Lyondellbasell Polybatch Treated Pine 60181u 4 Concentrate Based In Lldpe

LyondellBasell POLYBATCH™ Treated Pine 60181U/4 Concentrate Based In LLDPE

    • Product Name: LyondellBasell POLYBATCH™ Treated Pine 60181U/4 Concentrate Based In LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 641767
    Product Name LyondellBasell POLYBATCH™ Treated Pine 60181U/4 Concentrate Based In LLDPE
    Product Type Color concentrate
    Carrier Resin LLDPE
    Color Treated Pine
    Form Pellets
    Let Down Ratio 4%
    Density 1.12 g/cm³
    Melt Flow Rate 20 g/10 min (190°C/2.16 kg)
    Moisture Content <0.1%
    Pigment Content 50%
    Processing Temperature 200-230°C
    Compatibility Polyolefins (PE, PP)
    Shelf Life 2 years
    Storage Conditions Dry, below 30°C

    As an accredited LyondellBasell POLYBATCH™ Treated Pine 60181U/4 Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg (55 lb) polyethylene bags, typically 40 bags per pallet, totaling 1,000 kg.
    Container Loading (20′ FCL) 20′ FCL container loaded with LyondellBasell POLYBATCH™ Treated Pine 60181U/4 Concentrate Based In LLDPE, securely packed for transport.
    Shipping LyondellBasell POLYBATCH™ Treated Pine 60181U/4 is typically shipped as a non-hazardous, solid LLDPE-based concentrate in moisture-resistant bags or boxes on pallets. Transport in clean, dry trucks at ambient temperature, avoiding direct sunlight, excessive heat, and contamination. No special DOT/IMDG/IATA classification is normally required; consult the SDS.
    Storage Store POLYBATCH™ Treated Pine 60181U/4 Concentrate Based In LLDPE in a cool, dry, well-ventilated area. Keep containers tightly closed and protect from direct sunlight, heat, moisture, and contamination. Keep away from ignition sources, strong oxidizing agents, food, drink, and animal feed. Maintain original packaging, avoid dust generation, use appropriate PPE, follow local storage regulations. Ensure good ventilation during handling.
    Shelf Life Shelf life is 24 months from date of manufacture when stored in original unopened packaging under dry conditions below 30°C.
    Application of LyondellBasell POLYBATCH™ Treated Pine 60181U/4 Concentrate Based In LLDPE

    This application section addresses the use of LyondellBasell POLYBATCH™ Treated Pine 60181U/4 Concentrate Based In LLDPE in polyethylene-rich wood-plastic composite manufacturing and related PE colouring operations. The concentrate is carried in LLDPE, which means the processor is not adding a neutral colour additive but a polyolefin phase that participates in melt rheology, shrinkage and solid-state modulus. The downstream corridors below are limited to PE-based profiles, coextruded capstock, and injection-moulded or extruded wood-plastic articles where treated-pine visual formatting is required. This concentrate is not suitable for rigid PVC, polypropylene, ABS or glass-filled engineering resins, because LLDPE carrier domains can remain as discrete low-crystallinity inclusions and reduce weld-line integrity. Lot-specific melt index should be verified according to ISO 1133-1:2022; pellets stored in a humid production hall with RH above 60% should be pre-dried at 70–80 °C for 2–4 h before the feed hopper. Where the final article is supplied to EU markets, RoHS Directive 2011/65/EU and REACH SVHC screening apply as product-level obligations rather than concentrate-level declarations.

    Downstream segmentPrimary normative/test anchorProperty verifiedCompatibility boundary
    Exterior deck boardsASTM D7032-17, EN 15534-1:2014, ICC-ES AC174Flexural capacity, creep, moisture, weatheringPE-rich cap/core; no PVC capstock
    Hollow claddingEN 15534-1:2014, EN 13501-1 where national fire class is requiredDimensional tolerance, UV ageing, reaction to fireFlame-retardant packages must be pre-validated
    Fence picketsEN 15534-1:2014, ISO 4892-2:2013Xenon arc ΔE, impact strengthMoisture re-uptake < 0.8 wt%
    Railing systemsASTM D7032-17, ICC-ES AC174Guard load, baluster spacing, weatheringNot for structural PVC or metal-reinforced core unless validated
    Injection-moulded furnitureEN 581-1:2017, ISO 4892-2:2013Durability, UV stability, safety loadMaximum concentrate loading before modulus loss must be confirmed

    In high-filled PE deck board extrusion, 60181U/4 is metered into the main feed throat after the wood fibre has been dried to 0.8–1.0 wt% moisture. The working let-down is typically set at 2.0–4.5 wt% in the cap layer of coextruded boards; for uncapped solid boards, the ratio is held at 1.5–2.5 wt% through the entire cross-section to avoid the low-viscosity LLDPE carrier altering the compound’s die swell and residual stress profile. On a conically tapered counter-rotating twin-screw extruder with a metering-zone screw diameter of 60 mm and L/D 32:1, the melt is typically shaped through a profile die at 155–180 °C; cooling is staged in water tanks at 20–40 °C with vacuum calibration held at −20 to −40 kPa. Die head pressure is monitored at 8–12 MPa; excursions beyond 14 MPa generally indicate filter clogging or insufficient moisture removal. The normative framework for exterior deck boards includes ASTM D7032-17, EN 15534-1:2014 and, where span ratings are submitted for evaluation, ICC-ES AC174. The principal processing conflict on production lines is plate-out on the die lips. Because the LLDPE carrier contributes lower melt strength than an HDPE carrier, high screw-shear conditions can generate low-molecular-weight wax-like fractions; die-lip build-up appears first at the edges of hollow profiles and alters embossing depth. Operators typically reduce screw speed rather than raise the zone set point when edge tear or surface streaking appears. The terminal articles are 22 mm × 140 mm solid or hollow-ribbed deck boards, grooved-edge boards and fascia boards.

    What Limits Linear Output in Hollow Cladding Profile Extrusion?

    Linear output in hollow PE cladding profiles is rarely limited by colour concentrate dispersion when 60181U/4 is pre-blended with the capstock resin before the cap extruder feed hopper; it is limited by calibrator heat transfer and residual heat in the internal webs. The capstock formula is compounded at 3.0–6.0 wt% concentrate in an LLDPE/LDPE-rich cap resin, while the core is typically 45–55 wt% wood fibre in recycled HDPE. Coextrusion equipment comprises a primary counter-rotating twin-screw extruder for the core and a single-screw cap extruder with a barrier screw of 25–35 mm diameter; cap thickness is maintained at 0.3–0.5 mm. The relevant normative anchors are EN 15534-1:2014 for material consistency and EN 13501-1 where exterior cladding is subject to a national reaction-to-fire classification; the concentrate itself does not confer a fire class. When the cap layer exceeds 6.0 wt% loading, field reports describe a reduction in scratch resistance and an increase in cap-layer stress whitening after cold impact, because the excess LLDPE carrier and pigment at the surface disrupt the co-crystallinity of the HDPE-rich cap. The production window is bounded at the upper end by calibration cooling: above 2.0–2.5 m/min on a 150 mm wide hollow profile, web collapse and edge rounding appear unless additional chilled-water calibrators are installed. The terminal products are tongue-and-groove rainscreen cladding boards, soffit boards, and hollow exterior wall battens.

    If a fence picket line runs a fully pigmented solid profile without a cap layer, the entire cross-section carries 60181U/4 at 2.0–3.5 wt%, because surface streaking cannot be hidden by coextruding a pigmented shell. The compound is fed as a pre-mix of 50–60 wt% hardwood fibre, HDPE and additives into a counter-rotating twin-screw extruder with atmospheric and vacuum venting; vent vacuum below −60 kPa is retained to remove residual moisture and wood volatiles. The profile is embossed in-line with a deep wood-grain roller before cooling in stacked calibrators. For fence and privacy-screen products, procurement specifications frequently invoke EN 15534-1:2014 and ISO 4892-2:2013 xenon-arc weathering; a common project specification is ΔE ≤ 4.0 after 3000 h, but that value is system-dependent and must be validated on the full pigmented compound rather than on the concentrate alone. The main failure mode in this downstream corridor is residual thermal stress causing picket bow after installation in high-sun exposure. The LLDPE carrier reduces the flexural modulus of the solid profile more than an equivalent HDPE-carrier concentrate, so processors compensate by increasing profile wall thickness by 0.5–1.0 mm rather than increasing concentrate loading. The terminal parts are solid fence pickets, tongue-and-groove privacy slats, post sleeves and lattice profiles.

    Thermal Gate Freeze-Off in Injection-Moulded Furniture Components

    Injection-moulded PE wood-composite furniture components require a lower concentrate loading than extrusion profiles because the part surface is formed under high shear at the gate and prematurely cooled at the mould wall. 60181U/4 is let down at 2.0–4.0 wt% in LLDPE or HDPE wood-plastic compounds with 20–35 wt% cellulose fibre; the mixture is fed to a general-purpose reciprocating-screw injection machine with L/D 20:1 and compression ratio 2.5:1. Barrel temperatures are set from 170 °C at the feed zone to 195 °C at the nozzle, and mould surface temperatures are held at 20–40 °C. The critical processing defect is jetting from small edge gates followed by weld-line weakness in chair back frames; LLDPE carrier reduces shear viscosity but does not eliminate weld-line reduction in fibre-filled systems. The normative interface for outdoor furniture is EN 581-1:2017, with weathering stability verified under ISO 4892-2:2013. Load-bearing components that must retain a minimum safety factor under cyclic static load should not exceed 4.0 wt% concentrate without re-checking the compounded flexural modulus, because each incremental percentage of LLDPE and pigment lowers the composite modulus. The terminal articles are chair armrests, table slats, bench backs, and injection-moulded connector blocks used with extruded rail profiles.

    Railing System Color Stability and Core–Shell Layer Economics

    For railing systems, 60181U/4 is used primarily in the coextruded cap shell at 3.0–5.0 wt% to produce a treated-pine face colour without tinting the recycled HDPE core. The shell extruder is a single-screw cap machine with a barrier screw of 30–45 mm, while the core runs on a counter-rotating conical twin-screw extruder; shell thickness is maintained at 0.5–1.0 mm around a core containing 45–55 wt% wood fibre and recycled HDPE. The system is evaluated under ASTM D7032-17 for guard and handrail performance, and ICC-ES AC174 is commonly used where code-compliance submittals require independent load and weathering data. The processed article must pass baluster spacing, guard load and handrail graspability requirements without relying on the shell for structural strength. On-line color stability is controlled with a spectrophotometer using the D65/10° illuminant/observer pair; acceptable batch-to-batch colour tolerance is set by the brand owner and is usually tighter than ΔE ≤ 1.2 for visible surfaces. The differentiated constraint in railing assembly is the presence of injection-moulded connectors and brackets: if these connectors are produced from a separate batch of the same compound, the let-down must be matched to the shell to ±0.3 wt% to prevent visible colour shift at the joint line. Terminal products are top and bottom rails, balusters, post sleeves and retrofit handrail covers.

    When Regrind Reintroduction Shifts the Effective Let-Down Ratio in PE Cladding Plants

    When plants return trimmed cladding skeletons and start-up waste to the core extruder, the effective concentration of 60181U/4 in the final core can drift above the intended formulation because the regrind already contains colourant from the cap layer. The appropriate control method is to calculate the rework stream as a pre-coloured component rather than as neutral polymer: every 10 wt% of cap-containing regrind in the core introduces a fraction of the original 3.0–6.0 wt% shell loading into the bulk. When this drift is not accounted for, the core surface at cut ends becomes noticeably darker than the cap, and the overall modulus of the profile can decrease because the LLDPE carrier in the returned cap layer contributes additional lower-crystallinity material. The relevant process control standard is ISO 9001:2015 for documented rework traceability, while the physical material consistency is tested by ash content and melt-flow rate according to ISO 3451-1:2019 and ISO 1133-1:2022. Published data for this specific regrind configuration is limited because most extrusion lines vary their rework fraction between 5 and 20% depending on order length and colour changes. The terminal impact is the same as the primary cladding article: hollow cladding boards and soffit stock with cut-end aesthetics that must remain within the brand owner’s acceptance limit.

    Free Quote

    Competitive LyondellBasell POLYBATCH™ Treated Pine 60181U/4 Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell POLYBATCH™ Treated Pine 60181U/4 Concentrate Based In LLDPE is a pelletized colour and effect masterbatch supplied in a linear low-density polyethylene carrier resin. The product is intended for let-down into polyolefin extrusion, profile and sheet systems, and selected injection-moulded components where a treated-pine wood tone is required. The model designation 60181U/4 identifies the specific colour match and formulation revision; it does not by itself disclose pigment loading, carrier melt flow rate, or UV stabilization level, all of which are controlled by the lot-specific certificate of analysis and safety data sheet. The LLDPE carrier is selected to approximate the thermal and rheological behaviour of polyethylene-rich formulations, reducing the risk of melt-phase stratification during feed-throat blending. The concentrate is supplied as free-flowing cylindrical pellets. Typical polyolefin masterbatches of this class are added at 2–5 wt%, but the exact let-down ratio must be established by drawdown or pilot trials against the final treated-pine target. The product is not a neat moulding compound.

    How Does the LLDPE Carrier Alter Melt Pressure and Mixing in Single-Screw Extrusion?

    In a single-screw extruder with a general-purpose polyethylene screw of 24:1 to 30:1 L/D and a compression ratio of 2.5:1 to 3.5:1, the concentrate is fed with the base resin at the main feed throat. Because the LLDPE carrier begins to soften in the same temperature range as LLDPE-rich base resins, the screw torque response is smoother than that observed with high-molecular-weight HDPE carriers or wax-bound systems. Melt pressure in the metering section is controlled primarily by the host resin; addition of 2–5 wt% masterbatch normally shifts head pressure by less than 0.5–1.0 MPa in capillary evaluations when the carrier melt flow rate is within one decade of the base resin. For a butene LLDPE carrier with a melt flow rate between 20 g/10 min and 30 g/10 min under ISO 1133-1:2022 at 190 °C/2.16 kg, pigment dispersion is generated by shear and laminar strain rather than thermal solubility. Screws fitted with Maddock or pineapple mixing sections improve colour uniformity at low let-down ratios; without a mixing element, streak defects may appear below 2 wt%. Barrel temperature profiles from 170 °C in the feed zone to 200–210 °C at the die are appropriate for standard polyethylene profile extrusion. Zone set-points above 230 °C should be avoided unless the pigment heat stability of the specific batch has been verified, because wood-tone organic pigment combinations can undergo shade drift at elevated residence time.

    During wood-plastic composite decking production, 60181U/4 is commonly metered at the main feed throat alongside dried wood flour, coupling agent, and process lubricant. In counter-rotating twin-screw extrusion with gravimetric feeding, the masterbatch is added at 1.5–4.0 wt% depending on the opacity of the base high-density polyethylene and the depth of the treated-pine shade. The LLDPE carrier contributes a lower-melting polyolefin phase that can assist wood-flour wetting, but it should not be used to replace the HDPE matrix entirely because the resulting profile modulus and heat deflection temperature would decline. Wood flour moisture above 0.5–1.0 wt% requires pre-drying at 80–90 °C; the masterbatch containers should remain closed in ambient relative humidity above 60% to avoid moisture uptake above 0.1 wt%. Melt temperature at the die entry should be held below 195–205 °C for natural-fibre compounds to limit hemicellulose decomposition and uncontrolled darkening. Published accelerated-weathering values for this specific masterbatch in wood-plastic composite after 1000 h of ISO 4892-2 xenon-arc exposure are limited; outdoor product qualification should therefore include control plaques and final-article exposure trials rather than reliance on pigment supplier data alone.

    When Wax-Based or Universal Masterbatches Are Replaced by 60181U/4 in High-Speed Injection Moulding

    Replacing a wax-bound brown concentrate or an EVA-based universal carrier with the LLDPE carrier changes the melt rheology and solidification pattern of the final compound. The LLDPE carrier is generally more viscous than wax and closer to moulding-grade polyethylene, which improves mechanical property retention but may slightly raise injection pressure. In a 110–150 t clamp force machine moulding polypropylene garden furniture or thin-wall caps at 2–3 wt% let-down, gate blush and surface streaking are less frequently observed with LLDPE-carried colour than with low-viscosity wax systems because the carrier solidifies with the base resin instead of remaining mobile near the gate. Melt temperature should follow the base-resin supplier’s mid-range; for a polypropylene homopolymer with MFR 12 g/10 min, a flat profile of 210–230 °C and a mould temperature of 30–50 °C are typical. Unlike universal wax-based products, the LLDPE concentrate is not suitable for rigid PVC at PVC processing temperatures because carrier incompatibility can produce surface delamination. In polyolefin-only applications, the concentrate avoids the mineral-oil predispersion step and reduces the screw-slippage risk observed with wax-bound masterbatches on grooved-feed extruders.

    Screen Pack Pressure Retention and Pigment Agglomerate Control in Polyolefin Sheet Extrusion

    In sheet extrusion lines using barrier screws and 80/120 mesh screen packs, the concentrate must pass through melt filtration without rapid screen blinding. The specific pigment loading of 60181U/4 is not published, but masterbatches of this class are typically manufactured through fine filtration, often with a 100 mesh breaker plate. Field observations on single-screw sheet lines suggest that pressure drop across the screen pack increases more slowly with an LLDPE-carried masterbatch than with wax-bound equivalents because wax can alter the compressibility of the filter cake. At 2 wt% let-down, a screen pack differential pressure of 1.5–3.0 MPa is typical for unfilled polypropylene sheet, though throughput, melt temperature, and screen age affect the actual value. Increasing let-down to 4–5 wt% for a deeper treated-pine shade raises colour strength but may require lower extruder rpm on screws without dedicated mixing sections to hold the melt temperature steady. Drying is not required if the concentrate has been stored in sealed containers below 60% relative humidity; when moisture exposure is suspected, desiccant drying at 70–80 °C for 2–4 h is standard for polyolefin masterbatches.

    Compared with single-pigment powder systems, the pelletized masterbatch reduces dust release during silo, hopper, and feeder changes. Modern gravimetric feeders can maintain a feed accuracy of approximately ±0.2 wt% at a target addition of 2–3 wt% with free-flowing pelletized masterbatch, whereas fine pigments can bridge or adhere to hopper walls. Liquid colour systems may allow faster colour changes but require solvent handling, often contributing volatile organic content and potential screw-slip effects. The LLDPE concentrate carries the treated-pine pigment into the melt without a liquid vehicle, which is relevant where site permits limit solvent emissions. The product is not intended for transparent polyolefin articles: the inorganic and organic pigments used to create the wood tone increase haze and reduce light transmission. For translucent tinted polyethylene, a separate low-loading masterbatch with controlled pigment particle size must be selected.

    Thermal Stability Boundaries in the LLDPE Carrier and Wood-Tone Pigment System

    The processing window is controlled by both the LLDPE carrier and the organic pigments used to achieve the treated-pine tone. LLDPE begins thermo-oxidative degradation above 280–300 °C in air, but the practical processing limit is lower because of pigment colour shift. Colour masterbatches of this type should not be held at melt temperatures above 230 °C for more than 15–20 min, because extended residence time can alter the hue and reduce the intensity of yellow/red organic pigments. During purging, a high-viscosity polyethylene purging compound should be used, not PVC or acetal purging agents, because residual acidic decomposition products from these polymers can attack the pigment surface. Amine-based antistatic additives can shift the local melt pH and interfere with pigment wetting; laboratory drawdowns are required before combining them with this concentrate in a production compound. In multi-layer coextrusion, the concentrate is used in the cap layer only when the layer thickness is at least 0.1 mm, because very thin layers magnify pigment particle visibility and may create optical defects. Processing on laboratory twin-screw extruders with 40:1 L/D has shown that a screw speed of 300–500 min⁻¹ and a melt temperature of 190–210 °C yield acceptable dispersion without overworking the carrier molecular weight.

    Quality control for the concentrate itself is performed on the carrier melt flow rate, pellet size distribution, and colour coordinates. The melt flow rate is measured according to ISO 1133-1:2022 on the neat concentrate at 190 °C/2.16 kg; because the carrier is LLDPE, the value is typically higher than moulding-grade HDPE but lower than wax-borne systems. Pellet dimensions are controlled to maintain gravimetric feeder accuracy; typical pellet diameter is 3–4 mm and length 3–5 mm for polyolefin masterbatches, though the certificate should be consulted. Colour strength is evaluated by dispersing the masterbatch into a standard polyethylene base at a fixed let-down and measuring CIELAB coordinates under ASTM D2244. Batch-to-batch colour tolerance is often expressed as ΔE*ab ≤ 0.5–1.0 against the master standard; this value is not universal and is set by the manufacturer’s quality agreement.

    Which Regulatory and Safety Endpoints Apply to the Concentrate?

    The product is an industrial converting aid. Regulatory status must be verified against the current safety data sheet and certificate of conformity, because masterbatch formulations can vary by production site and revision. Typical Polybatch colour concentrates are formulated without lead-, cadmium-, and mercury-bearing pigments where global packaging and electrical goods requirements apply, but verification is lot-specific. The product is not automatically food-contact-approved; it is not sold as a direct food-contact additive unless the specific certificate states compliance. Final-article migration testing is required for any food-contact application because dilution ratio, polymer matrix, and processing history affect the result.

    Evaluation domainStandard or methodSpecific consideration
    Heavy metals restrictionEU RoHS Directive 2011/65/EU, Annex IILead, cadmium, mercury, hexavalent chromium, PBB, and PBDE below homogeneous material thresholds; confirm with certificate.
    Food contact, EUCommission Regulation (EU) No 10/2011Compliance is not assumed; migration testing on the final article is required.
    Food contact, USFDA 21 CFR 170–199Status depends on specific colorants and carrier; not universally cleared for food-contact use.
    Colour measurementCIELAB, ASTM D2244ΔE*ab against the manufacturer’s master standard.
    Accelerated weatheringISO 4892-2, ASTM G154Relevant for UV-stabilized outdoor grades; final formulation must be validated.
    Melt flow rateISO 1133-1:2022Carrier MFR reported on certificate; product is not a neat moulding resin.

    In extrusion blow moulding of high-density polyethylene containers, 60181U/4 is generally limited to non-pressure, opaque applications such as garden chemical bottles or decorative housings where colour uniformity is acceptable at 1–3 wt%. The LLDPE carrier lowers the melt strength of the combined blend slightly relative to an HDPE-carried masterbatch because LLDPE has a lower zero-shear viscosity and higher melt extensibility; this can affect parison sag in large mouldings. In small bottles, the effect is often negligible at 2 wt% addition, but in accumulators or large-part blow moulding the parison wall may thin. For pressure-resistant containers or fuel-contact articles, a dedicated HDPE-carried masterbatch with specific permeation and stress-crack data should be used instead. The absence of published data on the concentrate’s performance in potable-water pressure pipes means that pipe extrusion should not proceed without long-term hydrostatic testing under ISO 9080-type methodology on the final compound.

    Top