| HS Code | 195512 |
| Productname | LyondellBasell POLYBATCH White LL8970 TS Concentrate Based In LLDPE |
| Manufacturer | LyondellBasell |
| Producttype | White concentrate |
| Carrierresin | LLDPE |
| Pigment | Titanium dioxide |
| Color | White |
| Form | Pellets |
| Density | 1.90 g/cm³ |
| Meltflowrate | 2.0 g/10 min at 190°C/2.16 kg |
| Titaniumdioxidecontent | 70% |
| Moisturecontent | <0.10% |
| Letdownratio | 5% |
| Pelletsize | 2-3 mm |
| Foodcontactstatus | Complies with FDA |
| Thermalstability | Good |
As an accredited LyondellBasell POLYBATCH™ White LL8970 TS Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell POLYBATCH™ White LL8970 TS Concentrate Based In LLDPE comes in 25 kg polyethylene bags, 40 per pallet (1,000 kg). |
| Container Loading (20′ FCL) | 20′ FCL loaded with palletized 25 kg bags of LyondellBasell POLYBATCH White LL8970 TS LLDPE-based concentrate, stretch-wrapped and secured for ocean freight. |
| Shipping | POLYBATCH™ White LL8970 TS is a white color concentrate in LLDPE pellet form. Ship in original sealed bags, boxes, or octabins on pallets via covered truck, rail, or sea container. Handle as non-hazardous, non-DOT-regulated general cargo. Store cool, dry, away from moisture, contamination, and direct sunlight. Consult SDS for final classification. |
| Storage | Store POLYBATCH™ White LL8970 TS Concentrate in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep original containers tightly closed to prevent moisture, dust, and contamination. Avoid excessive stacking and temperatures that could soften or degrade the LLDPE-based pellets. Keep in original packaging until use. Follow good housekeeping and first-in, first-out stock rotation. |
| Shelf Life | Typically 24 months from manufacture when stored unopened in original packaging below 30°C, dry, and protected from direct sunlight. |
On a three-layer blown-film line configured with skin extruders of 45 mm and 55 mm screw diameter and a core extruder of 65 mm, all with L/D ratios from 24:1 to 30:1, POLYBATCH™ White LL8970 TS Concentrate Based In LLDPE is introduced at the feed throat through a gravimetric dosing unit rather than by tumble blending. The concentrate is metered into the skin layers at 3 wt% to 8 wt% and, when three-layer opacity is required, into the core at 2 wt% to 5 wt%. Because the concentrate is supplied as a titanium dioxide masterbatch in an LLDPE carrier, the final TiO₂ content must be derived from the batch-specific certificate of analysis using the mass-balance equation: let-down ratio = (target TiO₂ concentration / concentrate TiO₂ concentration) × 100. If the target final film TiO₂ content is 4 wt%, the required let-down is 5.7 wt% at a concentrate loading of 70 wt% TiO₂, 6.7 wt% at 60 wt%, and 5.0 wt% at 80 wt%. Melt temperature is controlled between 190 °C and 220 °C, the die gap is set at 1.8 mm to 2.4 mm, blow-up ratio is maintained from 2.2:1 to 3.0:1, and frost line height is positioned at 3 to 7 die diameters to stabilise bubble geometry. Screen pressure is recorded upstream and downstream of a 100/200/325 mesh pack; an increase in filter pressure value measured according to EN 13900-5:2005 indicates pigment agglomeration and poor dispersion. Dart impact of finished film is measured according to ASTM D1709, and tear resistance is evaluated according to ASTM D1922. At storage conditions above 60% relative humidity, the concentrate should be dried at 80 °C for 2 h to 4 h before processing to reduce surface moisture pickup. For food-contact applications, the finished film is assessed under Regulation (EU) No 10/2011, with overall migration not exceeding 10 mg/dm², and under U.S. FDA 21 CFR 177.1520 for olefin polymers; titanium dioxide used as a polymer colorant falls under 21 CFR 178.3297, while direct food colourant status is controlled separately under 21 CFR 73.575. Terminal products fabricated from this configuration include white opaque frozen food overwrap, heavy-duty shipping sacks, industrial liners, and coextruded silage bags. Field experience on production-scale blown-film towers indicates that concentrate overfeed above 9 wt% in the skin layer can generate die lip deposits and bubble instability due to local melt viscosity shifts, particularly when the carrier MFR diverges from the skin resin MFR by more than 1.5 g/10 min as measured under ISO 1133-1:2022 at 190 °C with 2.16 kg. Published data for this specific commercial concentrate configuration is limited, so lot-specific confirmation against the CoA and a short production trial remain necessary before prolonged runs.
| Declared concentrate TiO₂ | Target final TiO₂ | Required let-down ratio |
|---|---|---|
| 60 wt% | 4 wt% | 6.7 wt% |
| 70 wt% | 4 wt% | 5.7 wt% |
| 80 wt% | 4 wt% | 5.0 wt% |
Extrusion coating of white polyethylene onto paperboard, aluminium foil, and flexible barrier substrates places the concentrate into a thin melt curtain rather than a blown bubble, and the let-down ratio is therefore constrained by draw resonance, edge weave, and die lip teardrop streaking at high line speed. The concentrate is normally dosed into an LDPE or LLDPE coating resin at 5 wt% to 12 wt%, depending on coat weight and target hiding power. Melt emerges from a deckled flat die, passes through an air gap of 150 mm to 300 mm, and is quenched on a chill roll maintained at 10 °C to 20 °C; line speeds typically range from 150 m/min to 400 m/min. At the upper let-down range, the higher pigment volume concentration increases melt viscosity and can shift draw resonance onset to lower line speeds. Melt flow rate is measured before and after processing according to ISO 1133-1:2022 at 190 °C and 2.16 kg. Coating adhesion to paperboard is evaluated after extrusion by peel testing under controlled tension, and the final laminate is assessed for heat-seal strength according to ASTM F88/F88M. For liquid packaging board and aseptic structures, the applicable compliance framework includes U.S. FDA 21 CFR 176.170(c) for paper and paperboard components in contact with aqueous and fatty foods, Regulation (EU) No 10/2011 for the plastic layer, and 21 CFR 177.1520 for the olefin polymer matrix. Migration kinetics of titanium dioxide pigment in polyolefin are diffusion-limited and generally low; however, article-level overall migration testing remains mandatory because pigment agglomerates at cut edges and scored lines can behave differently from the continuous coating. The processor should predry the concentrate at 80 °C for up to 3 h when ambient humidity exceeds 60% RH, since moisture in the feed throat can destabilise the melt curtain and produce pinholes. Terminal products associated with this operation include gable-top carton board, aseptic brick packaging, white cupstock, barrier sachet laminates, and coated paper sacks.
Thin-wall polyethylene injection moulding shows a measurable relationship between concentrate addition and gate freeze-off because titanium dioxide concentrates raise melt viscosity when the carrier resin and base resin differ in molecular architecture. The concentrate is metered at 2 wt% to 5 wt% for general thin-wall containers, while higher let-downs of 7 wt% to 9 wt% are used only for thick-section opaque parts where impact requirements are less stringent. A reciprocating-screw injection moulding machine with clamp force from 80 t to 300 t, screw L/D of 20:1 to 24:1, and compression ratio of 2.0:1 to 2.5:1 is used. Barrel temperatures are profiled from a rear zone of 160 °C, centre zones from 180 °C to 200 °C, and a nozzle temperature from 200 °C to 220 °C; mould temperature is held at 15 °C to 40 °C. Gate diameters for thin-wall tubs and closures are between 0.5 mm and 1.2 mm, and injection speed is increased to 80 mm/s to 250 mm/s to counter premature gate solidification. Peak cavity pressure traces under identical shot weight are monitored to detect viscosity drift; a rise greater than 10% at constant melt temperature typically indicates pigment agglomeration or insufficient dispersive mixing. Tensile modulus is measured according to ASTM D638, flexural modulus according to ISO 178:2019, and notched impact according to ASTM D256. For food-contact articles, the applicable standards are U.S. FDA 21 CFR 177.1520 and Regulation (EU) No 10/2011; pharmaceutical packaging produced outside the food-contact scope may additionally require Ph. Eur. chapter 3.1.3 or USP 661.1 evaluation at the finished article level. The LLDPE carrier is not recommended for polypropylene matrix applications without a compatibility assessment, because immiscible carrier domains can reduce impact resistance and create grey streaks in hot-runner tools. Terminal products include margarine tubs, ice cream containers, overcaps, closures, pails, and thin-wall dairy portion cups. On the factory floor, one recurring failure mode is gate blush at pigment loadings above 7 wt%, which is resolved by reducing let-down, enlarging the gate, or increasing mould temperature within the specified window.
Additions above 4 wt% into HDPE blow-moulding grades produce a measurable reduction in parison hang time because the LLDPE carrier alters elongational viscosity and can increase parison sag under constant head pressure. Continuous shuttle or accumulator-head blow moulding machines are used with divergent die heads from 30 mm to 80 mm, parison temperatures between 180 °C and 205 °C, and blow pressures of 0.6 MPa to 1.0 MPa. The concentrate is dosed at 2 wt% to 5 wt% to achieve adequate opacity without excessively reducing top-load stiffness. At 6 wt% and above, converters may need to increase sidewall thickness by 0.1 mm to 0.3 mm to compensate for reduced stiffness in HDPE-rich formulations. Drop-impact testing of blow-moulded containers is performed according to ASTM D2463, and top-load resistance is measured by compression testing at constant crosshead speed. The applicable compliance framework for food-use containers includes U.S. FDA 21 CFR 177.1520 for olefin polymers and Regulation (EU) No 10/2011, with titanium dioxide assessed as a polymer colourant under 21 CFR 178.3297 where relevant. In personal care and household chemical packaging, regulation is less food-contact-oriented but still requires compliance with REACH Annex XVII restrictions and the RoHS heavy-metal limits if the finished article enters an electrical or electronic supply chain. Terminal products include opaque dairy-alternative HDPE bottles, personal care bottles, light-blocking household chemical bottles, and pharmaceutical-grade HDPE pack sizes where article-level compendial testing is completed. Field experience on production-scale shuttle machines indicates that uneven concentrate dispersion can cause wall thickness variation of ±0.2 mm across the same container, particularly when the regrind ratio exceeds 25 wt% and recycled flake carries heat history that modifies viscosity distribution.
Sheet extrusion with subsequent thermoforming uses the concentrate at 4 wt% to 8 wt% in polyethylene sheet formulations, with the concentrate introduced at the hopper of a single-screw extruder of 90 mm to 150 mm screw diameter and L/D from 24:1 to 34:1. Melt temperature is controlled between 190 °C and 230 °C, and the flat die width ranges from 800 mm to 1500 mm. A three-roll polishing stack is operated at 60 °C to 80 °C, producing sheet thicknesses from 0.5 mm to 2.5 mm. Thermoforming is performed by plug-assisted pressure forming at 0.4 MPa to 0.7 MPa with mould temperatures from 20 °C to 50 °C. At the upper end of the let-down range, sheet tensile properties are affected by pigment volume concentration; tensile yield is measured according to ISO 527-2 and flexural modulus according to ISO 178:2019. The concentrate must not be substituted with untreated anatase titanium dioxide, because coated rutile grades are required to limit photocatalytic polymer degradation during long indoor or outdoor exposure. For food-contact trays and cups, Regulation (EU) No 10/2011 overall migration requirements and U.S. FDA 21 CFR 177.1520 apply at the formed article level; industrial trays do not require food-contact positive listing but are typically sold under REACH registration and RoHS heavy-metal screening. Terminal products include opaque dairy cup stock, freezer trays, thin-gauge lids, industrial packaging trays, and non-sterile medical device packaging inserts where the polymer specification permits LLDPE carrier addition. In processing, the main field-observed defect is sheet edge brittleness at regrind ratios above 20 wt%, which is controlled by refining regrind particle size and reducing concentrate dosage rather than increasing screw speed.
| Requirement | Standard or regulation | Verification boundary |
|---|---|---|
| EU plastics food-contact migration | Regulation (EU) No 10/2011 | Overall migration ≤ 10 mg/dm²; article-level testing |
| U.S. FDA olefin polymer status | 21 CFR 177.1520 | Conditions of use must match the polymer citation |
| U.S. FDA polymer colourant | 21 CFR 178.3297 | Titanium dioxide as colourant; no direct food additive status implied |
| EU chemical registration | Regulation (EC) No 1907/2006 | REACH SVHC and Annex XVII screening |
| Pigment dispersion in polymer | EN 13900-5:2005 | Filter pressure value; threshold defined by converter specification |
Where a white/black agricultural film structure is coextruded, the white layer receives the concentrate at 5 wt% to 10 wt% to generate hiding power and reflect solar radiation. The production line is a monolayer or three-layer coextruded blown-film system with die diameter from 250 mm to 1000 mm, die gap from 1.8 mm to 2.8 mm, and a tower height configured for low-stalk extrusion. Melt temperature is kept below 210 °C to reduce the potential for interaction between the LLDPE carrier and stabiliser packages. The white layer is typically formulated with hindered amine light stabilisers and UV absorbers; the concentrate must be evaluated for additive compatibility before large-scale use because some stabiliser combinations can shift the film colour toward yellow under long ultraviolet exposure. Film weathering performance is assessed under ISO 4892-2 or ASTM G154, and mechanical properties are measured before and after ageing according to ISO 527-3. No food-contact positive listing is required for agricultural mulch or silage sheeting, but REACH registration and RoHS heavy-metal screening are commonly included in purchase specifications for European buyers. Terminal products include black/white silage sheeting, greenhouse side sheets, mulch film, and white agricultural cover film. Processing experience on wide agricultural lines shows that white layer melt viscosity must be monitored through extruder load and melt pressure rather than by opacity alone, because pigment dispersion failures can pass through a blown-film die without immediate visual detection and then appear as pinholes after orientation. Predrying at 80 °C for 2 h to 4 h is recommended when the concentrate has been stored in unsealed containers above 60% relative humidity, because surface moisture in the white layer feed throat can destabilise bubble geometry and create local thickness variation.
Competitive LyondellBasell POLYBATCH™ White LL8970 TS Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
POLYBATCH™ White LL8970 TS Concentrate Based In LLDPE is a white masterbatch whose carrier resin is a linear low-density polyethylene. The product is designed for dilution in polyolefin conversion lines where the host resin is LLDPE-rich. The colorant is titanium dioxide; final loading is determined by the let-down ratio and the lot-specific pigment content stated on the certificate of analysis. The concentrate is supplied as free-flowing pellets. Melt flow rate, density, residual moisture, and pigment content are not single fixed values; they are controlled within lot-specific limits and should be verified against the CoA before use. Published data for this specific configuration is limited when it is used outside the supplier’s documented application envelope. Substitution for another white concentrate should therefore be validated on the intended production line rather than inferred from the trade name alone.
On a blown film line, addition rates for this class of TiO₂ concentrate are gravimetrically controlled between 2 wt% and 10 wt%. If the lot-specific pigment loading is 70 wt%, a 3 wt% let-down yields 2.1 wt% TiO₂ in the melt. The LLDPE carrier enters the melt below 190°C; process melt temperatures for LLDPE-rich film are generally maintained between 190°C and 240°C. Screen packs with apertures from 100 µm to 250 µm are placed after the mixing section; dispersed TiO₂ raises the pressure drop across the screen relative to unpigmented LLDPE. The back pressure at the breaker plate should be recorded at constant screw speed because changes in carrier melt index can shift extruder output. The blend melt flow rate should be measured according to ISO 1133-1:2022 at 190°C/2.16 kg before film gauge or frost-line adjustments are made.
The carrier selection influences viscosity matching in LLDPE-rich film, coating, and lamination streams. If a white concentrate with an LDPE or EVA carrier is diluted into a high-molecular-weight LLDPE at 4–6 wt%, the melt-index difference between the carrier and the host resin can produce interfacial flow disturbances. The result on cast film lines is commonly gauge bands or pigment streaks; on blown film lines, the variation can appear as uneven frost-line height. An LLDPE carrier with a melt index within ±5 g/10 min of the host resin, measured per ISO 1133-1:2022, produces a more uniform melt curtain. The LLDPE carrier can, however, increase screw slippage in single-screw extruders with L/D below 24:1, particularly at feed-throat temperatures above 60°C. Grooved-feed extruders with forced barrel cooling and L/D of 30:1–36:1 are preferred when the concentrate is run at high let-down ratios.
The TS designation is a product-family differentiator within the POLYBATCH White range. It is not equivalent to a universal white masterbatch. Published data for this specific configuration is limited, and the TS suffix should not be interpreted as a substitute for the lot-specific CoA. When comparing with a non-TS white concentrate in the same carrier class, users should compare melt flow rate, pigment dispersion as measured by screen-pack pressure rise, and final whiteness index rather than assuming interchangeability.
Dispersion quality is judged by pressure rise across the melt filtration assembly and by optical defect counts in the finished film, not by pellet appearance. On a 75 mm single-screw extruder operating at 150–300 kg/h, a 4 wt% addition of a 70 wt% TiO₂ concentrate can raise screen pressure by 10–40% compared with unpigmented resin. The exact rise depends on screw compression ratio, screw speed, melt temperature, and agglomerate population. Staged screen packs from coarse to fine, such as 100 µm followed by 150 µm or 200 µm, reduce rapid blinding. An increase of 30–50 bar above the established baseline at constant throughput indicates agglomerate accumulation and requires filter replacement or inspection of the masterbatch lot. Because the product is a high-pigment concentrate, poor distributive mixing in a short single-screw design may leave undispersed TiO₂; use of a static mixer or dispersive mixing section after the screw is common on production lines where downstream defects occur.
In cast film, die shear rates between 100 s⁻¹ and 1000 s⁻¹ control melt curtain stability. The shear-thinning behavior of the LLDPE carrier must be considered against the host resin; a mismatch can increase neck-in and edge gauge variation. Melt pumps are used to stabilize output, but the suction pressure can decline if the masterbatch feed is interrupted or if the pellet bulk density varies. Bulk density variations affect gravimetric dosing accuracy; feeders should be calibrated with the actual concentrate rather than with the host resin. Because the concentrate pellets are harder than neat LLDPE and have a higher density, they can stratify in central blending systems if air conveyance is too aggressive.
In multi-layer coextrusion, the concentrate is usually dosed into the outer or core layer. The LLDPE carrier may have a different melting profile than metallocene plastomers or EVA sealants; it should not be used in a sealant layer where a low seal-initiation temperature is critical unless seal strength is revalidated per ASTM F88/F88M-21. For extrusion coating and lamination, the masterbatch is added to the LLDPE-rich coating melt. Optical performance of the final laminate is measured as haze and total luminous transmittance per ASTM D1003-21, and whiteness is evaluated by CIE whiteness index using ISO 11664-4:2008. If the masterbatch loading exceeds 6 wt%, the coefficient of friction can change; slip and antiblock additions should be adjusted after measurement per ISO 8295:1995. The LLDPE carrier also affects heat-seal curve shape in lamination; seal strength at given dwell and pressure must be rechecked when the concentrate is introduced at a new let-down ratio.
When the concentrate is used in film, tensile properties are measured according to ASTM D882-18 rather than ASTM D638-14 if the specimen is a thin film. For thicker sheet or molded plaques, ASTM D638-14 is applicable at 50 mm/min for Type IV specimens. The addition of TiO₂ increases stiffness slightly and reduces elongation at break depending on loading; these changes should be quantified on the final gauge film. Film impact toughness can be measured by ISO 7765-1:1988 or supplier-specific dart-drop methods. Because the LLDPE carrier contributes to the overall crystallinity and orientation, annealing history and blow-up ratio affect the mechanical data; the test conditions must be reported with the result.
Because the product is a concentrate, the final regulatory status is determined by the host resin, the let-down ratio, and the intended food-contact or industrial use. The polyethylene carrier is generally evaluated under FDA 21 CFR 177.1520, while the colorant is considered under FDA 21 CFR 178.3297. European migration compliance is assessed in the final article under EU 10/2011. Heavy-metal restrictions under RoHS 2011/65/EU Annex II and communication obligations under REACH 1907/2006 should be confirmed with the SDS and certificate of compliance. A supplier statement that the masterbatch is compliant without reference to the final article and its use conditions is insufficient for food-contact packaging.
Food-contact status is not an intrinsic property of the concentrate. Under EU 10/2011, the overall migration limit for plastic materials is 10 mg/dm², or 60 mg/kg for food intended for infants and young children, with testing performed in the appropriate simulant and time-temperature condition from Annex III and Annex V. The final article must be tested as a complete formulation. The LLDPE carrier is generally covered by FDA 21 CFR 177.1520 when the final olefin polymer meets the applicable specifications and conditions of use. Titanium dioxide as a colorant is evaluated under FDA 21 CFR 178.3297. The masterbatch supplier should state the approved let-down range; use outside that range invalidates the compliance statement and requires end-use migration testing.
| Reference | Scope | Relevant condition or clause |
|---|---|---|
| EU 10/2011 | Plastic food-contact materials | Overall migration limit; Annex III and Annex V testing |
| FDA 21 CFR 177.1520 | Olefin polymers for food contact | End-use conditions and specifications for polyethylene |
| FDA 21 CFR 178.3297 | Colorants for polymers | Permitted use conditions for titanium dioxide |
| REACH 1907/2006 | Chemical registration and SVHC communication | Article 33 notification duties |
| RoHS 2011/65/EU | Hazardous substances in electrical and electronic equipment | Annex II restricted substances |
| ISO 1133-1:2022 | Melt mass-flow rate of thermoplastics | 190°C/2.16 kg condition for polyethylene |
| ISO 1183-1:2019 | Density determination | Immersion method for non-cellular plastics |
| ASTM D1003-21 | Haze and luminous transmittance | Transparent plastic film measurement |
| Parameter | Typical production window | Measurement method or device |
|---|---|---|
| Let-down ratio | 2–10 wt% depending on final TiO₂ target | Gravimetric feeder; mass-balance calculation |
| Melt temperature | 190–240°C | Melt probe or IR pyrometer at die |
| Screen pack aperture | 100–250 µm | Mesh inspection and back pressure |
| Blend MFR | Within ±5 g/10 min of host resin | ISO 1133-1:2022 |
| Drying temperature for opened containers | 70–80°C for 2–4 h | Desiccant-air dryer |
Field observations indicate three recurring failure modes when this class of concentrate is mishandled. First, feed-throat bridging occurs when pellets soften at high feed-throat temperatures; keeping the feed zone below 60°C avoids clogging. Second, moisture in opened containers generates microvoids and lens-shaped defects in film; pre-drying is necessary at 70–80°C for 2–4 h. Third, screen-pack blinding with agglomerates produces pressure rise and film streaks; the corrective action is a lot inspection and staged filtration rather than increasing melt temperature, because excessive temperature can degrade the LLDPE carrier and shift the final film seal performance.
Production-scale substitution of POLYBATCH™ White LL8970 TS for another white masterbatch should not be based on pigment loading alone. The screw geometry, melt temperature profile, and screen-pack arrangement of the target line influence dispersion and pressure rise. Operators should record screw speed, back pressure, melt temperature, and gravimetric dosing accuracy against lot-specific CoA data before full production release. If the host resin is a metallocene LLDPE or a high-melt-strength LLDPE, shear heating in the metering section may differ from conventional Ziegler-Natta LLDPE; melt temperature should remain within the host resin limitation, typically 190–240°C for LLDPE film. When moisture is suspected because of opened containers stored at relative humidity above 60%, pre-drying at 70–80°C for 2–4 h with desiccant air may be required; the exact drying curve should be confirmed with the manufacturer. Published data for this specific configuration is limited; line-trial performance remains the final acceptance criterion.