Lyondellbasell Polybatch White Ll8575 Ap Concentrate Based In Lldpe

LyondellBasell POLYBATCH™ White LL8575 AP Concentrate Based In LLDPE

    • Product Name: LyondellBasell POLYBATCH™ White LL8575 AP Concentrate Based In LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 332515
    Carrier Resin LLDPE
    Color White
    Form Pellets
    Titanium Dioxide Content 75%
    Density 2.0 g/cm³
    Melt Flow Rate 20 g/10 min (190°C/2.16 kg)
    Moisture Content <0.1%
    Letdown Ratio 4-8%
    Processing Temperature 180-260°C
    Bulk Density 1.1 g/cm³
    Pellet Size 2-3 mm
    Ash Content 75%
    Food Contact FDA compliant

    As an accredited LyondellBasell POLYBATCH™ White LL8575 AP Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg polyethylene-lined bags, palletized with 40 bags per pallet and stretch-wrapped for transport.
    Container Loading (20′ FCL) 20′ FCL container loading: palletized LyondellBasell POLYBATCH™ White LL8575 AP Concentrate Based In LLDPE, shrink-wrapped and secured for transport.
    Shipping Shipping description: LyondellBasell POLYBATCH™ White LL8575 AP Concentrate Based in LLDPE is typically non-hazardous and not regulated for transport. Ship in original sealed bags or containers, keep dry, and protect from heat, moisture, and contamination. Use standard freight. Consult the SDS and applicable DOT/IMDG/IATA/ADR rules.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and moisture. Keep containers tightly closed and labeled, preferably in original packaging on pallets. Avoid contamination, dust generation, and strong oxidizing agents. Maintain moderate temperatures; avoid excessive heat. Use first-in, first-out stock rotation and inspect containers regularly for damage or leaks.
    Shelf Life Shelf life is typically 12 months from manufacture when stored unopened in original packaging, dry, cool, away from direct sunlight.
    Application of LyondellBasell POLYBATCH™ White LL8575 AP Concentrate Based In LLDPE

    Opacity Barriers in Three-Layer Blown Film: Melt Pressure, Die Build-Up, and Dart Drop

    LyondellBasell POLYBATCH White LL8575 AP Concentrate Based In LLDPE is specified for polyethylene film lines where the LLDPE carrier reduces the melting point gap between the white concentrate and metallocene LLDPE skin-layer resins. In three-layer agricultural silage film, white label film, or white backsheet structures, the concentrate is dosed at 4–10 wt% in the pigmented layer. If the certificate of analysis records a pigment loading of 50 wt%, a 6 wt% masterbatch addition yields a final titanium dioxide loading of 3 wt%; final TiO2 target is therefore verified against the CoA rather than assumed. Gravimetric feeding at the main throat is preferable to batch tumble blending because the pellet hardness and bulk density of LL8575 AP can allow size segregation in large silos. The extruder configuration normally includes a grooved feed section, a 25:1 to 30:1 L/D barrier screw, and a screen stack of 20/60/100 mesh to protect the die land from pigment agglomerates. Head pressure should be logged; when masterbatch addition moves from 2 wt% to 8 wt%, the pressure before the screen pack rises measurably because the inorganic phase increases apparent melt viscosity. Published data for this specific concentrate in a three-layer 40 µm line are limited, but plant qualification commonly uses a pressure transducer and a motor load ceiling of 85% of nameplate before reducing screw speed. The concentrate melt flow rate is stated by the producer and is normally measured by ASTM D1238-20 Condition 190°C/2.16 kg; incoming raw material checks should include this value because carrier MFI shifts the melting point gap in coextrusion. Die gap is typically set at 1.8–2.2 mm, blow-up ratio between 2.0:1 and 3.0:1, and frost line height is re-established after TiO2 addition because the white layer radiates heat differently than unpigmented LLDPE. Opacity is measured according to ASTM D1003-21, haze by ASTM D1003-21, specular gloss at 60° by ASTM D2457-21, tensile properties by ASTM D882-18, Elmendorf tear by ASTM D1922-15, and dart impact by ASTM D1709-16a. The most common process conflict is that TiO2 agglomerates act as stress concentration points; dart drop and machine-direction tear decline as addition rises, while opacity gains flatten after a certain pigment loading. Therefore, the upper dosing limit is not a single value but is determined by the relationship between the film’s required impact specification and the scattering efficiency of the selected TiO2 grade. Pre-drying is required when the pellets have been exposed to ambient air above 60% RH for more than 2 h; a desiccant dryer at 60–70°C for 2–4 h reduces moisture to below 0.05 wt% as determined by Karl Fischer titration. Moisture changes screen-pack pressure and produces surface specks at the die lip. The concentrate should not be combined in the same layer with calcium carbonate at a combined inorganic level above 8 wt% without re-qualification because the resulting film loses ductility and may fail tear specifications. Finished films include white opaque silage covers, label facestock, hygiene backsheet layers, and white shrink film where opacity must be achieved without white printing ink.

    Extrusion coating of white-pigmented LDPE/LLDPE layers onto bleached board or aluminium foil places LL8575 AP at the interface between melt curtain stability and pigment loading. The carrier is an LLDPE resin, so it has a higher zero-shear viscosity and a narrower drawdown window than a neat LDPE coating grade; addition of 5–12 wt% masterbatch is typical for final white opacity in liquid carton stock, cup stock, or lamination film. Melting is performed in a single-screw extruder with 24:1 to 30:1 L/D and a barrier screw, followed by a flat slot die with an internal deckle; melt temperatures for PE extrusion coating are normally maintained between 260°C and 310°C. At higher addition levels above 12 wt%, the LLDPE carrier can increase edge neck-in and reduce maximum line speed because the melt curtain has less strain hardening than a branched LDPE matrix. Coating weight is checked by gravimetric or beta-gauge systems, commonly in the range of 12–25 g/m² for white board; pinholes are minimised by controlling the air gap, chill roll temperature, and oxidative surface treatment. Adhesion to paperboard or aluminium requires corona or ozone treatment before the melt curtain contacts the substrate; the treated substrate surface energy is verified to at least 38 dyn/cm according to ASTM D2578-23. The white layer must meet food-contact requirements for non-fatty and fatty simulants under 21 CFR 176.170 and Regulation (EU) 10/2011, with migration of the carrier and pigment evaluated on the final laminate rather than on the masterbatch alone. Migration testing under Regulation (EU) 10/2011 is designed according to Annex III and Annex V, using food simulants A, B, D2, and E depending on the final food type. The process limitation is clear: chill roll surface temperatures below 15°C can cause quenching defects in thick white layers, while temperatures above 25°C can promote plate-out of low molecular weight LLDPE fractions on the roll surface. Finished goods include white extruded board for coffee cup stock, detergent cartons, industrial label liners, and laminated sachets where the white layer functions as both opacity source and adhesive tie layer.

    How Much LL8575 AP Can Be Added Before ESCR and Top Load Shift Outside Dairy Bottle Specifications?

    At addition rates above 3 wt% in an HDPE dairy blow moulding compound, the LLDPE carrier of LL8575 AP changes the parison sag behaviour and the weld-line strength of extrusion blow-moulded containers. The masterbatch is normally added at 3–8 wt% to produce white HDPE bottles for milk, yoghurt drinks, or personal care products. The carrier reduces die swell and supports parison hang time at standard melt temperatures of 180–220°C, but it also contributes a lower flexural modulus than the HDPE matrix. Top-load force, tested on empty blown containers using ASTM D2659-16 or ISO 12048:2000, tends to shift downward as the proportion of LLDPE carrier increases; the specification limit for a stackable 1 L dairy bottle may require a confirmation run at the upper concentrate addition. Environmental stress crack resistance is evaluated with ASTM D1693-15 on compression-moulded plaques produced from the bottle wall; LLDPE has high ESCR, but the disperse TiO2 phase can act as a stress riser if pigment agglomerates are not fully dispersed. Melt filtration through a 100 mesh screen pack and a vacuum vent are used to control agglomerates and volatiles. The concentrate must be pre-dried at 60°C for 3–4 h if moisture content is above 0.08 wt%. Regrind return above 25% of total feed weight should be avoided without sorting by pigment content because it destabilises the masterbatch-to-resin ratio and changes bottle wall thickness distribution. Final compliance is checked against 21 CFR 177.1520 for olefin polymers and Regulation (EU) 10/2011 for plastic food contact materials; the pigment itself must be listed under the applicable national positive list. Finished articles are white monolayer or tri-layer dairy bottles, cosmetic bottles, and pharmaceutical HDPE containers where UV light protection from the titanium dioxide phase is combined with the mechanical performance of the HDPE matrix.

    Thin-wall injection moulding of white HDPE closures and overcaps with a PE-based white concentrate introduces a viscosity differential that must be managed by melt temperature, injection speed, and gate size. In a reciprocating screw with 18:1 to 22:1 L/D, LL8575 AP is metered at 2–5 wt% into the HDPE resin. The melt temperature is maintained between 200°C and 240°C; mould temperatures are set to 10–30°C for rapid set-up in thin sections. The LLDPE carrier can lower the melt viscosity slightly relative to a full HDPE matrix at the same temperature, so maximum injection pressure may be reduced but the probability of gate blush and flow lines increases if the colorant is not dispersed. A back pressure of 5–15 bar and a screw recovery time of 1–3 s are common starting points; pigment dispersion is verified by preparing a 60×60×1 mm plaque and counting agglomerates above 20 µm under transmitted light. Mechanical acceptance is based on ASTM D638-14 for tensile yield stress, ISO 527-2:2012 for modulus, and ASTM D256-23 for notched Izod impact. The concentrate is not intended for polypropylene closure compounds above 2% unless the processor has qualified the immiscible carrier effect; in PP closures, the LLDPE phase causes gloss loss and reduces heat deflection temperature. Residence time at melt temperature must not exceed 5 min to avoid yellowing of the white pigment system. Finished applications include white HDPE caps, overcaps for aerosol cans, cosmetic jar closures, and tamper-evident lids.

    When Rotational Moulding Requires Whiteness Retention Without Grinding Auxiliary Pigments

    When rotational moulding requires whiteness retention without grinding auxiliary pigments, LL8575 AP is dry-blended into 35 mesh LLDPE powder after the powder has been screened through a 500 µm sieve. The concentrate pellets have a higher bulk density than the ground LLDPE powder; the mixture is therefore tumbled in a ribbon blender at low speed rather than dropped into the mould with only manual mixing. Addition of 1–5 phr is common for white tanks, agricultural bins, and playground panels. Oven temperatures for LLDPE rotational moulding are normally set at 260–288°C, while the mould interior is heated until the peak internal air temperature reaches 190–210°C; the biaxial rotation ratio is set between 3:1 and 5:1. The LLDPE carrier fuses at a slightly lower temperature than HDPE, which can improve surface healing at low oven temperatures but can also cause localised pigment pooling in under-vented moulds. Wall thickness distribution is measured with an ultrasonic gauge after demoulding, and tensile properties are tested according to ISO 527-2:2012 or ASTM D638-14. Impact strength at -20°C is assessed by ASTM D256-23 or instrumented falling-weight methods. White colour retention outdoors is evaluated with ISO 4892-2:2013 xenon-arc exposure and ASTM G154-23 UVA-340 testing; chalking of the titanium dioxide surface is possible after prolonged exposure unless the powder compound includes an adequate hindered amine light stabiliser package. The processing boundary is defined by demoulding: TiO2 can increase the coefficient of static friction of the moulded surface, so release agent type and mould surface condition must be re-qualified. The masterbatch should not be pre-blended at concentrations above 8 phr for highly filled tank formulations because the inorganic phase increases melt viscosity and reduces the ability of the powder to densify in corners. Finished rotomoulded articles include white storage tanks, agricultural bins, playground equipment, and outdoor enclosures.

    Polyethylene jacketing compounds for low-voltage power cables and fibre optic ducts use LL8575 AP because the LLDPE carrier does not compromise the low-temperature impact required by outdoor installation. The masterbatch is added at 2–5 wt% in a twin-screw compounding line or directly in a single-screw cable extruder with 24:1 L/D and a crosshead die. Melt temperature is held between 170°C and 210°C to prevent degradation of the white pigment system. Cable jacket compounds must be dried to below 0.03 wt% moisture before extrusion; otherwise, the white jacket shows pinholes at drawdown. The compound is tested for tensile strength and elongation after ageing according to IEC 60811-501:2012, hot set under EN 60811-507, and low-temperature impact by ASTM D746-20. For indoor white fibre ducts and conduits, flame propagation is evaluated under UL 94 or IEC 60695-11-10 depending on end-use. The operational boundary is the dielectric requirement: titanium dioxide raises the relative permittivity and dissipation factor of the compound, so the concentrate is generally excluded from primary insulation layers where capacitance stability is specified; its use is confined to outer jacketing and identification layers. Accumulation of pigment on the crosshead die generates surface roughness after 4–6 h of continuous extrusion, so die lips are cleaned at scheduled intervals. Finished products are white outer sheaths for low-voltage power cables, fibre optic ducts, and colour-coded building wire.

    Free Quote

    Competitive LyondellBasell POLYBATCH™ White LL8575 AP Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell POLYBATCH™ White LL8575 AP is identified in manufacturer documentation as a white concentrate based in linear low-density polyethylene (LLDPE). The grade combines rutile titanium dioxide pigment with an LLDPE carrier resin selected to preserve melt-phase compatibility when the concentrate is let down into LLDPE-rich film, coating and sheet formulations. Published data for this specific configuration is limited in open sources; consequently, numerical processing windows and property shifts cited in this document are representative of industrial LLDPE-based white concentrate practice and must be verified against the product certificate of analysis. White concentrates of this product class commonly contain 50–70 wt% rutile TiO₂, but the exact assay for LL8575 AP is determined gravimetrically by ISO 3451-1:2019. The material is typically supplied as cylindrical microgranulate, and pellet geometry directly influences gravimetric feeder discharge and screw feeding stability. Because the carrier is LLDPE, the concentrate is positioned for applications in which LLDPE itself is the major matrix resin: white agricultural film, white stretch film, label facestock, extrusion coating, and pigmented sealant layers. The product is not a multi-purpose carrier for polypropylene or polyamide. In quality-control terms, the class is characterized by melt mass-flow rate under 190 °C/2.16 kg conditions per ISO 1133-1:2022, density per ISO 1183-1:2019, and ash residue per ISO 3451-1:2019. The ash value is a direct estimate of inorganic pigment content and is used to calculate the required let-down ratio for a target oxide loading in the finished article.

    TiO₂ dispersion, screen-pack pressure and film optical density

    During extrusion of white concentrates, dispersion quality is inferred from pressure differentials across the melt filtration assembly and from transmitted-light defect counts in converted film. In a monolayer blown film line with a barrier screw and an L/D of 30:1, an undispersed white masterbatch manifests as a rising pressure gradient across a 150–250 µm screen pack, followed by optical defects in thin film. The pressure curve is more diagnostic than motor load. A stable screen-pack differential is 0.5–1.5 MPa; a continuous rise beyond 2.0 MPa within a production shift indicates pigment agglomerates or polymer gels. Optical transparency and surface appearance are measured on finished film as total luminous transmittance and haze using ASTM D1003-21; white films with sufficient opacification generally show transmittance below 50% at 100 µm gauge, but the exact value depends on titanium dioxide loading and let-down ratio. Particle-size analysis of the concentrate ash by laser diffraction per ISO 13320-1:2020 should identify whether agglomerates larger than 5 µm remain after incineration; such agglomerates are visible as white specks in 20–40 µm film under 1000 lux inspection. They are not corrected by downstream stretching and require cartridge filtration or a finer masterbatch dispersion. Because the carrier is LLDPE, melting temperatures above 260 °C may initiate oxidative yellowing of the resin phase and reduce whiteness retention; for blown film operations, the melt temperature is generally held between 200 °C and 240 °C. Operators should monitor the temperature profile at the adapter and die, not only at the barrel setpoints, because viscous dissipation in high-shear mixing sections can raise localized melt temperature by 5–15 °C.

    When the let-down ratio in a three-layer blown film line is adjusted to achieve a target oxide content, the process response is governed by the carrier melt viscosity and the screw recovery rate. LLDPE-carrier white concentrates are typically dosed into the middle or skin layer of coextruded structures where whiteness must be separated from heat-seal initiation temperature. A common let-down range for white polyolefin film is 5–10 wt%, but the final oxide content must be calculated from the concentrate ash content and the desired film gauge. On a 3-layer blown film die with die gap 1.8–2.4 mm, melt temperature 200–230 °C, and blow-up ratio 2.0–2.5:1, bubble stability can be sensitive to pellet-to-pellet variation in the masterbatch melt flow rate. Feeder segregation caused by particle size differences between virgin LLDPE and the white concentrate is controlled by maintaining granule diameter between 2.0 mm and 3.5 mm and avoiding bulk density differences greater than 10% between components. The optical density of the final film is measured by ASTM D1003-21; a reduction in total luminous transmittance is accompanied by an increase in film stiffness, which is monitored by secant modulus per ISO 527-3:2018. Tear resistance after opacification is evaluated by ISO 6383-2:1983; the observed value declines as mineral content rises and is therefore matched to the end-use requirement rather than optimized as an absolute maximum. Published quantitative tear-retention curves for this specific grade are limited; process-capability trials on the production line are required to establish the acceptable let-down window for a given film recipe.

    Which carrier-resin variables distinguish this grade from LDPE- or PP-based TiO₂ concentrates?

    Carrier resin selection determines thermal compatibility, melt rheology, let-down uniformity and final physical properties. An LLDPE carrier has a melting onset generally between 120 °C and 125 °C by differential scanning calorimetry per ISO 11357-3:2018, whereas an LDPE carrier typically melts between 105 °C and 115 °C and a polypropylene homopolymer carrier melts between 160 °C and 165 °C. These thermal transitions impose processing constraints when the concentrate is used outside its compatible resin family. The table below summarizes comparative carrier behavior for white concentrates in polyolefin film applications.

    Carrier resinThermal transitionCompatibility with LLDPE-rich filmMajor limitation
    LLDPE120–125 °C onset per ISO 11357-3:2018Preferred for LLDPE-rich structuresHigher viscosity may increase screw motor load
    LDPE105–115 °C onset per ISO 11357-3:2018Acceptable in LDPE/LLDPE blends at low additionLower melt strength may reduce dart impact
    PP homopolymer160–165 °C onset per ISO 11357-3:2018Not recommendedPhase-separated domains reduce stiffness above 2–3 wt%

    In comparison with LDPE-carrier white masterbatches, an LLDPE carrier contributes higher melt viscosity and higher extensional resistance, which can improve bubble stability in LLDPE-rich blown film but can increase extruder motor load when the same concentrate is run on a shallow screw designed for low-viscosity LDPE. The practical limit is not the pigment assay alone; the combined melt flow rate of the diluted system must remain within the machine’s plastication capacity. When an LLDPE-based white concentrate is introduced into a polypropylene homo-polymer stream, the melting point mismatch can produce dispersed LLDPE domains that reduce tensile stiffness and increase opacity variation at addition levels above 2–3 wt%. Tensile modulus of the resulting blend is evaluated by ISO 527-2:2012; a drop of more than 10% relative to the neat polypropylene matrix suggests that a polypropylene-carrier concentrate should be substituted. Conversely, an LDPE carrier may be acceptable in LLDPE-rich films at low addition levels, but the lower melt strength of the carrier can reduce dart impact and tear performance because the carrier behaves as a localized low-viscosity phase. For exact carrier compatibility data, the manufacturer’s product data sheet and melt adhesion tests under production conditions remain decisive.

    In extrusion coating and lamination, the concentrate is introduced into a polyolefin skin layer where a white surface finish must be achieved at low coating weights. Unlike blown film, extrusion coating applies a thin melt web at line speeds above 150 m/min; the LLDPE carrier must withstand high draw without causing edge neck-in or draw resonance. White pigment increases extensional viscosity, which is evaluated indirectly by neck-in measurements using a rectangular die of known width; a neck-in increase above 5% relative to unpigmented LLDPE indicates that the let-down ratio should be reduced or that a carrier with lower high-shear viscosity should be selected. Coating weights of 15–25 g/m² are typical for white barrier laminates and flexible packaging. At these gauges, agglomerates larger than 5 µm create pinholes and reduced seal integrity, so dispersion quality must be measured on the final coating, not only on the masterbatch pellet. Adhesion and tensile elongation of white extrusion-coated structures are evaluated by ISO 527-3:2018; the white pigment addition must not lower the seal initiation temperature of the base LLDPE beyond the range established for the packaging line. Published data for the exact seal initiation shift of this specific grade is limited. The product is processed on extrusion coating lines with screw L/D preferably above 24:1 to ensure adequate distributive mixing of the high pigment concentration, and the melt temperature is normally held below 260 °C to limit oxidative yellowing of the LLDPE carrier.

    When pre-drying and gravimetric feeding constraints intersect

    In high-humidity production environments, the moisture adsorbed on the surfaces of LLDPE-carrier white concentrate granules can create intermittent steam splay when the masterbatch is moved directly from cold storage to the extruder feed throat. The issue is more pronounced with high pigment loading because the pigment surface area increases water uptake. A desiccant pre-dryer with dew point below -20 °C and air temperature 70–80 °C for 2–4 h is applied when relative humidity exceeds 60%. Gravimetric feeding of dry blends is sensitive to bulk density stratification; the masterbatch is preferably metered with a separate low-rate feeder rather than preblended in silos. The feeder screw should be checked for pellet fracture because fines generation below 150 µm changes the apparent bulk density and leads to overfeeding of the concentrate. Blend uniformity is monitored by ash testing at the feed throat; an ash content variation of more than ±0.5% absolute across ten samples using ISO 3451-1:2019 indicates segregation in the handling system. These limits are operational boundaries applicable to white polyolefin concentrates and are not a substitute for process capability studies on the specific line.

    PropertyTest designationTypical use in evaluation
    Melt mass-flow rateISO 1133-1:2022Carrier consistency and feed behavior
    DensityISO 1183-1:2019Carrier resin identification
    Ash residueISO 3451-1:2019TiO₂ loading and let-down calculation
    Haze and luminous transmittanceASTM D1003-21Film optical density
    Tensile propertiesISO 527-3:2018Film strength after opacification
    Tear resistanceISO 6383-2:1983Film toughness