Lyondellbasell Polybatch White Ll8855 Gp Concentrate Based In Lldpe

LyondellBasell POLYBATCH™ White LL8855 GP Concentrate Based In LLDPE

    • Product Name: LyondellBasell POLYBATCH™ White LL8855 GP Concentrate Based In LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 379668
    Product Name LyondellBasell POLYBATCH™ White LL8855 GP Concentrate Based In LLDPE
    Supplier LyondellBasell
    Brand POLYBATCH™
    Product Type White masterbatch concentrate
    Carrier Resin LLDPE
    Color White
    Form Pellets
    Appearance White pellets
    Additive Titanium dioxide
    Titanium Dioxide Content 70%
    Density 2.0 g/cm³
    Melt Flow Rate 10 g/10 min (190°C/2.16 kg)
    Moisture Content <0.10%
    Recommended Let Down Ratio 4-8%
    Processing Temperature 180-240°C
    Packaging 25 kg bags
    Shelf Life 24 months

    As an accredited LyondellBasell POLYBATCH™ White LL8855 GP Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Typically supplied in 25 kg polyethylene-lined bags on pallets, with optional 1,000 kg bulk bags for industrial transport.
    Container Loading (20′ FCL) 20′ FCL container loaded with shrink-wrapped pallets of 25 kg bags of LyondellBasell POLYBATCH™ White LL8855 GP LLDPE-based concentrate.
    Shipping POLYBATCH™ White LL8855 GP ships as non-hazardous, free-flowing pellets in 25 kg polyethylene bags or 1000 kg bulk bags, palletized and stretch-wrapped. Not classified as dangerous goods. Transport in clean, dry trucks or containers; store cool, dry, away from direct sunlight. Handle with standard industrial hygiene.
    Storage Store LyondellBasell POLYBATCH™ White LL8855 GP Concentrate Based In LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep original containers tightly closed to prevent moisture, dust, and contamination. Avoid excessive heat, UV exposure, and prolonged high temperatures. Stack pallets securely, protect from damage, and rotate inventory following supplier guidance.
    Shelf Life Two years from manufacture when stored unopened in original packaging, dry, at ambient temperatures, protected from direct sunlight.
    Application of LyondellBasell POLYBATCH™ White LL8855 GP Concentrate Based In LLDPE

    In monolayer and coextruded blown film lines producing white opaque packaging for hygiene and consumer overwrap, POLYBATCH™ White LL8855 GP Concentrate Based In LLDPE is metered at a let-down ratio of 4–8% by mass into a dry-blended LLDPE/LDPE feedstock. The concentrate is added via a gravimetric feeder at the main feed throat rather than through a side feeder because the LLDPE carrier melts within the same temperature range as typical film-grade LLDPE and its viscosity remains close enough to maintain screw-fed pressure stability. Production-scale experience on 60 mm single-screw extruders with an L/D 30:1 barrier screw and a Maddock mixing section indicates that acceptable visible whiteness in 40–60 µm film is obtained at the lower end of the let-down range; thicker opaque overwrap at 80–120 µm commonly requires the upper end. Process settings for these runs include a die gap of 1.8–2.2 mm, a blow-up ratio of 2.2:1–2.8:1, and a frost line height maintained at 3–5 die diameters. Lowering the frost line below 3 die diameters while increasing let-down above 8% has been observed to produce die-lip deposition appearing as white streaking in the web. This build-up is a field failure mode associated with oxidized pigment-binder residues accumulating at the lip, and it is managed by periodic purging with unfilled PE or by metallic stearate-based purging compounds. Compliance for finished food-contact packaging film is assessed under EU Regulation 10/2011 Annex I and FDA 21 CFR 177.1520 for olefin polymers, with migration limits confirmed on the final film rather than on the raw concentrate; RoHS 2011/65/EU applies for non-food technical packaging. Terminal articles produced from this configuration include white opaque bag-in-box outer films, hygiene product overwrap, bakery bags, collation shrink film, and industrial sack liners. A process boundary applies when melt temperature exceeds 240 °C for more than 20 minutes: yellowing of the LLDPE carrier becomes measurable by ASTM E313 yellowness index and reduces perceived whiteness. Extruder zones are therefore normally held at 180–210 °C. If pellet surface condensation is observed after storage above 60% relative humidity, drying at 70 °C for 2 hours is required before feeding because water vapour is a known source of microvoids and gel defects in blown film.

    Does Thin-Wall Injection Moulding Change the Practical Let-Down Limit for LLDPE-Based White Concentrate?

    Thin-wall HDPE and LLDPE injection moulded articles, particularly caps, overcaps and food container lids, incorporate the concentrate at a let-down ratio of 3–6% by mass. The lower end is preferred when nominal wall thickness is below 1.0 mm and flow length-to-thickness ratios exceed 200:1, because the LLDPE carrier of POLYBATCH™ White LL8855 GP can increase injection pressure and alter the crystallization behaviour of the matrix. On a 120-ton hydraulic injection moulding machine with a 24 mm screw and a two-cavity hot-runner valve-gate tool, 4% let-down in an HDPE closure resin with a melt flow rate of 4 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022 requires a melt zone setpoint increase of 5–10 °C relative to natural HDPE to avoid gate blush and flow-line visibility. Processing personnel report that colour streaks are minimized when screw back pressure is maintained at 8–12 MPa and screw speed is kept below 80 min⁻¹; higher shear does not proportionally improve particle break-up and can generate frictional heat sufficient to yellow the LLDPE carrier. The compliance path for caps and lids intended for food contact includes FDA 21 CFR 177.1520 and EU Regulation 10/2011, with end-article total migration evaluated under Annex V of 10/2011. For pharmaceutical closures, the relevant compendial method is USP <661.1> for plastic packaging systems. Terminal finished products include white HDPE bottle caps, overcaps for cosmetic closures, tamper-evident caps, and lightweight food container lids. A known operational boundary appears at let-down ratios above 6% in very thin hinges or living hinge geometries: the LLDPE carrier phase elongates differently from HDPE and can leave visible flow-orientation marks. Published data for this specific concentrate in living hinge tools is limited, so production trials are required before final tool acceptance.

    Conversion RouteTypical Let-Down RangeMelt Temperature RangeCritical Process ParameterPrimary Test Method
    Monolayer blown film4–8%180–220 °CFrost line height, die-lip depositionASTM D1003-21
    Thin-wall injection moulding3–6%200–240 °CBack pressure, gate blushISO 1133-1:2022
    Extrusion blow moulding5–10%190–220 °CParison sag, pinch-off thicknessISO 1133-1:2022
    Cast film extrusion5–9%220–250 °CChill roll plate-out, vacuum controlASTM D1003-21
    Sheet extrusion and thermoforming4–8%210–240 °CMelt filtration, polishing roll gapISO 1183-1:2019
    White PE conduit and duct3–6%190–225 °CVacuum calibration, ESCR retentionASTM D1693-21

    Extrusion Blow Moulding Container White Coverage Requires a Narrow Carrier Viscosity Window

    Extrusion blow moulding of opaque HDPE containers for liquid soap, personal care products and pharmaceutical droppers uses POLYBATCH™ White LL8855 GP at 5–10% by mass in the hopper blend. The target opacity in sidewalls of 0.8–1.5 mm thickness usually requires 6–8% let-down; higher loadings are reserved for bright white heavy-wall industrial containers. The LLDPE carrier is lower in melt viscosity than a typical HDPE blow moulding grade, so addition above 8% can reduce parison melt strength and increase parison sag during extrusion from an accumulator head. On a 75 mm grooved-feed extrusion blow moulding machine with an L/D 20:1 screw and a diverging die head running at 190–220 °C, the parison length control system must be adjusted when the let-down ratio changes by more than 2 percentage points; otherwise bottom pinch-off wall thickness becomes inconsistent. Compliance for direct food-contact containers falls under FDA 21 CFR 177.1520 and EU Regulation 10/2011; for pharmaceutical containers, USP <661.1> and Ph. Eur. 3.1.3 apply to the final container and its extractable profile. Terminal products include white HDPE personal care bottles, low-density polyethylene squeeze bottles, pharmaceutical dropper bottles, and white industrial container bodies. A production boundary appears when regrind containing the white concentrate is re-extruded at 60% or more: double-pass TiO₂ particles alter melt elasticity and can generate gel-like defects at the die lip. Pre-drying is not normally required if the original bag remains sealed and storage is below 60% relative humidity; if pellet surface condensation is observed, drying at 70 °C for 2 hours is recommended before blowing. Dispersion is checked by monitoring pressure rise on a 63/88/125 mesh screen pack; a rise above 0.8 MPa over 10 min indicates agglomerates in the melt stream.

    Ordinarily, cast film extrusion for white opaque hygienic backsheet and film label facestock meters the concentrate at 5–9% by mass directly into the extruder throat of a 90 mm single-screw machine with an L/D 30:1 barrier screw and a slot die with flexible lip adjustment. The addition level depends on basis weight: 20–30 µm white cast films for diaper backsheet commonly use 5–6%, while 50–80 µm label facestock and printed film use 7–9% to maintain opacity after stretching and silicone coating. The process operates with melt temperatures of 220–250 °C at the die and a chill roll temperature of 18–30 °C; raising chill roll temperature above 35 °C during TiO₂-bearing film production can cause plate-out on the matte roll and reduce surface gloss. Vacuum box settings at -0.2 to -0.4 kPa are adjusted to maintain film-to-chill roll contact without creating edge pinning defects. Compliance for the finished film used in food laminations follows EU Regulation 10/2011; FDA 21 CFR 177.1520 applies for US olefin polymer food contact; REACH SVHC content and RoHS 2011/65/EU heavy metal limits are verified by XRF on the final white film. Terminal products include white backsheet for baby diapers and adult incontinence garments, direct thermal label facestock, printed wrappers, and white base films for technical lamination. A known failure condition occurs when edge trim regrind from white cast film is re-fed above 25%: TiO₂ concentration builds and the polymer phase receives additional heat history, increasing gel count and reducing tear resistance. Standard practice is to limit white regrind content or to side-feed screened regrind rather than adding it at the main feed throat.

    Standard or RegulationScopeVerification Parameter
    EU Regulation 10/2011Food-contact plastic articlesOverall migration limit 10 mg/dm²
    FDA 21 CFR 177.1520Olefin polymers for food contactEnd-article formulation and migration
    USP <661.1>Plastic packaging systems for pharmaceutical useExtractables and leachables profile
    Ph. Eur. 3.1.3Polyolefins for pharmaceutical packagingTotal oxidizable substances
    RoHS 2011/65/EUElectrical and electronic equipmentPb 1000 mg/kg, Cd 100 mg/kg, Hg 1000 mg/kg, CrVI 1000 mg/kg
    REACHEU chemical registration and SVHC obligationsSVHC declaration and communication

    HDPE/LLDPE Sheet Extrusion and Thermoforming for White Food-Contact Trays

    Sheet extrusion for white thermoformed food containers and dairy tubs incorporates the LLDPE-based white concentrate at 4–8% by mass in HDPE or HDPE/LLDPE sheet formulations. The concentrate is pre-dispersed in an LLDPE carrier, but the sheet line still requires melt filtration because the polished three-roll stack amplifies any pigment agglomerate into visible pimples on the sheet surface. A typical 120 mm single-screw extruder with L/D 34:1 and a gear pump delivers melt at 210–240 °C to a 1,200 mm wide coat-hanger die; the polishing roll gap is set to final sheet thickness plus 10–20% to accommodate die swell. Thermoforming is then performed on continuous roll-fed equipment with HDPE sheet temperatures around 130–160 °C. The whiteness of the formed tray is influenced more by uniform TiO₂ dispersion in the extruded sheet than by absolute let-down ratio; screen packs of 80/120/80 mesh are installed to rupture residual agglomerates. Compliance for food-contact dairy and deli containers follows EU Regulation 10/2011 and FDA 21 CFR 177.1520, with migration testing on the thermoformed tray rather than the pellet alone. Terminal products include white dairy cups, margarine tubs, deli containers, hot-fill food tubs, and white refrigerator inner liners. A process limitation emerges when concentrate addition exceeds 10%: higher solids content reduces melt extensibility and can cause edge sag at the die, while the increase in TiO₂ raises thermal conductivity and changes cooling times during thermoforming. Regrind from thermoform skeletons can be recycled into the coextruded cap or tie layer, but not into the glossy skin layer above 50% if surface gloss is controlled against production standards.

    When LL8855 GP Is Added to Polyethylene Electrical Conduit and Communications Duct

    White polyethylene electrical conduit and communications duct represent a non-food technical application for the concentrate. The addition ratio is 3–6% by mass in an HDPE/LLDPE blend, because the white code is intended for identification rather than high opacity; higher loadings are uncommon because they increase the risk of microvoid formation at the inner wall of corrugated duct. Extrusion is performed on a twin-screw or single-screw profile line with vacuum sizing, a 25:1–30:1 barrier screw, and a melt temperature of 190–225 °C. Vacuum calibration at -30 to -60 kPa controls the outer diameter of ribbed conduit, and downstream water spray maintains the surface finish. The finished conduit is tested for environmental stress-crack resistance under ASTM D1693-21 or ISO 22088-1:2020; the white pigment does not replace UV stabilization, so an outdoor-grade stabilizer package is required when the conduit is exposed to sunlight. Compliance for heavy metal content follows RoHS 2011/65/EU and REACH SVHC limits; electrical conduit performance is verified according to the relevant IEC 61386 series for conduit systems. Terminal products include white electrical raceway, communications cable duct, and white conduit fittings. A field limitation applies when the regrind fraction of white conduit exceeds 30%: repeated heat exposure can reduce ESCR and cause surface microcracking at flex points, so the white regrind is normally balanced with virgin polyethylene and screened through a 125 µm mesh pack.

    Free Quote

    Competitive LyondellBasell POLYBATCH™ White LL8855 GP Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell POLYBATCH™ White LL8855 GP Concentrate Based In LLDPE is a pelletized white masterbatch in which rutile TiO2 pigment is dispersed in a linear low-density polyethylene carrier. The grade is intended for let-down in polyolefin extrusion and molding rather than for direct finished-part production. Incoming quality control is performed using melt mass-flow rate under ISO 1133-1:2022, density under ISO 1183-1:2019, and ash content under ISO 3451-1:2019. The current manufacturer’s technical data sheet states nominal values; lot-specific values are shown on the certificate of analysis. Published third-party data for this exact configuration is limited, so plant qualification should include a controlled dispersion trial on the target production line.

    Rheological Measurement and Incoming Material Qualification

    The carrier melt index is measured at 190 °C under a 2.16 kg load. General-purpose white concentrates in this class typically exhibit a melt mass-flow rate between 5 g/10 min and 25 g/10 min. A value below the base resin’s melt index can produce poor pigment distribution in shallow-channel film dies, while a value far above the base resin reduces bubble stability in blown film and promotes die-lip plate-out. The LLDPE carrier softens near 120–125 °C; therefore, any drying step should remain below 70–80 °C and use desiccant air with a dew point below -20 °C. Moisture content above 0.10 wt% causes splay, pinholes, and optical haze. Ash content indicates titanium dioxide loading, commonly 55–70 wt% for this class; density correspondingly falls between 1.55 g/cm3 and 1.90 g/cm3. The specific nominal values for LL8855 GP are verified with the lot certificate and should not be assumed from similar-sounding grades.

    PropertyMethodConditionControl purpose
    Melt mass-flow rateISO 1133-1:2022190 °C, 2.16 kgCarrier compatibility and let-down
    DensityISO 1183-1:2019Method A, 23 °CTiO2 loading estimate
    Ash contentISO 3451-1:2019600 °C to constant massTitanium dioxide content
    Dispersed pigment specksISO 18553:2021Pressed film 100 µmAgglomeration control
    CIE whitenessISO 11475:2017D65 illuminant, 10° observerVisual consistency

    Dispersive mixing of rutile titanium dioxide requires exceeding the cohesive strength of pigment agglomerates. In a single-screw extruder with 25–30 L/D, the highest shear rates occur in the metering section and in the dispersive mixing element. For a 60 mm screw running at 80 rpm, wall shear rates in the metering section can exceed 100 s-1. A Maddock mixer or Egan mixing section increases residence time in high-stress zones and improves titanium dioxide wetting. Screen packs with 60/80/100 mesh layers and a breaker plate create additional backpressure, but sustained backpressure above 350 bar can overheat the LLDPE carrier and degrade the pigment surface treatment.

    In thin-gauge blown film below 30 µm, the concentrate should not be flood-fed alone into the main hopper. A gravimetric feeder with a vertical C-frame or static mixer at the feed throat provides distributive mixing. Dispersion quality is screened under ISO 18553:2021, with a common acceptance criterion of <10 visible specks per 100 cm2 in a pressed film. For high hiding power, let-down ratios of 4–8 wt% are generally required in this pigment-loading class; exact ratios are derived from target CIE whiteness under ISO 11475:2017 and contrast ratio under ISO 6504-3:2019. The extruder should be a barrier screw with 25–30 L/D and a Maddock mixer or equivalent dispersive mixing element. Melt temperature in the die should be maintained between 204 °C and 232 °C for LLDPE-based systems; higher temperatures can cause edge oxidation and yellowing of the pigment coating.

    What Let-Down Ratios Prevent Agglomerate-Induced Optical Defects in Thin Films?

    Optical defects in titanium dioxide concentrates arise when undispersed agglomerates scatter visible light locally, creating gel-like specks or white spots. The minimum let-down ratio is not fixed by the concentrate but by the base resin viscosity, the screw mixing regime, and the film thickness. In a typical extrusion line with a 60 mm barrier screw, reducing the concentrate dosage below 3 wt% may not provide sufficient color strength; increasing it above 10 wt% can raise the melt viscosity outside the stable window of the die. A designed experiment varying let-down ratio across 3, 5, 7, and 9 wt% and measuring CIE whiteness and contrast ratio is the reliable method. Each test point should use a 50 µm film sample and a calibrated spectrophotometer under ISO 11664-2:2007 traceability.

    When the Concentrate Is Substituted for an LDPE-Carrier White in Blown Film

    The choice between an LLDPE carrier and an LDPE carrier changes the shear and extensional viscosity responses in the two primary film deformation zones: the die land and the bubble. LLDPE carriers generally exhibit lower long-chain branching and a more linear backbone than LDPE carriers; this reduces shear-thinning sensitivity in the die and increases bubble stability under high-stalk conditions. In practice, replacing an LDPE-carrier white with an LLDPE-carrier concentrate in a monolayer blown film line may require a 5–10 °C increase in die temperature to keep die pressure within the extruder’s maximum specific torque. A 25 mm single-screw extruder with 24 L/D can show a 0.5–1.5 MPa increase in die pressure per 1 wt% increase in concentrate loading when the carrier molecular weight distribution differs from the base resin. These values are system-specific and must be measured on the actual line with pressure transducers installed upstream of the screen pack.

    Carrier typeDensity rangeMelt-flow behaviorCompatibility in PE filmProcessing consequence
    LLDPE0.918–0.940 g/cm3Linear structure; moderate shear thinningHigh with LLDPE/HDPEBetter bubble stability; higher die pressure
    LDPE0.915–0.935 g/cm3Long-chain branched; high shear thinningHigh with LDPE/LLDPELower die pressure; lower melt strength at high temperature
    PP0.900–0.910 g/cm3Semicrystalline; lower viscosity at high shearLow in LLDPE filmCan form separate domains and gel-like defects

    The viscosity mismatch between the concentrate and the base polymer is characterized by capillary rheometry under ISO 11443:2021. A ratio of concentrate viscosity to base resin viscosity between 0.7 and 1.3 at the die shear rate is usually acceptable for blown film. If the ratio exceeds 1.5, die-lip plate-out and visible melt fracture may appear at the film edges. In cast film, the critical shear stress for melt fracture of LLDPE is typically in the range of 0.10–0.30 MPa; exceeding this value results in sharkskin or cyclic surface roughness.

    High-speed cast-film lines running at 300 m/min or higher impose extensional strain rates that exceed the relaxation time of low-melt-strength carriers. If the white concentrate is diluted below the recommended level to save material, the film may exhibit poor surface wetting of titanium dioxide agglomerates, streak formation, and uneven opacity. In addition, over-dilution of an LLDPE carrier in a cast-film grade with high melt index lowers the blend’s extensional viscosity, which can shift the draw resonance boundary and reduce the stable draw ratio. Draw resonance is observed as periodic thickness variation in machine direction; it is minimized by maintaining a die gap between 0.5 mm and 0.8 mm and an air-knife position matched to the melt web. Because the carrier is LLDPE, melt temperature should be kept below 260 °C to suppress gel formation; at die temperatures above 280 °C, low-molecular-weight fractions may degrade and produce visible white specks. In extrusion coating of paper and board, a coat weight of 12–20 g/m2 requires a low let-down ratio because the optical path is short; titanium dioxide agglomerates become visible as pinpoints. Concentrate feed should be positioned after the primary resin feed but before the screw’s compression zone, not at the vent port, to avoid pigment loss. Die temperatures between 250 °C and 270 °C are typical for LLDPE extrusion coating, but the exact profile must be reduced if the line runs below 50 m/min to prevent thermal degradation.

    Injection Molding and Sheet Extrusion Operate Within a Narrow Thermal Window

    In injection molding of polyolefin caps, containers, and thin-wall parts, the LLDPE carrier of POLYBATCH™ White LL8855 GP influences the screw recovery phase and the melt-mixing zone. The concentrate should be metered into the main material feed, not into the regrind stream alone, to prevent pigment concentration gradients. For parts with wall thickness below 1.0 mm, a let-down ratio of 2–4 wt% is often sufficient for opacity when the base resin is a polypropylene copolymer; however, an LLDPE carrier may reduce the flexural modulus of the molded article relative to a PP-carrier white. This modulus shift is measurable under ISO 178:2019 and should be evaluated if the part is load-bearing. The melt temperature should follow the base resin recommendation, typically 200–250 °C for polypropylene, but the LLDPE carrier itself should not be processed above 260 °C to avoid discoloration. Back pressure of 0.5–1.5 MPa and screw speed of 50–150 rpm are common starting points on a 35 mm screw; actual settings depend on L/D ratio and check-ring condition.

    For sheet extrusion of HDPE or LLDPE, the concentrate can be added at 3–6 wt% to achieve a uniform white color in sheet thicknesses from 0.5 mm to 3.0 mm. The LLDPE carrier provides a broader compatibility window with polyethylene-based regrind than a PP-carrier white and reduces the risk of melt-index stratification in the die. In barrier sheet containing EVOH or polyamide layers, the concentrate should be confined to the polyolefin skins; if it is introduced into the barrier layer, the titanium dioxide may act as a nucleating heterophase and reduce gas barrier performance measured under ISO 15105-2:2020. A static mixer or melt pump is recommended upstream of the flat die to damp pressure fluctuations caused by viscosity differences between the concentrate and the base resin.

    End-use regulatory suitability must be assessed using the manufacturer’s current statement of composition. For food-contact applications in the European Union, the LLDPE carrier and the titanium dioxide must comply with Regulation (EU) No 10/2011 and its amendments; migration testing may be required according to EN 1186-1:2002 depending on contact conditions. In the United States, olefin polymers used in contact with food must conform to 21 CFR 177.1520, and colorants must conform to 21 CFR 178.3297. The presence of a masterbatch at typical let-down ratios does not automatically confer food-contact approval; the finished article must be tested by the converter under the applicable time and temperature conditions.

    For industrial packaging and durable goods, documentation should confirm that the pigment and carrier meet the restriction conditions of REACH Annex XVII and RoHS Directive 2011/65/EU if applicable. The product is not intended for medical device use unless explicitly validated under ISO 10993-1:2018 for the finished device. Storage should be in unopened bags at 10–35 °C and below 60% relative humidity. Opened bags should be re-sealed and consumed within 48 h in humid environments to prevent moisture uptake above 0.10 wt%. Shelf life is generally 24 months from date of manufacture when stored in unopened bags under the stated conditions. Direct sunlight exposure can oxidize the polyethylene carrier and shift CIE yellowness index measured under ISO 11664-4:2008.

    Top