| HS Code | 848246 |
| Manufacturer | LyondellBasell |
| Brand | POLYBATCH™ |
| Product Name | POLYBATCH™ White LL8000 AP |
| Product Code | LL8000 AP |
| Product Type | White masterbatch concentrate |
| Carrier Resin | LLDPE |
| Color | White |
| Form | Pellets |
| Compatible Polymers | Polyethylene |
| Density | 2.3 g/cm³ (typical) |
| Melt Flow Rate | 20 g/10 min at 190°C/2.16 kg (typical) |
| Titanium Dioxide Content | 80% (typical) |
| Let Down Ratio | 2-5% (typical for film) |
| Recommended Processing | Blown film, cast film, extrusion coating, injection molding, blow molding |
| Thermal Stability | Good |
| Light Fastness | Good |
| Moisture Absorption | Low |
| Packaging | 25 kg bags |
| Storage Conditions | Dry, below 30°C |
| Food Contact | Complies with applicable regulations |
As an accredited LyondellBasell POLYBATCH™ White LL8000 AP Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Supplied as pellets in 25 kg polyethylene bags, 40 bags per pallet, totaling 1,000 kg per pallet. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): LyondellBasell POLYBATCH™ White LL8000 AP LLDPE-based concentrate loaded in dry 20′ FCL, securely stowed, ambient conditions. |
| Shipping | LyondellBasell POLYBATCH™ White LL8000 AP Concentrate Based In LLDPE is a non-hazardous, free-flowing white masterbatch pellet. It is not classified as dangerous goods for transport. Ship in sealed, labeled bags or octabins; keep dry, cool, and protected from contamination. No special UN packaging required. Follow SDS and local regulations. |
| Storage | Store in original packaging, properly labeled, in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers or bags tightly closed to prevent moisture and contamination. Avoid prolonged high temperatures, physical damage, and excessive stacking. Use first-in, first-out stock rotation. Consult the manufacturer’s SDS and local regulations for additional storage and handling requirements. |
| Shelf Life | Shelf life is 12 months from date of production when stored in original, unopened packaging in a cool, dry area. |
LyondellBasell POLYBATCH™ White LL8000 AP is a titanium dioxide (TiO₂) colour concentrate dispersed in a linear low-density polyethylene (LLDPE) carrier resin. The grade is supplied as free-flowing cylindrical pellets compatible with standard polyolefin volumetric and gravimetric screw feeders. The masterbatch melt flow rate, TiO₂ loading, and carrier resin density are declared in the supplier technical data sheet and constitute the mandatory basis for all let-down ratio calculations. End-product opacity is governed by the final TiO₂ concentration in the finished article, not by the masterbatch brand designation alone. The concentrate is formulated for let-down in LLDPE, LDPE, and compatible polyolefin base resins where melt viscosity parity prevents screw slippage, phase stratification, or colour streaking.
Dispersed TiO₂ pigment in a polyolefin matrix is subject to food-contact and chemical regulations that vary by conversion process and end market. Verification of the applicable regulatory instrument against the supplier certification and the finished article composition is a prerequisite for commercial supply.
In blown film converting, let-down ratios for LLDPE-based white concentrates typically fall between 2% and 8% by weight, depending on target film thickness and required luminous transmittance. A 50 μm monolayer film containing 3% dispersed TiO₂ achieves luminous transmittance below 10% per ISO 14782, corresponding to a calculated let-down ratio of 6% when the masterbatch carries a 50% TiO₂ loading. The calculation is: final TiO₂ percentage equals masterbatch TiO₂ percentage multiplied by let-down ratio divided by 100. Where the supplier TDS specifies a different TiO₂ loading, the let-down ratio must be recalculated before production start-up. Single-screw extruders with screw length-to-diameter ratios of 24:1 to 30:1 and compression ratios of 2.5:1 to 3.5:1 provide sufficient distributive mixing for TiO₂ agglomerate breakage when barrel temperatures are profiled from 160°C at the feed throat to 210–230°C at the adapter. Die exit temperatures above 240°C induce TiO₂-catalysed thermo-oxidative chain scission in the LLDPE carrier, generating low-molecular-weight volatiles that deposit on the air ring lips. Air ring deposition appears as brownish residue within 45–90 minutes of continuous operation and requires line stoppage for mechanical cleaning. Melt pressure measured before the screen pack should not exceed 250 bar on a new screen set. Pressure rise above 30 bar differential indicates agglomerate accumulation and demands screen replacement or an upstream dispersion audit. Screen packs are typically configured as 60/80/120 mesh in monofilament stainless steel, with the 120 mesh layer facing the die to trap undispersed pigment clusters exceeding 125 μm.
Blow-up ratios between 2.0:1 and 3.0:1 generate balanced machine-direction and transverse-direction tensile properties per ISO 527-3. Frost line height positioned at 4–8 die diameters above the die face controls crystallite size and maintains dart impact resistance above 400 g per ISO 7765-1 for a 60 μm film. Die gaps of 1.5–2.5 mm on monolayer lines and 2.0–3.0 mm on coextruded structures produce stable bubble geometry at frost line velocities below 40 m/min. The LLDPE carrier contributes a lower seal initiation temperature than LDPE-carrier white concentrates. Seal strength values above 20 N/15 mm per ASTM F88/F88M are obtained at seal bar temperatures of 115–125°C on multilayer lines. Whiteness index and yellowness index are measured per ISO 11664-4 and ASTM E313 respectively; a yellowness index below 2.0 is considered specification-grade for printed label stock.
The table below presents the calculated let-down ratio gradient for blown film thickness of 50 μm. Values are engineering estimates based on Kubelka-Munk scattering principles and supplier formulating guides. Direct measurement per ISO 14782 and ISO 11664-4 is required for specification compliance on production film.
| Let-down ratio (wt%) | Masterbatch addition (kg per 100 kg base resin) | Final TiO₂ in film (wt%) | Luminous transmittance at 50 μm (%) | Whiteness index L* (indicative) |
|---|---|---|---|---|
| 2 | 2 | 1.0 | 35–45 | 90–92 |
| 4 | 4 | 2.0 | 15–25 | 93–95 |
| 6 | 6 | 3.0 | 6–12 | 95–96 |
| 8 | 8 | 4.0 | 3–6 | 96–97 |
End products manufactured from white opaque blown film include dairy powder sachets, printed stand-up pouch label stock, refuse sacks with white-on-black coextruded film structures, and agricultural mulch film where the white outer layer reflects photosynthetically active radiation while the black inner layer suppresses weed germination. The opacity performance is thickness-dependent; films below 25 μm require the upper end of the let-down ratio range to maintain equivalent luminous transmittance.
The substitution of unfilled LDPE with an LLDPE-based white concentrate in extrusion coating applications introduces a higher melt viscosity component that alters the neck-in profile on chill-roll lines. Melt temperatures at the coating die are maintained between 290°C and 320°C to achieve oxidative adhesion to corona-treated paper and board substrates. At these temperatures, TiO₂ surfaces act as heterogeneous nucleation sites for radical generation, accelerating thermo-oxidative degradation of the LLDPE carrier. Gel formation becomes measurable as specks in the coated web above 320°C, with speck counts exceeding 3 per m² triggering specification rejection. Let-down ratios for extrusion coating range from 5% to 12%, producing coating weights of 15–40 g/m² with optical density sufficient to mask reverse-printed graphics on the substrate. Die lip plate-out consists of oxidised low-molecular-weight species complexed with TiO₂ fines. Mechanical wiping intervals of 4–6 hours are documented on production-scale lines operating at 300 m/min. Compliance for food-contact coatings requires the finished article to satisfy 21 CFR 177.1520 for the olefin polymer phase and 21 CFR 178.3297 for the colorant, the latter limiting TiO₂ in the finished food-contact article to 2% by weight. End products include aseptic liquid packaging board, detergent carton liners, release paper for pressure-sensitive laminates, and white barrier liners for frozen food folding cartons. Published data for LL8000 AP in high-speed extrusion coating at line speeds above 400 m/min is limited; process validation on the target line is required.
Thin-walled injection moulded components coloured with LLDPE-based white concentrates exhibit splay defects when residual moisture in the masterbatch exceeds 0.05% by weight. Splay manifests as silver streaking radiating from the gate and is caused by steam evolution during plasticisation in the barrel. Pre-drying of the masterbatch at 70–80°C for 2–4 hours in a desiccant dryer with dew point below −30°C is recommended where ambient relative humidity exceeds 60%. Barrel temperature profiles follow a rising ramp from 180°C at the feed zone to 220–245°C at the nozzle, with back pressures of 5–10 bar hydraulic to maintain melt density uniformity. Let-down ratios between 2% and 5% are typical for thin-walled containers with wall sections below 1.2 mm. High injection speeds above 150 mm/s combined with mould temperatures of 15–30°C reduce visible flow lines at the surface layer. Weld lines in pigmented LLDPE compounds show reduced tensile strength retention compared to natural resin; the imbalance is mitigated by locating gates to displace weld lines to non-critical stress regions. Shrinkage of white LLDPE compounds measures 1.5–2.5% per ISO 294-4, depending on mould geometry and packing pressure. Ash content verification per ISO 3451-1 at the screw tip provides direct measurement of TiO₂ concentration and confirms let-down accuracy within ±0.3% absolute. End products include thin-walled food containers, beverage cup lids, closures, cosmetic jar bodies, and medical waste containers where opacity prevents content visibility and where dimensional stability under hot-fill conditions is governed by the LLDPE matrix.
Cast film converting feeds the LLDPE-based white concentrate through a slot die onto a chilled polishing roll. Chill roll surface temperatures between 15°C and 25°C provide rapid melt quenching that minimises TiO₂ pigment mobility and fixes surface gloss above 70 GU per ISO 2813 at 60° measurement geometry. Let-down ratios of 3–8% produce film thicknesses from 20 μm to 120 μm with haze values below 20% per ISO 14782 in the opaque range. Edge trim containing white concentrate is recycled into the extrusion feed at rates up to 30% by weight without measurable gloss reduction when regrind particle size is maintained below 10 mm. The LLDPE carrier contributes enhanced dart impact resistance relative to LDPE-carrier white masterbatches, with measured values above 350 g per ISO 7765-1 for 50 μm cast film. Melt temperature at the die exit is held at 220–250°C, with the upper limit constrained by discolouration onset in the TiO₂-polymer interface. End products include stretch wrap, hygiene film backsheets, barrier lamination substrates, and printed label facestock.
Extrusion blow moulding with LLDPE-based white concentrates requires assessment of parison melt strength because TiO₂ particles increase low-shear viscosity and reduce sag. Continuous shuttle or rotary wheel machines run melt temperatures of 190–220°C with let-down ratios of 3–6% for opaque dairy and personal care bottles. Parison wall thickness control via programmable die gaps compensates for the slight increase in melt stiffness imparted by pigment loading. Bottle weights are maintained within ±2% by adjusting the let-down ratio only when wall thickness distribution exceeds the capability envelope of the die gap controller. Drop impact testing per ASTM D2463 on filled bottles stored at 4°C documents failure heights above 1.2 m for 500 mL containers with 0.8 mm nominal wall thickness. The regulatory status of TiO₂ under EU Regulation 10/2011 requires verification for dairy bottle applications because titanium dioxide is not listed in Annex I as an authorised substance. End products include opaque shampoo bottles, body lotion containers, dairy bottles with light-barrier functionality, and pharmaceutical container bodies.
White sheet extrusion for thermoforming uses LLDPE-based white concentrates at let-down ratios of 4–10%, producing sheet thicknesses from 0.5 mm to 2.0 mm. Sheet extruders configured with screw L/D ratios of 30:1 or higher achieve optimal TiO₂ distribution before the die. Die lip temperatures are held below 220°C to avoid yellowing of the white pigment surface. Thermoforming of white LLDPE sheet proceeds at forming temperatures of 110–130°C, measured by surface pyrometry of the sheet prior to plug assist. Draw ratios of 2:1 to 4:1 are achievable without localised thinning below 200 μm in formed part sidewalls where let-down ratios are maintained below 8%. Sheet gloss after forming is reduced by 5–15 GU relative to unformed sheet per ISO 2813, attributable to surface microroughness induced by plug contact. End products include margarine tubs, dairy cups, decorative tray inserts, and single-use medical tray liners.
Coextruded polyolefin pipe with a white outer layer employs LLDPE-based white concentrates at let-down ratios of 5–10% in the cap layer. The cap layer thickness is proportioned to comprise 10–20% of total wall thickness, ensuring TiO₂ loading in the cap layer provides opacity sufficient to mask the carbon-black-filled core. Melt temperatures for the white cap layer are set at 190–210°C, which is 10–20°C below the core layer temperature, to preserve pigment dispersion and prevent interfacial flow instability at the die convergence point. Vacuum sizing calibration maintains outer diameter tolerances of ±0.1 mm on 32 mm diameter pipe. UV-reflective white surfaces reduce absorbed solar radiation by 40–60% compared to black pipe surfaces, based on hemispherical reflectance measurements above 70% in the visible range per ASTM E903. End products include agricultural irrigation pipe, electrical conduit, and district heating external jackets where temporary UV exposure occurs during installation staging before burial.
The following compliance matrix consolidates the regulatory provisions applicable to the dispersed TiO₂ phase and the LLDPE carrier across the applications described above.
| Regulatory instrument | Designation | Applicability | Condition / limit |
|---|---|---|---|
| US FDA food contact | 21 CFR 177.1520 | LLDPE carrier resin | Olefin polymer specification; no TiO₂ restriction under this section |
| US FDA colorants | 21 CFR 178.3297 | TiO₂ in food-contact articles | Maximum 2% by weight of finished food-contact article unless otherwise specified |
| EU food contact | Regulation (EU) 10/2011 | TiO₂ in plastic food-contact materials | Titanium dioxide not listed in Annex I Union List; use requires verification against national legislation or specific authorisation |
| EU food additive | Regulation (EU) 2022/63 | E171 withdrawal as food additive | Does not apply to polymer-bound TiO₂ in plastic articles; not a food additive |
| EU chemicals | REACH Regulation (EC) 1907/2006 | TiO₂ substance registration | Registered substance; no authorisation requirement for use in plastics compounds |
| EU classification | CLP Regulation (EC) 1272/2008 | TiO₂ powder | Carc. 2 by inhalation per Commission Delegated Regulation (EU) 2020/217; classification applies to powder form with aerodynamic diameter ≤ 10 μm, not polymer-bound pellets |
| EU RoHS | Directive 2011/65/EU | TiO₂ in electrical and electronic equipment | No restriction on TiO₂ |
| EU packaging | Directive 94/62/EC | Heavy metals in packaging | Sum of Pb, Cd, Hg, Cr⁶⁺ ≤ 100 ppm by weight |
Rotational moulding with LLDPE-based white concentrates requires grinding of the masterbatch pellet to a powder with median particle size below 500 μm to match the base resin powder. Let-down ratios of 1–3% are typical for opaque white tanks and containers produced in biaxially rotating moulds. Oven temperature profiles of 250–280°C and cycle times of 20–40 minutes per 6 mm wall thickness represent standard operating windows. Dispersion of TiO₂ in rotomoulded parts is controlled by the grinding step, which transfers pigment to the powder surface and affects colour uniformity across the moulded article. Published production-scale data for LL8000 AP specifically in rotational moulding is limited; the process window described above derives from general LLDPE white masterbatch behaviour in biaxial rotational moulding and must be validated on the target mould geometry.
Competitive LyondellBasell POLYBATCH™ White LL8000 AP Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell POLYBATCH™ White LL8000 AP Concentrate Based In LLDPE is a pelletized titanium dioxide masterbatch supplied in a linear low-density polyethylene carrier for letdown into polyethylene-based film, sheet, and coating processes. The grade belongs to the POLYBATCH white concentrate series and is intended for processors that require controlled white pigmentation without operating a separate pigment dispersion step. It is not sold as a finished white resin and is not processed neat; it is proportioned into a natural or tinted base resin at a ratio determined by target chromaticity, opacity, film thickness, and base resin type. The product’s conformance values are supplied through lot-specific certificates of analysis rather than through fixed commercial literature values, because pigment concentration and melt flow may vary within the manufacturer’s control plan. Any use of the numeric designation as a direct weight-percent loading should be avoided unless confirmed by the certificate of analysis.
The carrier phase determines whether the concentrate disperses uniformly into the host resin under standard polyethylene extrusion temperatures. Since the carrier is LLDPE, the melt mass-flow rate measured under ISO 1133-1 at 190°C and 2.16 kg should be compared with the host resin’s melt flow to avoid phase separation during screw plastication. When the carrier viscosity is significantly lower than the host, the masterbatch can act as a lubricating phase and inhibit solids conveying; when it is higher, undispersed pigment agglomerates can survive the metering section and appear as white specks in thin films. The melt flow of an LLDPE carrier is typically selected to fall within the same processing band as film-grade LLDPE, but the exact value remains lot-specific.
Melt temperature for letdown into LLDPE film is generally maintained at 180–240°C. The lower limit is set by the melting range of the LLDPE carrier and the upper limit by oxidative degradation of the carrier at extended residence times. Operation above 260°C should be avoided because gel formation from LLDPE degradation can become visible in cast film as fisheyes and can reduce seal strength in downstream converting. In blown film, the low melt strength of LLDPE relative to LDPE can reduce bubble stability when high letdown ratios are used; this effect is more pronounced in high-stalk processes and can be managed by blending the host resin with LDPE or by reducing the concentrate addition rate.
On single-screw extruders, a barrier screw with a metering section L/D of 24:1 to 30:1 is adequate for uniform distribution at letdown ratios below 10 wt% when pellets are preblended with the base resin. For higher letdown or high-speed cast lines above 150 m/min, a static mixer or cavity transfer mixer downstream of the screw improves spatial uniformity. In co-rotating twin-screw compounding, the specific energy input should be controlled so that pigment dispersion is achieved without breaking down the LLDPE carrier through excessive shear heating. Because titanium dioxide is abrasive, long campaigns should employ hard-faced or bimetallic screws and barrels, particularly when the concentrate is used above 12 wt% or in filled systems.
Specification testing for the concentrate includes melt flow, ash content, density, and visual dispersion. The certificate of analysis should be consulted for exact values. The following methods are relevant to incoming inspection and lot acceptance.
| Parameter | Test method | Technical significance |
|---|---|---|
| Melt mass-flow rate | ISO 1133-1 | Indicates carrier viscosity and letdown compatibility with PE hosts |
| Ash content | ISO 3451-1 | Quantifies inorganic residue; does not separately identify TiO2 |
| Density | ISO 1183-1 | Higher than unfilled LLDPE due to pigment loading |
| Luminous transmittance and haze after letdown | ASTM D1003 / ISO 14782 | Measures opacity development in the final film |
| Dispersion rating | ISO 18553 | Controls agglomerate count and size in thin-gauge film |
Because ash content reflects total inorganic residue, it does not separately quantify titanium dioxide. If TiO2 content is required for formulation calculations, X-ray fluorescence or thermogravimetric analysis calibrated against the supplier method should be used. Color coordinates should be measured on a letdown blend prepared from a defined base resin and not on the masterbatch alone. Tests for dispersion are relevant because titanium dioxide agglomerates larger than 10 µm can generate visible defects in films below 50 µm thickness.
Opacity development in white films is not linear with masterbatch letdown; it follows light-scattering and absorption behavior that depends on pigment volume concentration, particle size distribution, and film thickness. At low addition levels, the incremental opacity gain per unit of masterbatch may be high up to a threshold above which particle crowding and dilution effects change. For concentrates of the LLDPE carrier class, a letdown of 3–12 wt% is common, but the exact ratio must be established by trial on the intended film line. A film with thickness below 30 µm may require proportionally higher masterbatch loadings or a higher-TiO2 grade to reach the same luminous transmittance as a thicker film.
Measurement should use ASTM D1003 or ISO 14782 for luminous transmittance and haze, and CIE coordinates for color. The processor should produce a three-point letdown curve at the target thickness and measure not only opacity but also seal initiation temperature, because TiO2 and carrier addition can shift seal behavior. Published data for this specific configuration is limited; end-user trials remain the performance reference for opacity, coefficient of friction, and seal compatibility.
The principal difference between LL8000 AP and other white masterbatches is the carrier selection. An LLDPE carrier is chosen to limit the mechanical and thermal disturbance introduced when the concentrate is let down into LLDPE-rich film and coating structures. The table below summarizes the practical distinctions between carrier classes in polyethylene processing.
| Carrier class | Compatibility with LLDPE host | Processing implication | Use restriction |
|---|---|---|---|
| LLDPE carrier, such as LL8000 AP class | High; minimal dilution of host crystallinity and mechanical response | Moderate melt strength; suitable for cast, blown, and coating with LLDPE-rich formulations | Not for PP-rich hosts; high letdown in HDPE may require added mixing |
| LDPE carrier | High for LDPE/LLDPE blends | Higher melt strength and bubble stability; at high letdown may reduce dart impact in LLDPE film | Not suitable for PP; viscosity may be lower than HDPE |
| Low-molecular-weight wax or universal carrier | Variable; may migrate to surface | Lower-energy dispersion but can shift coefficient of friction, seal initiation, and organoleptics | Not recommended for food contact unless separately approved |
| PP carrier | Poor in PE film | Processing temperature mismatch; immiscible domains | Restrict to PP-based applications |
An LLDPE carrier contributes lower melt strength than an LDPE carrier, which can be disadvantageous in high-stalk blown film or heavy-wall blown film where bubble support is already marginal. However, LLDPE is closer in molecular architecture to the host resin, reducing the change in elongation, dart impact, and puncture resistance that may occur when a structurally dissimilar carrier is introduced. Universal carriers are frequently low-molecular-weight polyethylene waxes or ethylene copolymers; they can be dispersed at lower energy, but they may migrate, generate volatiles at high temperature, and affect sealing performance. The LLDPE base of LL8000 AP is therefore selected where film mechanical integrity and seal cleanliness outweigh the need for universal compatibility.
At production scale, the concentrate is often preblended with natural LLDPE pellets using a gravimetric blender or tumble mixer. Segregation can occur if pellet size distribution differs significantly; vertical hoppers with center discharge should be checked for fines accumulation. In cast film, excessive masterbatch moisture from condensation can generate splay. Although LLDPE itself is not hygroscopic, bags stored in unheated warehouses should be allowed to equilibrate before introduction into a warm extrusion area. Drying at 70–80°C for 2–4 h may be applied only if visible surface moisture is present; prolonged drying at higher temperatures can degrade antioxidants in the carrier.
Titanium dioxide is abrasive. For long campaigns, screws and barrels should be hard-faced or bimetallic; wear rates can increase when the concentrate is used above 12 wt% or when the line runs continuously at high screw speeds. Screen packs with 100–120 mesh are common to trap agglomerates; however, pressure build-up across the screen pack should be monitored because excessive screen changes can indicate poor dispersion or pigment agglomeration. Incompatibilities include direct blending with polypropylene-rich systems, uncontrolled peroxide masterbatches at high temperature, and contact with certain organotin-stabilized compounds that may interact with the carrier. The material should not be processed at temperatures exceeding the supplier’s stated maximum for the carrier, because oxidative degradation products can contaminate the film and reduce seal strength.
Regulatory compliance depends on the final application and the complete formulation, not the masterbatch alone. For food-contact uses, the masterbatch must meet the requirements of Commission Regulation (EU) No 10/2011 and FDA 21 CFR as applicable to titanium dioxide and the LLDPE carrier. Processors should obtain a product stewardship statement because titanium dioxide use in food-contact plastics has been subject to regulatory review. For electrical and electronic equipment, compliance with RoHS Directive 2011/65/EU for heavy metal restrictions is generally addressed through the supplier’s raw-material controls. The product is not intended for medical or pharmaceutical packaging unless separately validated under ISO 10993 or the relevant pharmacopoeia.
Storage should be at temperatures below 40°C in a dry, covered area, away from direct sunlight. Inventory should be managed under first-in-first-out control, and the product should be kept sealed when not in use to avoid atmospheric dust pickup, which can affect film appearance.