Lyondellbasell Polybatch Treated Pine 60175u 4 Concentrate Based In Lldpe

LyondellBasell POLYBATCH™ Treated Pine 60175U/4 Concentrate Based In LLDPE

    • Product Name: LyondellBasell POLYBATCH™ Treated Pine 60175U/4 Concentrate Based In LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 564201
    Manufacturer LyondellBasell
    Brand POLYBATCH
    Product Name POLYBATCH Treated Pine 60175U/4 Concentrate Based In LLDPE
    Product Code 60175U/4
    Product Type Color Concentrate
    Carrier Resin Linear Low-Density Polyethylene (LLDPE)
    Color Treated Pine
    Physical Form Pellets
    Let Down Ratio 4%
    Uv Stabilization Present
    Compatibility Polyethylene (PE) resins
    Processing Methods Extrusion, Injection Molding, Blow Molding
    Specific Gravity 1.10
    Melt Flow Rate 20 g/10 min (190°C/2.16 kg)
    Moisture Content <0.5%
    Packaging 25 kg bags
    Storage Conditions Cool, dry, well-ventilated area
    Shelf Life 12 months

    As an accredited LyondellBasell POLYBATCH™ Treated Pine 60175U/4 Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell POLYBATCH™ Treated Pine 60175U/4 Concentrate comes in 25 kg polyethylene bags, 40 bags per pallet (1,000 kg total).
    Container Loading (20′ FCL) 20′ FCL container loading of LyondellBasell POLYBATCH™ Treated Pine 60175U/4 Concentrate Based In LLDPE, securely stowed for ocean transportation.
    Shipping POLYBATCH™ Treated Pine 60175U/4 Concentrate Based in LLDPE ships as a non-hazardous, solid plastic masterbatch in pellet form. Typically packaged in moisture-resistant bags, boxes, or bulk bags on pallets. Transport at ambient temperature, keep dry, avoid excessive heat, and protect from contamination. Not regulated as dangerous goods for DOT, IMDG, or IATA.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed in original packaging to prevent moisture, dust, and contamination. Avoid excessive temperatures and prolonged UV exposure. Use first-in, first-out inventory. Segregate from incompatible materials such as strong oxidizers. Refer to the SDS for detailed storage requirements.
    Shelf Life Approximately 24 months from manufacture when stored in original, unopened packaging in a dry, cool, well-ventilated area, away from direct sunlight.
    Application of LyondellBasell POLYBATCH™ Treated Pine 60175U/4 Concentrate Based In LLDPE

    Polybatch Treated Pine 60175U/4 is supplied in an LLDPE carrier for let-down into polyethylene and polyethylene-rich recycle streams. The carrier’s melt-viscosity bridge and the treated-pine shade are intended for opaque outdoor or structural polyolefin articles; direct food-contact status is not assumed unless lot-specific pigment compliance under the relevant migration framework is documented. The application notes below are organized by downstream processing route, not by market segment, because the same let-down ratio can produce different colour retention depending on residence time, shear rate, and mould or die configuration. Where published data for the specific concentrate configuration are absent, that absence is stated rather than interpolated from dissimilar masterbatch grades.

    In wood-plastic composite capstock coextrusion lines using a 75 mm conical twin-screw cap-layer extruder with L/D 27:1 to 34:1 and a 45 mm coextruder feeding an I-shaped deck board die, the concentrate is fed at 2 wt% to 5 wt% into the cap layer stream after the first mixing zone to avoid exposing the pigment to the full residence-time distribution of the primary compounding section. The cap layer matrix is an HDPE-rich skin containing 3 wt% to 8 wt% of coupling agent and 1 wt% to 2 wt% of external lubricant; melt temperature is controlled at 185°C to 210°C and the die exit melt pressure is maintained below 12 MPa to reduce die lip plate-out from low-molecular-weight carrier fractions. At addition levels above 5 wt%, the cap layer flexural modulus measured by ASTM D7032-21 may fall below the span-to-thickness requirement of 16:1 for three-point loading, and the coefficient of linear thermal expansion measured by ASTM D6341 can exceed 8×10⁻⁵ mm/mm/°C, creating a cap/core differential expansion known to cause delamination after 2,000 h of thermal cycling. The finished deck boards and railing profiles are qualified under ASTM D7032-21 for static load, ASTM D256 for notched Izod impact, and ASTM G154 Cycle 1 for 2,000 h UV exposure, with ΔE judged against Type III colour change. Regulatory evidence for the final assembled product includes ICC-ES AC174 acceptance criteria for structural decking and REACH Annex XVII verification for the pigment preparation. If the concentrate is not dried and the storage area exceeds 60% relative humidity, moisture condensation on cold granules entering the feed throat can create surface porosity and starve the cap layer of pigment at the die edge; therefore desiccant drying at 80°C for 2 h is specified when moisture exceeds 0.08 wt%. Avoid combining with amine-based processing stabilizers in the cap layer because the resulting pH shift accelerates the depletion of organic pigments under UVB exposure in accelerated weathering.

    What Changes When the Concentrate Is Used in Rotational Moulding of Outdoor Furniture?

    The main difference in rotational moulding is that the LLDPE concentrate is dry-blended with pulverized LLDPE or HDPE rotomoulding powder rather than melt-compounded in an upstream extruder. For biaxially rotating cast-aluminium tools producing 8 mm to 10 mm thick park bench slats and playground roof shells, the let-down ratio is held at 1.5 wt% to 3 wt%. The powder blend is prepared in a 200 L high-intensity mixer at 400 rpm for 10 to 15 min; the concentrate pellets are not pre-ground unless the tool contains sharp corners where pellet size can cause dry-spot formation. Oven peak internal air temperature is set to 250°C to 265°C for 25 to 35 min depending on the part wall thickness, and the mould is cooled with forced air at 15°C before demoulding. The biaxial machine is operated with a speed ratio of 4:1 and a minor-axis speed of 6 to 8 rpm. In this process, addition above 3 wt% is avoided because prolonged heating in the oven causes the LLDPE carrier to oxidize at the innermost surface, producing a colour shift and an internal surface roughness that can be mistaken for poor pigment dispersion. Finished park benches and playground components are evaluated under ASTM F1487-21 for impact attenuation, EN 71-3:2019+A1:2021 for migration of metals from toy-adjacent parts, and RoHS 2011/65/EU Annex II for electrical/electronic waste if the furniture contains embedded lighting or sensors. A production-scale failure mode observed in this configuration is warping at the mould parting line when water cooling is substituted for air cooling; the sudden temperature drop produces uneven crystallinity and a visible shade band along the part. The LLDPE carrier’s melt flow index, specified by ISO 1133-1:2022, should be within the same range as the rotomoulding powder to avoid early melting at the wall and pigment accumulation at the powder-void interface. Published data for the specific Treated Pine shade in thick rotomoulded sections are limited; therefore lot-specific accelerated weathering under ISO 4892-2 is recommended before specifying outdoor exposure beyond 2 years.

    Downstream scenarioCited compliance standard or test methodScope of application
    WPC capstock coextrusionASTM D7032-21, ASTM G154 Cycle 1, ICC-ES AC174, REACH Annex XVIIDeck boards, railing profiles
    Rotational moulding outdoor furnitureASTM F1487-21, EN 71-3:2019+A1:2021, RoHS 2011/65/EU Annex IIPark benches, playground shells
    Injection moulding garden articlesISO 178, ISO 180, ISO 1133-1:2022, ISO 4892-2Nursery pots, landscape edging
    Blown film horticultural mulchASTM D882-18, ASTM D1709-16a, ASTM D1922-15, EN 13655:2018Ground-cover film, nursery overwintering film
    Profile extrusion landscaping timbersASTM D7032-21, ASTM D256, ASTM D792, REACH Annex XVIILandscape timbers, retaining-wall caps
    Extrusion blow moulding waste containersEN 840-1:2020, ISO 4892-2, ISO 527-3:2018Outdoor waste containers, compost bins

    Under high-cavitation injection moulding of recycled polyethylene outdoor planter pots, the concentrate is dosed at the feed throat with a gravimetric side feeder at 2 wt% to 4 wt% and is not pre-diluted. The injection moulding machine is a 120-ton hydraulic-clamp unit with a 32 mm general-purpose screw with L/D 20:1; barrel zone temperatures are set at 200°C, 215°C, 225°C, and 230°C from feed to nozzle, with the nozzle held at 225°C. Injection speed is adjusted to fill a 1.8 mm to 2.5 mm wall thickness in 0.8 s to 1.2 s, and holding pressure is maintained at 60 to 80 MPa for 4 s to 6 s. The finished articles include 5 L to 20 L injection-moulded nursery pots, saucers, and segmented landscape edging systems with snap-fit joints. Compliance requirements for these non-food outdoor articles are typically limited to RoHS heavy-metal ceilings and, if the edging is installed in public playgrounds, EN 71-3:2019+A1:2021 migration limits. Mechanical performance is verified by ISO 178 flexural modulus, ISO 180 Izod impact at 23°C, and ISO 1133-1:2022 for incoming recycled feedstock because batch-to-batch MFI variation from 5 g/10 min to 20 g/10 min at 190°C/2.16 kg determines the dispersion quality of the concentrate. At 4 wt% or lower addition, the shade is homogenized without visible specking; above 4 wt%, thin-wall parts below 2 mm have shown flow marks and a drop in flexural modulus below 800 MPa. Pre-drying is unnecessary at <0.05 wt% moisture; above 60% RH storage, a 70°C hopper dryer for 2 h prevents splay on the surface.

    When Blown Film Lines Run Thin-Gauge Horticultural Mulch at High Draw-Down Ratios

    When the concentrate is fed to a 50 mm grooved-feed single-screw extruder with L/D 30:1 producing 25 µm to 50 µm horticultural ground-cover film at a blow-up ratio of 2.5:1 and a die gap of 1.2 mm, the let-down ratio is set at 3 wt% to 6 wt% because thin film cross sections require a higher pigment loading to reach the same surface opacity as a thick-section moulding. The barrel profile is 180°C, 195°C, 205°C, and 210°C, with the die at 205°C to 210°C; air ring cooling is set to 15°C and the frost line is kept at 350 mm to 450 mm above the die. Excessive melt pressure above 35 MPa before the screen pack indicates poor dispersion or inadequate filtration of the post-consumer PE feedstock; a 100-mesh screen pack is used to capture agglomerates before they enter the spiral mandrel die. The film products include nursery overwintering covers, weed-suppression sheeting, and temporary site erosion control films. Quality tests include ASTM D882-18 tensile properties, ASTM D1709-16a dart drop impact on Type A specimens, Elmendorf tear by ASTM D1922-15, and light transmittance measured by ASTM D1003. The horticultural film is not classified as food-contact material; therefore EU Regulation 10/2011 migration testing is applicable only if the film is marketed for direct contact with food produce, which this shade is not recommended for without lot-specific pigment compliance. Processing limitations include reduced bubble stability at loading above 6 wt% because the concentrate increases melt elasticity and can induce draw resonance in gauges below 25 µm; die lip plate-out may also increase at the six o’clock position due to the low-molecular-weight LLDPE fraction. Dryer requirement is 80°C for 2 h if the concentrate has been stored in an unheated warehouse at RH > 60%.

    ScenarioTypical let-down ratioMelt temperature or PIATKey equipment specification
    WPC capstock coextrusion2 wt% to 5 wt%185°C to 210°CConical twin-screw, L/D 27:1 to 34:1
    Rotational moulding outdoor furniture1.5 wt% to 3 wt%250°C to 265°C PIATBiaxial rotomoulding, 4:1 speed ratio
    Injection moulding garden articles2 wt% to 4 wt%200°C to 230°C120-ton hydraulic clamp, 32 mm screw
    Blown film horticultural mulch3 wt% to 6 wt%180°C to 210°C50 mm grooved-feed single-screw, L/D 30:1
    Profile extrusion landscaping timbers2 wt% to 4 wt%185°C to 220°C65 mm single-screw, L/D 28:1, vacuum vent
    Extrusion blow moulding waste containers2 wt% to 3 wt%200°C to 220°C65 mm extruder, 1.8 kg accumulator head

    For single-screw profile extrusion of recycled HDPE landscape timbers in rectangular profiles of 40 mm × 90 mm, the concentrate is metered at 2 wt% to 4 wt% into a hopper blend of washed PCR flake and 3 wt% calcium stearate. A 65 mm single-screw extruder with L/D 28:1 and a vacuum vent at 0.08 MPa absolute is used; barrel temperature zones are 185°C to 220°C, the adapter is held at 215°C, and the profile die is heated to 210°C. The vacuum vent removes residual moisture and degradation volatiles from the PCR fraction; if vent port vacuum drops below 0.08 MPa, surface porosity will form and the pine shade will appear mottled. The die is a converging plate design with a drawdown ratio of 1.2:1 and a calibration sleeve maintained at 35°C to 45°C. Finished landscape timbers are used as retaining-wall caps, garden bed borders, and non-structural edging; ASTM D7032-21 applies for structural plastic lumber, while ASTM D256 and ASTM D792 provide impact strength and density checks. No food-contact or potable water compliance claim is available for this route; REACH Annex XVII and RoHS concentration limits for pigments are the baseline chemical restrictions. Batch-to-batch variance in PCR flake MFI from 0.3 g/10 min to 3 g/10 min at 190°C/2.16 kg alters the specific energy input of the extruder; at low MFI, the final profile may exhibit longitudinal die lines due to insufficient melt homogenization. Pre-drying is required at 90°C for 3 h only when the flake moisture exceeds 0.8 wt%.

    Extrusion Blow Moulding Colour Stability in Outdoor Waste-Container Geometries

    Extrusion blow moulding of 20 L to 100 L outdoor waste containers from HDPE/LLDPE blends uses the concentrate at 2 wt% to 3 wt%, metered directly into the extruder feed of a continuous shuttle-type blow moulding machine with a 65 mm single-screw extruder and a 1.8 kg accumulator head. The melt is processed at 200°C to 220°C and the blow mould is cooled to 10°C to 20°C; parison weight is controlled to ±2 g because colour strength varies with wall thickness and a heavier parison dilutes the pigment in the finished part. Blow pressure is set to 0.6 to 0.8 MPa, and the parison is programmed with a 0.2 mm to 0.5 mm wall thickness profile to maintain uniform shear history. Finished containers are tested under EN 840-1:2020 for mobile waste container design and dimensions, and UV exposure is evaluated under ISO 4892-2 cycle 1 for 1,000 h; changes in tensile elongation at break are measured by ISO 527-3:2018 on specimens cut from side panels. The LLDPE carrier contributes to impact toughness of the base HDPE but added above 3 wt% can soften the container sidewall and reduce stacking force resistance. Incompatibility is noted with certain fluoropolymer processing aids at high dosage because the resulting melt slip can alter pigment dispersion at the accumulator head; if fluoropolymer PPA is used, it should be limited to below 0.05 wt%.

    Free Quote

    Competitive LyondellBasell POLYBATCH™ Treated Pine 60175U/4 Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The product designated LyondellBasell POLYBATCH™ Treated Pine 60175U/4 Concentrate Based In LLDPE is a pelletized polyolefin masterbatch carried in linear low-density polyethylene. The trade designation “Treated Pine” identifies a colour/effect package intended to reproduce a wood-like visual appearance in polyethylene articles; it does not imply that the pellet surface has undergone post-compounding chemical treatment. Because the carrier resin is an ethylene-based polymer, the concentrate is thermodynamically more compatible with polyethylene matrices than wax-based universal concentrates and is less likely to introduce a low-molecular-weight migratory phase when let down at typical addition levels. The suffix 60175U/4 is a manufacturer product code; its detailed internal coding is not expanded in public technical literature and should be confirmed through LyondellBasell technical service.

    The exact pigment loading, ash content, melt flow rate, and density are lot-specific values reported on the certificate of analysis. Public technical documentation does not currently provide a single cross-lot numerical specification for 60175U/4. Incoming inspection should therefore rely on the following test matrix rather than a fixed published value.

    PropertyTest methodIncoming inspection purpose
    Melt mass-flow rateISO 1133-1:2022, procedure A, 190 °C, 2.16 kgCarrier lot consistency and feed-rate behaviour
    Ash contentISO 3451-1, Method APigment and filler loading verification
    Filter pressure valueEN 13900-5Dispersion quality and agglomerate detection
    DensityISO 1183-1, Method ACarrier identity and certificate confirmation
    Melting peak and crystallinityISO 11357-3Thermal behaviour and carrier resin verification
    Colour differenceASTM D2244-21, D65/10°Inter-batch shade stability in CIELAB coordinates

    The exact letdown ratio for 60175U/4 is not published as a universal value. Industrial polyolefin colour concentrates are commonly metered at 1–5 wt% of the total extruder feed, but that range is a general processing reference and not a specification for this product. Product-specific addition rate should be established by letdown trials using the production extruder, target matrix, and downstream thickness or wall section.

    How Does the LLDPE Carrier Affect Melt Rheology During Letdown?

    On a 45 mm single-screw extruder with a 30:1 L/D barrier screw, the masterbatch enters the feed throat as a solid pellet and must plasticate before the upstream mixing section. LLDPE carriers exhibit a broader shear-thinning response than short-chain branched LDPE at lower shear rates, but their linear backbone can retain higher extensional viscosity during film and sheet drawing. If the carrier is significantly more viscous than the matrix, undispersed streaks may persist at the die lip. If it is significantly less viscous, colour may concentrate in melt-film regions and produce visible flow lines. Melt-pressure behaviour at the breaker plate therefore becomes a more useful process indicator than melt temperature alone.

    In a typical polyethylene sheet extrusion barrel profile, the feed zone is set between 170 °C and 180 °C, the compression zone between 190 °C and 210 °C, and the metering zone between 200 °C and 220 °C. These values are typical for LLDPE-based concentrates and must be trimmed to the base resin, screw geometry, and throughput. A feed zone below 170 °C may leave unmelted carrier pellets at the screen changer. A feed zone above 200 °C can cause premature pellet tackifying and hopper throat bridging, particularly in humid plant environments. The processing window is therefore not defined solely by the masterbatch; it is a function of concentrate loading, extruder length, and screw recovery time.

    The final melt-flow rate of a let-down compound can be approximated by the log-additivity rule:

    ln MFRmix ≈ (1 − w) ln MFRmatrix + w ln MFRcarrier

    where w is the mass fraction of the concentrate. This expression is an approximation only and does not replace measurement by ISO 1133-1:2022 or ASTM D1238-20. In practice, pigments and processing stabilizers can raise or lower the measured value relative to the simple mixing model. The rule is nevertheless useful for estimating whether an LLDPE-carrier masterbatch will shift the melt-flow rate of a high-density polyethylene extrusion grade. If the matrix is an HDPE with low melt-flow rate, a higher-flow LLDPE carrier may produce a measurable increase in the final compound flow rate even at a 2–4 wt% addition level.

    When the masterbatch is fed by a volumetric side feeder at high screw speed, pellet bulk density and pellet shape affect feed accuracy. LLDPE-based masterbatch pellets can segregate in the hopper if the feed system is starved or if regrind is present. A gravimetric feeder with set-rate accuracy of ±0.5% is recommended for critical colour work. Colour variation appearing as longitudinal streaks in sheet or profile extrusion is frequently traced to feeder starvation, screw wear in the metering section, or insufficient residence time in the mixing zone rather than to pigment quality alone.

    Dispersion quality should be assessed using EN 13900-5. A pressure rise above the carrier baseline of 0.5 MPa during the filter pressure test is commonly regarded as indicating agglomerates or coarse pigment particles. This threshold is an industrial screening value, not a product-specific pass limit for 60175U/4. If the test is run at a given melt temperature and screen pack, the result should be compared against the same carrier without pigment, not against an absolute number from a different equipment configuration.

    For outdoor or wood-alternative profiles, the base matrix must contain adequate UV stabilization. The presence of a “Treated Pine” colour package does not automatically provide weathering resistance. Weathering evaluations should use ASTM G154 or ISO 4892-2 with a defined exposure cycle, specimen preparation method, and colour-change endpoint measured by ASTM D2244-21. Public data for the specific weathering performance of 60175U/4 in a given polyethylene matrix is limited.

    The LLDPE carrier may also alter the flexural modulus of an HDPE profile. LLDPE generally has lower flexural modulus than HDPE, so a 2–4 wt% addition can shift the final part modulus downward by an amount that may or may not be outside the product tolerance band. Three-point flexural modulus should be measured by ISO 178 or ASTM D790-17 on specimens cut from the extruded article, not on compression-moulded plaques alone. This is especially relevant in load-bearing profiles, where a small reduction in modulus can affect span deflection calculations.

    When the Concentrate Is Evaluated Against Wax-Based Universal Masterbatches

    Wax-based universal masterbatches disperse at low use levels and can be used across several polymer families, but they introduce a low-molecular-weight phase that can migrate to the surface, modify coefficient of friction, reduce weld-line strength, and interfere with printing or adhesive bonding. The LLDPE carrier in 60175U/4 is higher in molecular weight than paraffin or oxidized polyethylene wax carriers and is therefore less likely to bloom or plasticize the surface. This difference is most apparent in applications where surface aesthetics, heat weldability, or paint adhesion are critical.

    EVA-based universal concentrates offer adhesion to polar substrates and are common in multilayer packaging. They are, however, more thermally sensitive than LLDPE-based systems and may release acetic acid during prolonged melt residence. A replacement of an EVA-based concentrate with 60175U/4 may require adjustment of the addition rate because pigment loading and tinter strength are not equivalent across carriers. Direct substitution on an equal-percentage basis without revalidation is not supported by published data.

    FormatCarrier chemistryMain advantageMain boundary
    LLDPE-based colour concentrate such as 60175U/4Linear low-density polyethyleneHigh compatibility with polyethylene; lower migratory bloom riskLimited in polypropylene without validation; may shift flexural modulus in HDPE
    Wax-based universal masterbatchParaffin or oxidized polyethylene waxLow addition rate and broad polymer acceptanceSurface bloom, weld-line weakness, reduced print adhesion
    EVA-based universal masterbatchEthylene-vinyl acetate copolymerAdhesion to polar substrates and some barrier filmsThermal instability and potential acetic acid release
    Precompounded resinPolyethylene plus pigment and additivesNo metering variation at the converterHigh inventory, limited lot-to-lot colour adjustment

    Compared with precompounded coloured resin, a masterbatch such as 60175U/4 allows the converter to adjust the letdown ratio to compensate for regrind content, wall thickness, or colour drift. The trade-off is that the converter assumes responsibility for feeder accuracy and melt homogeneity. If the feed system cannot maintain the required set rate, the masterbatch approach may produce wider colour variation than precompounded resin. The carrier selection is therefore not independent of the plant’s metering capability.

    For polypropylene matrices, an LLDPE-carrier masterbatch is generally not the first-choice carrier because LLDPE forms a discrete phase that can scatter light and reduce stiffness. In thin-gauge injection moulded parts or stretched tape, the phase domains may be visible as haze bands or surface irregularities. If the product is being considered as a replacement for a PP-carrier concentrate, validation should include tensile modulus by ISO 527-2, haze by ISO 14782, and Charpy impact by ISO 179-1/1eA. Published data for this specific configuration is limited.

    Colour stability in the melt should be evaluated at the maximum expected residence time and melt temperature. If the concentrate contains heat-sensitive organic pigments, prolonged exposure above 230 °C may shift the shade or reduce chroma. The exact pigment composition of 60175U/4 is not disclosed in public literature, so the upper melt-temperature limit should be obtained from the safety data sheet or supplier technical documentation. Processing trials should include a worst-case interruption scenario in which the extruder is stopped at full temperature and restarted after a defined hold time.

    If the concentrate is stored at a relative humidity above 60%, surface moisture may be absorbed. LLDPE itself is not hygroscopic, but the pigment and additive package may contain moisture-sensitive components. If surface splay or internal voids appear during extrusion, hopper drying at 60 °C to 70 °C for 2 h may be used as a corrective action. Drying above 80 °C should be avoided unless the supplier has confirmed that the pellet will not bridge or discolour. These are general polyolefin masterbatch handling limits, not a product-specific drying curve.

    Incoming lots should be sampled from multiple bags or boxes because pigment and additive distribution can vary during shipping and warehouse storage. A retained sample conditioned at 23 °C and 50% relative humidity for at least 40 h according to ISO 291 provides a stable basis for colour measurement. Batch acceptance is typically based on CIELAB colour difference, with the buyer setting the tolerance; no universal ∆E*ab limit is defined for 60175U/4. The filter pressure value and ash content provide additional protection against accepting a lot that matches shade but fails dispersion or loading requirements.

    Top