| HS Code | 898377 |
| Productname | LyondellBasell POLYBATCH™ White LL8844 GP |
| Manufacturer | LyondellBasell |
| Producttype | White masterbatch |
| Appearance | White pellets |
| Carrierresin | LLDPE |
| Pigment | Titanium dioxide |
| Titaniumdioxidecontent | 75% |
| Density | 1.95 g/cm³ |
| Meltflowrate | 8 g/10 min at 190°C/2.16 kg |
| Moisturecontent | <0.10% |
| Bulkdensity | 1.10 g/cm³ |
| Thermalstability | 250°C |
| Recommendeddosage | 5-10% |
| Processingtemperature | 180-260°C |
| Foodcontactcompliance | FDA and EU 10/2011 compliant |
| Shelflife | 24 months |
| Storagetemperature | Below 30°C |
As an accredited LyondellBasell POLYBATCH™ White LL8844 GP factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell POLYBATCH™ White LL8844 GP is supplied in 25 kg polyethylene-lined bags, typically palletized for industrial handling. |
| Container Loading (20′ FCL) | A 20′ FCL container loaded with LyondellBasell POLYBATCH™ White LL8844 GP chemical, palletized bags, securely stowed for ocean freight. |
| Shipping | LyondellBasell POLYBATCH™ White LL8844 GP is a non-hazardous, solid white masterbatch. It is not regulated for transport by DOT, IMDG, or IATA; no UN number, hazard class, or packing group applies. Ship in sealed 25 kg bags or octabins, keep dry, avoid excessive heat, and handle as normal industrial freight. |
| Storage | Store LyondellBasell POLYBATCH™ White LL8844 GP in original, tightly sealed packaging in a cool, dry, well-ventilated warehouse. Protect from direct sunlight, heat, moisture, and contamination. Keep away from ignition sources, oxidizers, and incompatible materials. Avoid excessive stacking and dust generation. Close containers after use, maintain stable ambient temperature, and rotate stock to preserve shelf life. |
| Shelf Life | Shelf life: 24 months from manufacture when stored unopened in original packaging, dry, below 30°C, away from direct sunlight. |
In monolayer LLDPE blown-film lines where film thickness is reduced below 40 µm, POLYBATCH™ White LL8844 GP is introduced by gravimetric dosing at the feed throat, not by hot-melt pre-dispersion, because the masterbatch’s nominal 70 wt% rutile titanium dioxide payload requires screw mixing rather than additional heat history. For dairy overwrap and bakery bag applications, the finished film falls under EU 10/2011 food-contact migration testing with an overall migration limit of 10 mg/dm² and under FDA 21 CFR 177.1520(c) for olefin polymers; if titanium dioxide must be listed as a color additive in a specific export market, FDA 21 CFR 73.575 is the applicable designation. The recommended dry-blend let-down ratio is 4–8 wt% for films between 40 µm and 70 µm, yielding a nominal final TiO2 concentration of 2.8–5.6 wt%; the upper half of that range is used where luminous transmittance below 10% under ASTM D1003-13 is required for frozen food packaging or white label facestock. Processing on a grooved-feed extruder with 30:1 L/D, barrier screw, and die gap 1.4–1.8 mm is maintained at melt temperature 195–210 °C, blow-up ratio 2.0:1–2.8:1, and frost line height between 2 and 4 die diameters to balance bubble stability against crystalline orientation. Die-lip deposit formation becomes measurable after 12–16 h continuous running at the top of the recommended addition range, and screen-pack differential pressure increases by 0.4–0.8 MPa before a breaker-plate change is scheduled, which is the primary production bottleneck rather than extruder motor load. Pre-drying is not required below 60% RH, but above 60% RH the blend transfer lines must avoid condensation because surface moisture on the masterbatch granules produces TiO2 agglomerates that appear as white specks at the die lip. Terminal products include white dairy overwrap film, bread bags, frozen food packaging, can liners, and white label facestock where opacity and stiffness are simultaneously required.
Extrusion coating at line speeds above 150 m/min places the masterbatch into a 290–315 °C melt stream with oxygen exposure at the die exit, so thermal stabilization of the carrier and dispersant package is more process-critical than in film blowing. In foodservice paperboard coating, compliance is assessed under EU 10/2011 overall migration limit 10 mg/dm², FDA 21 CFR 177.1520(c), and EU Directive 94/62/EC Article 11 for total lead, cadmium, mercury, and hexavalent chromium not exceeding 100 mg/kg. The let-down ratio for a 15–25 g/m² white LDPE or LLDPE coating layer is 8–12 wt%, corresponding to a nominal final TiO2 level of 5.6–8.4 wt%; below 8 wt%, pinholes in the coating become visible when dark paperboard is folded at crease lines, while above 12 wt% melt-curtain cohesion declines and edge waviness increases. A typical line configuration uses a 90 mm single-screw extruder with 30:1 L/D, die gap 0.6–0.7 mm, air gap 150–250 mm, chill roll temperature 10–18 °C, and corona treaters after the chill roll to raise dyne level above 42 mN/m. Neck-in increases by 5–10 mm per side at the highest addition rates because highly filled TiO2 melts exhibit a steeper rise in elongational viscosity under curtain draw; operators compensate by widening the deckle and increasing melt pressure slightly, but adhesion to paperboard remains acceptable only if the oxidised melt curtain is not quenched below 15 °C before contact. Processing above 320 °C is not recommended because the LLDPE carrier degrades and TiO2-catalysed carbonyl formation may raise odour levels and reduce heat-seal strength. Terminal end uses include paper drinking cups, foodservice carton stock, coated paperboard plates, and the white pigmented layer in laminated flexible food packaging.
Because gate shear rates exceed 30,000 s-1, POLYBATCH™ White LL8844 GP in thin-wall polyolefin container molding is judged primarily by dispersion quality rather than opacity alone. Food-contact compliance for molded dairy tubs and spread portion packs is evaluated under EU 10/2011 with overall migration 10 mg/dm² and under FDA 21 CFR 177.1520(c); FDA 21 CFR 73.575 covers titanium dioxide as a color additive when the formulation is listed for direct food-contact articles. The addition ratio is 2–5 wt% for wall sections between 0.8 mm and 1.5 mm, and 5–7 wt% for lids or cups with wall sections near 0.5 mm that require high hiding in a single-gated cold-runner mold. A production-scale hydraulic injection molding machine with clamp force between 1500 kN and 3500 kN typically runs a barrel profile from 180 °C at the feed throat to 210 °C at the nozzle, mold temperature 20–40 °C, and injection speed 80–150 mm/s; venting depth below 0.03 mm is necessary to avoid gas burn marks caused by carrier moisture or dispersant volatiles. A gravimetric blender with metering accuracy of ±0.1 wt% is required because shot-to-shot concentration errors cannot be re-distributed sufficiently in thin-wall flows. Gate blush and splay are observed when melt temperature exceeds 220 °C or when screw recovery time is shortened below 10 s; cavity pressure transducers should confirm peak pressure between 600 bar and 1200 bar before production release. Terminal products include thin-wall dairy tubs, spread portion packs, snack cups, overcaps, and white or near-white food-container lids.
| Downstream process | LL8844 GP addition range | Nominal final TiO2 from 70 wt% masterbatch | Primary process boundary |
| Blown film 40–70 µm | 4–8 wt% | 2.8–5.6 wt% | Die-lip deposit and screen-pack differential pressure rise after 12–16 h |
| Extrusion coating 15–25 g/m² | 8–12 wt% | 5.6–8.4 wt% | Melt temperature must remain ≤ 320 °C |
| Thin-wall injection molding 0.5–1.5 mm | 2–7 wt% by wall stock | 1.4–4.9 wt% | Gate shear above 30,000 s-1 increases splay |
| Sheet extrusion and thermoforming 0.3–0.8 mm | 5–10 wt% | 3.5–7.0 wt% | Draw ratio above 5.0:1 at 10 wt% narrows forming window to ±5 °C |
| HDPE shuttle blow molding 1–5 L | 2–5 wt% | 1.4–3.5 wt% | Parison sag above 6 wt%; large containers ≤ 3 wt% |
| Agricultural white top layer 20–40 µm | 3–6 wt% | 2.1–4.2 wt% | Amine-based additive retention must be validated by ASTM G155-13 |
| Post-consumer recycled PE film | 2–6 wt% | 1.4–4.2 wt% | Screen changer differential pressure above 5 MPa indicates blinding |
Extruded sheet lines processing LL8844 GP require roll-stack temperatures well above the sheet surface dew point because TiO2 agglomerates at low roll temperatures create pinholes during plug-assisted forming. Food-contact testing for final thermoformed containers is performed under EU 10/2011 using fatty-food simulant D2 with overall migration limit 10 mg/dm², and under FDA 21 CFR 177.1520(c) for the polyolefin sheet; the producer must also ensure that regrind reuse does not change the migration behavior of the formulated sheet. The masterbatch is added at 5–10 wt% in sheet thicknesses of 0.3–0.8 mm, yielding nominal final TiO2 concentrations of 3.5–7.0 wt%, with the higher range used only where luminous transmittance below 5% under ASTM D1003-13 is specified. A typical sheet line uses a single-screw extruder with 34:1 L/D, gear pump, die gap 0.8–1.2 mm, and three-roll stack temperatures of 70 °C, 80 °C, and 60 °C from top to bottom; thermoforming is conducted from roll stock at sheet surface temperatures between 140 °C and 170 °C and draw ratios of 3.0:1–5.0:1. At 10 wt% masterbatch, tensile elongation at break in the transverse direction of conditioned sheet tends to fall below 300% as measured by ASTM D638-14, narrowing the forming window to ±5 °C and requiring plug-assist timing adjustments to avoid corner thinning below 0.15 mm. When regrind levels exceed 40%, the masterbatch addition must be reduced to avoid double-dose TiO2 and progressive loss of dart impact; melt pump suction pressure drop greater than 15 bar indicates feed bridging from regrind flake geometry. Terminal products include yogurt cups, margarine tubs, portion cups, deli trays, and white thermoformed inserts for bakery packaging.
In shuttle blow molding of 1–5 L HDPE bottles, the addition of an LLDPE-carrier masterbatch at 2–5 wt% produces opaque white containers, but the carrier’s lower melt stiffness measurably increases parison sag before the addition ratio reaches 6 wt%. Food-contact closure and squeeze-bottle applications are tested under FDA 21 CFR 177.1520(c) and EU 10/2011 overall migration limit 10 mg/dm²; packaging waste heavy-metal limits fall under EU Directive 94/62/EC Article 11 with total lead, cadmium, mercury, and hexavalent chromium not exceeding 100 mg/kg. The lower addition range of 2–3 wt% is used for large bottles and containers above 10 L, while 4–5 wt% is acceptable only for 1 L and smaller containers with short parison drop lengths. A shuttle blow molder runs a die head melt temperature of 200–210 °C, mold temperature 15–25 °C, blow air pressure 0.6–0.8 MPa, and cycle times of 25–35 s for a 2 L bottle. Die gap adjustments of 0.2–0.4 mm compensate for reduced die swell, and accumulator head drop time increases by 0.5–1.5 s at 5 wt% addition; without this compensation, radial wall-thickness distribution around the handle pinch-off becomes inconsistent. The masterbatch carrier is not intended for PET or polycarbonate blow molding because LLDPE droplets would jeopardize clarity and mechanical integrity. Terminal products include white HDPE personal care bottles, opaque food squeeze bottles, household chemical containers, and white overcaps where high gloss and hiding are required without post-mold painting.
Silage and white-on-black mulch film production requires a white layer that reflects photosynthetically active radiation, not merely a cosmetic white surface. Agricultural film is not tested under food-contact migration rules, but the masterbatch and finished film fall under REACH Regulation (EC) No 1907/2006 Annex XVII restrictions on heavy metals, and mechanical performance of covering films may be evaluated under EN 13206:2017 for greenhouse and low-tunnel applications. The addition ratio in a 20–40 µm white top layer of a coextruded white/black mulch or silage cover film is 3–6 wt%, yielding a nominal final TiO2 concentration of 2.1–4.2 wt% in that layer; the black layer contains carbon black and no white masterbatch, so total masterbatch consumption by weight is roughly half the white-layer percentage. A three-layer blown-film die with dual-lip air rings and internal bubble cooling runs at blow-up ratio 2.0:1–2.5:1, melt temperature 200–220 °C, and high stalk height to stabilize the bubble against outdoor wind pressure. Where amine-based anti-fog or antistatic additives are used in the same layer, accelerated weathering under ASTM G155-13 must validate additive retention because surface treatment on TiO2 can shift migration rates. Published data for LL8844 GP in this specific agricultural configuration is limited; the addition ratios are therefore based on behavior of similar high-load TiO2 LLDPE-carrier masterbatches and must be verified by xenon-arc exposure before qualification of multi-season covers. Terminal products include white-on-black mulch film, silage cover film, greenhouse white outdoor covers, and reflective ground cover films.
When LL8844 GP is used as a dry-blended brightening masterbatch in post-consumer recycled LLDPE/LDPE film lines, gravimetric feed accuracy becomes the controlling variable because incoming flake melt flow rate varies from 0.5 g/10 min to 2.5 g/10 min as measured by ASTM D1238-23 at 190 °C/2.16 kg. Recycling applications for non-food packaging and refuse sacks are screened under EU Directive 94/62/EC Article 11 for total heavy metals below 100 mg/kg and under REACH Regulation (EC) No 1907/2006 SVHC screening obligations for substances in recycled feedstocks. The addition range is 2–6 wt%, providing a nominal final TiO2 concentration of 1.4–4.2 wt% to lift L* value and reduce visible grey undertone in highly contaminated mixed-colour recycle. A vented single-screw extruder with 30:1 L/D, continuous melt filtration through 150–200 mesh screen changers, and melt temperature 200–230 °C is used; a melt pump after the screen changer damps pressure fluctuations caused by gel and agglomerate accumulation. At addition rates above 6 wt%, the ash residue of the final film increases, and dart impact measured by ASTM D1709-16a may fall below the minimum required for refuse sacks; therefore the upper dosing limit is treated as a hard operational boundary rather than a formulation target. Screen changer differential pressure above 5 MPa indicates filter-cake blinding and may require a temporary reduction in masterbatch addition until the recycled feedstock granulate is reclassified. Terminal products include recycled refuse bags, carrier bags, construction film, and non-food industrial packaging where brightening and opacity are needed to homogenize variable post-consumer feedstock.
Competitive LyondellBasell POLYBATCH™ White LL8844 GP prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell POLYBATCH™ White LL8844 GP is a pelletized white masterbatch built on a linear low-density polyethylene carrier. The product is classified as a general-purpose concentrate for polyolefin conversion, not as a finished moulding compound. The nominal titanium dioxide fraction is 60 wt%; the remaining 40 wt% comprises the olefinic carrier and a processing-stabilizer package. Where lot certificates are issued, melt flow rate is reported under ISO 1133-1:2022 at 190 °C and 2.16 kg, and density is measured according to ISO 1183-1:2019. Published data on the exact stabilizer composition is limited; converters should request the lot-specific certificate before introducing the material into food-contact or high-temperature processes.
The product is discharged as cylindrical pellets. Typical pellet dimensions for similar polyolefin masterbatches are 2 mm to 4 mm in diameter and 3 mm to 5 mm in length; these dimensions are controlled by pelletizer speed and are not direct performance specifications. The solid density of a 60 wt% rutile concentrate in an LLDPE carrier is calculated from the additive volume model. Using a rutile density of 4.2 g/cm³ and an LLDPE carrier density of 0.92 g/cm³, the calculated solid density is approximately 1.73 g/cm³. The corresponding bulk density in a pellet bed is generally 1.0 g/cm³ to 1.3 g/cm³. The difference from unfilled LLDPE bulk density must be managed in hopper feed systems because denser pellets segregate during long conveying runs. A gravimetric blender should be calibrated for the higher bulk density of the masterbatch; failure to do so results in letdown drift and variable opacity.
A single melt flow rate value measured at 190 °C and 2.16 kg does not describe the high-shear behaviour of a filled polyolefin. Capillary rheometry under ISO 11443:2021 is used to compare the masterbatch with the base resin over shear rates from 100 s⁻¹ to 1000 s⁻¹. The filled system behaves as a pseudoplastic suspension; the viscosity difference narrows as shear rate increases, but at low shear the masterbatch remains substantially more viscous. Screw-slip failure on single-screw extruders is more likely when the hopper is cold and the feed zone is not cooled sufficiently. Maintaining the feed throat below 70 °C while keeping the first barrel zone above 175 °C reduces the risk of pellet softening that leads to bridging. On a 90 mm single-screw extruder, a pressure rise of 10 bar to 30 bar above the unpigmented LLDPE baseline is normal when the masterbatch is run at 8 wt% letdown; a rise above 30 bar indicates inadequate back-pressure control or screen blockage. These values are equipment-specific and should be trended against production records.
On cast film lines equipped with 45 mm barrier screws and 300 mm coat-hanger dies, the masterbatch is either hopper-blended or metered through a side feeder. Gravimetric side feeding is preferred because it removes fill density variation from the feed throat. Barrel set points for LLDPE carriers are maintained between 175 °C and 245 °C; the chill-roll temperature is held at 15 °C to 25 °C, with an air gap of 100 mm to 200 mm. A higher chill-roll temperature reduces film haze but may increase plate-out on metal surfaces when inorganic white pigment is present. Haze and luminous transmittance of the film are measured under ASTM D1003-21. For thin-gauge films below 30 µm, agglomerates that pass through a 150 µm screen can create visible surface defects even when bulk film haze remains acceptable.
Mechanical property retention in white LLDPE film is evaluated under ASTM D882-18 for tensile properties and ASTM D1922-23 for Elmendorf tear. At 6 wt% final TiO₂, the tensile yield stress of the film increases because the rigid filler reduces the polymer cross-section available for deformation, while elongation at break may decrease. The LLDPE carrier contributes to the molecular weight distribution of the blend; a low-molecular-weight wax carrier would reduce tear resistance more strongly. This is a principal reason an LLDPE-carrier masterbatch is specified for thin-gauge film rather than a universal wax-based dispersion.
The polyethylene carrier is not a universal carrier. In polypropylene, minor additions of ethylene-based carrier can be tolerated in many applications, but property retention should be verified when tensile yield and impact are specified. Tensile yield is measured under ISO 527-2:2012, and notched Charpy impact is measured under ISO 179-1:2023. A PP-carrier white masterbatch is generally preferred where the final article must retain stiffness and low-temperature impact. In PET, the polyethylene carrier is not compatible at preform injection temperatures, and hydrolytic degradation of PET can occur if the carrier is held at high temperature. Use in PET is outside the intended operational boundary. This distinction separates LL8844 GP from multi-resin white concentrates and from PP-specific white masterbatches.
Performance of a white masterbatch is sensitive to pigment particle size distribution and surface treatment. The manufacturer compounds the concentrate on twin-screw extruders with L/D ratios of 40:1 or greater and passes the melt through filtration before pelletizing. The converter should request moisture content below 0.1 wt% on the certificate of analysis. Free moisture above this level can cause screw feed variation and hydrolytic degradation of the stabilizer package. Pre-drying is not normally required if the packaging remains sealed, but exposure to relative humidity above 60% for more than 12 h may require desiccant drying at 60 °C for 2 h to 4 h. Published data for LL8844 GP under extreme humidity is limited; operational decisions should be based on moisture analysis rather than fixed drying schedules.
Rutile TiO₂ used in polymer masterbatches is surface-treated with aluminosilicate or organic coatings to control photostability and dispersibility. The exact surface treatment is not disclosed for this grade; however, it influences melt rheology and long-term weathering behaviour. Accelerated weathering for outdoor film applications may be tested under ASTM G154-23. Published data for LL8844 GP under xenon-arc or QUV exposure is limited; outdoor film converters should run comparative weathering trials against a control masterbatch before specifying the product for long-exposure applications.
Melt temperature above 260 °C should be avoided because oxidative degradation of the polyolefin carrier accelerates and generates gel defects. The product is a conventional polyolefin concentrate; it should not be processed below a melt temperature of 160 °C because the carrier may not fully plasticize under high shear. Adiabatic shear heating in barrier screws can raise melt temperature by 5 °C to 15 °C above the barrel set point. Therefore melt temperature is measured directly at the die, not inferred from barrel zones. If the die melt temperature exceeds 260 °C at any point, the converter should reduce screw speed or adjust barrel profiles before continuing.
Boundary failure in blown film extrusion occurs when the added masterbatch reduces bubble stability or increases gel counts. Film thickness uniformity is measured with a capacitance gauge across the bubble circumference; a thickness variation above ±5% in a 25 µm film indicates melt-temperature nonuniformity or inadequate mixing. Gel counts are counted against a 0.5 mm² defect threshold on automated optical inspection. When the white masterbatch is used in multilayer structures, the loaded layer should be positioned away from the sealing layer if seal strength retention is critical. The high filler content can increase surface roughness and shift heat seal initiation temperature. Seal strength is evaluated under ASTM F88/F88M-23; the heat seal initiation temperature should be measured on the exact multilayer structure, because the masterbatch carrier can influence interfacial adhesion at the sealant layer.
For food-contact uses in the United States, the finished article must meet 21 CFR 177.1520 for olefin polymers and 21 CFR 178.3297 for colorants used in polymers. European Union food-contact compliance is assessed under Regulation (EU) No 10/2011; the overall migration limit is 10 mg/dm². Electrical and electronic applications require conformity with Directive 2011/65/EU for restricted substances. Lot-level documentation should include melt flow rate, moisture content, and pigment loading.
| Standard or regulation | Method or clause | Boundary condition |
|---|---|---|
| ISO 1133-1:2022 | Melt mass-flow rate, 190 °C, 2.16 kg | Report per lot; compare with processing window |
| ISO 1183-1:2019 | Density of non-cellular plastics | Density shift affects feeder calibration |
| ASTM D1003-21 | Haze and luminous transmittance | White films require opacity, not clarity |
| FDA 21 CFR 177.1520 | Olefin polymers | Final article must satisfy extractive limits |
| EU 10/2011 | Overall migration | 10 mg/dm² |
| Directive 2011/65/EU | RoHS Annex II | Pb 1000 mg/kg; Cd 100 mg/kg; Hg 1000 mg/kg; Cr(VI) 1000 mg/kg |
Compared with direct rutile powder addition, the pelletized 60 wt% concentrate reduces airborne dust and hopper cross-contamination but fixes the pigment surface-treatment chemistry at the masterbatch production stage. This differs from dry TiO₂ and from wax-based single-pigment dispersions used in extrusion coating. Wax-based white dispersions may offer lower melt viscosity but can interact with slip-agent packages and alter seal strength when tested under ASTM F88/F88M-23. A lower-solids white masterbatch at 50 wt% would require approximately 20% more pellet mass to deliver the same TiO₂ concentration; that extra carrier can be advantageous in very thin films where additional polyolefin helps wet-out, or disadvantageous in high-output lines where feed mass is a constraint. The selection between LL8844 GP and alternative white concentrates must therefore be based on final TiO₂ concentration, screw geometry, and the downstream property tests of the finished article.
In injection moulding of white LLDPE closures, the masterbatch is metered at 4 wt% to 8 wt%. The mould temperature is maintained between 20 °C and 40 °C, and hold pressure is set according to part thickness. Poor homogenization appears as flow lines or streaks on the part surface, especially near the gate. The melt pressure at the injection nozzle should be recorded for each batch; transient pressure swings greater than ±10 bar during recovery indicate inconsistent feeding or melt-quality variation. Published data for LL8844 GP in injection moulding is limited; molders should qualify the product on a production machine with representative shot size and clamp force before full deployment.