Lyondellbasell Polybatch Tan Ll60139 2 Concentrate Based In Lldpe

LyondellBasell POLYBATCH™ Tan LL60139/2 Concentrate Based In LLDPE

    • Product Name: LyondellBasell POLYBATCH™ Tan LL60139/2 Concentrate Based In LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 804759
    Product Name LyondellBasell POLYBATCH™ Tan LL60139/2 Concentrate Based In LLDPE
    Manufacturer LyondellBasell
    Product Line POLYBATCH™
    Product Type Color Concentrate
    Carrier Resin LLDPE
    Color Tan
    Form Pellets
    Density 1.10 g/cm³
    Melt Flow Rate 20 g/10 min at 190°C/2.16 kg
    Let Down Ratio 2%
    Pigment Content 50%
    Moisture Content <0.10%
    Processing Temperature 180-230°C
    Recommended Applications Blown film, cast film, injection molding, blow molding, extrusion
    Compatibility Polyolefins
    Packaging 25 kg bags
    Storage Dry, cool, well-ventilated area
    Shelf Life 12 months

    As an accredited LyondellBasell POLYBATCH™ Tan LL60139/2 Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell POLYBATCH™ Tan LL60139/2 Concentrate Based In LLDPE is packaged in 25 kg polyethylene-lined bags, palletized for convenient handling.
    Container Loading (20′ FCL) 20′ FCL container loaded with LyondellBasell POLYBATCH™ Tan LL60139/2 Concentrate Based In LLDPE, packed in 25 kg bags on pallets.
    Shipping LyondellBasell POLYBATCH™ Tan LL60139/2 Concentrate Based In LLDPE is typically shipped as a non-hazardous solid in moisture-resistant bags, boxes, or octabins, palletized and stretch-wrapped. No UN/DOT hazard class is normally required. Store in a cool, dry area away from direct sunlight and ignition sources.
    Storage Store indoors in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep containers tightly closed in original packaging to prevent moisture, dust, and contamination. Maintain stable, secure pallets, avoid excessive stacking, and follow FIFO stock rotation. Observe recommended shelf life, local regulations, and avoid prolonged UV or extreme temperatures. Protect from physical damage.
    Shelf Life Typically 24 months from production when stored unopened in original packaging, cool, dry, below 30°C, away from direct sunlight.
    Application of LyondellBasell POLYBATCH™ Tan LL60139/2 Concentrate Based In LLDPE

    Agricultural mulch films, silage covers and industrial shrouds produced from LLDPE-rich blown film lines commonly incorporate LyondellBasell POLYBATCH™ Tan LL60139/2 to control transmitted radiation and provide batch-to-batch colour consistency in film sold to construction and agricultural distributors. The masterbatch is pre-blended with virgin LLDPE and LDPE via low-shear paddle mixers or gravimetric batch blenders; gravimetric side-feeding on high-output lines with barrel diameters above 55 mm avoids screw slippage caused by pellet-pellet lubrication differences. Industry compliance for food-contact films is assessed under EU Regulation 10/2011, FDA 21 CFR 177.1520 for olefin polymers, and FDA 21 CFR 178.3297 for the colourant component; the finished film, not the masterbatch, carries the migration responsibility; for soil-contact agricultural films, REACH Annex XVII restrictions and local biodegradable/oxo-degradable rules must be checked. A starting addition ratio of 3 wt% is used for films in the 25–50 µm gauge range, while thicker silage covers at 100–150 µm may require 4–5 wt% to maintain the same transmitted colour depth because pigment concentration per unit area, not per unit mass, determines spectral absorbance. Downstream production commonly runs on a three-layer coextrusion die with a blow-up ratio of 2.0:1 to 2.5:1, frost-line height between 600 mm and 900 mm, and melt temperature set at 200–220 °C; the pigment package may raise the crystallization onset, causing a higher frost line if no adjustment is made, and increasing die lip plate-out on long runs. Optical performance is verified by ASTM D1003 haze and ASTM D2457 gloss, mechanical integrity by ASTM D882 tensile and ASTM D1709 dart drop; pigment dispersion quality is commonly assessed by ISO 18553 or film surface defect count per square metre. Terminal products include monolayer and coextruded agricultural mulch, silage covers, grain storage covers, industrial shrouds, and coloured overwrap for construction films; the concentrate is not suited to high-clarity food packaging where haze below 10% is required, because the pigment addition inherently raises wide-angle scattering.

    Does a 4 wt% Let-Down Shift Part Surface Scatter and Impact Resistance in Thin-Wall Injection Moulding?

    Before a tan-coloured thin-wall part is approved for freezer-rated logistics use, injection moulders dose colour masterbatch directly at the machine throat using a volumetric or gravimetric feeder synchronized to screw recovery. The sector's compliance framework includes REACH Annex XVII for restricted substances, ISO 294-1 for specimen preparation, and ASTM D638-14 tensile and ASTM D256 Izod impact for incoming lot validation; parts for food transport are evaluated under EU Regulation 10/2011 with an overall migration limit of 10 mg/dm², while non-food articles may only require a signed REACH SVHC declaration. A let-down ratio of 2–4 wt% is typical for wall thicknesses from 1.5 mm to 4.0 mm; below 1.2 mm wall, the same ratio can produce visible colour non-uniformity around gates and weld lines because high shear rates align pigment agglomerates differently than the surrounding matrix. Processing is carried out on a reciprocating-screw injection moulding machine with a 22:1 to 25:1 L/D barrier screw, back pressure set to 0.5–2.0 MPa, melt temperature held at 200–230 °C, and mould temperature maintained at 20–45 °C; injection speed is profiled so that the flow front velocity does not exceed 200 mm/s through thin ribs, minimizing jetting and non-uniform pigment orientation. Although the LLDPE carrier is not hygroscopic, surface condensation on cold pellets should be avoided when relative humidity exceeds 60%; a 60 °C hopper dryer for 2 h eliminates splay in humid plant conditions. Terminal finished products include tan-coloured industrial crates, agricultural harvest bins, freezer-rated tote boxes, bottle crates, and logistics trays where colour is used for line-of-sight sorting or brand differentiation. Published data for this specific concentrate in thin-wall injection moulding is limited; converters should run a plaque trial per ASTM D3641 to establish the relationship between let-down ratio and weld-line colour difference before full-scale release.

    Rotational moulding lines running pulverized LLDPE at oven temperatures of 260–320 °C confront a specific segregation failure when pelletized masterbatch is charged without particle size reduction: the denser pigment particles separate from lighter polymer powder during mould rotation, producing swirl marks, colour streaks, and non-uniform opacity at parting lines. For tan-coloured tanks and outdoor furniture, the LLDPE-based concentrate is cryogenically ground to a particle size distribution between 300 µm and 500 µm, then dry-blended with 35-mesh pulverized LLDPE to prevent density-driven demixing. Compliance for water-contact rotomoulded articles is assessed under NSF/ANSI 61 and, in some jurisdictions, AS/NZS 4020; the masterbatch constituents must be included in a migration risk assessment, and the final tank must satisfy ASTM D1998 for polyethylene upright storage tanks where applicable. Addition ratios in rotomoulding are higher than in film because oven dwell and long thermal exposure partially degrade the carrier and reduce pigment dispersion; a starting ratio of 3–5 wt% is typical for wall sections between 3 mm and 10 mm, with the higher value reserved for thin-wall parts requiring a low L* value. Downstream production uses a biaxial rotational machine with a 4:1 primary-to-secondary rotation ratio, oven dwell of 20–35 min, and internal air temperature measured by a Rotolog or equivalent; the peak internal air temperature is held between 190 °C and 205 °C for LLDPE, and the pigmented layer must pass a cold impact test because colourant agglomerates can reduce low-temperature ductility. Terminal products include tan-coloured agricultural water storage tanks, outdoor furniture such as benches and planters, industrial totes, and corrosion-resistant storage containers; any use in potable water plumbing requires the moulder to submit the exact formulation to the certification body, as the masterbatch alone carries no potable-water listing. Incompatibilities include peroxide-initiated PE crosslinking systems: if the tan pigment contains transition-metal oxides, the peroxide decomposition path may shift, reducing gel fraction and compressive creep resistance in crosslinked rotomoulded parts; a small-scale gel content test per ASTM D2765 is required before replacing natural carrier resin with pigmented masterbatch in a crosslinked product.

    Pinch-Off Weld Structural Integrity and Colourant Plate-Out in Continuous Extrusion Blow Moulding

    At the pinch-off weld of continuous extrusion blow moulded containers, LyondellBasell POLYBATCH™ Tan LL60139/2 sits at the interface between the parison and the weld zone, where local pigment concentration can influence weld strength and environmental stress crack resistance. Compliance for industrial containers typically involves ASTM D638-14 for welded tensile strength, ASTM D1693 for ESCR under stress-cracking media, ASTM D256 for notched impact, and, for dangerous goods packaging, the UN 3H1 or UN 31H1 certification tests; food-grade bottles are evaluated under EU Regulation 10/2011 and FDA 21 CFR 177.1520, with the understanding that the masterbatch is not the final migration barrier. A let-down ratio of 2–3 wt% is common for side walls of 1.5–3.0 mm thickness, while a ratio above 4 wt% can reduce pinch-off ductility because inorganic pigment agglomerates create stress concentration points at the weld line; this effect is quantified by comparing welded tensile strength with an uncoloured control using ISO 527-2. The downstream process on a shuttle or rotary wheel blow moulding machine runs a melt temperature of 190–210 °C, die gap of 0.8–1.5 mm, blow air pressure of 0.55–0.70 MPa, and mould temperature of 10–30 °C; the parison length is adjusted for swell because the LLDPE carrier has higher shear thinning than a HDPE base resin, shifting diameter swell by 5–15% relative to uncoloured HDPE. Pigment plate-out on the die lip and pinch-off insert is managed by reducing melt temperature at the die by 5–10 °C and specifying chromium-coated or nitride-treated flow surfaces. Terminal products include tan-coloured 20 L industrial jerrycans, automotive washer-fluid reservoirs, agri-chemical containers with UN certification, and large-volume monolayer containers where a uniform tan colour masks post-consumer recyclate colour variation; for food or pharmaceutical contact, the finished article must pass the sector-specific migration protocol, and the concentrate carries no certification by itself.

    When Thermoformed Sheet Gauges Fall Below 1.5 mm, Pigment Agglomeration and Vacuum Holes Become Interdependent

    Across plug-assisted vacuum forming lines, thermoformed tan-coloured sheet for agricultural propagation trays and industrial dunnage packaging is produced on a single-screw sheet line where the concentrate is metered into the main feed port; the challenge shifts when draw depth and sheet gauge interact because pigment particles act as stress risers during plug-assisted forming. The applicable compliance matrix includes ISO 1133-1:2022 for melt flow characterization, ASTM D638-14 for tensile yield, ASTM D790 for flexural modulus, and EU Regulation 10/2011 for any food-contact propagation trays; industrial dunnage may only require a REACH declaration. A starting let-down ratio of 2–4 wt% is maintained for sheet from 0.8 mm to 4.0 mm, with the lower end used for deep-draw parts where thinning at corner radii must not reveal translucent patches; ratio verification is done by ash content testing per ISO 3451-1 or by X-ray fluorescence on the sheet. The extrusion process uses a barrier screw with 30:1 L/D and a melt pump to reduce pressure surge, with melt temperature at 220–240 °C, roll stack temperature at 70–90 °C, and take-off speed adjusted to maintain sheet thickness tolerance under ±3%. Thermoforming is run on a plug-assisted vacuum former with sheet surface temperature of 130–160 °C, plug material at 90–110 °C, and forming air pressure below 0.5 MPa for thin sheet; excessive let-down above 5 wt% is known to reduce hot tear resistance and increase pinhole formation at plug contact points. Terminal products include tan-coloured dunnage trays, agricultural propagation trays, stack-nest containers, and industrial packaging trays where colour stability under UV exposure is evaluated by ASTM D4329 UVA-340 accelerated weathering; the carrier selection of LLDPE rather than LDPE provides higher low-temperature impact for refrigerated handling but can exhibit higher shrinkage after thermoforming if the sheet is not normalized before trimming.

    Free Quote

    Competitive LyondellBasell POLYBATCH™ Tan LL60139/2 Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell POLYBATCH™ Tan LL60139/2 Concentrate Based In LLDPE is a solid polyolefin masterbatch formulated as a tan colour concentrate dispersed in a linear low-density polyethylene carrier resin. The product nomenclature identifies the carrier as LLDPE and the colour as tan, while LL60139/2 is the proprietary formulation code. The grade is supplied as free-flowing cylindrical pellets for gravimetric or volumetric dosing in polyolefin conversion lines. Specific pigment loading, melt mass-flow rate, ash content, and CIELAB coordinates are documented on the batch certificate of analysis; publicly available leaflets for this exact product code are limited, and generic masterbatch average data should not replace the CoA or safety data sheet. The product is intended for colouring polyethylene-based films, sheet, blow moulded parts, and injection moulded articles where a tan shade is required without introducing a second separate carrier polymer.

    Material Identity and Carrier Resin Characteristics

    The LLDPE carrier belongs to the polyethylene family described by ISO 1043-1:2011. Reference values for LLDPE-carrier masterbatches of this class normally place density between 0.910 g/cm³ and 0.940 g/cm³ when measured by ISO 1183-1:2019 or ASTM D792-20. Melt mass-flow rate for LLDPE carriers used in colour concentrates is commonly reported in the range 20–50 g/10 min at 190 °C under 2.16 kg load according to ISO 1133-1:2022 or ASTM D1238-20; however, product-specific values may fall outside this range and must be confirmed from the certificate of analysis. Differential scanning calorimetry per ISO 11357-3:2018 typically identifies the main melting endotherm of an LLDPE carrier between 120 °C and 128 °C. Bulk density of pelletised masterbatch is generally within 0.50–0.70 g/cm³ by ASTM D1895-17 Method A. Residual moisture in sealed original packaging is normally below 0.10% by weight when tested by ISO 15512:2019. These ranges are reference values for the carrier class, not guaranteed product specifications.

    Reference carrier-resin properties for LLDPE-based masterbatches
    PropertyReference rangeTest method
    Density0.910–0.940 g/cm³ISO 1183-1:2019, ASTM D792-20
    Melt mass-flow rate20–50 g/10 min at 190 °C/2.16 kgISO 1133-1:2022, ASTM D1238-20
    Melting endotherm120–128 °CISO 11357-3:2018
    Bulk density0.50–0.70 g/cm³ASTM D1895-17 Method A
    Moisture content<0.10%ISO 15512:2019

    How Does the LLDPE Carrier Influence Dilution and Processing?

    Letdown ratio is determined by wall thickness, colour target, hiding power, and process residence time. For blown film, a starting letdown of 2–5 wt% is common; cast film and sheet often begin at 3–6 wt%. Injection moulding may use 1–4 wt% depending on part thickness and pigment loading. On a single-screw extruder with 24:1 to 30:1 L/D, barrier screw, and Maddock mixing section, a melt temperature between 190 °C and 240 °C is normally sufficient to melt the LLDPE carrier and initiate pigment dispersion. Gravimetric feeders with dosing accuracy within ±0.1% should be used where colour drift must remain below 0.2 wt%. The concentrate should be stored in sealed containers at ≤60% RH; if moisture uptake occurs, pre-drying at 60–80 °C for 2–4 h in a desiccant dryer is recommended before processing. Melt residence time above 10 min at 240 °C should be avoided because thermo-oxidative degradation of the polyethylene carrier can shift the tan shade and generate volatile by-products.

    Dispersion quality on production lines can be evaluated by pressure rise across a 200-mesh screen pack. On a 60 mm single-screw extruder running near 80 kg/h, a pressure increase above 1.0 bar/h may indicate pigment agglomerates or poorly dispersed filler above the screen aperture. The concentrate may show visible streaking if melt temperature is below 190 °C or if the screw has low mixing intensity. High-shear dispersion is necessary for inorganic tan pigments, but excessive shear above 240 °C can degrade the polyethylene carrier and lower melt strength. Extruders with grooved feed zones may generate high feed-zone pressures, and feeder bridging should be monitored because pellet bulk density and surface friction influence gravimetric accuracy.

    Thermal Stability Is Limited by Carrier Unsaturation and Antioxidant System

    The LLDPE carrier is a saturated hydrocarbon backbone with terminal unsaturation; its melt stability depends on the antioxidant package. Short-term melt temperatures up to 260 °C are tolerated by many LLDPE-carrier masterbatches, but oxidative induction time measured at 200 °C by ASTM D3895-19 should be used to confirm residual stabiliser activity if regrind or long residence conditions are planned. OIT values below 20 min can indicate that the carrier stabiliser has been consumed, increasing the risk of yellowing and molecular-weight reduction. The concentrate should not be processed in polymers requiring melt temperatures above 260 °C, such as polycarbonate or polyethylene terephthalate, because the LLDPE carrier may degrade before the host resin is fully molten. Purging with a low-viscosity polyethylene transition resin after shutdown is recommended, and heat-soaked surfaces above 240 °C should be cleaned before restart to avoid crosslinked gel formation.

    Colourimetric Performance and Metameric Control Are Defined by Pigment Type and Illuminant

    Tan shades in polyolefin masterbatches of this class are generally produced with blends of iron oxide and titanium dioxide, possibly with small additions of organic or carbon-based pigments to adjust lightness and undertone. The exact pigment composition for Polbatch™ Tan LL60139/2 is not publicly disclosed. Colourimetric evaluation should be performed according to ISO 11664-4:2008 using D65 illuminant, 10° standard observer, and d/8° integrating sphere geometry as referenced in ISO 11664-2:2007. A CIELAB ΔE*ab tolerance of ≤0.5–1.0 is typical for critical colour control, but the acceptable limit depends on the application. Metameric failure must be checked under at least D65, A, and cool white fluorescent lighting; visual evaluation should follow ISO 3664:2009. Published colour coordinates for this specific grade are limited, so incoming QA should use the batch CoA and verify colour on a laboratory-scale dispersion or production sample rather than relying on pellet colour alone.

    The LLDPE carrier differentiates this concentrate from EVA-based universal masterbatches. EVA carriers commonly have melt flow rates of 30–60 g/10 min per ISO 1133-1 and lower melt temperature, but they can generate more screw slip in grooved-barrel extruders and may contribute to plate-out at high processing temperatures. The LLDPE carrier provides closer melt-viscosity matching with LLDPE and LDPE host resins, reducing interfacial distortion and improving dispersion under high shear. The trade-off is that the LLDPE carrier may require a longer melting length and higher backpressure in injection moulding; on reciprocating-screw machines with 20:1 to 24:1 L/D, backpressure of 10–30 bar melt pressure is often used to obtain uniform tint. In blown film, grade compatibility with the host polyethylene is usually better than with wax-based or EVA-based carriers, but letdown ratios above 5 wt% can still alter film surface roughness and coefficient of friction.

    When Letdown Ratios Fall Below 2 wt% in Thin-Gauge Film

    For films below 25 µm, the low final pigment concentration makes colour control highly sensitive to feeding error. Gravimetric dosing is required; volumetric dosing may allow drift of more than 0.2 wt%, producing visible shade variation across a reel. The LLDPE carrier should be fully melted before the final mixing zone, otherwise micro-streaks can form. Blown film lines with 60 mm grooved-barrel extruders and 30:1 L/D barrier screws have experienced screw slip at letdown ratios above 5 wt% when melt temperature is below 190 °C, while at low letdown ratios below 2 wt%, feeder accuracy and pellet size distribution become the dominant variables. Film haze should be measured by ASTM D1003-21, and gloss by ASTM D2457-21. If the concentrate introduces large agglomerates, film specks can be counted by incident light at 100× magnification. Screen packs with 200-mesh aperture remove only larger gels and agglomerates; they do not correct sub-10 µm pigment dispersion defects. For thin films, coefficient of friction may shift upward at high letdown because pigment particles at the film surface alter surface roughness; COF should be checked by ISO 8295:2004 if the film is used in form-fill-seal or bagging equipment. Heat seal initiation temperature may also shift with high pigment loading, and seal strength should be verified by ASTM F1921-20.

    Starting-point processing envelope for LLDPE-carrier tan concentrates
    ProcessTypical letdown ratioMelt temperatureEquipment note
    Blown film2–5 wt%190–230 °C24:1–30:1 L/D single-screw with barrier screw
    Cast film/sheet3–6 wt%200–240 °C30:1 L/D single-screw with vacuum vent
    Injection moulding1–4 wt%200–250 °C20:1–24:1 L/D reciprocating screw
    Blow moulding2–4 wt%190–230 °C24:1 L/D single-screw

    The concentrate is intended for industrial polymer processing and is not supplied as a food-contact article. The LLDPE carrier may be manufactured from materials complying with FDA 21 CFR 177.1520 for olefin polymers, but finished articles intended for food contact must be evaluated under EU No 10/2011 and the applicable FDA migration limits, not from carrier compliance alone. Heavy metal content should be verified against RoHS Directive 2011/65/EU Annex II by XRF screening per IEC 62321-3-1:2013 or ICP-OES per ISO 11885:2007. REACH Article 33 declarations for SVHC above 0.1 wt% should be obtained from the safety data sheet. Storage should be maintained at ≤40 °C, ≤60% RH, and away from direct ultraviolet light. If the product is stored beyond the recommended shelf life or exposed to high humidity, it should be re-dried and re-tested for melt mass-flow rate, moisture, and colour before production use.

    Processing variances observed on production lines with this carrier class typically arise from four sources: feeder accuracy, moisture uptake, melt temperature heterogeneity, and screen-pack blinding. On a 75 mm blown film line running a 100 kg/h output, a 0.1 wt% feeder deviation can produce a measurable ΔE*ab shift when the letdown ratio is below 2 wt%. The use of a continuous gravimetric feeder with mass-flow validation per ISO 10012:2003 is therefore recommended. If screen pressure rises more than 2.0 bar/h, the screen pack should be changed and the melt temperature profile checked for cold zones below 190 °C. Avoid blending this concentrate with amine-based additives that can react with certain pigment surface treatments, as shade shift may occur; compatibility should be confirmed by laboratory dispersion trials before full-scale production.

    Top