| HS Code | 360340 |
| Productname | POLYBATCH™ Weatherwood 60190U |
| Manufacturer | LyondellBasell |
| Brand | POLYBATCH™ |
| Producttype | Color Concentrate |
| Carrierresin | LLDPE |
| Color | Weatherwood |
| Form | Pellets |
| Additive | UV Stabilizer |
| Density | 0.94 g/cm³ |
| Meltflowrate | 20 g/10 min (190°C/2.16 kg) |
| Recommendedletdown | 4% |
| Processingtemperature | 180-220°C |
| Application | Outdoor polyolefin applications |
| Compatibility | Polyolefins |
| Packaging | 25 kg bags |
| Shelflife | 12 months |
| Storageconditions | Cool, dry place |
As an accredited LyondellBasell POLYBATCH™ Weatherwood 60190U Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell POLYBATCH™ Weatherwood 60190U Concentrate Based In LLDPE is typically supplied in 25 kg polyethylene bags, with 1,000 kg bulk bags available. |
| Container Loading (20′ FCL) | 20′ FCL loaded with LyondellBasell POLYBATCH™ Weatherwood 60190U Concentrate Based In LLDPE, palletized, shrink-wrapped, and securely lashed for ocean transport. |
| Shipping | LyondellBasell POLYBATCH™ Weatherwood 60190U Concentrate Based in LLDPE is shipped as non-hazardous solid LLDPE pellets in sealed bags, octabins, or bulk containers. It is not regulated for DOT, IMDG, or IATA transport. Store cool, dry, away from direct sunlight and ignition sources. Avoid moisture and contamination. |
| Storage | Store LyondellBasell POLYBATCH™ Weatherwood 60190U Concentrate Based In LLDPE in original packaging in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed when not in use to prevent moisture absorption and contamination. Avoid excessive temperatures, prolonged stacking, and contact with strong oxidizers. Use secondary containment, maintain good housekeeping, and follow local regulations. |
| Shelf Life | Shelf life is 24 months from manufacture when stored unopened in original packaging, dry, below 30°C, away from direct sunlight. |
In capstock coextrusion of wood-plastic composite decking profiles, POLYBATCH™ Weatherwood 60190U Concentrate Based In LLDPE is introduced into the cap-layer polyolefin at a let-down ratio of 2–5 wt% of the cap compound mass, with the exact upper boundary governed by the supplier technical data sheet and the target cap thickness. The rationale for this low loading is the cap layer thickness of 0.3–0.8 mm: overloading the LLDPE carrier in a thin cap raises linear expansion differential between cap and core and lowers flexural modulus, while underloading reduces the density of weathered-wood striations visible after embossing. The capstock polymer is plasticated on a separate single-screw extruder with an L/D ratio of 25:1–32:1, a melt temperature of 190–210°C, and a screw surface speed below 0.2 m/s; the WPC core compound contains 50–60 wt% wood flour or cellulose fiber dispersed in HDPE or recycled polyolefin and is processed on a counter-rotating conical twin-screw extruder with barrel set points of 160–180°C. If ambient relative humidity exceeds 60%, wood flour must be dried to below 1 wt% moisture according to ASTM D4442 before compounding. The two melt streams are joined in a feedblock or multi-manifold die; cap thickness uniformity must hold within ±0.1 mm across a 140–220 mm-wide profile, otherwise visual grain intensity varies across the board face. Production-scale failure modes include die-lip plate-out when cap melt exceeds 220°C, longitudinal striation inversion when feedblock shear rate exceeds 150 s⁻¹, and surface haze when moisture is not fully removed from the core compound; published data for this specific product under shear rates above that threshold is limited, and confirmatory line trials are required. Compliance for the decking profile is anchored to ASTM D7032-17 for span rating, fastener withdrawal, and dimensional stability, while the European regulatory route requires conformity to EN 15534-4 for composite decking profiles and EN 15534-1 for physicochemical characterization; chemical reporting follows REACH and the article-level restriction under Directive 2011/65/EU RoHS applies to lead, cadmium, mercury, and hexavalent chromium. Terminal product types are grooved, solid, and embossed deck boards for exterior flooring systems, with the capstock carrying the coloring function while the core supplies the structural load path.
For hollow WPC cladding and siding profiles, the concentrate is let down at 3–5 wt% of the total compound weight; below 3 wt% the streaking density in thin walls is often insufficient after embossing, while above 5 wt% the LLDPE carrier can reduce profile stiffness and create dimensional variation in the cooling calibrator. The compound is formulated with 40–55 wt% wood flour, 45–55 wt% HDPE or PP, a maleic anhydride-grafted polyolefin coupling agent at 1.5–2.5 wt%, and a processing lubricant at 1.0–1.8 wt%; wood flour moisture must be reduced below 1 wt% according to ASTM D4442 before extrusion. The profile is produced on a 50–60 mm counter-rotating conical twin-screw extruder with barrel set points of 155–175°C, vent vacuum below -0.06 MPa, and a die temperature of 175–185°C. The melt is passed through water-cooled calibration sleeves held at 10–20°C with vacuum between -0.01 and -0.03 MPa; field observations on production lines show that die land length below 20 mm produces blurred striations, and die land length above 40 mm can erase the two-phase pigment alignment through excessive plug flow, so die geometry rather than concentrate loading becomes the controlling factor for grain definition. Accelerated weathering is assessed according to ISO 4892-2 xenon-arc exposure with ISO 105-A02 grey scale evaluation; the masterbatch does not itself confer Euroclass reaction-to-fire performance, and the final hollow profile must be tested under EN 13501-1. The compound and profile test matrix follows EN 15534-1:2014+A1:2017; chemical inventory obligations follow REACH and the final product must meet Directive 2011/65/EU RoHS restrictions. Terminal products are hollow tongue-and-groove cladding boards, ventilated façade battens, and fascia profiles, where the visual weathered-wood effect is generated in the uncoated polymer matrix rather than by surface paint or lamination.
| Scenario | Reference addition window | Primary compliance and test standards | Processing equipment configuration |
|---|---|---|---|
| Capstock decking | 2–5 wt% | ASTM D7032-17, EN 15534-4, EN 15534-1 | 25:1–32:1 L/D single-screw cap extruder |
| Hollow cladding | 3–5 wt% | EN 15534-1:2014+A1:2017, ISO 4892-2, EN 13501-1 | 50–60 mm counter-rotating conical twin-screw extruder |
| Injection-molded furniture | 2–4 wt% | EN 581-1:2017, ISO 4892-3, ASTM D2244 | Reciprocating-screw injection unit with L/D ≥ 20:1 |
| Railing capstock | 3–6 wt% | ASTM D7032-17, ICC-ES AC174, ASTM G155-13 | 25:1 L/D single-screw cap extruder |
| Rotational molding | 3–5 wt% | ISO 4892-3, ASTM D2244 | Biaxial rotational molding oven with vented internal air probe |
When the same concentrate is let down into injection-molding grade PP or HDPE for structural outdoor furniture components, the recommended addition ratio is 2–4 wt% of the shot mass; the bottom of this range is applied to PP matrices because the LLDPE carrier can localize at gate-weld lines and reduce tensile impact in parts with wall thickness below 3.0 mm. Injection molding is performed with a reciprocating-screw unit with L/D ≥ 20:1, melt temperature of 200–230°C for PP or 180–220°C for HDPE, mold temperature of 20–45°C, back pressure of 50–80 bar, and screw surface speed below 0.2 m/s. The low-to-moderate back pressure is deliberate: higher dispersive mixing fully homogenizes the effect pigments and destroys the required weathered-wood domain orientation, while lower back pressure causes color separation and flow lines. Production-scale defects observed on multicavity furniture molds include gate blush, sink marks over thick bosses, and warpage when the LLDPE carrier content is not fully integrated into the PP matrix; published data for this specific product in thin-wall PP furniture applications is limited, so pre-production spiral-flow tests according to ISO 1133-1:2022 and weld-line tensile evaluations should be completed before tool approval. Compliance for outdoor seating is governed by EN 581-1:2017 for mechanical safety and durability; weathering performance is evaluated with ISO 4892-3 UV-A fluorescent exposure and ASTM D2244 CIELAB color difference; substance restrictions follow REACH and Directive 2011/65/EU RoHS for lead, cadmium, mercury, and hexavalent chromium. Terminal product types include seat slats, backrest frames, armrest profiles, and connector brackets made from mineral-filled or unfilled polyolefin, where the weathered wood appearance replaces paint, staining, or secondary decorative films.
Capstock coextrusion for composite railing profiles places a different visual demand on the concentrate because the surface includes compound curves, embossed grain, and shorter viewing distance. The addition ratio in the cap layer is 3–6 wt% of the cap compound mass; for cap thickness below 0.5 mm, the upper bound is preferred to maintain streak density, while for cap thickness above 0.7 mm, the lower bound avoids cap delamination caused by differential shrinkage between the LLDPE-rich surface and the HDPE/wood core. The cap layer is extruded on a 25:1 L/D single-screw extruder at 185–205°C and joined with a core stream containing 50–60 wt% wood flour through a feedblock manifold; line speeds of 0.8–1.5 m/min create variable shear history that can shift striation intensity, so line speed should be fixed during lot-to-lot shade validation. The hollow profile is calibrated in sequential dry and wet vacuum tanks with first-stage vacuum of -0.02 to -0.04 MPa and dry-sleeve temperature of 30–45°C; if the die temperature deviates by more than 5°C from the cap melt temperature, surface mottling or die lip residue becomes evident. Structural and weathering compliance for railing systems is established under ASTM D7032-17 and ICC-ES AC174; accelerated xenon-arc exposure is performed according to ASTM G155-13, and the European WPC characterization route follows EN 15534-1. The concentrate does not provide a structural rating; the core profile must independently pass guardrail load and deflection requirements. Terminal product types are railing top caps, bottom rails, baluster sleeves, and post cladding, all of which carry the weathered wood appearance as a molded-in effect.
In rotational molding, the absence of high shear means the weathered-wood effect develops as a mottled or low-orientation grain rather than the long striations produced by extrusion, and that visual difference must be explicitly accepted in the part specification. The concentrate is dry-blended with 35 mesh (500 µm) LLDPE powder at 3–5 wt% of the mold charge; because the product is supplied as a pelletized concentrate in LLDPE, effective dispersion requires either cryogenic grinding to a particle size below 500 µm or pre-compounding into a micropellet to prevent segregation during mold rotation. The mold is heated in a biaxial rotational molding oven with a peak internal air temperature of 190–205°C, rotation speed of 4–8 rpm, oven residence time of 20–45 min, and cooling by forced air followed by water mist; internal air temperature is measured by a vented probe because the low-shear process cannot self-monitor melt temperature. Process boundaries include the upper oven temperature limit of 205°C for LLDPE carrier stability and the requirement to avoid compounding with strong oxidizing external release agents that can shift color. Weathering compliance is assessed by ISO 4892-3 UV-A fluorescent exposure and ASTM D2244 color difference; final articles must conform to REACH substance restrictions and Directive 2011/65/EU RoHS. Mechanical and durability requirements for outdoor furniture made by rotational molding are specified at the final part level, and the concentrate itself does not confer structural properties. Terminal product types include rotomolded outdoor planters, bench platforms, storage boxes, and decorative garden elements in LLDPE-based polyolefin systems, where the weathered wood appearance is dispersed through the entire wall section.
Competitive LyondellBasell POLYBATCH™ Weatherwood 60190U Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell POLYBATCH™ Weatherwood 60190U Concentrate Based In LLDPE is a pelletized polyolefin masterbatch in which the carrier phase is identified as linear low-density polyethylene. The numerical grade code differentiates it from other Weatherwood or POLYBATCH products, but the public trade description does not provide pigment concentration, total inorganic residue, melt volume-flow rate, light-stabilizer chemistry, or final colorimetric tolerance. Because the product is a concentrate rather than a fully attributable compound, downstream qualification begins with a lot-specific certificate of analysis and a supplier technical data sheet. The following treatment separates generic linear low-density polyethylene carrier behavior from claims that require product-specific verification.
The principal processing distinction is the molecular architecture of the LLDPE carrier. Linear low-density polyethylene is a copolymer of ethylene with an alpha-olefin such as butene, hexene, or octene. The short-chain branches reduce density, but the polymer remains essentially linear and typically exhibits a narrower molecular-weight distribution than conventional autoclave or tubular LDPE. Under capillary rheometry in accordance with ISO 11443, LLDPE generally shows less shear thinning than LDPE at equivalent melt index. Consequently, when Weatherwood 60190U is added to a polyethylene base resin, the carrier does not act as an inert diluent; it contributes to head pressure, melt temperature, and die swell. A concentrate based in high-flow LDPE may reduce viscosity at high shear, while an LLDPE carrier may retain more viscosity and can stabilize melt strength in profile extrusion. Published data for the exact melt flow rate of Weatherwood 60190U is limited in public trade material, so converters should not assume that the carrier matches a generic LLDPE film grade. The difference from a universal masterbatch is material-specific compatibility: the LLDPE carrier is more appropriate for polyethylene-rich formulations than for polypropylene, PVC, or other polar or dissimilar matrices.
In a production-scale polyolefin masterbatch operation, an LLDPE-carrier concentrate is usually produced on a co-rotating twin-screw extruder with distributive and dispersive mixing elements. The selection of a linear low-density polyethylene carrier rather than an amorphous or low-molecular-weight wax affects pellet hardness, melt viscosity, and the ability of the concentrate to be dosed reliably. Feeder bridging can occur if pellets are too soft or irregular, especially in humid conditions. A gravimetric feeder with an agitating hopper is preferred for this class of pelletized concentrate, because bulk-density variation can otherwise introduce shot-to-shot color drift in injection molding.
On a single-screw extruder with a 25:1 L/D or 30:1 L/D general-purpose screw, an LLDPE-carrier concentrate can raise head pressure before the screen changer more than an LDPE-carrier product at identical let-down. The effect is strongly dependent on the melt temperature and the base resin viscosity. Molders and extruders should record melt pressure, melt temperature, and motor load against a control run without concentrate. A rise in melt pressure is not a defect by itself, but it indicates that the carrier is participating in melt rheology rather than acting as a low-viscosity carrier. For thin-wall injection molding, a mixing nozzle or a screw with a barrier section and moderate back pressure improves homogenization of the LLDPE-carrier color concentrate.
In a linear low-density polyethylene carrier, the crystalline melting range is generally observed at 120–126 °C by differential scanning calorimetry according to ISO 11357-3, although exact values depend on comonomer content and thermal history. The lower melting onset compared with HDPE permits polyolefin extrusion lines to operate in a melt temperature range of 160–220 °C for many general-purpose profiles, but the concentrate carrier does not solely determine the melt temperature. When Weatherwood 60190U is dosed into a base resin that already has a higher melting point, the carrier must be fully molten before the mixing section of the screw. Otherwise, undispersed pigment agglomerates or gel-like visual defects can appear at the die or on the surface of extruded profiles.
For grooved-feed extruders, high solids-conveying efficiency can increase melt temperature faster than in smooth-bore machines. A melt pump can decouple pressure generation from extruder speed and reduce overall shear history, which is beneficial when a color concentrate is temperature-sensitive. Pre-drying is not normally required for LLDPE carriers under sealed dry storage. If sacks are stored at relative humidity above 60%, condensation on pellet surfaces may introduce moisture that appears as surface splay in open extrusion or as voids in thick profiles. The use of a vented twin-screw extruder during masterbatch production controls volatiles; at the converter, however, the concentrate is physically mixed and melted rather than compounded again. A desiccant dryer is generally unnecessary, but a dry-air purge on the hopper can be considered if condensation is visible or if the plant has high humidity and cold pellet storage.
In injection molding, the LLDPE carrier’s lower melt elasticity compared with LDPE can alter gate freeze and packing behavior. Thin-wall components may show flow lines if the concentrate is not homogenized before the injection nozzle. A screw with a Maddock barrier and dispersive mixing elements is more effective than a plain compression screw. Back pressure is commonly set at 5–15 bar for polyolefin color masterbatches, but the setting should be derived from the masterbatch viscosity and not assumed from a different carrier chemistry. Higher back pressure can improve color distribution but may also increase shear heating and degrade heat-sensitive pigments.
When the exact let-down for Weatherwood 60190U is not stated on the technical data sheet, a common starting range for polyolefin color or effect concentrates is 2–6 wt%. This range is an industry reference and is not a substitute for the product-specific recommendation. The final ratio should be confirmed by a color match against a physical standard plaque or profile section. Because the product is based in LLDPE, addition to polyethylene base resins is straightforward, but addition to polypropylene is not generally recommended without verification. The carrier resin phase separation can reduce low-temperature impact properties and create visible streaks.
Addition of the concentrate to a LLDPE, LDPE, or HDPE base resin is performed with gravimetric dosing, preferably before the main feed throat. If the let-down ratio is changed, the pigment concentration in the final part changes linearly only if the feeder maintains consistent pellet mass flow. Volumetric feeders can drift with pellet geometry and bulk density variation. For high-speed extrusion of thin profiles, a side feeder may be used to introduce the concentrate after the base resin has begun to soften, but this requires sufficient residence time for distributive mixing. The melt pressure before the breaker plate should be recorded during a preproduction trial, and the final setpoint should be established against a control run without the concentrate.
A filter pack with screen sizes of 40/60/80 mesh or finer can trap undispersed particles, but the carrier phase must be molten enough to pass the pack without excessive pressure rise. When the filter pack is changed or when the base resin is switched from HDPE to LLDPE, melt pressure and melt temperature must be re-recorded. The lower crystallization temperature of LLDPE compared with HDPE can alter cooling behavior in thick profiles. The final article may require adjusted water-spray or calibration-block settings because the carrier affects the overall crystallization front, particularly at higher let-down ratios.
For extrusion blow molding, the LLDPE carrier can contribute to parison sag resistance, but the effect is limited because the concentrate is diluted at low levels. Machine settings should not be changed drastically for color concentrates unless the let-down exceeds the supplier-recommended upper limit. For sheet extrusion, roll stack temperatures should be adjusted based on the final sheet gloss and the release behavior of the LLDPE-containing melt. Visual evaluation alone is insufficient for color acceptance; the use of ASTM D2244 and a spectrophotometer is required to quantify CIE L*a*b* coordinates and to set lot-to-lot tolerances.
The trade name “Weatherwood” suggests a wood-like appearance; it does not by itself establish UV resistance, colorfastness, or outdoor durability. A technical data sheet that identifies only the carrier resin and appearance class is insufficient for high-specification profiles. The converter must obtain lot-specific values for melt volume-flow rate, density, ash content, and, if relevant, regulatory status. Table 1 provides a comparative resin-class processing profile, while Table 2 lists the minimum documentation required for a reproducible qualification.
| Carrier class | Typical density at 23 °C | Typical melting range by DSC | Rheological characteristic | Compatibility consequence in Weatherwood 60190U use |
|---|---|---|---|---|
| LLDPE | 0.916–0.940 g/cm³ | 120–126 °C | Narrower molecular-weight distribution, less shear thinning than LDPE | Preferred carrier for PE-rich matrices due to phase compatibility |
| LDPE | 0.912–0.930 g/cm³ | 105–115 °C | Broad molecular-weight distribution, strong shear thinning | Easier high-shear processing but lower toughness than LLDPE |
| HDPE | 0.941–0.970 g/cm³ | 130–137 °C | Higher melt stiffness, moderate shear thinning | Higher processing temperature may intensify thermal load on pigments |
| PP | 0.895–0.910 g/cm³ | 160–170 °C | Incompatible with PE at high addition levels | Not recommended without verification; may delaminate or reduce impact strength |
The values in Table 1 are representative of resin classes, not a certificate of analysis for Weatherwood 60190U. They demonstrate why a weatherwood or wood-effect masterbatch based in LLDPE cannot be exchanged weight-for-weight with a polypropylene-based effect concentrate in a polyethylene matrix. The PP carrier would remain as discrete domains and can reduce low-temperature impact strength, whereas an LLDPE carrier is compatible with the PE-rich phase at typical let-down ratios. The LLDPE carrier also differs from an EVA or EMA carrier: those polar copolymers may provide better pigment wetting but can shift the viscosity curve and may introduce polar adhesion to PVC or metal surfaces.
| Parameter | Method or standard | Purpose of review |
|---|---|---|
| Melt mass-flow rate | ISO 1133-1 or ASTM D1238 | Compare carrier viscosity to base PE resin and set dosing conditions |
| Ash content | ASTM D5630 or ISO 3451-1 | Estimate inorganic pigment or filler loading |
| Density | ISO 1183-1 or ASTM D1505 | Confirm carrier class and detect gross formulation shifts |
| Color coordinates | ASTM D2244, CIE L*a*b*, D65/10° | Establish lot-to-lot color tolerance and acceptance limits |
| Thermal transitions | ISO 11357-3 | Set melt processing window and confirm carrier melting range |
| Regulatory status | EU 10/2011, FDA 21 CFR 178.3290, REACH, RoHS Directive 2011/65/EU | Verify end-use compliance for food contact or restricted substances |
For an outdoor profile or siding application, the end-user should not rely on the word “Weatherwood” as an accelerated-weathering result. A reproducible trial requires a laboratory color reading, a melt pressure trace, a melt temperature trace, and a retained sample of the concentrate lot. If the specification requires exterior performance, accelerated weathering should be performed in accordance with ISO 4892-2 or ASTM G154. The pass/fail limits must be defined by the end-use specification, because the trade designation alone does not provide a test result. Published data for this specific configuration is limited, so the technical approval depends on lot-specific measurements and supplier documentation rather than class-level assumptions.