| HS Code | 925012 |
| Product Name | LyondellBasell POLYBATCH™ XAMF-500-T |
| Manufacturer | LyondellBasell |
| Brand | POLYBATCH™ |
| Product Code | XAMF-500-T |
| Product Type | Process Aid Concentrate |
| Carrier Resin | Linear Low Density Polyethylene (LLDPE) |
| Process Aid Type | Fluoroelastomer |
| Form | Pellets |
| Color | White to off-white |
| Density | 0.92 g/cm³ |
| Melt Flow Rate | 2.0 g/10 min (190°C/2.16 kg) |
| Melting Point | 120-130 °C |
| Packaging | 25 kg bags |
| Recommended Dosage | 1-5% |
| Shelf Life | 2 years |
| Storage Conditions | Cool, dry conditions |
As an accredited LyondellBasell POLYBATCH™ XAMF-500-T Process Aid Concentrate, Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaged in 25 kg polyethylene bags, palletized for shipment: LyondellBasell POLYBATCH™ XAMF-500-T Process Aid Concentrate, an LLDPE-based concentrate. |
| Container Loading (20′ FCL) | 20′ FCL container loading description: LyondellBasell POLYBATCH™ XAMF-500-T process aid concentrate in LLDPE, palletized and securely stowed for ocean transport. |
| Shipping | POLYBATCH™ XAMF-500-T is typically shipped as non-hazardous LLDPE-based pellets in sealed 25-kg bags or bulk containers, palletized and stretch-wrapped. Transport in clean, dry trucks or containers at ambient temperature; avoid moisture, direct sunlight, and excessive heat. Normally no UN number or special dangerous-goods classification applies. |
| Storage | Store in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed, on pallets, and protect from moisture, dust, and incompatible materials. Maintain moderate temperatures; avoid excessive heat or freezing. Use original packaging and follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Shelf life is typically 24 months from manufacture when stored in original unopened packaging under cool, dry, well-ventilated conditions. |
Linear low-density polyethylene blown film exhibits a sharkskin defect as transverse ridges oriented perpendicular to the extrusion direction at the die exit when wall shear stress exceeds 0.14 MPa in narrow die gaps, although the precise threshold shifts with molecular weight distribution, die land length, and melt temperature. The addition of POLYBATCH™ XAMF-500-T Process Aid Concentrate based in LLDPE modifies the boundary condition at the die wall by depositing a low-surface-energy layer that converts stick-slip flow into stable plug flow, but this conditioning requires an induction period. On a production line fitted with a 75 mm grooved-feed extruder, 30:1 L/D, and a 1.8 mm die gap, die pressure commonly decreases by 8–20% within 20–60 min after switching to a compound containing 1.0 wt% of the concentrate; before the fluoropolymer layer is established, surface haze and sharkskin may persist and should not be interpreted as formulation failure.
Industry compliance for food-contact and agricultural film applications must address both the carrier resin and the final film. The LLDPE carrier falls under FDA 21 CFR 177.1520 for olefin polymers intended for food contact, while the finished monolayer or coextruded film must be evaluated under EU Regulation 10/2011 for overall migration and specific migration limits; the concentrate itself is subject to REACH registration and downstream communication obligations. The recommended addition ratio for blown film is 0.5–2.0 wt% of the concentrate, with a starting point of 1.0 wt% for converters running fractional-melt LLDPE with melt index below 1.0 g/10 min as measured by ISO 1133-1:2022. During scaled production, the concentrate is dry-blended with LLDPE granules via a gravimetric dosing unit at the main feed throat; pre-compounded pellets are avoided where layer ratio changes are required on site. Extrusion parameters include barrel zone temperature profile 160–200 °C, die temperature 200–215 °C, blow-up ratio 2.5:1–3.5:1, and frost line height 250–500 mm depending on bubble stability. Terminal product types include food contact freezer bags, bakery films, agricultural greenhouse films, construction vapour barriers, and collation shrink film; all exhibit reduced die lip build-up and lower gel incidence after the conditioning period.
Operational boundaries are material-specific. Addition above 2.5 wt% of the concentrate in thin-gauge film may reduce transparency because excess fluoropolymer at the die wall can generate low-amplitude haze bands, and inorganic antiblock packages containing silica or talc at levels above 2,000 ppm can compete for the die surface and delay conditioning by 30–60 min. The concentrate does not substitute for adequate melt filtration; a screen pack with 60/80/100 mesh layers remains necessary to remove degraded gel particles before the die.
When cast film lines run fractional-melt LLDPE above 250 m/min, edge tear and die lip build-up typically originate from high shear stress in the die land region, not from insufficient chill roll cooling. The use of LLDPE-based process aid concentrate at 0.3–1.5 wt% shifts the distortion regime to higher throughput by forming a stable coating on the die metal, but cast film has a shorter contact time between melt and die lip than blown film; therefore the level of fluoropolymer required at the die surface must be reached through higher initial addition and then stepped down. A typical step-down sequence starts at 1.2 wt% for the first 30 min, then 0.8 wt% for the following 30 min, then 0.5 wt% steady state, with die pressure and cast film haze monitored against ASTM D1003-21 and tensile properties against ASTM D882-18.
Compliance in cast film applications involves EU Regulation 10/2011 for hygiene and food contact laminates, FDA 21 CFR 177.1520 for the polyethylene carrier, and CONEG or EU Directive 94/62/EC for heavy metals in packaging. The downstream production process is a flat-die extrusion line with a 90–150 mm single-screw extruder, 30:1 L/D, barrier screw, coat-hanger die with adjustable lip gap 0.4–0.8 mm, vacuum box, air knife, and chill roll maintained at 15–30 °C. Terminal products include hygiene backsheet film, lamination film for coffee pouches, industrial stretch wrap, agricultural silage wrap, and surface protection film. Process aid use is particularly relevant in cast stretch film containing high levels of tackifier; metal stearates in tackifier masterbatches can deposit on the die and are displaced more readily when the PPA concentrate is present at 0.5 wt% or above.
Published data for this specific configuration is limited, but industrial practice indicates that the conditioning window may lengthen when chill roll release agents are used on the same line. Waxes and silicones from chill roll sprays can transfer to the die lip during edge trimming and interfere with fluoropolymer deposition; the mitigation is to purge with clean LLDPE for 20 min before reintroducing the additive.
On pressure pipe lines operating at the low end of the melt temperature window to preserve molecular weight and slow crack growth resistance, the die exit can accumulate oxidized low-molecular-weight fractions from the outer layer of the melt stream. The concentrate based in LLDPE is compatible with HDPE pipe grades at 0.5–1.5 wt% addition, and the fluoropolymer layer reduces the adhesion of these oxidized fractions to the die land. On a pipe extrusion line using a 90 mm grooved-feed single-screw extruder with 33:1 L/D and a barrier screw, die pressure typically decreases by 6–15% over 45–90 min when the concentrate is introduced at 1.0 wt%, while melt temperature measured at the die adapter is held at 195–215 °C to avoid thermal degradation of the HDPE.
The regulatory framework for pressure pipe includes ISO 4427 for polyethylene piping systems, ISO 9080 for long-term hydrostatic strength extrapolation, ASTM D3350-21 for material classification, and NSF/ANSI 61 for potable water contact in North America; the carrier LLDPE must meet the same migration limits as the pipe compound when used in drinking water service. Downstream production involves dry-blending the concentrate with natural HDPE pipe resin at the main hopper, feeding through a screen pack of 60/80/100 mesh, forming the pipe through a spiral mandrel die, and calibrating under vacuum at water temperature 20–35 °C. Terminal products include PE100 pressure pipes for municipal water distribution, industrial slurry pipes, mining tailings pipes, telecom conduits, and corrugated drainage pipes. The process aid does not alter the hydrostatic design basis; long-term pressure ratings remain governed by the base HDPE resin and its ISO 9080 regression curve, not by the additive package.
| Process | Extruder type | Concentrate addition ratio | Conditioning time | Typical die pressure response |
|---|---|---|---|---|
| Blown film | 75 mm grooved-feed, 30:1 L/D | 0.5–2.0 wt% | 20–60 min | 8–20% reduction |
| Cast film | 90–150 mm barrier screw, 30:1 L/D | 0.3–1.5 wt% | 30–60 min step-down | 5–15% reduction |
| Pipe extrusion | 90 mm grooved-feed, 33:1 L/D | 0.5–1.5 wt% | 45–90 min | 6–15% reduction |
| Wire and cable jacketing | 60–120 mm low-compression screw, 24:1–30:1 L/D | 0.8–2.0 wt% | 30–90 min with ATH/MDH | 10–25% pressure reduction or stabilization |
Where low-smoke zero-halogen jacketing compounds contain more than 50 wt% ATH or MDH, the melt phase exhibits elevated viscosity and a pronounced tendency toward wall slip instability at conventional extrusion speeds. The LLDPE-based PPA concentrate is introduced at 0.8–2.0 wt% into the filled jacketing compound, with the higher end of this range reserved for formulations above 60 wt% mineral filler. On a 90 mm low-compression screw with 24:1 L/D and a 1.5:1 compression ratio, die pressure stabilization is typically observed within 30–90 min; melt temperature at the die is restricted to 140–170 °C because ATH begins endothermic dehydration near 180–200 °C and premature decomposition creates surface pitting and odour.
Regulatory compliance for wire and cable jacketing includes IEC 60502-1:2021 for power cable insulation and sheathing, BS 6724 for low-smoke halogen-free cables, RoHS Directive 2011/65/EU as amended, and REACH candidate list screening for SVHCs; the process aid concentrate must not introduce heavy metals or restricted flame retardants. The downstream process is single-screw extrusion with a vacuum vent, pressure-relief screen pack, and a crosshead die that applies the jacket over the insulated conductor at line speeds from 50–400 m/min depending on conductor cross-section. Terminal product types include low-smoke zero-halogen building wire jackets, photovoltaic cable sheathing, railway transit car wiring, and control cable jackets for marine and offshore installations. Dispersion quality is quantified by the filter pressure value test according to EN 13900-5:2005, with a maximum pressure rise criterion defined by the cable compound specification; the PPA concentrate reduces pressure fluctuations in the crosshead region but cannot compensate for severe filler agglomeration.
The concentrate is not a replacement for filler surface treatment. Halogen-free systems with high levels of zinc borate or magnesium hydroxide may delay fluoropolymer deposition onto the die wall; in these formulations, the initial addition should be held at 1.5 wt% for the first 45 min before stepping down to the steady-state level. Pre-drying is required at relative humidity above 60% because moisture uptake in LLDPE carrier can generate surface voids in the jacket wall.
In extrusion blow moulding, post-consumer recyclate introduces polar contaminants, printing ink residues, and metal stearate soaps that accumulate on the die face as drool and then transfer to the parison surface. A LLDPE-based process aid concentrate at 0.5–1.2 wt% reduces the adhesion of these residues by coating the die lip and promoting slip at the metal–melt boundary. The addition ratio is raised to 1.2 wt% when the recyclate content exceeds 25 wt% or when the melt index of the base HDPE falls below 0.4 g/10 min at 190 °C/2.16 kg per ISO 1133-1:2022. Production-scale observations on shuttle blow moulding machines with 60–120 mm extruders and parison die diameters from 40–200 mm show that die face cleaning intervals can be extended from 4–8 h to 16–24 h once the fluoropolymer layer is conditioned, but this improvement is lost if the die is aggressively cleaned with abrasive pads during the conditioning period.
Compliance standards include FDA 21 CFR 177.1520 for olefin polymer articles in food contact and EU Regulation 10/2011 for food containers; where the bottle contains post-consumer recyclate, EU Regulation 2022/1616 governs the suitability of the recycling process and the use of recycled material in food contact. The downstream process is extrusion blow moulding with a continuous or accumulator head, parison programmer, and mould clamp force typically between 100–500 kN for bottles up to 5 L; melt temperature is controlled between 180–210 °C to balance parison sag against surface finish. Terminal products include HDPE detergent bottles, household chemical containers, dairy bottles, personal care bottles, and industrial jerrycans. The additive does not increase melt strength and does not prevent parison sag in high-melt-index resins; sag resistance must be controlled by selecting a suitable blow moulding grade and parison programming.
For extrusion coating lines applying low-density polyethylene to paperboard or aluminium foil, the narrow air gap and high draw ratio amplify any melt flow disturbance originating at the die lip. The LLDPE-based process aid concentrate is let down at 0.5–1.0 wt% in the coating resin; because the melt curtain is drawn down to 8–25 µm thickness, even minor die face oxidation can cause web breaks or edge pinning instability. In industrial operations using a 120 mm extruder with 30:1 L/D and a coat-hanger die with 0.4–0.8 mm lip gap, the addition of PPA concentrate stabilizes the melt curtain and reduces edge neck-in by 2–5 mm under constant tension, but the effect is less pronounced when corona treatment is not applied before winding.
The regulatory framework for food-contact extrusion coating includes FDA 21 CFR 176.170 for components of paper and paperboard in contact with aqueous and fatty foods, FDA 21 CFR 175.300 for resinous and polymeric coatings, and EU Framework Regulation 1935/2004 with overall migration testing under EN 1186-1:2002. The downstream production process is an extrusion coating and lamination line with a chilled polishing roll maintained at 10–20 °C, a pressure roller system with nip loads from 50–150 N/mm, and an inline corona treater operating above 42 mN/m surface energy. Terminal product types include liquid carton board for milk and juice, sachet and stick pack laminations, food service cup stock, pharmaceutical blister lidding foil, and aseptic packaging. The fluoropolymer can migrate to the coating surface and reduce wetting tension; inline corona treatment of the coated web to 44–48 mN/m is therefore part of standard operating practice before lamination or printing.
Competitive LyondellBasell POLYBATCH™ XAMF-500-T Process Aid Concentrate, Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
The pelletized concentrate identified as LyondellBasell POLYBATCH™ XAMF-500-T Process Aid Concentrate is supplied on a linear low-density polyethylene carrier and belongs to the POLYBATCH additive masterbatch range. Its designated function is to alter the wall-polymer boundary condition in the die land during extrusion, thereby suppressing surface irregularities associated with melt fracture and reducing the rate of oxidized deposit accumulation on the die lip. The product is not intended as a bulk slip agent, coefficient-of-friction modifier, antiblock, or filler. The active system is released from the LLDPE carrier under melt shear, and the resulting die-wall conditioning produces a process effect that is rate-dependent and reversible. In LLDPE-rich blown film, cast film, and sheet operations, the carrier selection is significant because the carrier becomes a minor phase in the melt and must not introduce visible gel contamination or local haze.
The term “process aid concentrate” distinguishes this material from neat processing aid powders and from blended additive packages. As a concentrate, the product is metered by pellet feeders rather than low-ppm liquid or powder dosing systems. The LLDPE carrier simplifies letdown in polyethylene-based compounds because the carrier melts within the same thermal window as the matrix. However, the exact numeric melt flow rate of the concentrate is not encoded in the grade designation; it must be read from the certificate of analysis and compared with the matrix resin using ISO 1133-1:2022 or ASTM D1238 at 190 °C and 2.16 kg. This measurement is only a single-point indication of viscosity; it does not substitute for shear rheology when the target effect occurs in a high-shear die land.
Linear low-density polyethylene differs from branched low-density polyethylene in molecular architecture. The carrier therefore influences melt elasticity, additive release rate, and optical compatibility with the surrounding matrix. In a process aid concentrate, the carrier is not inert; it controls whether the active additive disperses rapidly at the feed throat or remains localized until a later melting zone. This distinction becomes visible in blown film when a poorly chosen carrier creates melt-haze streaks or in cast film when it creates localized surface gel. The use of an LLDPE carrier is especially relevant for formulations that already contain 80 wt% to 100 wt% LLDPE in the skin layer, because the rheological discontinuity between the carrier and the matrix is reduced relative to an LDPE carrier.
Published data for XAMF-500-T carrier melt index and additive loading is not detailed in this document; therefore, scale-up trials should be based on the manufacturer’s current certificate of analysis and not on generic class averages. Nonetheless, the carrier type is explicitly stated by the producer as LLDPE, and this provides a boundary condition for material handling. Compared with a polypropylene carrier, an LLDPE carrier avoids the tendency of a higher-melting carrier to remain as an unmelted phase in early compression zones of polyolefin extruders running at 190 °C to 220 °C barrel temperatures.
| Attribute | LLDPE carrier | LDPE carrier | Neat processing aid |
|---|---|---|---|
| Carrier compatibility with LLDPE-rich films | High | Moderate | Not applicable |
| Feeding method | Pellet gravimetric or volumetric feeder | Pellet gravimetric or volumetric feeder | Dedicated low-volume powder or liquid feeder |
| Die-wall conditioning action | Carrier releases active additive under shear | Carrier releases active additive under shear | Direct, but dispersion is harder to control |
| Risk of feed-throat melting inconsistency | Low in PE-rich formulations | Low in PE-rich formulations | High if not compounded |
Two separate surface defects are commonly addressed by polymer processing aid concentrates: sharkskin, which appears as transverse ridges on the surface of extrudate, and stick-slip, which produces alternating rough and smooth bands. The onset conditions are not additive-specific; they are functions of molecular weight distribution, die land shear rate, melt temperature, and die metallurgy. Capillary rheometry according to ISO 11443:2021 provides a laboratory measurement of the apparent shear rate at which the extrudate surface transitions from smooth to matte. In production-scale blown film, the evaluation criterion is often the time needed for the first die-lip deposit to become visible at constant back pressure and screw speed.
The active process aid in XAMF-500-T is understood to condition the die wall by forming a low-energy boundary layer in the final land region. The practical consequence is that the onset of sharkskin shifts to a higher shear rate or larger die gap for the same resin. The effect requires a conditioning period. On a 45 mm single-screw blown film extruder with a 30:1 L/D high-shear barrier screw and a 250 mm spiral mandrel die, conditioning may require 20 min to 60 min depending on the active level and melt temperature. These figures are class-typical and should not be treated as product-specific guarantees. Published data for this specific configuration with XAMF-500-T is limited; therefore, pressure, motor load, and film surface records must be kept for each trial.
Addition-level optimization should begin at the lower end of the class-typical concentrate range and step upward only after two full conditioning periods have elapsed. For polymer processing aid masterbatches of this class in LLDPE film, starting letdowns of 0.5 wt% to 1.0 wt% are frequently used, with a maximum benefit often observed between 1.0 wt% and 2.0 wt%. Over-addition can produce chill-roll plate-out, die-lip coating that transfers to the film edge, or a reduction in heat-seal strength. Because XAMF-500-T is a concentrate, the active additive level is diluted by the carrier; this reduces the risk of feeder-induced concentration spikes but does not eliminate the need for calibration of the pellet feeder.
A separate production-scale observation is that the pressure drop across the die pack does not always decrease when the process aid is active. In some LLDPE lines, the effect appears as a change in the high-frequency pressure fluctuation amplitude in the die land rather than a change in mean pressure. Therefore, the use of a pressure transducer installed as close as possible to the die entrance is recommended; a transducer mounted only before the breaker plate cannot separate screen-pack plugging from die-wall conditioning. If the pressure fluctuation amplitude decreases by more than 30% while mean pressure changes by less than 5%, the process aid is likely conditioning the die wall rather than merely reducing bulk viscosity. This is an interpretation used in process troubleshooting and should be confirmed against surface roughness data generated under ISO 4287 or a profilometric equivalent.
In coextruded structures and high-clarity LLDPE films, the carrier resin of a process aid masterbatch can operate as a contaminant if the refractive index and melt elasticity differ from the skin layer. An LLDPE carrier is selected when the converter must avoid the long-chain branching of LDPE or when the final film is subjected to optical testing according to ASTM D1003 and ASTM D2457. The carrier contribution to haze cannot be assumed to be negligible; it should be separated from the additive effect by running a control compound containing the same LLDPE carrier at the same letdown without the active process aid.
Compared with an LDPE-carrier process aid concentrate, the LLDPE-carrier product may show a different response to screw speed. Linear low-density polyethylene has a different shear-thinning profile from branched LDPE, and this difference can alter the point in the screw where the active material is released. The result is that the same active content can produce a longer or shorter conditioning time depending on carrier molecular architecture. The practical consequence is that a formulation change from an LDPE carrier to XAMF-500-T should not be made at the same letdown without a controlled transition trial.
Against siloxane-based process aids or amide slip additives, the distinction is functional. A siloxane-based additive may modify the bulk surface of the film and reduce the coefficient of friction measured under ASTM D1894, while a process aid concentrate of the XAMF series acts primarily at the die wall. If the film specification includes coefficient of friction or seal strength, those properties should be measured separately. The process aid is not a replacement for erucamide or oleamide slip, and it does not provide the same bloom-dependent performance. Surface energy measurements under ISO 8296 may remain unchanged or show minor shifts, but this is not a reliable indicator of die-wall conditioning.
The product should also be differentiated from external lubricants such as zinc stearate or paraffin wax. Those additives lower bulk apparent viscosity and may migrate to the film surface; they do not produce a stable die-wall conditioning layer and can interfere with heat sealing. XAMF-500-T, as a polymer processing aid concentrate, is not a torque-reducing lubricant in the same sense. Its effect is localised and does not scale directly with the melt index increase of the compound.
When the concentrate is removed from the feed, the die-wall layer does not disappear immediately. Carry-over can persist for 20 min to 2 h depending on die land dimensions, melt temperature, and the previous conditioning history. Therefore, line trials that compare surface quality before and after XAMF-500-T use must include a defined purge protocol. A return of the die pressure trace to its pre-trial signature is a more reliable end point for the run than visual disappearance of haze or surface roughness. If the same line alternates between film grades, the transition sequence should be recorded with melt temperature and back-pressure data.
In coextruded films, the process aid is typically added to the skin layer or to a layer that contacts the die lip. If the concentrate is added to a core layer only, the die wall may not be conditioned efficiently unless the outer layer transmits the active material to the metal interface. This is a structural constraint, not a defect of the concentrate. The choice of layer for letdown should be confirmed by a die-lip evaluation after a stable period of operation, not by measuring the bulk melt index of the combined feed.
For direct food contact, the final converter must verify the regulatory status of the complete formulation. The presence of an LLDPE carrier and a processing aid additive does not provide automatic clearance under 21 CFR 177.1520 or Commission Regulation (EU) No 10/2011. The producer’s statement of composition is required for the specific grade and lot. For industrial applications in the EU, the final article remains subject to REACH Regulation (EC) No 1907/2006 and RoHS Directive 2011/65/EU at the end-article level; masterbatch composition alone does not determine the final classification.
Storage and handling boundaries are conventional for polyolefin masterbatches. The material should not be mixed with incompatible carrier systems such as polyamide or polyester unless the processor has verified that the carrier remains a minor component below the threshold that affects the continuous matrix. If pellet surface condensation occurs, drying at 60 °C to 70 °C for 2 h to 4 h in a desiccant dryer is generally sufficient; higher temperatures may cause pellet agglomeration and should be avoided.
| Measurement or regulatory area | Reference designation | Use in qualification |
|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022, ASTM D1238 | Carrier-to-matrix viscosity comparison |
| Capillary rheometry | ISO 11443:2021 | Shear-rate onset of melt fracture |
| Film haze and clarity | ASTM D1003, ASTM D2457 | Carrier and additive optical contribution |
| Surface roughness | ISO 4287 | Sharkskin quantification |
| Coefficient of friction | ASTM D1894 | Confirms process aid is not acting as slip agent |
| Surface wetting tension | ISO 8296 | Secondary surface characterisation |
| US food-contact polyolefin base resin | 21 CFR 177.1520 | Requires producer confirmation for specific grade |
| EU plastic food-contact materials | Commission Regulation (EU) No 10/2011 | Requires producer confirmation for full formulation |
| EU industrial chemicals | REACH Regulation (EC) No 1907/2006 | Final article assessment |
| Restriction of hazardous substances | RoHS Directive 2011/65/EU | Final article assessment |
Process aid concentrates of this class are qualified by sequential trials rather than by a single melt-flow measurement. The relevant acceptance profile includes surface roughness, die-lip deposit rate, pressure fluctuation amplitude, and optical properties measured before and after the conditioning period. Without those measurements, comparisons between masterbatches with different carriers or active systems are not technically meaningful.