| HS Code | 807848 |
| Product Name | LyondellBasell POLYBATCH™ Woodland Green 30233U/4 Concentrate Based In LLDPE |
| Manufacturer | LyondellBasell |
| Product Type | Color Concentrate |
| Carrier Resin | LLDPE |
| Color | Woodland Green |
| Form | Pellet |
| Appearance | Green pellets |
| Density | 1.05 g/cm³ |
| Melt Flow Rate | 20 g/10 min (190°C/2.16 kg) |
| Let Down Ratio | 4% |
| Processing Temperature | 170–230°C |
| Moisture Content | ≤0.20% |
| Light Fastness | 7 |
| Heat Stability | 260°C |
| Shelf Life | 2 years |
| Packaging | 25 kg bags |
| Storage Conditions | Dry, below 30°C |
| Compatibility | Polyolefins |
As an accredited LyondellBasell POLYBATCH™ Woodland Green 30233U/4 Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell POLYBATCH™ Woodland Green 30233U/4 concentrate is supplied in 25 kg (55 lb) polyethylene-lined bags, typically 40 bags per pallet. |
| Container Loading (20′ FCL) | 20′ FCL container securely loaded with LyondellBasell POLYBATCH™ Woodland Green 30233U/4 concentrate based in LLDPE for safe chemical transport. |
| Shipping | Shipping Description: LyondellBasell POLYBATCH™ Woodland Green 30233U/4 is a non-hazardous, LLDPE-based color concentrate. It is typically shipped as solid pellets in moisture-resistant bags, boxes, or totes. Not regulated for DOT, IATA, or IMDG transport. Store dry, away from heat and ignition sources. No UN number required. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed when not in use to prevent moisture pickup and contamination. Store in original packaging, protect from physical damage and excessive temperatures, and use secondary containment where required. Avoid contact with incompatible chemicals. Follow local regulations and the manufacturer’s SDS recommendations. |
| Shelf Life | Shelf life is typically 12 months from manufacture when stored in unopened original packaging under cool, dry, dark conditions. |
In three-layer agricultural silage and mulch film extrusion, POLYBATCH™ Woodland Green 30233U/4 is introduced at the extruder throat through a gravimetric or volumetric feeder, with the main polyolefin pellets delivered from the resin silo. The preferred starting let-down ratio for a 100–150 µm LDPE/LLDPE film is 2–3 wt%; when thickness drops below 75 µm or when the film is stretched on a high-stalk blown-film die, the addition level is often raised toward 3–4 wt% to maintain opacity and avoid visible fold-line whitening. Processing parameters commonly evaluated on a blown-film line with a 1.6–2.4 mm die gap and blow-up ratio of 2.2:1–3.0:1 include melt temperature between 185°C and 210°C, extruder barrel profile flat-to-reverse for LLDPE-rich blends, and a barrier screw with a modest Maddock mixer to disperse pigment aggregates. Incoming screen packs are typically arranged at 80/120 mesh; a rising head-pressure trend across the screen pack during a 6–8 h production run indicates pigment agglomeration or gel accumulation from the carrier. Batch-specific pigment loading and carrier melt flow rate should be read from the certificate of analysis before gravimetric feeder constants are set. Colour consistency is measured on film samples using a benchtop spectrophotometer according to ISO 7724 with D65 illumination and 10° observer; the target lot-to-lot CIELAB ΔE* should be held below 1.0 against the approved reference chip. The concentrate contributes no ultraviolet stabilisation. Agricultural films intended for 12–24 month outdoor service must therefore combine this material with a separate HALS/UV masterbatch and pass accelerated weathering checks under ASTM G154 Cycle 1 or ISO 4892-2 before commercial extrusion. Regulatory documentation should confirm compliance with EU REACH Article 33 obligations and verify absence of restricted heavy metals by IEC 62321-5 screening.
The dosing position at the machine throat should be selected so that the masterbatch falls into the solids-conveying zone rather than the hopper bypass. For rigid LLDPE/HDPE industrial totes and crates, a let-down of 2–3 wt% is evaluated first; thick-walled parts with nominal wall thickness above 3 mm may require 3–4 wt% to prevent light transmission through gate scars and weld lines. Barrel temperatures are set with a rear zone near 180–200°C and a nozzle zone near 210–240°C, with the injection speed profiled to avoid jetting in multi-cavity tools. Back pressure is maintained at 5–15 bar hydraulic to homogenise the colourant without over-shearing the LLDPE carrier. Clamp force per projected area should be checked against 3–5 kN/cm² for high-flow polyolefin grades; short-shot and flash trials are conducted before colour acceptance because the carrier can shift the effective melt viscosity of the base resin. Mould shrinkage is recorded according to ASTM D955 after 24 h and 48 h conditioning at 23°C ± 2°C and 50% ± 10% RH. For crates used in cold-room logistics, environmental stress-crack resistance is screened by ASTM D1693 under 10% Igepal CO-630 at 50°C. Colour uniformity across a shot series is evaluated with a handheld sphere spectrophotometer; the acceptance window typically requires average CIELAB ΔE* below 1.0 and no streak heavier than a visual grey-scale rating of 4 under ISO 105-A02. Since the pigment is present as a single batch, lot-to-lot shade variation at injection machines is managed by retaining a sealed reference plaque and requiring the supplier to certify batch pigment strength before release.
Because rotational moulding is a pressureless, low-shear process, colour development depends on dry-blend homogeneity and particle-size compatibility rather than screw mixing. The concentrate should be ground or selected in micropellet form to track the mean particle size of the LLDPE powder, commonly below 500 µm; segregation occurs when the colourant particles are significantly finer or coarser than the base powder during loading, rotation, and powder flow into deep cavities. A starting addition of 1–3 wt% is used for decorative and outdoor tanks, playground components, and industrial containers. Oven temperatures are generally set between 260–300°C for LLDPE rotational moulding, with peak internal air temperature monitored in the 190–220°C range before cooling; lower peak internal air temperature can produce under-cured parts with reduced tensile properties, while higher peaks risk colour shift. Mechanical acceptance testing includes tensile properties according to ASTM D638, notched impact according to ASTM D256, and ESCR according to ASTM D1693 for tanks subjected to aggressive liquids. Wall thickness and warpage are measured after 24 h conditioning; uneven cooling rates at the mould surface may create visible shade bands that are unrelated to pigment distribution. Published data for this specific concentrate in rotational moulding tools are limited; the conversion should be validated on the intended tooling. Processors should verify that the green pigment system does not accelerate warpage or reduce demoulding efficiency when mould-release additives are absent; trial mouldings should be compared against natural resin under identical peak internal air temperature profiles.
| Application scenario | Test method or standard | Parameter | Operational relevance |
|---|---|---|---|
| Agricultural film | ISO 7724 | CIELAB ΔE* under D65/10° | Lot-to-lot shade control |
| Agricultural film | ASTM G154 Cycle 1 | UV exposure | Separate stabiliser qualification |
| Injection moulded totes | ASTM D955 | Mould shrinkage after 24/48 h | Dimensional acceptance |
| Injection moulded totes | ASTM D1693 | ESCR in Igepal CO-630 | Cold-room durability |
| Rotational moulding | ASTM D638, ASTM D256 | Tensile, notched impact | Part validation |
| Artificial turf yarn | ISO 2062 / ASTM D2256 | Tensile tenacity | Oriented yarn strength |
| Artificial turf yarn | ISO 105-B02 | Colourfastness to light | Outdoor shade retention |
| LLDPE geomembrane | ASTM D3895 / ASTM D5885 | Oxidative induction time | Antioxidant interaction check |
| LLDPE geomembrane | GRI-GM17 | LLDPE geomembrane specification | Project compliance |
| Irrigation tubing | ISO 1167, ISO 9080 | Hydrostatic strength | Pressure retention |
Slit-tape and monofilament extrusion of artificial turf yarn requires a pigment dispersion that survives orientation; agglomerates above 20 µm cause fibrillation defects and local tenacity loss in the final yarn. In LLDPE/LDPE tape lines, the masterbatch is metered at 2–4 wt% into blends with a typical melt index of 0.8–2.0 g/10 min, through an extruder with a 0.4–1.2 mm die gap and water-bath quenching at 30–50°C. The hot-air or oven orientation stage draws the tape at 4:1–8:1; the green shade must be evaluated before and after fibrillation because pigment migration and film draw can shift perceived colour. Finished yarn is measured for denier per filament, usually 800–1,500, and tensile tenacity according to ISO 2062 or ASTM D2256. Colourfastness to light is checked according to ISO 105-B02 or ASTM G154; however, the concentrate itself is not an outdoor weathering package. Turf systems exposed to continuous sunlight must include a separate UV stabiliser masterbatch and should be tested under the specific sports surface performance criteria referenced by EN 15330-1 or the local sports federation. Pre-drying is not required for previously sealed bags; if bags have been opened and stored above 60% RH, the concentrate should be dried at 70–80°C for 2 h before extrusion.
In LLDPE geomembrane extrusion, the green concentrate is run in flat-die or blown-film lines producing sheet from 1.0 mm to 2.5 mm thickness. The addition level is normally 2–3 wt%, but the exact loading is set on a trial run because transition-metal pigments can interact with the antioxidant package and reduce the oxidative induction time measured by ASTM D3895 or high-pressure ASTM D5885. Before production, sheet should be tested against the current version of GRI-GM17 for LLDPE geomembranes or the project specification; tensile properties are measured according to ASTM D6693 or ISO 527-3, tear resistance according to ASTM D1004, puncture resistance according to ASTM D4833, and hot-wedge seam strength according to ASTM D6392. Because 30233U/4 is not a carbon black masterbatch, it does not provide the long-term ultraviolet shielding normally specified for exposed geomembranes; exposed applications require a separate carbon black or UV-stabiliser package, while the green concentrate is used primarily for identification, layered separation, or decorative surfaces. Surface oxidized layers formed during flat-die extrusion can affect welding; if weld peel strength falls below project acceptance, the melt temperature should be adjusted before attributing the failure to the colorant. The processor should also verify batch-specific transition metal content from the certificate of analysis, as the presence of certain metals at trace level can degrade the antioxidant package during 80°C ageing tests. Published data for this specific masterbatch in welded geomembrane seams are limited; weld trials should be performed on the exact base resin and stabiliser formulation intended for production.
Flexible irrigation tubing and micro-irrigation laterals use 30233U/4 at 2–4 wt% in small-diameter LLDPE extrusion lines with vacuum calibration. Tubing dimensions are commonly 12–20 mm outside diameter with wall thickness from 1.0 mm to 2.0 mm; the die and calibrator must be matched to maintain ovality below the specified tolerance after cooling. Melt temperature is held at 190–220°C, and the extruder is fitted with a 60/80/60 screen pack in most evaluations; pressure rise across the screen pack is logged because pigment agglomerates above 20 µm can accumulate and create microvoids that reduce hydrostatic pressure resistance. Hydrostatic design testing is carried out according to ISO 1167 with stress levels and test temperatures selected from the relevant compound standard; long-term strength predictions are developed using ISO 9080. The green colorant is not a stabiliser, and irrigation tubing exposed to chlorinated water or outdoor UV requires a separate additive package validated by the end user. When bags are opened in humid environments above 60% RH, pre-drying at 70°C for 2 h prevents moisture streaks. No potable-water certification should be inferred from this concentrate unless the finished pipe formulation is separately approved under the applicable national drinking-water standard.
Competitive LyondellBasell POLYBATCH™ Woodland Green 30233U/4 Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell POLYBATCH™ Woodland Green 30233U/4 is a pelletised colour concentrate supplied with a linear low-density polyethylene carrier resin. The product is intended for controlled let-down into polyolefin conversion processes, principally blown film, cast film, extrusion coating, and injection moulding using LLDPE, LDPE, HDPE, or compatible polyolefin copolymers. The grade designation identifies a woodland green shade within the POLYBATCH range. The suffix U/4 may encode a stabiliser modification or a product-specific additive package; confirmation from the current LyondellBasell technical data sheet is required before production use. The concentrate is not a finished polymer compound and is not intended for direct moulding or extrusion without dilution into a compatible resin stream. Because the carrier is nonpolar LLDPE, the concentrate is not suitable for polar polymers such as polyamide, polyethylene terephthalate, or polycarbonate.
The applicable specification framework for this product class includes melt mass-flow rate measurement under ISO 1133-1:2022 at 190°C and 2.16 kg, density under ISO 1183-1:2019 or ASTM D1505, and colour-difference evaluation under ASTM D2244 or ISO 11664-4. Product-specific numerical values for 30233U/4 are not reproduced here; published data for this exact formulation is limited. Incoming inspection should use the certificate of analysis and a laboratory-scale let-down plaque or film for optical verification against an agreed CIELAB target. The concentrate is normally supplied as free-flowing pellets, and handling should follow standard practices for polyolefin masterbatches to avoid moisture pickup and contamination.
In cast film and blown film lines, the LLDPE carrier melts through a combination of barrel heat and shear generated by the screw. The carrier’s higher shear viscosity relative to LDPE can assist pigment wetting, but it also requires sufficient screw torque. Single-screw extruders with 24:1 to 36:1 L/D ratios and barrier or Maddock mixing sections are commonly used for this product class. The melt temperature must be maintained within a window that prevents solid carrier particles from reaching the die while avoiding degradation of the pigment system. For LLDPE-based colour concentrates of this type, the melt temperature is generally held between 190°C and 240°C. The exact set-point depends on film gauge, screw design, throughput, and the temperature profile across the barrel.
Dispersion quality is strongly influenced by residence time distribution in the metering section and pressure drop across the screen pack. A screen pack that is too fine may increase back pressure beyond the extruder limit and generate excessive shear heating. A screen pack that is too coarse may not remove pigment agglomerates or gelled carrier fragments. The pressure rise across the screen pack can be used as a manufacturing control variable. An upward drift at constant throughput often indicates pigment agglomeration or incomplete dispersion. Filtration mesh selection is a function of film thickness. For films above 50 µm, a 60/100/60 mesh pack is representative for many polyolefin colour concentrate applications. For thin-gauge films below 25 µm, finer filtration may be required. The specific dispersion limit for 30233U/4 should be obtained from the supplier, because published data for this exact configuration is limited.
| Parameter | Representative condition | Equipment or test reference |
|---|---|---|
| Let-down ratio | 2 wt% to 6 wt% depending on film thickness and colour intensity | loss-in-weight feeder, gravimetric dosing |
| Melt temperature | 190°C to 240°C | single-screw extruder 24:1 to 36:1 L/D |
| Screw speed | 30 rpm to 80 rpm for screw diameters 60 mm to 90 mm | barrier screw with mixing section |
| Screen pack | 60/100/60 mesh typical for film above 50 µm | screen changer or breaker plate |
| Predrying | not required for sealed packaging; dry at 70°C for 2 h if exposed to RH above 60% | desiccant or hopper dryer |
On production-scale blown film lines, lot-to-lot variation in the concentrate can appear as colour drift, die-lip buildup, or screen-pack pressure instability. When a new lot of 30233U/4 is introduced, the converter should record the feeder calibration and the let-down ratio at which the agreed CIELAB target is reached. Because LLDPE carriers are shear-sensitive, changes in extruder throughput should not be compensated only by barrel temperature. If the melt temperature exceeds 240°C, oxidative degradation of the carrier may generate gels and odour. If the melt temperature remains below 190°C, the carrier may not fully melt and may appear as clear flecks in the film. The actual operating range for a given line should be established by a temperature profile study and confirmed by film inspection under ASTM D1003 for haze and by visual rating under standard lighting.
Optical density and colour strength of the diluted concentrate depend on pigment loading, dispersion quality, and film thickness. In thin-gauge blown film, the path length is short, so a higher let-down ratio is generally required to reach the same visual shade as in thicker film. Colour acceptance is typically assessed by CIELAB colour-difference measurements using a spectrophotometer with D65/10° illuminant/observer geometry. The specific target coordinates for Woodland Green 30233U/4 are held by the converter and the supplier; they are not universal values. Published data for this specific formulation is limited, so laboratory let-down at three ratios is recommended to generate a colour-response curve before production scale-up.
Haze and transmission of the final film are measured by ASTM D1003. The pigment particles and the LLDPE carrier can influence haze through surface scattering and bulk scattering. Overdosing the concentrate may raise haze and reduce gloss. Underdosing may produce off-spec colour and higher visual variation. The relationship between let-down ratio and optical density is not linear across all thicknesses. A ratio that is acceptable at 100 µm may be insufficient at 20 µm. Therefore, the colour concentrate should not be specified solely by a fixed percentage without a film-gauge reference. When a converter moves from 80 µm to 25 µm film, the appropriate response is to increase the let-down ratio or select a more heavily pigmented grade, if available.
For outdoor applications such as agricultural film, geomembranes, or protective packaging, weathering performance must be confirmed separately from colour matching. The carrier resin and pigments do not inherently provide adequate UV stability unless the concentrate includes a stabiliser package. The U/4 suffix may indicate a UV-stabilised formulation, but this must be verified against the technical data sheet. Artificial accelerated weathering is commonly conducted under ASTM G154 or ISO 4892-2 with defined irradiance and condensation cycles. The end product is evaluated for colour change, gloss retention, and tensile property retention. A colour concentrate may display acceptable initial colour but fail outdoor exposure if the pigment system lacks sufficient lightfastness. Product-specific weathering data for 30233U/4 should be requested for the intended exposure geography. Food-contact suitability, where required, must be confirmed under 21 CFR 178.3297 for colourants used in polymers and under Commission Regulation (EU) No 10/2011 for plastic materials intended to contact food. The LLDPE carrier alone is not sufficient to establish food-contact status; the pigments and additives must be individually cleared.
When a converter replaces a wax-carrier or EVA-carrier colour concentrate with an LLDPE-based concentrate such as 30233U/4, the differences are most visible in pressure generation, mixing, and final film mechanical properties. EVA and wax carriers generally melt earlier and wet pigments quickly, but their lower molecular weight can contribute to screw slip, die buildup, or reduced tensile modulus at high addition rates. LLDPE carriers maintain the mechanical integrity of the polyolefin matrix more closely and are less likely to plasticise the final film. The trade-off is that LLDPE carriers have higher viscosity and may require more energy input and a more robust screw mixing design.
Compared with LDPE-based colour concentrates, an LLDPE carrier typically has a higher melting point in the range of 120°C to 126°C when measured by ASTM D3418 or ISO 3146. This higher melting point can reduce blocking in warm storage but may require higher barrel temperatures to achieve full melting. Compared with universal carrier systems, an LLDPE-based concentrate is narrower in compatibility but more predictable in polyolefin film applications. It is not recommended for use in polyvinyl chloride, polyamide, polycarbonate, or other polar resins because the carrier is nonpolar and will not co-dissolve. The result is delamination, streaking, or particle formation. For polypropylene, LLDPE carrier can be used at low let-down ratios in some cases, but the effect on crystallisation, shrinkage, and impact should be evaluated by differential scanning calorimetry and mechanical testing.
| Carrier type | Rheological behaviour | Main compatibility boundary | Processing consequence in polyolefin film |
|---|---|---|---|
| LLDPE carrier | higher shear viscosity, linear molecular structure | nonpolar polyolefins | higher torque; closer film toughness retention |
| LDPE carrier | long-chain branching, lower shear viscosity | nonpolar polyolefins | lower torque; may soften film at high let-down |
| EVA/wax carrier | low viscosity, broad wetting | some polar blends; limited thermal stability | rapid dispersion; possible die buildup and haze |
| Universal carrier | mixed polymer/wax system | variable; not equivalent across all resins | dosing convenience; may depress mechanical properties |
Liquid colourants differ from this concentrate in that they require a metering pump and may introduce a carrier liquid into the process. They can achieve colour uniformity at low addition levels but often require more complex feed equipment and may be unsuitable for high-temperature processes due to volatility. Pre-compounded resin eliminates dosing error but increases inventory and is less flexible across product shades. 30233U/4 occupies an intermediate position: a pelletised concentrate that allows ratio adjustment against a natural resin stream, with the carrier contributing to the polymer matrix rather than acting only as a low-viscosity wetting agent.