| HS Code | 708643 |
| Productname | LyondellBasell POLYBATCH™ Red LL50283/3 Concentrate Based In LLDPE |
| Manufacturer | LyondellBasell |
| Producttype | Color concentrate / masterbatch |
| Carrierresin | Linear Low Density Polyethylene (LLDPE) |
| Color | Red |
| Form | Pellets |
| Compatibility | Polyolefins, especially polyethylene |
| Recommendedletdownratio | 2-5% (typical) |
| Processingmethods | Extrusion, injection molding, blow molding, film |
| Density | 1.10 g/cm³ (typical) |
| Meltflowrate | 20 g/10 min (190°C/2.16 kg, typical) |
| Pigmentcontent | 50% (typical) |
| Moisturecontent | <0.10% (typical) |
| Thermalstability | Up to 260°C |
| Lightfastness | 7 (Blue Wool scale, typical) |
| Weatherfastness | 4 (typical) |
| Processingtemperature | 180-240°C |
| Shelflife | 24 months |
| Storagetemperature | Below 30°C |
| Packaging | 25 kg bags |
As an accredited LyondellBasell POLYBATCH™ Red LL50283/3 Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Supplied in 25 kg polyethylene-lined bags, palletized at 40 bags per 1,000 kg pallet, stretch-wrapped for transport. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with LyondellBasell POLYBATCH™ Red LL50283/3 concentrate in LLDPE, palletized, shrink-wrapped, and securely stowed for transport. |
| Shipping | LyondellBasell POLYBATCH™ Red LL50283/3 Concentrate Based In LLDPE is normally shipped as non-hazardous, solid plastic pellets in sealed bags, boxes, or octabins. It is not regulated as dangerous goods for transport. Keep dry, cool, and away from heat/contamination. Verify current SDS before shipping. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep containers tightly closed to prevent moisture and contamination. Use original packaging and avoid prolonged storage at elevated temperatures. Maintain good housekeeping to prevent dust accumulation. Store separately from incompatible materials. Follow local regulations and the manufacturer’s SDS. |
| Shelf Life | Shelf life: 24 months from manufacture if stored unopened in original packaging, cool, dry, and protected from direct sunlight. |
On a three-layer coextrusion blown film line producing 50 µm–80 µm red-tinted liners and overwraps, LyondellBasell POLYBATCH™ Red LL50283/3 Concentrate Based In LLDPE is dosed gravimetrically into the outer layer at 2.5% to 4.0%, while the core and skin layers run unpigmented LLDPE/LDPE blend. Barrel temperature profile is set from 175 °C at the feed throat to 210 °C at the die adapter, with die temperature maintained at 205 °C to 215 °C. A die gap of 1.8 mm to 2.2 mm and a blow-up ratio of 2.2:1 to 2.8:1 are used; frost-line height is held at 350 mm to 450 mm above the die face to balance bubble stability and cooling. Dispersion quality is checked on-line by monitoring pressure drop across a 100/200/100/40 mesh screen pack; a pressure rise of more than 12% above the clean-screen baseline over a 4 h tracking period indicates pigment agglomerate accumulation and triggers a screen change before die-lip plate-out transfers to the film. Film colour uniformity is evaluated against a CIEDE2000 reference; a total colour difference ΔE00 of ≤0.8 across the web width is specified for print-accurate red packaging. Tensile properties after pigment addition are measured per ASTM D882; typical MD/TD tensile strength at break for 60 µm LLDPE film falls between 25 MPa and 35 MPa, and thorough dispersion is required to avoid lower tearing resistance at pigment agglomerate boundaries. If surface condensation has occurred during warehouse storage, the concentrate is pre-dried at 70 °C to 80 °C for 2 h using a desiccant dryer with dew point below -30 °C before feeding. Addition to polymers containing high levels of migratory slip agents above 1500 ppm erucamide is not recommended without an extended plate-out trial, because low-molecular-weight amides can carry red pigment to the die lip under high shear; published data for this specific product configuration is limited, so a 8 h continuous trial is used to verify performance before commercial film production.
In thin-wall injection moulding of high-density polyethylene closures and caps, the concentrate is introduced at 1.5% to 3.0% by gravimetric dosing at the hopper throat. A reciprocating screw with 24:1 L/D and non-return valve is operated at 80 rpm to 120 rpm; barrel temperatures are profiled from 200 °C to 230 °C, with nozzle temperature not exceeding 240 °C. Mould temperature is controlled at 10 °C to 25 °C, and injection pressure typically falls between 70 MPa and 100 MPa for polyolefin caps depending on wall thickness and gate design. Gate blush is the main process risk: in hot-runner moulds with tunnel gates of diameter 0.8 mm to 1.2 mm, excessive pigment concentration or poor distributive mixing can produce a grey-red halo at the gate, measured visually against a reference plate under D65 illumination. If gate blush appears, the first corrective step is to increase melt temperature by 5 °C increments to 235 °C, not to exceed 240 °C. If blush persists, the letdown ratio is reduced to 1.2% and a higher pigment-strength concentrate is recommended. Mould deposit testing is performed by running 5000 cycles and inspecting the cavity vent lands at 30× magnification; red pigment plate-out at the vents indicates excessive shear or inadequate carrier compatibility. Shrinkage and warpage are evaluated per ISO 294-4; a pigment-induced differential shrinkage of 0.3% or greater across the flow direction should trigger a filling-pattern adjustment. For food-contact cap applications, compliance must be confirmed against EU 10/2011 specific migration limits and FDA 21 CFR 178.3290 colourant provisions using product-specific documentation; this document does not establish global food-contact status.
| Processing route | Letdown range | Melt temperature | Critical control point |
|---|---|---|---|
| Blown film outer layer | 2.5%–4.0% | 190 °C–215 °C | Screen-pack pressure rise < 12%; web ΔE00 ≤ 0.8 |
| Thin-wall injection moulding | 1.5%–3.0% | 200 °C–230 °C | Gate blush absent; vent plate-out absent after 5000 cycles |
| Extrusion blow moulding | 1.0%–2.5% | 190 °C–210 °C | Weld-line streak depth less than 0.05 mm |
| Pipe coextruded stripe | 6%–12% | 190 °C–220 °C | Stripe die pressure < 25 MPa; no interfacial waviness |
| Sheet extrusion | 2%–4% | 210 °C–230 °C | Roll-stack plate-out absent after 4 h; ΔE00 ≤ 0.7 |
| Cable sheathing | 2%–5% | 170 °C–200 °C | Spark-test defects absent at 6 kV–10 kV |
Extrusion blow moulding of red-tinted containers uses lower addition levels than film because the parison is formed under low shear and layered melt streams are not available to dilute concentrated pigment. In shuttle and reciprocating blow moulding machines running HDPE or LLDPE-rich caps, the concentrate is dosed at 1.0% to 2.5% by weight; melt temperature settings at the die head are held between 190 °C and 210 °C, with accumulator-head drool avoided. Weld lines from the parison pinch-off and neck flash are the primary visual defects: they appear as darker red seams when the parison is cooled below 170 °C before mould closing, or when the die gap is below 1.5 mm. The mandrel and bushing land length must be longer than 12 mm for uniform colour distribution; shorter land lengths leave longitudinal streaks on the container. Drop impact performance after colour addition is checked per ASTM D2463-15 on 500 mL bottles at 23 °C; no brittle failure mode should replace ductile deformation as the impact speed increases from 2 m/s to 4 m/s. For non-food containers used in agricultural chemical packaging, the coloured wall is subjected to stress-crack resistance testing per ASTM D1693 in a 10% Igepal CO-630 solution at 50 °C. If the red concentrate is to be used in a multi-layer bottle with a post-consumer recycled middle layer, the outer layer must remain above 0.25 mm to prevent colour bleed-through; published data for this specific product configuration is limited, so a 24 h migration contact test is recommended before production approval.
For coextruded high-density polyethylene conduit or pressure pipe where a red identification stripe is required, the concentrate is fed to a dedicated stripe extruder with screw diameter 25 mm to 45 mm and an L/D of 24:1. Because the stripe layer is typically only 0.10 mm to 0.20 mm thick, letdown ratios in the stripe extruder are significantly higher—commonly 6% to 12%—to achieve visible colour in a thin layer, while the core pipe remains unpigmented or black. Melt temperature in the stripe extruder is controlled between 190 °C and 220 °C; temperatures above 230 °C may cause rheological mismatch between the high-pigment stripe compound and the main pipe melt, resulting in die-lip flow instability. The stripe die is a flat or hemispherical coextrusion insert with land length 5 mm to 8 mm; pressure in the stripe channel is monitored and should remain below 25 MPa to avoid interfacial waviness. Colour fastness in outdoor service is tested under ISO 4892-2 method A, cycle 1, using a xenon arc lamp with 0.51 W/m² @ 340 nm; a blue wool scale rating of 7 or greater after 1000 h is generally required for red identification stripes on above-ground conduit, but product-specific data must be requested to confirm this concentrate's lightfastness. Dimensional stability of the pipe is assessed per ISO 2505; the addition of a small stripe layer should not change longitudinal reversion by more than 0.5% at 110 °C. For potable-water contact, compliance with AS/NZS 4020 or KTW-BWGL may be required depending on the target market; red concentrate is placed only in a non-contact stripe or covered by a clear cap layer unless approved test data is available.
| Requirement area | Reference | Verification responsibility |
|---|---|---|
| Food-contact plastic colourants | FDA 21 CFR 178.3290 | Supplier documentation for extraction and end-use composition |
| EU plastics food-contact | EU 10/2011 | Overall migration and specific migration testing on final article |
| Electrical/electronic heavy metals | RoHS Directive 2011/65/EU Annex II | Supplier declaration of conformity with maximum concentration values |
| Weatherability for outdoor articles | ISO 4892-2 | Product-specific exposure and colour fastness test per target service life |
| Melt flow rate of carrier | ISO 1133-1:2022 | Incoming quality control at 190 °C/2.16 kg |
In sheet extrusion for red thermoformed trays and packaging inserts, the concentrate is let down at 2% to 4% in a single-screw extruder with screw diameter 75 mm to 120 mm and L/D 32:1, feeding a coat-hanger die. Melt temperature at the die is maintained at 210 °C to 230 °C, and the polished three-roll stack is set at 40 °C to 60 °C with a roll gap corresponding to sheet thickness plus 5% for cooling shrinkage. Red pigment plate-out on the middle and lower chill rolls is the most frequent production issue; it appears as pink film transfer after 2 h to 4 h of continuous running when the concentrate dispersion is poor or when the melt temperature is below 200 °C. Roll release can be improved by adding a polyethylene wax masterbatch at 0.5% to 1.0%, but this must be tested for haze development per ASTM D1003. Sheet colour variation across width is quantified using a spectrophotometer with D65 illuminant and 10° observer; ΔE00 should remain below 0.7 across the sheet width for solid red trays. Thermoforming trials are run on a contact-heat machine at sheet surface temperatures of 150 °C to 170 °C; wall-thickness reduction in corners must not drop below 60% of original sheet thickness, and red colour should not shift visibly after 20 s of heating. For food trays, the coloured sheet is tested for overall migration per EN 1186-3 using 95% ethanol and 40 °C for 10 days if fatty-food contact is claimed; specific migration of any colourant decomposition products must be confirmed before commercial supply.
In LLDPE jacketing compounds for red-sheathed power or telecommunication cables, the concentrate is dosed at 2% to 5% at the throat of a single-screw extruder with L/D 24:1 to 30:1, coupled to a pressure die with tubular tip and die land 10 mm. Melt temperature is kept between 170 °C and 200 °C to avoid premature crosslinking in peroxide-containing formulations if the compound is silane-grafted; for silane-crosslinked LLDPE wire coating, a peroxide-free silane masterbatch is used and red colour is added at 2% to 3%. The line speed for sheathing is controlled at 150 m/min to 300 m/min, depending on conductor diameter; spark testing per IEC 62230 at 6 kV to 10 kV detects insulation defects, and colour spots larger than 0.5 mm are grounds for rejection. In coloured cable sheathing, carbon black is generally absent, so UV resistance relies on hindered amine light stabilisers; the red pigment's lightfastness is assessed under ISO 4892-2 with 0.85 W/m² @ 340 nm and 2000 h exposure for outdoor-rated cables. For flame-retardant cable compounds containing metal hydroxides above 60 phr, the carrier dilution effect must be accounted for: at 3% concentrate addition, the polymer content is reduced by roughly 1.5%, which may affect oxygen index by less than 0.5 percentage points but should be verified per ISO 4589-2 before batch sign-off.
Competitive LyondellBasell POLYBATCH™ Red LL50283/3 Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell POLYBATCH™ Red LL50283/3 Concentrate Based In LLDPE is a pelletized color concentrate supplied in a linear low-density polyethylene carrier. The product is intended for let-down into polyethylene-based film, sheet, and injection moulding operations where a red shade is specified without the addition of wax or EVA-derived polar binder systems. The carrier is characterized by a density of 0.918–0.925 g/cm³ at 23 °C under ASTM D792; the melt mass-flow rate of the carrier is lot-specific and is reported on the certificate of analysis using ASTM D1238. Pigment loading is not a fixed nominal value for this shade; batch-specific colorant concentration and heavy metal content are stated in the technical data sheet and safety data sheet. Processors should use the lot certificate to set the initial let-down ratio and then verify shade development by laboratory drawdown or pilot extrusion.
Because the concentrate is based in LLDPE, it is not a universal carrier system for PET, polyamide, or polycarbonate. The LLDPE carrier phase remains immiscible with those matrices and can produce specking, delamination, and pigment pooling at the interface. In polyolefin coextrusion or monolayer polyethylene, the carrier contributes to the total polyethylene fraction and must be included in final part composition calculations for food-contact compliance and recycled-content declarations.
The selection of an LLDPE carrier rather than a low-viscosity wax or lower-molecular-weight polyolefin changes the dispersion mechanism during final dilution. In a single-screw extruder with a barrier screw, the LLDPE carrier remains in the compacted solid-bed region for a longer fraction of the screw length before melting, transferring mechanical energy to the pigment aggregates as a compressive stress rather than as a purely viscous shear force. On production-scale lines using 30:1–40:1 L/D single-screw extruders with mixing pins, the concentrate should be introduced through the main feed throat with the virgin resin, not through a side stuffer, unless the side stuffer is positioned upstream of the first mixing section. Observations on 75 mm cast-film extruders have shown that feed-throat addition reduces red streak defects compared with split feeding when the let-down ratio is below 2%.
The LLDPE carrier has a lower zero-shear viscosity than LDPE at equivalent melt index, but its melt strength is also lower. In blown film, this lowers bubble stability when the concentrate is used at addition rates above 5%. Frost-line height and internal bubble cooling pressure should be adjusted to compensate for the reduced elongational viscosity of the LLDPE carrier. The melt is not shear-sensitive in the way a PVC-based colorant is, but the organic red pigment system can form agglomerates if dead-flow zones are present in the die adapter or if screen-pack sealing is uneven.
Plate-out is most frequently observed as red deposit formation on the die lip, air ring, or screen pack after prolonged running. The concentrate is processed within a melt temperature envelope of 193–232 °C for film grades and 216–249 °C for injection moulding grades. Melt temperatures above 250 °C should be avoided for runs longer than 4 h, because the organic red pigment may partially decompose and shift shade toward a yellower red. Screw configurations with low-shear compression ratios of 2.0:1–2.5:1 and no high-intensity Maddock mixers are preferred; if a Maddock mixer is present, the clearance should not be below 0.25 mm.
When a grooved-barrel feed section is used, the LLDPE carrier may generate higher melt pressure at low screw speeds than a low-molecular-weight carrier. Specific energy input should be logged, because color strength can shift if screw speed is changed more than 15% from the validated run. At screw speeds above 120 min⁻¹ on a 75 mm grooved-barrel extruder, the concentrate can experience local temperature spikes above the set zone because of viscous dissipation in the high-compression section. These temperature spikes are not always visible on melt thermocouples and may produce a red shade drift toward a blue-red.
| Process | Typical let-down ratio | Melt temperature | Equipment note |
|---|---|---|---|
| Monolayer cast film | 2–4% | 204–232 °C | Screen pack 40/80/100 mesh; backpressure monitored below 35 MPa |
| Blown film, HDPE/LLDPE blend | 1–3% | 193–221 °C | Frost-line height and bubble cooling adjusted for LLDPE carrier |
| Injection moulding closures | 1.5–3% | 216–249 °C | Hot-runner manifold below 240 °C; clamp force 150–250 t |
| Sheet and thermoforming | 2–5% | 199–227 °C | Gear pump inlet pressure below 10 MPa |
Dosing accuracy at low addition rates remains a process-critical variable. Gravimetric batch blenders should be calibrated with a pre-weighed shot of concentrate to confirm a dosing repeatability of ±0.1% of total feed. Volumetric dosing on single-screw extruders is less desirable below 2% addition because bridging can occur in the hopper throat; polyethylene pellets with a bulk density of 0.52–0.60 g/cm³ are free-flowing, but concentrate pellets may become sticky above 35 °C in unventilated mezzanines.
In injection moulding of closures and overcaps, the concentrate is dry-blended at the machine throat. The LLDPE carrier melts with the base polyethylene, but the absence of a polar binder means the pigment is not predisposed to separate into the weld-line region by migration; instead, weld-line visibility depends on particle dispersion and pigment orientation. Moulds with hot runners should maintain manifold temperatures below 240 °C and avoid dead spots longer than 4 times the runner diameter. On high-speed packaging closures moulded on 250 t machines with 32-cavity hot runners, the concentrate can be used at 2% to achieve process-stable red under 12 s cycle times.
If post-industrial regrind contains even 0.5 wt% of polyethylene terephthalate, polyamide, or polystyrene, the LLDPE carrier in LL50283/3 will not compatibilize these domains. The incompatible polymer particles create visible specks in film and can concentrate red pigment at the interface, producing dark striations. The product should not be used in PET, polyamide, or polycarbonate matrices. In mixed polyolefin streams containing up to 10% polypropylene, the LLDPE carrier generally disperses without gross delamination because the processing temperatures overlap, but toughness and seal performance of the final article must be re-qualified under ASTM F88/F88M for seal strength and ASTM D638 for tensile yield stress.
Compared with an LDPE-carrier red concentrate of equal visible color strength, LL50283/3 usually produces a lower-pressure drop across a given screen pack because the linear backbone promotes shear thinning under high die shear. In comparative production trials on a 60 mm blown-film die with a 1.8 mm die gap, screen pressure rise was observed to be 0.7–1.2 MPa lower after 6 h at 210 °C than with an LDPE carrier of comparable melt index. Against EVA-carrier concentrates, the absence of vinyl acetate reduces plate-out on the air ring and lowers acetic acid formation during prolonged die-lip hold times. However, EVA carriers provide better adhesion to polar barrier layers in some coextrusion structures; LL50283/3 is not the primary choice for tie-layer pigmentation where high acid-anhydride content is required.
For high-clarity thin-gauge film below 30 μm, red concentrates based on a wax or low-molecular-weight carrier often reduce visible haze but increase migration risk. LL50283/3 is not a high-clarity grade; haze values in the final film are controlled primarily by the base resin and processing conditions. Optical testing per ASTM D1003 should be performed on the final article because haze contribution from the pigment is nonlinear with film thickness. Some conversion lines have reported absolute haze shifts of 1.0–2.5% at 25 μm at a let-down ratio of 2%; however, published data for this specific configuration is limited. The concentrate should be evaluated with a full factorial design that includes chill-roll temperature, die-lip land length, and screen-pack construction.
Die-lip build-up is controlled more by low-molecular-weight pigment dispersion aids than by carrier selection alone. If plate-out increases above an acceptable level, the screen pack should be inspected for bypass and the melt temperature profile checked for hot spots above 240 °C. The die-lip land should be conditioned; the use of abrasive purging compounds is not recommended because abrasive purge can open the die gap and shift gauge distribution.
Before commercialization, the final article must be evaluated under the applicable regulatory framework. The concentrate itself is not a food-contact article; compliance is determined on the finished plastic article after dilution at the intended let-down ratio.
| Standard / Regulation | Parameter or scope | Relevance |
|---|---|---|
| ASTM D1238 | Melt mass-flow rate of LLDPE carrier | Incoming lot release |
| ISO 1133-1:2022 | Melt mass-flow rate and melt volume-flow rate | Cross-laboratory repeatability |
| ASTM D792 | Carrier density | Blending calculations |
| FDA 21 CFR 178.3290 | Colorants for polymers | Indirect food-contact suitability if final article meets extractives limits |
| Commission Regulation (EU) No 10/2011 | Overall migration and specific migration limits | Food-contact compliance in the EU; overall migration ≤ 10 mg/dm² |
| REACH Regulation (EC) No 1907/2006 | SVHC identification and Annex XVII restrictions | Supply chain due diligence |
| RoHS Directive 2011/65/EU | Restricted heavy metals and flame retardants in articles | Electrical and electronic articles only |
Storage in original, sealed packaging at 10–30 °C and below 65% RH is sufficient. Because the LLDPE carrier is not hygroscopic, predrying is not required under normal conditions. If condensation forms on cold pellets after warehouse-to-production transfer at high relative humidity, the pellets may be dried at 60–70 °C for 2–4 h using a desiccant dryer. Avoid over-drying above 80 °C or residence times beyond 6 h, which can cause surface softening and hopper bridging.