the exact 20232U formulation are limited, particularly for high-temperature food-contact use or high-shear injection moulding. The LLDPE carrier is specified where a non-polar, olefinic carrier reduces the risk of additive surface bloom and avoids introducing vinyl acetate or wax components into a polyolefin film construction. The concentrate is not a universal colour preparation for unmodified PET, polyamide, or polycarbonate because phase separation at the interface can produce visible specks and delamination.
The product is supplied in pelletised form; pellet geometry and bulk density are batch-specific. LLDPE-based colour concentrates are generally free-flowing at room temperature, but hopper bridging may occur in humid plants because surface moisture increases interparticle friction. In central conveying systems, pellet velocity should be limited to avoid dust formation and fines. Fines below 500 µm can segregate from the pellet column and cause local colour concentration changes at the feed throat.
Melt-flow matching should be confirmed under ISO 1133-1:2022 at 190 °C and 2.16 kg. Commercial LLDPE carriers used for colour concentrates are typically found within a melt flow rate range of 1 g/10 min to 20 g/10 min, but the specific value for 20232U is not established by this range. A mismatch of more than one MFI decade between concentrate and natural LLDPE can result in visible pigment banding in films below 50 µm when extruded through a die gap of 1.5 mm to 2.0 mm. Use of a spiral mandrel die with a uniform coat-hanger distribution section and die temperature uniformity of ±2 °C reduces transverse colour variation.
Dosing accuracy should be maintained with a gravimetric feeder, not a volumetric device, because pellet bulk density variations can produce letdown errors above ±0.5 percentage points. For thin-gauge film, initial trials are commonly run at a letdown ratio of 2 wt% to 4 wt%; higher ratios may be workable but can increase screw torque and film haze. If sacks have been stored at relative humidity above 60%, surface moisture may produce splay. Drying at 70 °C for 2 h to 4 h or vented barrel operation is required before extrusion.
Capillary rheometry at shear rates from 100 s⁻¹ to 1000 s⁻¹ provides better viscosity matching than a single MFI point. LLDPE carriers often show less shear thinning than LDPE; at die-lip shear rates, the viscosity difference between concentrate and base resin may be larger than the MFI values suggest. A converter processing a blend of 70% natural LLDPE and 30% concentrate should measure the apparent viscosity of the blend rather than assuming linear additivity because the pigment phase is a suspended solid that increases low-shear viscosity but contributes less at high shear.
In LLDPE blown film, bubble stability is generally lower than that of LDPE at the same melt temperature because the linear backbone has less extension thickening. A high-stalk bubble configuration may require a dual-lip air ring or internal bubble cooling when the concentrate is added at upper addition rates. Melt temperatures above 230 °C can shift the apparent shade of some organic yellow pigments when residence time exceeds 5 min; therefore, screw speed, melt pressure, and temperature profile should be logged during production trials. Batch-to-batch variation in pellet geometry can also change hopper discharge and dosing accuracy.
Pigment dispersion in 20232U is fixed during concentrate compounding. Co-rotating twin-screw extruders used for polyolefin-based colour concentrates typically operate with L/D ratios of 40:1 to 52:1 and contain two or more kneading blocks. Specific energy input commonly falls between 0.15 kWh/kg and 0.25 kWh/kg for this product class; the actual compounding conditions for 20232U are proprietary and are not published. Dilution at the film extruder does not correct agglomerates because the single-screw residence time and shear stress are insufficient to break down coherent pigment packages.
Screen-pressure rise can serve as an indirect dispersion check. A poorly dispersed colour concentrate can produce a pressure rise above 2 MPa across a clean 100-mesh screen pack within 30 min of extrusion; a well-dispersed product should show a lower rate of pressure rise. The acceptance limit for 20232U must be obtained from the supplier and matched to the converter’s screen changer configuration. Use of a melt pump after the screen changer stabilises downstream pressure and reduces colour concentration cycling.
Compliance must be verified against the end-use matrix and food-contact application. Table 1 summarises the standard framework documents that are typically requested for a LLDPE-based yellow concentrate supplied in the EU and United States. The presence of a standard test method in the table does not constitute a declaration of conformity; batch-specific documentation remains dispositive.
| Framework | Relevant designation or limit | Documentation requirement |
|---|---|---|
| EU food contact | Commission Regulation (EU) No 10/2011 | Declaration of compliance with overall migration limit of 10 mg/dm² under simulant conditions suitable for the end article. |
| US food contact | FDA 21 CFR 178.3290 | Colourant suitability for polymers and use condition confirmation for the final article. |
| EU packaging heavy metals | Directive 94/62/EC Article 11 | Sum of lead, cadmium, mercury, and hexavalent chromium not to exceed 100 mg/kg. |
| RoHS | Directive 2011/65/EU Annex II | Maximum 0.1 wt% for lead, mercury, hexavalent chromium, PBB, and PBDE; maximum 0.01 wt% for cadmium. |
| REACH | Regulation (EC) No 1907/2006 Article 33 | Communication if a substance of very high concern is present above 0.1 wt% w/w. |
For food-contact film, migration behaviour is not controlled solely by pigment chemistry; carrier purity, final thickness, and sealing-layer construction also matter. The specific pigment class in 20232U is proprietary. If the final article is intended for fatty-food contact, migration testing should be conducted under Commission Regulation (EU) No 10/2011 with simulant D2 or a validated alternative. If the final article is intended for dry food at room temperature, the overall migration limit of 10 mg/dm² still applies unless a specific exemption or restriction is established. The converter must issue the final declaration of compliance because the end-use conditions are outside the concentrate supplier’s control.
Heavy-metal limits are not simply a function of pigment purity. Contamination can enter from process equipment wear, recycled packaging, or cross-contamination in multi-product compounding lines. A robust certificate of analysis should therefore report both the pigment-related metals and the carrier-related ash profile. X-ray fluorescence screening may be sufficient for lot-to-lot verification if correlated with acid digestion and inductively coupled plasma analysis using methods such as ISO 11885:2009 or US EPA 3051A.
The substitution of an EVA- or LDPE-based yellow concentrate with an LLDPE-based product changes both bubble physics and film properties. LLDPE generally contributes higher tensile strength and puncture resistance than LDPE, but it exhibits lower melt strength. In cast film, this can improve drawdown at line speeds above 150 m/min; in blown film, it may require a lower blow-up ratio unless the bubble is stabilised by internal bubble cooling. EVA carriers reduce melt temperature and can widen heat-seal latitude, but they may increase blocking and coefficient of friction in the final winding.
The LLDPE carrier avoids vinyl acetate incorporation when the converter must maintain a pure olefin-grade recycle stream. Table 2 provides general carrier behaviour for polyolefin colour concentrates; it does not represent product-specific values for 20232U.
| Carrier system | Test condition | Typical general MFI range (g/10 min) | Relative melt strength | Main processing limitation in LLDPE film |
|---|---|---|---|---|
| LDPE | 190 °C / 2.16 kg (ISO 1133-1:2022) | 0.2–70 | Higher | May dilute stiffness and seal peak temperature if overloaded. |
| LLDPE | 190 °C / 2.16 kg (ISO 1133-1:2022) | 0.5–100 | Moderate | Lower bubble stability in high-stalk blown film. |
| HDPE | 190 °C / 2.16 kg (ISO 1133-1:2022) | 0.1–80 | Lower | Can increase haze and reduce tear strength in film. |
| PP homopolymer | 230 °C / 2.16 kg (ISO 1133-1:2022) | 0.5–100 | Lower | Phase separation with PE can create surface specks. |
If a converter replaces an EVA-based concentrate with the LLDPE-based 20232U, the seal initiation temperature may increase because the carrier does not supply a low-melting comonomer phase. Seal strength should be measured according to ASTM F88/F88M-23 or ISO 527-3:2018 for the final film. Dart impact, tear strength, and haze must also be retested because the change in carrier resin can shift property balances even when the pigment colour strength is matched.
Compared with a wax-based universal concentrate, the LLDPE carrier resides in the crystalline phase of the final film rather than as a low-molecular-weight boundary phase. This can reduce surface bloom during extended storage, but it narrows the processing window because the carrier melt viscosity must match the natural resin. If the natural resin is an autoclave LDPE with high melt strength, adding 4 wt% of an LLDPE carrier may reduce bubble stability. If the natural resin is a metallocene LLDPE with higher toughness, the same addition may dilute puncture resistance only slightly.
Spectrophotometric evaluation should be performed on plaques or films produced at a fixed letdown ratio, not on pellets. Data are recorded under D65 illumination with the 10° observer according to ISO 11664-4:2008; colour differences are calculated as ΔE*ab in the CIELAB space. A total colour difference above 1.0 units may be visually perceptible in side-by-side film comparison; the optical end use must define the tolerance.
Colour tolerances for film converting are commonly set at ΔE*ab below 1.0 to 1.5 units, but the limit should be based on visual assessment thresholds in the final laminate or printed structure. Ink adhesion and surface treatment can alter perceived colour; corona treatment above 38 mN/m may change the surface scattering of the film and should be standardised before colour measurement.
For injection-moulded caps, closures, or thin-wall containers, cavity-to-cavity melt-temperature variation greater than 5 °C can alter apparent colour and pigment dispersion. Hot-runner systems should be balanced to hold melt-residence-time variation below 2 min when processing above 220 °C. Some yellow chromophores lose intensity after prolonged high-temperature residence, so the converter should perform a residence-time challenge test before full production. Published data for the proprietary 20232U colourant are limited, and the final article must be evaluated in the intended thickness and residence-time window.
Property cliff-edges may occur at high addition rates. At a letdown ratio above 6 wt%, LLDPE carrier dilution can reduce machine-direction tear strength by more than 5% depending on the base resin and film gauge. Elmendorf tear testing should follow ASTM D1922-23 or ISO 6383-2:2022. A design of experiments across 2 wt%, 4 wt%, and 6 wt% is recommended before high-speed production because the reduction is not necessarily linear and can interact with frost-line height and blow-up ratio.
In coextruded barrier films, the LLDPE-based concentrate is usually placed in a polyolefin skin layer rather than in a polyamide or EVOH core. If the skin layer is below 15 µm, pigment concentration in that layer must be higher to maintain overall colour, which increases local carrier dilution and can reduce layer adhesion. Tie-layer adhesion testing by ASTM F904-16 or ISO 11339:2022 should be performed if the concentrate is used at more than 5 wt% in a thin skin layer.
For injection-moulded HDPE or LLDPE parts, an LLDPE carrier concentrate can be added at the machine throat at low letdown ratios. If the base resin has a melt flow rate of 20 g/10 min at 190 °C and 2.16 kg, a lower-MFI concentrate may create colour swirls or unmelted pellets in short-shot regions. Raising the rear barrel temperature by 10 °C to 15 °C improves carrier melting but may reduce pigment heat stability in the hot runner. Storage should be in sealed sacks below 40 °C, away from direct sunlight. Cold pellets moved into a warm production hall may develop surface condensation; such pellets should be brought to room temperature before opening and dried at 70 °C for 2 h to 4 h if visible moisture is present.