| HS Code | 443712 |
| Product Name | LyondellBasell POLYBATCH™ Weathered Wood 10418U Concentrate Based In LLDPE |
| Brand | LyondellBasell |
| Product Type | Color Concentrate |
| Carrier Resin | Linear Low Density Polyethylene (LLDPE) |
| Color | Weathered Wood |
| Physical Form | Pellets |
| Specific Gravity | 1.12 |
| Melt Flow Rate | 12 g/10 min at 190°C/2.16 kg |
| Moisture Content | <0.50% |
| Ash Content | 30% |
| Let Down Ratio | 4:1 to 10:1 |
| Processing Temperature | 177-232°C (350-450°F) |
| Shelf Life | 12 months |
| Storage Temperature | Below 30°C (86°F) |
As an accredited LyondellBasell POLYBATCH™ Weathered Wood 10418U Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaged in 25 kg (55 lb) polyethylene bags, 40 bags per pallet, totaling 1,000 kg per pallet. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with LyondellBasell POLYBATCH™ Weathered Wood 10418U Concentrate Based in LLDPE, securely palletized and braced for transport. |
| Shipping | LyondellBasell POLYBATCH™ Weathered Wood 10418U Concentrate Based In LLDPE is generally not regulated as dangerous goods for transport. It ships as plastic pellets in 25-kg moisture-barrier bags or 1,000-kg octabins. Keep clean, dry, out of direct sunlight and excessive heat. Follow SDS and local regulations. |
| Storage | Store LyondellBasell POLYBATCH™ Weathered Wood 10418U Concentrate Based in LLDPE in a cool, dry, well-ventilated area using original sealed containers. Keep away from direct sunlight, heat, sparks, flames, and strong oxidizers. Protect from moisture and contamination. Maintain moderate temperatures, avoid excessive heat, and follow first-in, first-out stock rotation. Close containers when not in use and comply with local regulations and SDS guidance. |
| Shelf Life | Shelf life is 24 months from date of manufacture when stored unopened in original packaging in a dry, protected environment. |
Technical scope for POLYBATCH™ Weathered Wood 10418U Concentrate Based In LLDPE. The following application entries are restricted to polyolefin conversion methods where an LLDPE-based carrier is process-compatible: capstock coextrusion, rotational moulding, thin-wall injection moulding, extrusion blow moulding, calendered sheet thermoforming, and profile extrusion. The concentrate is a let-down colour/effect additive; it is not supplied as a ready-to-use compound. Where melt-flow compatibility is uncertain, the carrier and base resin should be compared under ASTM D1238-20 (190 °C, 2.16 kg) before production. Regulatory screening for EU export includes EU REACH Regulation EC No 1907/2006 candidate list obligations and RoHS Directive 2011/65/EU Annex II substance restrictions. Food-contact uses require independent migration testing against 21 CFR 177.1520 and EU Regulation No 10/2011, because masterbatch composition determines overall migration limits.
| Conversion method | Wall thickness range | Typical let-down | Primary process limit |
|---|---|---|---|
| Capstock coextrusion | 0.3–0.6 mm | 3.0–5.0 wt% | Melt temperature 190–205 °C |
| Rotational moulding | 3.0–6.0 mm | 1.5–3.0 wt% | Dry-blend mixing 20–30 min |
| Thin-wall injection moulding | 1.5–3.0 mm | 2.0–4.0 wt% | Gate shear heating ≤10 °C |
| Extrusion blow moulding | 2.0–4.0 mm | 3.0–5.0 wt% | Parison melt 180–210 °C |
| Calendered sheet/thermoforming | 0.8–2.0 mm | 2.0–4.0 wt% | Calender stack 80–100 °C |
| Profile extrusion | 1.5–6.0 mm | 3.0–5.0 wt% | Vacuum calibration −0.05 to −0.08 MPa |
The capstock route for wood-plastic composite decking introduces the concentrate at 3.0–5.0 wt% against the capstock compound on a 75 mm counter-rotating twin-screw extruder with 30:1 L/D. At loadings below 2.5 wt%, opacity in a 0.3–0.6 mm cap layer is frequently insufficient when measured under ASTM D2244-23e1; at addition above 5.5 wt%, melt pressure at the screen pack typically rises and surface drag lines can appear at the coextrusion die exit. The cap layer is processed over a wood-flour-filled HDPE core at 190–205 °C melt temperature. Exceeding 210 °C for cumulative residence time beyond 45 min has been associated with carrier viscosity drift and a visible shift in the weathered-wood shade, particularly in dark-brown and grey monotone systems. Published data for this specific shade under capstock coextrusion is limited; the cumulative residence figure is a class-level benchmark for LLDPE-carrier colour concentrates. Mechanical acceptance for exterior deck boards is anchored to ASTM D7032-17 for deck board performance, ASTM D790-17 for flexural modulus, and ASTM D256-23 for Izod impact. Weathering durability is assessed with ASTM D4329-13 (340 nm UVA lamps) and ISO 4892-2:2013 xenon-arc exposure; colour retention is reported in ΔE*ab using ASTM D2244-23e1. The terminal article class produced by this route is capped wood-plastic composite deck boards and railing profiles.
In rotational moulding, the concentrate is not pre-compounded but dry-blended with 35 mesh LLDPE powder at 1.5–3.0 wt% for wall sections of 3.0–6.0 mm. Dry-blend homogeneity is the dominant process variable; ribbon blender mixing below 15 min has produced streaking on the inner mould surface because the carrier pellets and ground powder develop different electrostatic charging. Production batches usually require 20–30 min of low-shear mixing before charging the mould. The oven cycle is controlled by internal air temperature rather than oven set point: peak internal air temperature should remain at 190–205 °C; at 210 °C or above, carrier degradation accelerates and the weathered-wood tone can shift yellow when measured under ASTM D2244-23e1. Bi-axial rotation ratios between 4:1 and 8:1 are typical, with forced-air cooling rates of 10–20 °C/min to limit warpage in large flat panels. Compliance for outdoor furniture and planters is anchored to ASTM D638-14 tensile elongation, ASTM D790-17 flexural properties, and weathering programmes based on ISO 4892-2:2013 and ASTM D4329-13. Terminal products are LLDPE garden furniture, outdoor planters, and decorative storage containers.
Injection moulding of 1.5–3.0 mm wall outdoor planters and nursery containers uses 2.0–4.0 wt% let-down in an LLDPE or HDPE base. Gravimetric dosing stability must hold within ±0.2 wt%; batch-to-batch colour drift appears outside this window under ASTM D2244-23e1. On a 1,200 kN clamp injection moulding machine equipped with a 22–25 mm diameter reciprocating screw, the melt temperature is held at 190–215 °C. When hot runner gate diameters fall below 1.0 mm, injection velocities above 100 mm/s can generate local shear heating of 8–10 °C, which may initiate pigment decomposition and produce dark specks in moulded surfaces. Mould temperature is typically held at 15–30 °C; cooling time is adjusted on the production line when the concentrate is used at the upper loading boundary to reduce sink marks near bosses. Mechanical integrity is verified with ASTM D638-14 and ASTM D256-23; exterior durability is assessed by ISO 4892-2:2013 and ASTM D4329-13. The terminal product class comprises thin-wall injection moulded nursery pots, saucers, and stackable garden containers.
For extrusion blow moulded outdoor storage panels, the concentrate is let down at 3.0–5.0 wt% into HDPE or LLDPE-rich blends with wall thickness 2.0–4.0 mm. The extruder is typically a 60–80 mm single-screw machine with 25:1 L/D, feeding a parison die head with gap 1.0–2.5 mm. Melt temperature is set to 180–210 °C; holding the parison at 210 °C for more than 20 min at the die head has been related to melt fracture and inversion of the wood-grain surface effect. Pre-drying at 70–80 °C for 2–4 h is required when storage relative humidity exceeds 60%, because moisture in the masterbatch can generate splay and gloss variation. Blow moulding clamp force for such panels typically ranges from 500 kN to 1,500 kN, with blow pressure 0.6–0.8 MPa. Compliance for outdoor exposure includes ASTM D638-14 tensile properties, ASTM D790-17 flexural modulus, ASTM D1693-15 environmental stress-cracking resistance, and ASTM D4329-13 UV weathering. Finished articles are blow moulded deck boxes, outdoor cabinets, and shed wall panels.
Calendered sheet extrusion for wood-grain polyolefin trim uses 2.0–4.0 wt% let-down in HDPE or polypropylene-compatible LLDPE blends with sheet thickness 0.8–2.0 mm. The concentrate is pre-dispersed through a 45 mm twin-screw extruder with 28:1 L/D before entering the sheet die; melt temperature is held at 190–205 °C, and calendering stack roll temperatures are set to 80–100 °C. Lower roll temperatures have produced free-surface unevenness that appears as gloss banding after thermoforming. During thermoforming, local thinning below 0.4 mm can amplify colour density variation by 1.5–2.0 ΔE*ab under ASTM D2244-23e1, especially in high-draw corners. For automotive or recreational vehicle interior trim, flammability is tested to FMVSS 302 or ISO 3795. Mechanical acceptance uses ASTM D638-14 and ASTM D790-17. Published data for this specific masterbatch in automotive interior trim is limited; therefore final-sheet validation under FMVSS 302 and OEM fogging standards must be completed before serial production. The terminal product class includes thermoformed interior trim panels and wall cladding for recreational vehicles.
Profile extrusion of landscape edging and fencing accessory profiles employs the concentrate at 3.0–5.0 wt% in HDPE/LLDPE blends with cross-sections from 1.5 mm to 6.0 mm. The line is configured with a 50 mm single-screw profile extruder with 30:1 L/D, a vacuum calibrator, and a puller/cutter station. Melt temperature is set to 185–205 °C; vacuum calibration pressure is maintained at −0.05 to −0.08 MPa to prevent surface drag marks and dimensional variation. At addition above 5.0 wt%, published data for thick-section shrinkage is limited; downstream calibration must be re-confirmed on the production line. Mechanical compliance is evaluated under ASTM D638-14 and ASTM D790-17; outdoor colour stability is assessed to ASTM D4329-13 and ISO 4892-2:2013. Terminal products are landscape edging, garden border profiles, and fencing accessory rails.
Competitive LyondellBasell POLYBATCH™ Weathered Wood 10418U Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell POLYBATCH™ Weathered Wood 10418U Concentrate Based In LLDPE is a pelletized color/effect masterbatch formulated with a linear low-density polyethylene carrier. The product is intended for let-down into polyolefin-based matrices to produce a weathered wood visual in extruded profiles, injection-molded components, and capstock layers. It is not a standalone molding resin; it is a concentrate that must be diluted into a compatible base polymer. The masterbatch is supplied in pellet form suitable for gravimetric or volumetric dosing. Lot-specific values for pigment loading, melt flow rate, density, and additive content are provided in the certificate of analysis and technical data sheet; published data for this specific configuration is limited, and processing trials are required to establish final surface appearance.
Differences from conventional single-pigment concentrates arise from the multi-component color package and the LLDPE carrier. The product is not intended as a white, black, or standard brown concentrate. Unlike wood-fiber masterbatches, the 10418U grade does not introduce lignocellulosic filler into the melt stream; therefore it does not add the same moisture vapor release, odor, or interfacial adhesion constraints associated with natural fibers. It is also not formulated for use in rigid or plasticized PVC; contact with polyvinyl chloride at processing temperatures can generate acidic species and should be avoided unless explicit compatibility data exists.
Dispersion of the pigment package in the let-down matrix is governed by the shear stress applied in the final processing step. For LLDPE-carrier wood-effect concentrates, residual agglomerates are visible as surface specking in thin-walled profiles and capstock layers. On a co-rotating twin-screw extruder with an L/D ratio of at least 40:1, dispersive mixing is typically generated through kneading blocks with two or three lobes. Barrel temperatures in the melt zone are often held between 190°C and 230°C to maintain carrier viscosity without thermal degradation. Low-pressure operation below 5.0 MPa at the die can reduce shear history and leave visible pigment aggregates; a screen pack of 60/80/100 mesh is used on some lines to raise backpressure. Published data for this specific product is limited, so dispersion acceptance should be established by a filter pressure value test per ISO 23900-5:2015 or equivalent.
Residual moisture and low-melt-viscosity carriers can also influence dispersion. If the base resin contains above 0.05% moisture, steam formation at the feed throat can disturb pigment wetting and reduce shear transfer. Desiccant drying at 70–80°C for 2–4 h is a common corrective action for exposed polyolefin/pigment blends, but the concentrate itself should be kept sealed until use. On single-screw extruders with L/D ratios below 30:1, uniform color development may require pre-blending at 2–4 wt% addition before extrusion. Production-scale observations on a 58 mm co-rotating twin-screw line show that feeder surge of more than ±0.15% can produce longitudinal color variation in capstock co-extrusion.
The carrier phase affects the minimum shear stress required for pigment agglomerate breakage. LLDPE carriers exhibit shear-thinning behavior similar to the polyolefin matrix, but their lower melt temperature relative to HDPE can create a transient low-viscosity phase. If addition rates exceed 6 wt%, a separate carrier phase may persist and alter the surface grain fidelity. Therefore, addition ratios should be optimized in increments of 1 wt% between 2 wt% and 6 wt%, with visual assessment using a D65 light source.
Gravimetric feeders with mechanically assisted hoppers are preferred for pelletized color concentrates. Volumetric screw feeders may produce inconsistent let-down in multi-component wood-plastic composite formulations because bulk density of the masterbatch can vary between lots. On an extrusion line running a 75 mm parallel twin-screw at 250 kg/h, feed hoppers with bridge-breaking agitation reduce void formation and maintain color consistency. The masterbatch is introduced through the main feed throat or a downstream side feeder; side feeding is preferred when the matrix contains high levels of wood flour or mineral filler.
| Parameter | Reference range | Notes/Equipment |
|---|---|---|
| Melt temperature | 190–230°C | LLDPE carrier class; thermocouple at die |
| Let-down ratio | 2–6 wt% | Visual evaluation increments of 1 wt% |
| Pre-drying | Not normally required if sealed; dry if moisture > 0.05% | Desiccant dryer at 70–80°C for 2–4 h |
| Screw L/D ratio | ≥40:1 | Co-rotating twin-screw compounding |
| Screen pack | 60/80/100 mesh | Extrusion final screen; raises backpressure |
| Feeder accuracy | ±0.15% | Loss-in-weight with mechanical agitation |
With HDPE matrices, the rheological mismatch between the LLDPE carrier and the higher-melt-temperature HDPE phase can influence mechanical property retention. Tensile properties should be measured according to ISO 527-2 on the final molded or extruded compound, because pigment inclusions and carrier domains can reduce elongation at break relative to unfilled HDPE. The extent of reduction depends on addition level and dispersion quality; published data for this specific configuration is limited. Flexural modulus should be evaluated according to ISO 178. For wood-plastic composite capstock layers, Charpy impact testing per ISO 179-1 is used to detect brittle behavior caused by overconcentration of inorganic pigment.
Recycled polyolefin streams present additional variables. Residual acid scavengers, metallic stearates, and unknown antioxidant packages can shift color and thermal stability. The concentrate should be evaluated in the specific recyclate lot rather than assumed compatible. Addition rates at the low end of the range, typically 2–3 wt%, reduce exposure to unknown contaminants while still providing a wood tone. When the recyclate contains polypropylene contamination above 5 wt%, phase separation can appear as surface haze; compatibility testing under differential scanning calorimetry at a heating rate of 10 K/min per ISO 11357-3 may be used to identify mixed-polyolefin fractions.
Compared with an EVA-carrier masterbatch, the LLDPE carrier has a lower vinyl acetate content and is generally less hygroscopic. Compared with a PP-carrier masterbatch, the LLDPE carrier reduces melt temperature but may slightly reduce flexural modulus in HDPE-based compounds. These differences are not universal; they should be confirmed on the target line because batch-to-batch variation in pigment surface treatment can dominate visual and mechanical effects.
| Carrier type | Density range | Melt temperature range | Compatibility boundary |
|---|---|---|---|
| LDPE | 0.917–0.930 g/cm³ | 105–115°C | High polyethylene compatibility; lower heat resistance |
| LLDPE | 0.918–0.940 g/cm³ | 120–125°C | Higher tensile and elongation; good polyethylene compatibility |
| PP | 0.895–0.915 g/cm³ | 160–170°C | Limited polyethylene miscibility; suitable for polypropylene matrices |
| EVA | 0.930–0.950 g/cm³ | 85–100°C | Adhesion contribution; higher acetate content; possible odor |
Moisture uptake in pigment-containing polyolefin masterbatches is usually lower than in wood-flour-filled compounds, but the product should be stored in sealed containers below 35°C and protected from direct sunlight. If a polyethylene liner is opened and not resealed, the pellets can adsorb surface moisture. For critical capstock applications, a desiccant dryer at 70–80°C for 2–4 h with a dew point below −20°C is recommended after exposure to relative humidity above 60%. Drying should not exceed 90°C for LLDPE carriers to avoid pellet sintering.
Feed system design must account for the bulk density and pellet geometry of the masterbatch. Bridging over the hopper throat can occur if pellets are irregular or if static charge is high. Loss-in-weight feeders with mechanical agitation and stainless-steel contact surfaces reduce electrostatic build-up. On injection molding machines with clamp forces above 150 t, plastication units with L/D ratio below 20:1 may not provide sufficient dispersive mixing; back pressure in the range of 5–10 MPa hydraulic is often used for polyolefin color concentrates, but the specific value should be set to avoid screw recovery delays.
Compliance statements should be verified against current regional regulations. The product is not declared as food-contact grade unless explicitly stated in a document from the manufacturer. For European Union applications, the manufacturer’s REACH and RoHS statements should be obtained; no self-declaration should be inferred from this description. For outdoor building products exposed to climatic conditions, accelerated weathering of the final compounded part should be conducted per ISO 4892-2 or ASTM G154; the concentrate alone does not replace a UV stabilizer package unless the technical data sheet lists such additives.
Process validation on the target line should quantify color variability and physical property retention. Sampling at 30 min intervals during a 4 h extrusion trial is used to capture feeder drift. The acceptance window for color difference in a capstock layer is often specified as ΔE*ab < 1.0 under D65 illumination; this is not a property of the masterbatch alone but of the complete extrusion or molding system. Published data for this specific product is limited, and the manufacturer’s certificate of analysis remains the authoritative source for batch-specific values.