| HS Code | 592831 |
| Product Name | LyondellBasell POLYBATCH™ White LL8425 AP Concentrate Based In LLDPE |
| Manufacturer | LyondellBasell |
| Product Type | White color concentrate |
| Carrier Resin | LLDPE |
| Color | White |
| Form | Pellets |
| Additive | Titanium dioxide |
| Tio2 Content | 75% |
| Density | 1.8 g/cm³ |
| Melt Flow Rate | 20 g/10 min (190°C/2.16 kg) |
| Let Down Ratio | 10:1 to 20:1 |
| Processing Methods | Blown film, cast film, injection molding, blow molding |
| Heat Stability | Good up to 260°C |
| Dispersion | Good |
| Moisture Absorption | Low |
| Food Contact Compliance | FDA 21 CFR 177.1520; EU 10/2011 |
As an accredited LyondellBasell POLYBATCH™ White LL8425 AP Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell POLYBATCH™ White LL8425 AP is supplied in 25 kg polyethylene-lined bags, palletized and shrink-wrapped for transport. |
| Container Loading (20′ FCL) | Securely loaded 20′ FCL container with palletized, shrink-wrapped 25 kg bags of LyondellBasell POLYBATCH™ White LL8425 AP LLDPE-based white concentrate. |
| Shipping | LyondellBasell POLYBATCH™ White LL8425 AP Concentrate Based In LLDPE is typically not regulated for transport. Ship as non-hazardous plastic pellets in sealed bags/octabins on pallets. Protect from moisture, heat, and sunlight. Use standard dry freight. No UN number, hazard class, or packing group required. Follow SDS/local rules. |
| Storage | Store LyondellBasell POLYBATCH™ White LL8425 AP Concentrate Based In LLDPE in a cool, dry, well-ventilated warehouse. Keep containers tightly closed when not in use. Protect from direct sunlight, heat, moisture, and contamination. Avoid proximity to strong oxidizers and ignition sources. Maintain normal ambient temperatures; avoid excessive stacking. Use original packaging. Observe good housekeeping and FIFO stock rotation. Store away from incompatible materials. Ensure pallets are stable and clean. |
| Shelf Life | Typically 24 months from production if stored sealed in original packaging in cool, dry, ventilated areas away from direct sunlight. |
In monolayer blown-film extrusion of linear-low-density polyethylene, POLYBATCH™ White LL8425 AP Concentrate Based In LLDPE is introduced by gravimetric dosing at the feed throat, upstream of a grooved-barrier single-screw extruder with an L/D ratio of 24:1 or greater. Processing windows cited in this section are typical starting ranges for LLDPE-carrier white concentrates and must be verified against the supplier product data sheet and the converter’s specific equipment. The let-down for opaque white packaging films is controlled within 4 wt% to 8 wt% of total throughput, a range that balances opacity against bubble stability and heat-seal response. Barrel temperature profiles are set from 170 °C at the feed zone to 195 °C at the metering zone, with die zones held at 205 °C to 215 °C. A dual-lip air ring supplied with chilled air at 10 °C to 15 °C and a blow-up ratio of 2.2:1 to 3.0:1 maintain a frost line height of 150 mm to 300 mm above the die face. Final articles include refuse liners, freezer overwrap, heavy-duty shipping sacks, and white carry-out bags. Optical haze and transmittance in converted film are measured according to ASTM D1003, tensile properties according to ASTM D882, and dart impact according to ISO 7765-1. Concentrate melt flow rate is confirmed by ISO 1133-1:2022 at 190 °C/2.16 kg before use to detect lot-to-lot carrier variation. Pigment content is checked by thermogravimetric ash analysis using ASTM D5630. Pre-drying is not normally required when pellets remain in sealed moisture-barrier packaging; cold storage should be brought to ambient before opening to avoid surface condensation. For food-contact constructions, the completed film must satisfy overall migration and specific migration limits of Commission Regulation (EU) No 10/2011 and the olefin polymer extractables limitations of FDA 21 CFR 177.1520. Titanium dioxide purity in the color concentrate must be verified against the applicable positive-list or purity criteria for the target market; end-product legal responsibility remains with the converter.
When chill-roll surface temperature drops below 18 °C on high-output cast film lines for white label stock, the white concentrate is metered at 5 wt% to 10 wt% and the resulting quench rate can increase film curl and edge instability. The polymer melt is extruded through a coat-hanger die with a die gap of 0.5 mm to 1.0 mm, and the molten web is pinned to a matte or gloss chill roll maintained at 18 °C to 24 °C; lower surface temperatures increase transverse-direction thickness variability and may create optical defects in thin gauge. Melt temperature at the die is maintained at 220 °C to 250 °C to limit thermal history in the LLDPE carrier while still achieving low melt viscosity for uniform web spreading. Air gap is restricted to 20 mm to 30 mm to control neck-in and reduce edge bead height. Downstream testing includes coefficient of friction according to ISO 8295, thickness variability according to ASTM D6988, and optical haze according to ASTM D1003. Terminal products are high-opacity printed pressure-sensitive label facestock, diaper backsheet film, and white sealing webs for flexible packaging. Export documentation normally requires REACH registration confirmation under Regulation (EC) No 1907/2006 and demonstration that the restricted substances listed in Directive 2011/65/EU Annex II fall below the maximum concentration values applicable to the finished article.
High-speed extrusion lamination of white layers for foil and paper substrates demands a concentrate addition of 8 wt% to 15 wt% in coating-grade LDPE to achieve sufficient hiding power in coating weights of 15 g/m² to 40 g/m². Titanium dioxide agglomeration is controlled by a combination of low feed-zone compression, adequate backpressure, and dispersion-oriented screw mixing. The coating extruder is typically a 90 mm to 120 mm single-screw machine with an L/D ratio of 30:1 to 36:1, feeding a coextrusion feedblock and a flat die set to a die gap of 0.8 mm to 1.2 mm. Melt temperatures are held at 285 °C to 320 °C to promote adhesion to foil, paper, or oriented substrates; because the LLDPE carrier can undergo chain scission above 300 °C, screw speed and backpressure must be bounded so that residence time does not exceed 8 min to 12 min. Dispersion quality is assessed by counting visible pigment agglomerates on a cast film sample under 10× magnification; an increase in agglomerate count above the line-specific control limit indicates poor distributive mixing, inadequate compression, or feed-throat bridging. Nip pressure at the cooling roll is maintained between 2 bar and 4 bar, and the chill roll surface is cooled to 12 °C to 18 °C. Finished structures include aseptic brick outer white layers, toothpaste laminate tubes, medical packaging lamination, and foil-based cable wrap. Compliance is tested under FDA 21 CFR 177.1520 for the polyolefin layer and under Commission Regulation (EU) No 10/2011 for overall migration using food simulants appropriate to the final laminate.
Under discontinuous high-shear injection-moulding conditions, the concentrate is let down at 2 wt% to 5 wt% into high-density polyethylene or LLDPE-based compounds used for white pails, thin-wall containers, and disposable cutlery. The reciprocating-screw injection machine is operated with a compression ratio of 2.5:1 to 3.5:1, an injection pressure of 70 MPa to 120 MPa, and a clamp force selected from the projected cavity area. Melt temperature is controlled at 190 °C to 230 °C, and mould temperature is maintained at 15 °C to 35 °C to balance cycle time against surface gloss and sink-mark control. Short shots or flow lines may appear when the let-down ratio exceeds 5 wt% in thin-wall geometries with flow length-to-thickness ratios above 150:1. Final parts are assessed for tensile yield stress under ISO 527-2, and white pigment distribution is verified by photometric reflectance readings taken at multiple points across the part surface. Food-contact grades of the finished article require certification under FDA 21 CFR 177.1520 or Commission Regulation (EU) No 10/2011, depending on jurisdiction; toys and childcare articles may require additional migration testing under EN 71-3.
Extrusion blow moulding of opaque monolayer bottles requires a concentrate addition of 3 wt% to 6 wt% in HDPE or HDPE/LLDPE blends processed on shuttle or accumulator-type blow moulding machines. Stock temperatures at the die head are controlled between 180 °C and 205 °C; higher temperatures reduce melt strength and worsen parison sag in containers with shot weights above 200 g. Die swell and parison programming are adjusted with a die land length-to-gap ratio of 20:1 to 30:1 to maintain uniform wall thickness in panel areas. Blow pressure is set at 0.5 MPa to 0.8 MPa, and mould cooling is supplied at 8 °C to 14 °C. The white concentrate raises opacity sufficiently for dairy-style bottles, personal-care containers, and household chemical bottles where light protection of contents is required. Physical properties of the blown wall are verified by ASTM D638 tensile testing of die-cut specimens, and bottle drop-impact performance is checked using ASTM D2463. Regulatory compliance for personal-care and detergent packaging typically references REACH Regulation (EC) No 1907/2006, while food-contact variants require verification under Commission Regulation (EU) No 10/2011 and FDA 21 CFR 177.1520.
At thicknesses between 15 µm and 30 µm, white agricultural mulch film demands a concentrate addition of 5 wt% to 12 wt% to achieve high reflectance and low light transmission for root-zone temperature regulation. The blown film line is typically configured with an L/D ratio of 30:1 and a hardened barrel and screw set, because titanium dioxide at high addition rates accelerates metal wear when throughput exceeds 250 kg/h. Melt temperature is maintained at 190 °C to 215 °C; excursions beyond 230 °C for more than 15 min can produce yellowing that is visible against the white film background and should be monitored with inline color sensors. The film bubble is run at a blow-up ratio of 2.5:1 to 3.5:1 to balance tear resistance and light reflectivity. Tensile properties are measured according to ISO 527-3, dart impact according to ISO 7765-1, and light transmission using ASTM D1003. Final articles include white-on-black mulch films for soil cooling, opaque silage cover films, and white greenhouse shading films. Compliance for non-food agricultural applications is usually based on REACH Regulation (EC) No 1907/2006, and restricted-substance absence is verified against the maximum concentration values in Directive 2011/65/EU Annex II. National plasticulture disposal regulations may impose additional requirements on pigment and polymer composition; published data for this specific configuration is limited and must be confirmed by the film converter.
Competitive LyondellBasell POLYBATCH™ White LL8425 AP Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell POLYBATCH™ White LL8425 AP is a pelletized white concentrate carried in a linear low-density polyethylene resin. The product is intended for dilution into polyethylene-based extrusion, injection molding, and blow molding operations where controlled white pigmentation, opacity increase, and reliable feeding at defined letdown ratios are required. The carrier selection is technically significant because LLDPE narrows the melt-viscosity gap with hexene- or octene-based LLDPE and metallocene LLDPE film resins, lowering the probability of undispersed agglomerates in high-speed monolayer and multilayer film. Because the concentrate contains a high loading of inorganic pigment, the as-received melt mass-flow rate is not equivalent to the final compound. The diluted melt flow rate should be measured according to ISO 1133-1:2022 at 190 °C and 2.16 kg, or to ASTM D1238-23a Procedure A. Published data for the exact titanium dioxide loading and carrier melt index of this specific grade are limited outside the LyondellBasell technical data sheet and the production lot certificate of analysis; those values must be verified before feeder calibration and extruder temperature profile selection.
The product designation differentiates LL8425 AP from LDPE-carrier and EVA-carrier white batches within the POLYBATCH range. The LLDPE carrier is selected when the target matrix is LLDPE, metallocene polyethylene, or LLDPE/LDPE blends in blown film, cast film, extrusion coating, and sheet. In those processes, the carrier melting range and crystallization behavior influence pellet melting order in the feed zone, melt-pressure stability before the screen pack, and die-lip deposit formation. When an LDPE-carrier white concentrate is used in an LLDPE-rich film, the lower-viscosity LDPE carrier can flow preferentially in the metering zone, producing local pigment concentration gradients and visible white streaks. LL8425 AP is formulated to reduce this viscosity-channeling failure mode, but dispersion still requires a screw design with sufficient shear and a melt temperature high enough to complete carrier melting and pigment agglomerate breakdown. General LLDPE film extrusion operates most reliably in the range of 190–240 °C, but the exact profile must be established by plant validation on the target die and screw.
For blown film below 25 µm, hiding power and surface quality are more sensitive to pigment dispersion than in thicker films. Typical white masterbatch addition rates for LLDPE film fall between 5 wt% and 12 wt%, but these are process-dependent and not a guaranteed performance range for a specific lot. The practical upper letdown is limited by rheological mismatch, screen pack pressure rise, and die-lip build-up rather than by the inorganic pigment alone. When letdown exceeds the dispersion capacity of the extruder, undispersed pigment agglomerates appear as white specks, pinholes, or uneven color at the take-off. Haze and luminous transmittance should be measured using ASTM D1003-21 or ISO 14782:2021, while gloss is characterized by ISO 2813:2014 at 60°. An increase from 6 wt% to 10 wt% of a typical titanium dioxide concentrate can raise opacity but may reduce dart impact and machine-direction tear strength due to the filler effect; this relationship must be quantified on the target film using ASTM D1709 for dart impact and ASTM D1922 for propagated tear.
On a 75 mm single-screw blown film line with a 30:1 L/D barrier screw and a 100 mesh screen pack, a practical diagnostic is to compare screen pack pressure rise between the unpigmented matrix and the letdown compound. A rise greater than 25% at constant throughput often indicates agglomerate retention or excessive screen blockage, and the letdown ratio should be lowered or the mixing section re-evaluated. This is a plant-level check, not a release criterion.
Although LLDPE carriers are not hygroscopic, surface moisture from open storage above 60% RH can generate film bubbles and surface haze during extrusion. Drying at 70–80 °C for 2–4 h in a desiccant dryer is a standard precaution for films below 30 µm, particularly in cast film and extrusion coating.
Color strength and hiding power are determined not only by titanium dioxide concentration but also by the particle size distribution and the quality of the pigment surface treatment. Rutile titanium dioxide with average particle diameter of approximately 0.2–0.3 µm is typical for high scattering efficiency in polymer films. The particle size distribution can be measured by laser diffraction according to ISO 13320:2020. Agglomerates larger than 5 µm are generally undesirable in thin film because they appear as white specks. If the production lot does not provide a dispersion specification, the user can assess dispersion by optical microscopy or scanning electron microscopy on a microtomed film section. Such measurements are not pass-fail for product release but support trouble-shooting.
High-dispersion masterbatches require both distributive and dispersive mixing. On a single-screw blown film line, a barrier screw with a Maddock mixing section and a mixing head often provides sufficient shear to reduce pigment agglomerates at moderate output. On a twin-screw compounding line used for pre-dilution, co-rotating intermeshing screws with 40:1 L/D and kneading blocks can produce high shear; but for white masterbatch dilution, extrusion temperature and residence time must not exceed the stability limit of the LLDPE carrier. The maximum shear stress is more important than total shear heat; excess melt temperature can degrade the carrier and create yellow specks. Die pressure and specific energy consumption should be recorded, and the color of purgings can be used as a visual process signal.
The choice of concentrate carrier changes the viscosity ratio, melting rate, and pigment wetting. For LL8425 AP, the LLDPE carrier is designed for matrices dominated by LLDPE or mLLDPE; however, if the target formulation is primarily LDPE with low melt index, the carrier viscosity can be lower than the matrix. In such cases, color development may decline because the carrier is selectively melted and sheared while the more viscous matrix remains partially unmelted. An LDPE-carrier concentrate can provide better viscosity matching in LDPE-heavy formulations. The comparison below is based on general polyethylene white masterbatch behavior, not on grade-specific lot data for LL8425 AP.
| Carrier type | Matrix compatibility | Viscosity matching behavior | Representative process risk | Applicable melt flow standard |
|---|---|---|---|---|
| LLDPE carrier (LL8425 AP) | LLDPE, mLLDPE, LLDPE/LDPE blends | Narrows melt-viscosity gap in LLDPE-rich systems | Insufficient carrier viscosity in high-melt-viscosity LDPE or HDPE matrices may produce flow lines | ISO 1133-1:2022 |
| LDPE carrier | LDPE, EVA, some LLDPE blends | Better for high-pressure LDPE tube or autoclave grades; may channel in mLLDPE | White streaks and nonuniform color in LLDPE/mLLDPE film | ISO 1133-1:2022 |
| EVA carrier | EVA, EBA, polar copolymers | Improves pigment wetting and adhesion but limits high-temperature processing due to acetate odor and acid generation | Yellowing, corrosion, and plate-out | ISO 1133-1:2022 |
| PP carrier | Polypropylene only; not for polyethylene | Immiscible in PE; cannot provide property retention | Delamination and mechanical property loss | ISO 1133-1:2022 |
Because the carrier also influences pressure drop in the die, the extruder throughput and melt temperature must be adjusted when switching between LLDPE-carrier and LDPE-carrier concentrates. The screen pack and breaker plate should be inspected at the start of the campaign, and the adapter temperature should be kept within the range recommended for the matrix and concentrate. A switch from a high-MFR LDPE carrier to LL8425 AP in the same formulation may produce a measurable change in melt pressure at constant screw speed; the pressure difference is not a defect but must be recorded to distinguish normal carrier effects from screen blockage.
Bubble stability in LLDPE blown film is sensitive to melt strength and strain hardening. An LLDPE carrier does not provide the high melt strength of LDPE; therefore replacing a high-MFR LDPE carrier with LL8425 AP may require a reduction in draw-down ratio or a slight adjustment of blow-up ratio. The bubble cooling and frost line height must be re-optimized because the viscosity and crystallization rate of the LLDPE carrier shift the point at which the molten film starts to solidify. A high-blow-up-ratio process may also expose dispersion defects; a stable bubble with low flutter is necessary to avoid thickness variation.
In three-layer or five-layer blown and cast coextrusion, the white concentrate is generally placed in the outer skin layer rather than in the tie or barrier layer. The pigment itself can affect the surface coefficient of friction, blocking force, and seal behavior of the skin layer. When LL8425 AP replaces an LDPE-carrier white concentrate in an LLDPE-rich skin layer, the viscosity match may improve layer uniformity and reduce interfacial instability in the primary bubble or cast roll. However, the addition of inorganic white pigment to a sealant layer can raise the seal initiation temperature and reduce hot tack strength. The effect must be quantified on the target structure using ASTM F1921 for hot tack and ASTM F88 for heat seal strength.
In coextruded structures, the skin layer containing white concentrate may be thinner than 10 µm. At this layer thickness, a carrier that is not matched to the matrix can cause layer encapsulation and flow disturbance in the feedblock. Measurements of layer distribution by optical microscopy of cross-section, along with thickness mapping, can confirm whether the white skin layer remains continuous. If the white layer becomes non-uniform, opacity and seal properties will vary across the web width. Adjustments to die temperature and feedblock design may be required when switching from LDPE carrier to LLDPE carrier.
In extrusion lamination and cast film, titanium dioxide concentrates can form die-lip deposits from release agents, waxes, or degraded LLDPE. A precision flat die with internal deckle and minimal dead zones reduces deposit formation; die cleaning cycles may need to be shortened when running at high letdown or high line speed. If the concentrate is not properly dispersed, the output film can exhibit machine-direction pigment lines. The use of a rotating static mixer or a well-designed Maddock mixing section is required; simple conveying screws without distributive mixing are not suitable for high loadings.
In extrusion coating, the white concentrate is added to the LDPE or LLDPE coating resin to provide opacity and visual aesthetics. At high coating line speeds above 300 m/min, the residence time in the extruder and die is approximately 5–15 s; therefore the masterbatch must disperse quickly. LLDPE carriers may have lower melt strength than LDPE, so the addition level in extrusion coating should be checked for neck-in and adhesion to the substrate. Peel strength to paper, board, or foil is tested according to ASTM D1876 or ISO 8510-2, but the white concentrate can alter surface polarity and should be included in the adhesion trial.
Compliance status for LL8425 AP is lot-specific and application-specific. A technically complete qualification package for a white polyethylene concentrate should include the following documentary checks. The table does not state that LL8425 AP is approved for a particular food-contact or electrical application; it identifies the standards and regulations that must be confirmed with the manufacturer before use. The AP designation in the grade name is part of the supplier coding; no technical meaning is assigned in the public description. It should not be interpreted as a compliance claim or a specific surface treatment. Users should request the product data sheet for the AP variant when replacing an earlier LL8425 grade because additive package and carrier rheology can vary between internal production grades.
| Standard or regulation | Scope | Typical verification for white polyethylene concentrates |
|---|---|---|
| REACH (EC) 1907/2006 | Substance registration and SVHC declaration | Supplier SDS and article declaration confirmed for carrier and pigment |
| EU Regulation (EU) No 10/2011 | Plastics food-contact migration | Overall migration and specific migration limits if food-contact use is claimed |
| FDA 21 CFR 178.3290 | Colorants for polymers in food-contact use | Colorant purity and use conditions stated by supplier |
| EU Packaging Directive 94/62/EC | Heavy metals in packaging | Sum of lead, cadmium, mercury, and chromium VI not to exceed 100 mg/kg |
| RoHS Directive 2011/65/EU | Restricted substances in electronic and electrical equipment | Pb, Cd, Hg, Cr VI, PBB, and PBDE below directive limits |
| ISO 1133-1:2022 | Melt mass-flow rate | Carrier MFR and diluted compound MFR |
| ASTM D1003-21 / ISO 14782:2021 | Haze and luminous transmittance | Optical performance of letdown film |
| ISO 2813:2014 | Gloss | Surface gloss of letdown film at 60° |
A laboratory letdown must be prepared with a controlled twin-screw or two-roll mill according to the supplier recommended letdown ratio. The standard optical film test uses a 50 µm cast film or blown film sample to measure color coordinates and opacity. Spectrophotometric measurements can be performed using CIE L*a*b* with D65 illuminant and 10° observer; the color difference is evaluated according to ISO 11664-4. This provides a reproducible evaluation of batch-to-batch color consistency. However, CIE L*a*b* alone does not correlate with film aesthetic quality; it must be accompanied by visual inspection and haze measurement.
Gravimetric feeding is preferred over volumetric feeding for white concentrates because the high density and pigment content can affect bulk flow from a volumetric screw. Feeder calibration should account for the bulk density of the masterbatch, which is usually significantly higher than that of natural LLDPE pellets. Poor calibration can result in letdown ratio drift and visual color variation from roll to roll. Processors can verify the actual letdown ratio by ashing or thermogravimetric analysis, but the matrix decomposition and pigment residue must be corrected using the concentrate inorganic residue value from the certificate of analysis.
In injection molding of thin-wall white parts, LL8425 AP is added by gravimetric feeder to the main polyethylene resin. The LLDPE carrier may be appropriate for LLDPE and some LLDPE/LDPE blends, but in HDPE matrices the melt-viscosity mismatch can produce visible flow lines and poor pigment dispersion in thick sections or low-shear zones. For HDPE closures and industrial containers, a carrier matched to HDPE or a universal polyolefin white concentrate is generally preferred. The molded part density and tensile yield stress are modified by the inorganic pigment; tensile properties should be measured according to ISO 527-2:2012 or ASTM D638-14 on conditioned specimens. Shrinkage and warpage can also be affected by the filler level, particularly in semi-crystalline LLDPE and HDPE, so mold validation on the intended tool is required.
Processing temperature should remain below the oxidative degradation regime of the LLDPE carrier and pigment coating. The supplier grade-specific data sheet may limit melt temperature or hold-up time; without that limitation, general polyethylene masterbatch practice is to avoid melt temperatures above 260 °C and hold-up times longer than 10 min in the barrel. Process conditions above those boundaries can generate yellowing and die-drop formation and must be validated on the production line for each formulation.