Lyondellbasell Polybatch Teal 30316 Concentrate Based In Lldpe

LyondellBasell POLYBATCH™ Teal 30316 Concentrate Based In LLDPE

    • Product Name: LyondellBasell POLYBATCH™ Teal 30316 Concentrate Based In LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 811621
    Productname LyondellBasell POLYBATCH™ Teal 30316 Concentrate Based In LLDPE
    Manufacturer LyondellBasell
    Brand POLYBATCH™
    Productcode 30316
    Producttype Color concentrate
    Carrierresin LLDPE
    Color Teal
    Physicalform Pellets
    Compatibility Polyolefins
    Density Typical 0.92–1.10 g/cm³
    Meltflowrate Typical 10–30 g/10 min
    Letdownratio Typical 2–5%
    Processingtemperature Typical 180–230°C
    Moisturecontent Typical <0.2%
    Shelflife Typical 12 months
    Storageconditions Dry, below 30°C

    As an accredited LyondellBasell POLYBATCH™ Teal 30316 Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell POLYBATCH™ Teal 30316 Concentrate Based In LLDPE is supplied in 25 kg polyethylene bags for protected storage and handling.
    Container Loading (20′ FCL) 20′ FCL container loaded with LyondellBasell POLYBATCH™ Teal 30316 Concentrate Based in LLDPE, securely palletized and stowed for ocean freight.
    Shipping Typically non-hazardous LLDPE-based teal color concentrate. Ships in polyethylene bags, boxes, or octabins. Store in cool, ventilated area. Keep containers closed, dry, and away from heat and ignition sources. Not regulated as dangerous goods for DOT, IMDG, or IATA transport. Use appropriate PPE. Follow SDS and local regulations.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed when not in use to prevent moisture and contamination. Avoid extreme temperatures and stack pallets safely. Use original packaging, follow the SDS, and maintain good housekeeping. Protect from physical damage. Keep away from ignition sources and incompatible materials. Ensure labeling.
    Shelf Life Shelf life is typically 24 months from manufacture when stored cool, dry, in original unopened packaging, away from direct sunlight.
    Application of LyondellBasell POLYBATCH™ Teal 30316 Concentrate Based In LLDPE

    On three-layer blown film lines running LLDPE-rich skins at 60–80 µm total gauge, LyondellBasell POLYBATCH™ Teal 30316 Concentrate Based In LLDPE is introduced at 2.0–3.0 wt% with a gravimetric feeder mounted at the main feed throat. The melt index delta between the concentrate carrier and the film resin is maintained below 2.0 g/10 min as measured under ISO 1133-1:2022 at 190°C/2.16 kg. Extruders with 25:1–30:1 L/D barrier screws and screen packs of 60/80/100 mesh are typical; melt temperature at the die lip is maintained between 190°C and 215°C. With die gaps of 1.8–2.4 mm and blow-up ratios of 2.0:1–3.0:1, colour uniformity stabilizes after 20–30 min of transition purging, provided the masterbatch is not starve-fed. Terminal products include frozen-food bags, bakery over-wrap, industrial liners and collation shrink film. Converters must verify food-contact status against EU Regulation 10/2011 Annex I and 21 CFR 177.1520 for the olefin polymer; the colourant itself falls under 21 CFR 178.3290 in the United States. Packaged-article heavy-metal concentration must not exceed the sum limit of 100 mg/kg for lead, cadmium, mercury and chromium VI under EU Directive 94/62/EC Article 11. Over-addition beyond 4.5 wt% produces local melt elasticity differences at the freeze line that can trigger bubble flutter; in films below 20 µm, the let-down is held at or below 2.0 wt% to avoid teal pigment speck formation after 8–10 h of continuous operation. Pre-drying is not required for material stored in sealed packaging; if the package is opened above 60% relative humidity for more than 48 h, moisture-generated pinholes may appear, and the concentrate is dried at 60°C for 4 h in a desiccant hopper dryer before use.

    What Controls Let-Down Ratio in High-Cavitation Thin-Wall Injection Moulding?

    The teal masterbatch is metered at 1.5–2.5 wt% into natural HDPE or LLDPE moulding compound at the machine throat of high-cavitation tools with 8–32 cavities and valve-gated hot runners using a loss-in-weight feeder. Pigment agglomerates larger than 10–15 µm create gate blush and flow lines at injection speeds above 120 mm/s, so screw back pressure is set between 8 bar and 15 bar to maintain melt homogeneity without excessive shear heating. Melt temperature is maintained between 200°C and 240°C, injection pressure between 80 MPa and 120 MPa, and mould temperature between 15°C and 40°C. Cavity-to-cavity colour consistency is verified with a laboratory spectrophotometer under D65/10 illuminant/observer; acceptable lots fall within dE*ab ≤ 1.0 against the approved master standard under ISO 11664-4. Terminal products include caps, closures, housewares, crates and thin-wall storage containers. Compliance records for these durable goods are typically maintained under RoHS Directive 2011/65/EU Annex II, with lead below 1,000 ppm and cadmium below 100 ppm, and under REACH Article 33 for SVHC screening. Published data for this specific product configuration is limited for applications requiring e-beam or gamma sterilization; the converter should test colour shift after 25 kGy and 50 kGy doses if medical or laboratory packaging is targeted.

    During solvent-free cast film extrusion of 25–50 µm teal-tinted stretch, agricultural and hygiene films at line speeds above 300 m/min, die-lip build-up rather than colour dispersion becomes the limiting quality variable after 6–10 h of uninterrupted operation. Teal 30316 is dosed at 2.0–3.0 wt%; melt temperature at the slot die is held at 220–240°C, and die gap is maintained at 0.5–0.8 mm. Polished chill rolls at 20–40°C and an air-knife pinning system provide film contact and suppress gauge bands. Terminal products include pallet wrap, silage film, hygiene backsheet and protective masking film. For food-contact grades, the converter must verify that the final film meets EU Regulation 10/2011 Annex I and 21 CFR 177.1520, with colorants assessed under 21 CFR 178.3290 in the United States. Where optical clarity is specified, film haze is characterized per ASTM D1003-13. Phthalocyanine-based teal pigments may accumulate at the die lip when polymer processing aid is absent; converters running long campaigns add 400–800 ppm of a fluoropolymer process aid in the skin layer to reduce deposit incidence. Published data for this specific product formulation under high-line-speed cast film conditions is limited; therefore, a 2 h die-lip inspection interval is used during first production qualification. Chill roll release problems increase above 3.5 wt% addition, and the concentrate should not be combined with excessive metal stearate antiblock in the same layer without evaluating plate-out tendency under production conditions.

    Extrusion Blow Moulding Parison Wall-Thickness Mapping and ESCR Drift

    Extrusion blow moulding of HDPE containers with 2.0–3.5 wt% Teal 30316 requires attention to the LLDPE carrier because it modifies parison sag and die swell behaviour relative to uncoloured HDPE. Melt temperature at the accumulator head is maintained between 180°C and 210°C; parison programming is set with 10–30 point wall-thickness curves to compensate for the slightly higher melt extensibility of the LLDPE carrier. Terminal products include detergent bottles, industrial drums, personal-care containers and agricultural chemical jerrycans. For aggressive contents, converters should map environmental stress crack resistance with ASTM D1693-15 condition B; published data for this specific product configuration is limited, and the LLDPE carrier can shift failure time relative to 100% HDPE by a measurable but formulation-dependent margin. Density of the final article typically shifts less than 0.002 g/cm³ at 2.5 wt% addition, but this must be confirmed on the production line rather than from concentrate data alone. Compliance records for packaging of dangerous goods require compatibility testing under the applicable UN packaging code and 49 CFR Part 178 where relevant; heavy metals in the packaging article remain bounded by EU Directive 94/62/EC Article 11 at the 100 mg/kg sum limit. Over-addition above 5.0 wt% is not recommended because localized teal pigment agglomerates can form visible specks in the pinch-off weld and handle flash zones.

    In rotomoulding plants charging 35-mesh (500 µm) LLDPE micropowder into cast aluminium or steel moulds, pelletized Teal 30316 must be pre-ground to pass 35 mesh unless the concentrate is supplied as a powder. The masterbatch is dry-blended at 3.0–5.0 wt% in a high-intensity mixer at 25–35 rpm for 10–15 min to prevent particle segregation during transfer. Oven set temperature is maintained between 280°C and 320°C, with peak internal air temperature reaching 200–230°C and total cycle time of 20–30 min depending on wall thickness. Terminal products include water tanks, kayaks, playground components, outdoor furniture and agricultural storage bins. Compliance for toys and childcare articles requires migration testing under EN 71-3; general packaging articles fall under EU Directive 94/62/EC Article 11 heavy-metal limits of 100 mg/kg. Dry-colour segregation across pneumatic conveying lines is a known failure mode; if the concentrate powder particle size distribution is not matched to the micropowder base, colour streaking appears at the mould parting line after the first oven cycle. Published data for this specific product under rotomoulding sintering conditions is limited; therefore, the first production run includes a 100% visual inspection of the parting line and threaded boss areas.

    When the Concentrate Is Introduced Into Monofilament and Tape Extrusion Lines

    Synthetic turf thatch and geotextile tape lines running LLDPE-rich formulations can incorporate 3.0–5.0 wt% Teal 30316 if the pellet is melt blended before the metering pump. Extruder melt temperature is maintained between 200°C and 230°C; the extrudate is quenched in a water bath at 20–35°C, stretched at a ratio of 1:4–1:8, and annealed in a hot-air oven at 90–110°C. Terminal products include artificial turf thatch filaments, geotextile reinforcement tape, baler twine and industrial strapping. Tensile properties are measured under ISO 527-3; weathering resistance is assessed under ISO 4892-2 xenon arc exposure where colour retention is specified. The concentrate alone does not provide sufficient UV stabilization for exterior synthetic turf or geotextile applications; the final compound must include a separate HALS and UV absorber package to meet end-use service life requirements. Published data for the intrinsic lightfastness of this specific concentrate is limited, so outdoor grades are qualified at the customer-specific xenon arc radiant exposure rather than from masterbatch pigment data alone. Over-addition above 5.0 wt% can reduce tenacity in highly oriented tapes because pigment particles act as stress concentrators during stretching.

    Where thick-gauge LLDPE sheet is converted into reusable material-handling trays, industrial dunnage and thermoformed packaging, Teal 30316 is metered at 2.0–3.0 wt% into the main extruder feed. Sheet lines with 30:1–34:1 L/D extruders and melt pumps deliver melt to a flat die at 210–230°C; the die gap is set at 0.6–1.0 mm before the sheet enters a three-roll stack held at 60–80°C. Terminal products include reusable trays, pallet dividers, dunnage sheets and thermoformed industrial packaging. Compliance records follow REACH Article 33 SVHC screening and RoHS Directive 2011/65/EU Annex II where electronic equipment packaging is specified. Roll-stack plate-out becomes a production bottleneck when the concentrate is combined with high levels of stearyl stearamide slip; if the slip additive exceeds 1,000 ppm, a continuous cleaning film or roll-stack release evaluation is performed before full campaign. Published data for this specific product in thick-gauge sheet is limited; therefore, thickness uniformity is verified gravimetrically across the sheet width at 10 cm intervals after the first 30 min of line operation.

    Free Quote

    Competitive LyondellBasell POLYBATCH™ Teal 30316 Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell POLYBATCH™ Teal 30316 Concentrate Based In LLDPE is a pelletized color concentrate in which a teal pigment system is dispersed in a linear low-density polyethylene carrier resin. The product is supplied for dry blending with polyolefin letdown resins at the extruder feed throat or through gravimetric dosing equipment. Published lot-specific values for melt mass-flow rate, ash content, volatiles, and pigment loading are not uniformly available in public documentation and should be verified against the supplier’s technical data sheet. The selection of an LLDPE carrier is operationally significant because it influences melt-viscosity continuity when the concentrate is diluted in LLDPE-rich blown film, cast film, or extrusion coating formulations. As a masterbatch rather than a precompounded finished resin, POLYBATCH™ Teal 30316 does not by itself define the mechanical properties of the final article.

    Carrier-Resin Identity and Melt-State Rheology of the Concentrate

    LLDPE carrier resins used in commercial polyolefin color concentrates frequently exhibit a density range of 0.918–0.925 g/cm³ when determined in accordance with ASTM D1505 or ISO 1183-1:2019, and melt mass-flow rate values from 1.0 g/10 min to 20 g/10 min at 190 °C/2.16 kg when tested to ASTM D1238-20 or ISO 1133-1:2022. The specific carrier grade in POLYBATCH™ Teal 30316 has not been published in the sources reviewed, so incoming inspection should include melt-index and density verification against the certificate of analysis. On single-screw blown film lines with spiral mandrel die gaps from 0.8 mm to 1.5 mm, a carrier-induced viscosity mismatch may appear as surface haze, edge tear, or die-lip deposit if the concentrate is not uniformly dispersed before the final metering zone. Melt pressure fluctuation across a 40/60/100 mesh pack can be used to monitor pigment agglomeration, but acceptance limits are product-specific and must be derived from baseline runs on the target extruder.

    In blown film conversion, dry-blended concentrate pellets are metered at the feed throat using gravimetric or volumetric dosing. The target letdown is verified by weight-loss per unit time or by feeder calibration, and the dilution ratio is adjusted according to film opacity, thickness, and downstream printing requirements. For thin-gauge LLDPE packaging films in the 25–50 µm range, letdown ratios from 3 wt% to 5 wt% are commonly evaluated as starting points; however, the pigment concentration in Teal 30316 determines whether a lower letdown achieves equivalent color intensity. Published data for this specific configuration is limited, and no universal letdown ratio should be transferred between different POLYBATCH grades without press trials. Melt temperature measured at the die entrance should remain within the normal LLDPE film extrusion envelope of approximately 190–230 °C, but the optimum set point depends on screw speed, back pressure, and the viscosity of the letdown resin.

    What Processing Restrictions Apply in Coextruded Film Structures?

    In coextruded structures, POLYBATCH™ Teal 30316 is typically confined to a skin or print layer where color development is maximized without increasing pigment cost in the core. The concentrate is diluted in that specific layer by a separate extruder, and the layer thickness may require a higher letdown than monolayer film to achieve equivalent visual density. Adjacent layers with significantly different melt elasticity can alter interface stability, particularly when the skin layer contains a high loading of teal concentrate and the core layer is a fractional-melt LLDPE or HDPE. Die-lip build-up behavior is not governed solely by the concentrate; it also depends on die geometry, temperature uniformity, and the presence of processing aids in the letdown resin. When replacing an LDPE-carrier teal concentrate with an LLDPE-carrier grade on an existing line, the melt-pressure trend through the die may change because the shear-viscosity response of LLDPE differs from that of highly branched LDPE. Operators should compare extruder amperage, melt temperature, and die pressure at equal screw speed before adjusting the barrel profile.

    Compared with LDPE-carrier teal concentrates, an LLDPE-carrier variant reduces the proportion of highly branched polymer introduced into LLDPE-rich film formulations and may provide a closer match to the rheology of the primary resin. Compared with PP-carrier teal concentrates, the LLDPE carrier limits the risk of discrete polypropylene domains in polyethylene film and better matches the melting peak of LLDPE letdown resins. These differences are compositional rather than universally qualitative; actual dispersion behavior, color development, and melt fracture thresholds must be confirmed on the target production line. In cast film and extrusion coating applications, the lower draw resonance tendency of LLDPE-rich melts can be affected by concentrate dilution, but no published data for this specific Teal 30316 formulation in cast film is available.

    The following evaluation matrix summarizes typical starting conditions for LLDPE-based color concentrates in blown film. It is not a certificate of analysis and does not replace product-specific processing parameters.

    Evaluation variableTypical starting rangeMeasurement method or equipment
    Concentrate letdown2–5 wt%Gravimetric feeder calibration
    Die gap0.8–1.5 mmSpiral mandrel die geometry
    Melt temperature at die190–230 °CMelt thermocouple probe
    Film gauge25–75 µmMicrometer or optical gauge
    Screen pack40/60/100Melt filtration pressure drop

    Regulatory Status and Documentation Boundaries

    Food-contact compliance cannot be assumed from carrier identity alone. In polyolefin color concentrates, regulatory status is governed by the pigment system, carrier resin, and any processing aids or antioxidants. Potentially applicable frameworks include 21 CFR 178.3290 for colorants used in polymers, EU Regulation 10/2011 as amended for plastic food-contact materials, and RoHS Directive 2011/65/EU for restricted substances. Registration obligations under REACH may also apply depending on the market region. The specific regulatory status of POLYBATCH™ Teal 30316 should be confirmed through the supplier’s regulatory statement because public literature does not list the complete additive composition or migration test data for this product.

    At incoming inspection, the concentrate is characterized for melt mass-flow rate, pellet size distribution, and color strength in a standardized letdown plaque or film. A laboratory twin-screw extruder with a 25:1 L/D screw is often used to prepare compression-molded plaques under ISO 293 conditions for optical evaluation. Color difference measurements using CIE Lab coordinates and ISO 11664-4:2008 provide a numerical basis for batch-to-batch acceptance, but tolerance limits must be established between converter and supplier. Pellets should be stored in closed containers at ambient warehouse conditions. Moisture uptake in LLDPE carriers is low, but high-humidity environments above 60% RH may warrant drying before extrusion if surface condensation is observed. Product-specific drying temperature and residence time recommendations are not available in the public sources reviewed.

    Carrier-resin comparison across color concentrate families demonstrates why LLDPE carriers are selected for LLDPE-dominant film structures. The following table presents typical published polymer-property ranges rather than product-specific values for POLYBATCH™ Teal 30316.

    Carrier polymerTypical densityTypical melting peakCompatibility with LLDPE letdownRelevant standard
    LDPE0.917–0.930 g/cm³105–115 °CGood; higher branching may reduce melt strength locallyASTM D1505, ASTM D3418-21
    LLDPE0.918–0.925 g/cm³120–126 °CPreferred for LLDPE-rich film linesISO 1183-1:2019, ASTM D3418-21
    PP0.895–0.905 g/cm³160–168 °CLimited; discrete PP domains may form in polyethyleneISO 1183-1:2019, ASTM D3418-21

    On a production blown film line running a 1.0 g/10 min LLDPE letdown resin at 220 °C die temperature, the introduction of POLYBATCH™ Teal 30316 should be monitored through screw-speed compensation and die-pressure variation. The teal pigment system can shift the heat-absorption behavior of the melt slightly, although published data for this specific colorant formulation is limited. If the line previously used an LDPE-based teal concentrate, the change to an LLDPE carrier may require barrel-temperature adjustments in the transition zone to maintain the same melt quality. Final optical properties should be measured on flat film or lay-flat blown film samples with a haze meter to ASTM D1003-21 and a spectrophotometer using CIE Lab coordinates, rather than by visual inspection alone.

    Top