Lyondellbasell Polybatch White Ll8425 Mg Concentrate Based In Lldpe

LyondellBasell POLYBATCH™ White LL8425 MG Concentrate Based In LLDPE

    • Product Name: LyondellBasell POLYBATCH™ White LL8425 MG Concentrate Based In LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 526301
    Product Name LyondellBasell POLYBATCH™ White LL8425 MG Concentrate Based In LLDPE
    Manufacturer LyondellBasell
    Product Type White Masterbatch Concentrate
    Carrier Resin Linear Low Density Polyethylene (LLDPE)
    Color White
    Form Pellets
    Pigment Titanium Dioxide (TiO2)
    Tio2 Content 75%
    Density 1.90 g/cm³
    Melt Flow Rate 10 g/10 min (190°C/2.16 kg)
    Processing Temperature 180-230°C
    Recommended Let Down Ratio 5-10%
    Moisture Content <0.1%
    Food Contact Complies with FDA and EU food contact regulations
    Storage Conditions Dry, below 30°C
    Shelf Life 24 months

    As an accredited LyondellBasell POLYBATCH™ White LL8425 MG Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell POLYBATCH™ White LL8425 MG is typically supplied in 25 kg polyethylene-lined bags, palletized at 1,000 kg per pallet.
    Container Loading (20′ FCL) 20′ FCL loaded with LyondellBasell POLYBATCH™ White LL8425 MG Concentrate Based In LLDPE, securely stowed, palletized bags for ocean transport.
    Shipping LyondellBasell POLYBATCH™ White LL8425 MG Concentrate Based In LLDPE ships as non-hazardous solid pellets. It is not regulated by DOT, IMDG, or IATA. Use original sealed 25 kg bags or 1,000 kg octabins; protect from moisture, heat, and contamination. Store in a cool, dry area. No special transport labeling required.
    Storage Store at ambient temperature in a dry, cool, well-ventilated area away from direct sunlight, heat, ignition sources, and moisture. Keep original containers tightly closed when not in use. Avoid excessive heat that may soften or fuse the concentrate. Use first-in, first-out rotation. Protect from contamination and incompatible materials. Follow local regulations and the supplier’s SDS. Store separately from foodstuffs.
    Shelf Life Shelf life is typically 24 months when stored unopened in a dry, cool place, away from direct sunlight and heat.
    Application of LyondellBasell POLYBATCH™ White LL8425 MG Concentrate Based In LLDPE

    In monolayer LLDPE blown film lines producing opaque white packaging for edible oils and dairy powders, LyondellBasell POLYBATCH™ White LL8425 MG Concentrate Based In LLDPE is introduced at the feed throat along with the primary LLDPE resin. The LLDPE carrier reduces melt-phase incompatibility when the dilution resin is linear-low-density or high-density polyethylene, but the supplier’s technical datasheet and statement of composition remain the controlling documents. Industrial practice for white opaque film places the addition ratio between 6 wt% and 10 wt% of total compound mass, with 12 wt% reserved for thick-gauge films where reduced tear resistance is acceptable; optical and mechanical tests must be conducted on the final film because titania concentration alters MD tear propagation and seal initiation. Compliance for food contact uses 21 CFR 177.1520 for US-specified olefin polymer end articles, Regulation (EU) No 10/2011 as amended and its Annex I and Annex III migration rules for EU food contact, and GB 9685-2016 for China. The film is processed on single-screw LLDPE extruders with barrier screws of 25:1 to 30:1 L/D, die gaps of 1.8–2.4 mm, and blow-up ratios of 2.2–3.0:1; frost-line height is maintained at 1.5–2.5× the die diameter to control bubble stability and thickness band. Downstream conversion produces white opaque pouches, dairy powder films, edible oil wrappers, and frozen-food overwraps. Tensile properties are checked under ASTM D882-18, tear resistance under ASTM D1922-15, opacity by contrast ratio under ASTM D2805-11, and seal initiation under ASTM F88/F88M-21; specimens are conditioned at 23±2 °C and 50±5% RH for 40 h under ISO 291:2008. The main operational boundary is pre-drying: at relative humidity above 60%, the masterbatch should be dried for 2 h at 80 °C before processing to prevent surface moisture defects; no amine-based processing aids should be combined with the masterbatch because the interaction can degrade whiteness at high temperature.

    Why Does Extrusion Coating Demand Controlled Titanium Dioxide Dispersion in High-Line-Speed LLDPE Carriers?

    When the masterbatch is introduced into an extrusion coating line running 250–320 °C melt temperatures and line speeds up to 300 m/min, the LLDPE carrier must disperse rapidly in LDPE/LLDPE blends without generating draw resonance. The addition ratio in white liquid-paperboard coating falls between 8 wt% and 15 wt%, with the upper limit constrained by edge-trim recycling and die-lip oxidation buildup. The relevant food contact framework is 21 CFR 176.170(c) for paper and paperboard components in contact with aqueous and fatty foods when the coated board is used in the United States, and Regulation (EU) No 10/2011 with its overall migration limit of 10 mg/dm² under the simulant selections in Annex III for the European Union. The process uses a single-screw extruder with a coathanger die, 0.5–0.9 mm die gap, air gap 150–250 mm, and polished chill roll at 10–20 °C to solidify the extrudate at coating weights of 15–30 g/m². Terminal articles include white gable-top cartons, paper cupstock, and frozen food board, where whiteness is measured by ISO 2470-2:2019 or CIE L* under ISO 11664-4:2019. Gloss is checked under ASTM D523-14 or ISO 2813:2014. The main incompatibility is the tendency of oxide pigments to deposit on the die lip during long runs; die-lip cleaning intervals shorten when let-down exceeds 12 wt% and may require automatic die-lip cleaners or scheduled shutdowns to maintain coating adhesion consistency.

    Mandate or methodJurisdiction / scopeRelevant requirementVerification output
    21 CFR 177.1520United States olefin polymersExtractable and density specificationsSupplier statement of composition
    Regulation (EU) No 10/2011European Union plastic food contactAnnex I positive list; Annex III migration testingOverall migration ≤ 10 mg/dm²
    GB 9685-2016China food contact additivesPositive-list colorant addition limitsDeclaration of conformity
    REACH Regulation (EC) No 1907/2006EU chemicalsSVHC candidate list screeningSDS Section 2 and Annex II
    USP 661.1Pharmaceutical packaging when applicablePhysicochemical plastic component testsMaterial certificate
    ISO 1133-1:2022Melt flow consistencyMethod A/BLot-to-lot MFR drift

    Thin-Wall Injection Moulding and Solidification of TiO₂-Agglomerate-Free Melts at the Gate

    Thin-wall moulding of white opaque polyethylene containers subjects the masterbatch to a short, high-shear injection phase in which the LLDPE carrier must not delay gate freeze or produce visible flow marks. Addition ratios of 3–6 wt% are typical for HDPE-rich thin-wall formulations with melt flow rates above 5 g/10 min under ISO 1133-1:2022; the lower limit is used when drop-impact resistance and environmental stress-crack resistance are prioritized because titania can nucleate crystallization and alter shrinkage anisotropy. Drop-impact resistance is measured under ASTM D2463-15. Processing takes place on hydraulic injection moulding machines with clamping force 1,500–4,000 kN, barrel temperatures 180–230 °C, and mould temperatures 10–30 °C; valve-gated hot runners are preferred over edge gates because the gate diameter should remain above 0.8 mm to limit shear heating and pigment agglomerate build-up. Compliance for dairy cups, lids, and creamer capsules is assessed under 21 CFR 177.1520 and Regulation (EU) No 10/2011, with the masterbatch supplier’s statement of composition confirming that the titanium dioxide and carrier are within positive-list requirements. Terminal product types are injection-moulded white dairy cups, lids, and HDPE closures. Shrinkage is checked with ASTM D955-08, part tensile yield strength with ASTM D638-14, and environmental stress-crack resistance under ASTM D1693-15. Processing at the upper end of the addition range may require increases in holding pressure to compensate for faster gate freeze caused by higher solidification rates.

    Rotational moulding of opaque white tanks and coolers imposes a low-shear, long-residence thermal cycle in which the masterbatch is dry-blended with linear-low-density or high-density polyethylene powders. The addition ratio should remain between 1 phr and 3 phr by total polymer mass, because pigment agglomerates do not disperse under rotomoulding shear and therefore the masterbatch must be supplied as a powder-compatible pellet or be pulverized to the same particle-size distribution as the base resin. Processing requires biaxial rotational speed ratios near 4:1, oven temperatures 260–315 °C, peak internal air temperature 165–190 °C, and cooling rates controlled below 8 °C/min to avoid warpage in white tanks. Compliance for potable water contact may require NSF/ANSI/CAN 61 certification when the finished rotomoulded vessel is connected to drinking-water lines, while food contact liners fall under 21 CFR 177.1520 and Regulation (EU) No 10/2011. Terminal products include non-food caustic storage tanks, marine coolers, and agricultural hoppers, with low-temperature impact tested under ASTM D1998-21 and material density checked by ASTM D1505-18. Direct substitution of liquid colorant is not recommended because the LLDPE carrier, not the pigment alone, contributes to the required melt flow and demoulding consistency during cooling.

    For cast film lines converting white hygiene backsheet or label facestock, the masterbatch’s LLDPE carrier is melt-blent with LDPE and LLDPE let-down resins to produce thin white film at low melt temperatures. Let-down ratios for cast film are commonly 5–9 wt%, with higher concentrations reserved for 30–60 µm film where opacity is required. The process uses an extruder with L/D 30:1, melt temperature 220–260 °C, and a chilled roll at 15–25 °C, with winding tension 0.1–0.3 N/mm of web width to prevent blocking. Blocking resistance is checked under ASTM D3354-15. Compliance for hygiene packaging may include ISO 10993-5 or ISO 10993-10 for medical packaging biological evaluation when declared; industrial film constituents are assessed under REACH Regulation (EC) No 1907/2006 and, in the United States, under 21 CFR 177.1520 where the material is used in food contact. The cast film is converted into adhesive tape labels, sanitary product backsheet lamination, and medical device pouches. Optical performance is verified using ASTM D1003-21 for haze and luminous transmittance, while thickness uniformity is measured inline with beta gauges traceable to ISO 4593. Published data for this specific masterbatch in cast film hygiene backsheet are limited; therefore contrast ratio and heat-seal strength should be confirmed on the converter line before production.

    Monolayer White HDPE Bottle Extrusion Blow Moulding with an LLDPE-Carrier Concentrate

    Blow moulding of monolayer white HDPE bottles with an LLDPE-carrier white masterbatch introduces a viscosity mismatch between the carrier and the main polymer that affects die swell and flash trimming. Let-down ratios of 4–8 wt% are typical for bottle-grade HDPE with melt flow rates of 0.3–0.7 g/10 min under ASTM D1238-20 at Condition 190 °C/2.16 kg; higher ratios may reduce parison melt strength and increase the frequency of bottle weight variation. The process is executed on shuttle or continuous-extrusion blow moulding machines with die head temperatures of 180–210 °C, blow pressure 0.6–1.0 MPa, and mould cooling water at 8–12 °C. US food-contact status for olefin polymers is 21 CFR 177.1520, and EU food contact is assessed under Regulation (EU) No 10/2011; pharmaceutical packaging may require USP 661.1 plastic component testing when the bottle is a packaging component. Terminal bottles include opaque personal-care and home-care bottles, as well as light-protective pharmaceutical packaging. Wall thickness distribution is checked by ASTM D2911-15, and top-load resistance is measured under ASTM D2659-16. Recycle streams high in calcium stearate should not be combined with the masterbatch because the TiO₂ surface can form hard agglomerates that survive screen filtration and generate visible specks.

    Free Quote

    Competitive LyondellBasell POLYBATCH™ White LL8425 MG Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The product designated LyondellBasell POLYBATCH™ White LL8425 MG Concentrate Based In LLDPE is a white pigment masterbatch supplied as free-flowing cylindrical pellets in a linear low-density polyethylene carrier. The grade is intended for melt dilution in polyolefin film and extrusion-coating substrates where opacity, whiteness, and ultraviolet scattering are required. It is not a finished film or molding resin; final optical and mechanical properties depend on letdown ratio, dispersion quality in the processing equipment, and the selected dilution resin. The grade name identifies the Polybatch concentrate platform, the white color designation LL8425, and the supplier-specific MG production code. The MG suffix does not by itself define the titanium dioxide concentration; exact pigment loading, melt mass-flow rate, and density are declared in the supplier’s certificate of analysis and product datasheet. The product contains a rutile titanium dioxide pigment dispersed in an LLDPE carrier; the pigment surface treatment is selected to reduce photoactivity and improve dispersion in polyolefin matrices.

    Incoming inspection commonly includes melt mass-flow rate according to ISO 1133-1:2022, density according to ISO 1183-1:2019, ash content according to ASTM D5630-22, and visual pellet uniformity. For high-speed letdown operations, a loss-in-weight feeder with a dosing accuracy of ± 0.25% to ± 0.5% of set rate is used to maintain the target concentration. Industrial white PE masterbatches are often let down at 3 wt% to 10 wt%, but the specific range for White LL8425 MG must be based on the grade datasheet and final film specification.

    The specification categories for White LL8425 MG include melt mass-flow rate, density, pigment concentration, film optical test response, and pellet contamination. Release limits for each category are defined by the supplier’s internal document and are verified by the certificate of analysis. The product is supplied in an LLDPE carrier; the exact melt flow index is not assigned by the MG suffix and must be read from the product datasheet. For quality planning, the incoming material should be assigned to a control plan using ISO 1133-1:2022, ISO 1183-1:2019, and ASTM D5630-22. Lot-to-lot reproducibility is controlled within a narrow melt-flow window, but the exact window is proprietary release data.

    Which Melt-Processing Parameters Control Dispersion Quality in LL8425 MG?

    Dispersion of the concentrate is controlled by shear rate history, melt temperature, residence time distribution, and the viscosity ratio between the pigment phase, the LLDPE carrier, and the dilution resin. In single-screw extruders with an L/D of 30:1 or greater and a barrier screw, the concentrate is introduced with the base resin at the main feed throat. A Maddock or Egan mixing section improves distributive mixing, but complete agglomerate reduction may require a dispersive mixing element and sufficient head pressure. Co-rotating twin-screw extruders with L/D 40:1 to 48:1 and segmented kneading blocks provide higher specific energy; however, excessive energy input can generate shear heating that degrades the polyethylene carrier and shifts the film yellowness index measured by ASTM E313-20.

    The supplier-recommended melt temperature for LLDPE film processing is commonly between 190 °C and 240 °C. Exceeding 260 °C may initiate oxidative degradation, generate color bodies, and reduce the whiteness index. The processing window in high-speed cast film can be as narrow as ± 5 °C around the supplier’s optimum melt temperature when throughput, screw speed, and back-pressure are held constant; this boundary is equipment-specific and must be mapped on the production line. Screen packs from 100 µm to 250 µm and a breaker plate with a 40:60 to 50:50 open area to blank ratio are commonly used to build head pressure and complete dispersion without exceeding the extruder pressure limit. Pressure transducers should be monitored before and after the screen pack; an increase greater than 10% from baseline at constant throughput may indicate melt filtration, screen blinding, or agglomerate accumulation.

    Moisture-related defects in LLDPE-based masterbatches are primarily caused by condensation on cold pellet surfaces rather than bulk moisture absorption. If storage conditions exceed 60% relative humidity, surface water may enter the feed zone and create lenses or fish-eyes in thin-gauge films. In such cases, pre-drying at 80 °C for 2 h to 4 h in a desiccant dryer is applied unless the supplier’s handling guide prohibits hot-air drying. The titanium dioxide phase is not hygroscopic, but the surface treatment can alter water adsorption; therefore, pellets should not be transferred directly from cold storage to a warm processing room without allowing package stabilization to prevent condensation.

    Letdown uniformity in a single-screw extruder is also influenced by the particle feeding behavior of the masterbatch and the base resin. Pellet geometry and bulk density differences can cause segregation in hoppers; therefore, a mixer or in-line static mixer is used downstream of the extruder to reduce thermal gradients. The melt temperature should be measured with an immersion probe at the die; relying solely on barrel set points can underestimate the actual melt temperature due to viscous dissipation in LLDPE systems.

    In white cast film and extrusion coating, the letdown ratio of White LL8425 MG determines scattering efficiency and opacity. Opacity is measured by ISO 13468-2:2021 or ASTM D1003-21; whiteness and yellowness are tracked by ASTM E313-20. The relationship between pigment concentration and optical properties is nonlinear. At low additions, each incremental increase in TiO₂ raises light scattering; above a saturation concentration, pigment particles begin to crowd and the incremental opacity gain per unit of added concentrate declines. For thin films below 30 µm, a higher letdown of a lower-loaded concentrate may reduce gel-like defects and pinholes compared with a lower letdown of an ultra-high-loaded concentrate, because local viscosity discontinuities are smaller. Published data for this specific configuration is limited; a dilution series on the target film line is required to establish the optimum addition rate. On cast film lines equipped with chill-roll units, quench rate differences between the outer and inner surfaces can affect spherulitic size and surface haze. A chill-roll temperature of 15 °C to 30 °C is typical for LLDPE cast film, and the resultant quench rate influences crystallinity and optical quality. The relative contribution of the concentrate to haze is smaller than the contribution of base resin and quench parameters, but using a carrier with similar melt rheology minimizes optical distortion.

    In three-layer blown film structures, White LL8425 MG is often placed in the skin layer or a middle opacity layer, while the seal layer is formulated separately to preserve seal initiation. For coextruded cast films, the concentrate is added only to the layers where opacity is required; this minimizes the overall TiO₂ content and reduces the effect on sealing performance. When the concentrate is used in barrier films, oxygen transmission rate testing by ASTM D3985-24 and water vapor transmission rate testing by ASTM F1249-24 should be repeated after pigment addition, because mineral fillers can alter the permeability path length and free volume of the polyolefin. Published data for this specific configuration is limited.

    When LL8425 MG Replaces LDPE-Carrier or PP-Carrier White Masterbatches

    The selection of an LLDPE carrier rather than an LDPE carrier affects extensional viscosity, seal initiation, and dilution uniformity in polyethylene film. LLDPE carriers exhibit a more linear molecular architecture and a narrower shear-thinning response; this matches the melt behavior of LLDPE and metallocene PE film resins more closely. When a PP-carrier masterbatch is introduced into PE film at letdown ratios above 5 wt%, the immiscible PP phase can form discrete domains that may increase gel counts, reduce dart impact, and shift seal initiation. Published quantitative comparisons for LL8425 MG against LDPE-carrier or PP-carrier products are limited; equivalence must therefore be established on the target line using melt rheology and film property testing. Comparative melt viscosity data can be generated by capillary rheometry at 190 °C and 210 °C or by oscillatory shear according to ISO 6721-10:2021.

    From a recycling standpoint, an LLDPE carrier is preferable for PE film structures because it does not introduce a PP fraction that can create incompatibility in post-consumer PE recycling streams. A high-MFR PE carrier may distribute more readily in injection molding but can reduce melt strength and bubble stability in blown film. The LL8425 MG grade uses an LLDPE carrier to balance letdown viscosity against final film mechanical properties. No formulation change should be made without running a full comparison on the actual film line, including dart impact to ASTM D1709-22, Elmendorf tear to ASTM D1922-23, and seal strength to ASTM F88/F88M-23.

    The effect of a carrier change is most visible in thin-gauge films below 30 µm. The carrier contribution to the total refractive index mismatch can be evaluated by measuring the haze of a 100% dilution resin film and comparing it with the haze of the letdown film under the same chill-roll temperature and die gap. A significant change in internal haze can indicate dispersion problems or a viscosity mismatch that causes morphological changes during drawdown. For blown film, bubble stability and frost line height should be recorded, because the concentrate can alter the elongational viscosity of the melt and change the inflation pattern. These line observations must be coupled with standardized tests, not used alone.

    Compliance of the final article is determined by the complete formulation, not by the concentrate alone. The polyethylene carrier may be used in food-contact applications within the scope of FDA 21 CFR 177.1520 and EU Regulation 10/2011, provided that the titanium dioxide grade and surface treatment are approved for the intended use. Overall migration testing according to EN 1186 and specific migration testing for any additives must be conducted on the finished food-contact article. The masterbatch is not a food-contact article; it must be diluted in a compliant base resin before use. For non-food applications, the REACH registration status of the grade must be confirmed with the current extended SDS. RoHS 2011/65/EU does not typically restrict TiO₂ or polyethylene, but lot traceability documents should be retained for technical files.

    Regulatory Compliance Matrix and Operational Boundaries

    Standard or regulationScopeRelevance for White LL8425 MG
    ISO 1133-1:2022Melt mass-flow rate of thermoplasticsIncoming carrier viscosity and letdown uniformity
    ISO 1183-1:2019Density of non-cellular plasticsIdentity verification and blend density calculation
    ASTM D5630-22Ash content in thermoplasticsPigment loading verification in letdown compounds
    ASTM D1003-21Haze and luminous transmittanceOptical acceptance of films
    ISO 13468-2:2021Total luminous transmittanceOpacity determination in thin films
    ASTM E313-20Yellowness and whiteness indicesColor control after processing
    ASTM D1709-22Dart impact of plastic filmMechanical integrity of final film
    ASTM D1922-23Elmendorf tear of plastic filmTear resistance after pigment addition
    ASTM F88/F88M-23Seal strength of flexible barriersEffect of concentrate on sealing performance
    FDA 21 CFR 177.1520Olefin polymers in food contactCarrier regulatory status for food applications
    EU Regulation 10/2011Plastics for food contactOverall migration and composition compliance
    EN 1186Migration testing methodsFinal article compliance verification

    Operational boundaries include the following: Do not expose the melt to temperatures above 260 °C for extended periods. Avoid melt blending with polymers that require processing temperatures above the LLDPE carrier’s degradation range, such as PET or polycarbonate. Do not use in food-contact structures unless the titanium dioxide surface treatment and the letdown resin meet the applicable migration limits. When high ambient humidity is present, pre-dry or condition the pellets before processing. The supplier’s product datasheet and certificate of analysis are the controlling documents for lot-specific release limits.

    Storage of unopened original packaging at ambient temperatures below 40 °C and away from direct sunlight is recommended for polyolefin masterbatches. Under these conditions, the product should be used within 24 months from the production date unless the certificate of analysis specifies otherwise. The storage area should be kept below 60% relative humidity to reduce condensation on pellet surfaces. Pallets should not be stacked beyond the supplier’s maximum recommendation because pellet compaction can increase fines generation during conveying. For vacuum conveying systems, line velocities below 25 m/s minimize pellet fracture and angel-hair formation; dense-phase conveying is preferred over dilute-phase conveying for LLDPE masterbatches.

    If white specks or surface roughness are observed on cast film, the cause may be insufficient dispersion or solid-bed breakup. Screen pack differential pressure should be monitored; an increase of more than 10% from baseline at constant throughput suggests melt filtration or agglomerate accumulation. Reducing screw speed without lowering additive feed rate may increase residence time and cause thermal yellowing. These checks should be performed with data logging on the extruder pressure transducers and compared with the supplier’s processing guide for White LL8425 MG. The product is not recommended for rotational molding or for processes with low shear mixing and long residence times, because dispersion may be insufficient and the carrier may thermally degrade before full homogenization.

    Top