| HS Code | 102071 |
| Product Name | LyondellBasell POLYBATCH™ Opaque Blue 40356 Concentrate Based In LLDPE |
| Manufacturer | LyondellBasell |
| Brand | POLYBATCH™ |
| Product Code | 40356 |
| Product Type | Color Concentrate / Masterbatch |
| Carrier Resin | Linear Low Density Polyethylene (LLDPE) |
| Color | Blue |
| Opacity | Opaque |
| Form | Pellets |
| Compatibility | Polyolefins including LLDPE, LDPE, HDPE, and PP |
| Processing Methods | Extrusion, Injection Molding, Blow Molding |
| Recommended Let Down Ratio | 2% to 5% (typical) |
| Density | 1.12 g/cm³ (typical) |
| Melt Flow Rate | 15 g/10 min (190°C/2.16 kg, typical) |
| Pigment Content | 50% (typical) |
| Moisture Content | <0.1% (typical) |
| Heat Stability | Up to 260°C (typical) |
| Lightfastness | 7 (Blue Wool Scale, typical) |
| Storage Conditions | Dry, below 30°C |
| Shelf Life | 2 years |
As an accredited LyondellBasell POLYBATCH™ Opaque Blue 40356 Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell POLYBATCH™ Opaque Blue 40356 Concentrate is packaged in 25 kg polyethylene bags, palletized, stretch-wrapped, and labeled for industrial shipment. |
| Container Loading (20′ FCL) | 20′ FCL loaded with palletized LyondellBasell POLYBATCH™ Opaque Blue 40356 Concentrate Based In LLDPE, 25 kg bags, shrink-wrapped and secured. |
| Shipping | LyondellBasell POLYBATCH™ Opaque Blue 40356 Concentrate Based In LLDPE is typically shipped as a non-hazardous solid masterbatch in moisture-resistant bags or cartons, palletized and shrink-wrapped. Use standard freight; not normally regulated as dangerous goods. Store cool, dry, away from direct sunlight. Confirm current SDS. |
| Storage | Store POLYBATCH™ Opaque Blue 40356 Concentrate in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep original containers tightly closed on pallets, off the floor, and protected from moisture, dust, and contamination. Avoid excessive stacking or physical damage. Rotate stock first-in-first-out. Follow the manufacturer’s SDS and applicable local storage regulations. Store at moderate ambient temperature. |
| Shelf Life | Recommended shelf life is 24 months from manufacture when stored unopened in a dry, cool place, protected from direct sunlight. |
During blown film conversion of LLDPE-rich monolayer structures, LyondellBasell POLYBATCH™ Opaque Blue 40356 Concentrate Based In LLDPE is metered at the extruder throat through a gravimetric dosing unit into a host resin with melt flow index 0.8–2.0 g/10 min at 190 °C under 2.16 kg load per ISO 1133-1:2022. Letdown is held at 1.5–3.0 wt% for film gauges of 25–120 µm; below 40 µm, the 1.5–2.0 wt% range is preferred to limit pigment agglomerates and die-lip deposit on lines fitted with 80/100/120 mesh screen packs. Processing uses a single-screw extruder with 24:1–30:1 L/D, barrel profile 180–210 °C, and die 210–230 °C; blow-up ratio is set between 2.0:1 and 3.5:1. Light transmission of the pigmented film is measured per ASTM D1003-13; because the concentrate contains a high pigment loading in an LLDPE carrier, final optical density is a function of film thickness, letdown ratio, and frost-line cooling rate. The concentrate is not hygroscopic under sealed storage; bags opened at relative humidity above 60% should be pre-dried at 60–70 °C for 2 h in a desiccated-air hopper, while pre-drying above 80 °C should be avoided to prevent pellet surface melting and hopper bridging. Terminal non-food structures include opaque blue collation shrink film, freezer film, and heavy-duty shipping sacks; direct food-contact use requires lot-specific migration testing under EU 10/2011 Annex I and Annex V with an overall migration limit of 10 mg/dm², carrier resin assessment under 21 CFR 177.1520(c), and colorant compliance with 21 CFR 178.3297. A documented operational boundary is that the LLDPE carrier can reduce machine-direction tear propagation measured by ASTM D1922; comparative tear trials at 1.5 wt% and 3.0 wt% letdown are necessary before fixing the formulation.
In cast film extrusion, the same concentrate is exposed to higher melt temperature and shorter residence time than in blown film, and letdown is typically reduced to 1.5–2.5 wt% for film thicknesses of 20–60 µm. The extruder is a single-screw machine with 30:1 L/D, barrel profile 200–240 °C, and a flat die with die gap 0.5–0.8 mm; the chill roll is maintained at 15–25 °C to freeze the LLDPE carrier before pigment particles can re-agglomerate. Die-lip deposit and streaking are the principal failure modes observed on production lines; increasing filtration to 100/120/150 mesh and reducing screw speed are more effective than increasing letdown when hue strength is insufficient. The terminal non-food articles are blue-tinted cast stretch film, hygiene packaging overwrap, and temporary surface-protection film. For food-contact converters, the final printed or laminated structure must comply with EU 10/2011 Annex II for plastic materials and 21 CFR 177.1520(c) for the PE carrier, but lot-specific documentation for the complete formulation is required. Because cast film can run at line speeds of 200–400 m/min, masterbatch particle size and carrier melt index must be matched to the host resin to avoid melt-pressure fluctuation at the feed throat; published lot-specific data for this product in ultra-thin film below 20 µm is limited, so a line trial at 1.5 wt% is required before commercial conversion.
For injection moulded blue caps and closures, the masterbatch is pre-blended by low-speed tumble mixing at 15–30 rpm for 10–15 min before gravimetric dosing into the machine feed throat. Letdown is generally 2.0–3.5 wt%; the host resin is HDPE or LLDPE with melt flow index of 4–20 g/10 min at 190 °C under 2.16 kg per ISO 1133-1:2022. Melt temperature is maintained at 200–230 °C and nozzle temperature at 210–240 °C; mould temperature is controlled between 15 °C and 30 °C for caps and closures with wall sections of 1.0–2.5 mm. Gate diameter is not reduced below 1.0 mm because small gates increase shear heating and can produce gate blush and flow lines around the hinge. The terminal articles are cosmetic tube closures, dispensing caps for household and industrial chemicals, and tamper-evident pail lids. Compliance for non-food closures falls under REACH and EU 94/62/EC heavy-metal limits; food-contact closures require migration testing under EU 10/2011 and 21 CFR 177.1520(c) plus colorant conditions under 21 CFR 178.3297. The dispersed pigment can act as a nucleating agent in polyolefins, and post-moulding shrinkage should be compared at 2.0 wt% and 3.5 wt% letdown on the production tool before dimensional capability is accepted.
| Jurisdiction / Use | Reference standard or regulation | Typical limit or test requirement | Assessment status for LLDPE-based concentrate |
|---|---|---|---|
| United States food-contact | 21 CFR 177.1520(c); 21 CFR 178.3297 | Carrier olefin polymer compliance; colorant clearance subject to conditions of use | Carrier assessed; lot-specific final article migration required |
| European Union food-contact plastics | EU 10/2011 Annex I, II, V | Overall migration 10 mg/dm²; 60 mg/kg for infant food articles | Final article responsibility; concentrate not directly food-approved |
| EU packaging waste | 94/62/EC with EC 1907/2006 REACH | Pb+Cd+Hg+Cr(VI) ≤ 100 mg/kg | XRF verification per lot recommended |
| Electrical and electronic equipment | 2011/65/EU RoHS Recast Annex II | Pb ≤ 1000 mg/kg; Cd ≤ 100 mg/kg | Relevant only if final EEE article is within scope |
| Potable water contact | NSF/ANSI/CAN 61 or BS 6920 | Extraction testing based on surface-to-volume ratio | Finished pipe/tank testing mandatory; concentrate does not provide approval |
Extrusion blow moulding uses a letdown of 2.0–4.0 wt% in HDPE homopolymer or copolymer with melt flow index 0.3–0.8 g/10 min at 190 °C under 2.16 kg (ISO 1133-1:2022). Barrel melt temperatures are maintained at 180–210 °C, while the die head is set at 190–220 °C; parison swell is typically 20–35% above the die gap for monolayer containers. The terminal articles are opaque blue HDPE bottles for personal care, household cleaning, and agrochemical products; the blue concentrate supplies sidewall opacity to mask fill-level variation and reduce transmission of visible light. Sidewall opacity is measured as luminous transmittance per ASTM D1003-13 at the specified wall thickness. Drop impact retention is evaluated by ASTM D2463-15; because dispersed pigment can act as a nucleating agent and modify crystalline morphology in HDPE, impact retention should be compared between unpigmented and pigmented containers at the specified letdown rather than assumed from resin datasheets. Compliance for non-food containers falls under REACH and 94/62/EC heavy-metal limits; food-contact bottles additionally require migration testing under EU 10/2011 and 21 CFR 177.1520(c) plus colorant compliance under 21 CFR 178.3297. A limitation is that the LLDPE carrier can reduce melt strength of HDPE slightly; on deep-draw containers above 4.0 wt%, parison sag may increase, so drop impact per ASTM D2463-15 and column crush per ASTM D2659-16 should be included in the line trial.
In extrusion coating and lamination onto paperboard, paper, or aluminium foil, the concentrate is added at 2.0–4.0 wt% to an LDPE/LLDPE blend with melt flow index of 4–15 g/10 min at 190 °C under 2.16 kg. The extruder is a 30:1–36:1 L/D single-screw machine with barrel temperatures from 280–320 °C; melt temperature at the adapter should not exceed 320 °C to avoid thermal hue shift and pigment degradation, and residence time should be kept below 10 min. Die-to-nip geometry is set to control draw-down and neck-in; chill-roll temperature is normally 15–25 °C, and corona pre-treatment of paperboard at 38–42 mN/m wetting tension is used before the molten web is applied. The terminal articles are opaque blue barrier wraps for non-food industrial packaging, paperboard cup outer layers, and coated paper for construction films. Because the LLDPE carrier contributes to draw-down and neck-in behaviour, the edge bead trim may increase with letdown; processors should measure neck-in at the specified line speed and adjust the deckle position accordingly. Food-contact laminates require the complete multilayer structure to meet EU 10/2011 overall migration limits and the PE layer to comply with 21 CFR 177.1520(c); heavy-metal content must remain within the 94/62/EC sum limit of 100 mg/kg for Pb, Cd, Hg, and Cr(VI).
| Conversion route | Indicative letdown | Melt barrel range | Critical equipment parameter | Typical failure mode |
|---|---|---|---|---|
| Blown film | 1.5–3.0 wt% | 180–210 °C | 80/100/120 mesh screen pack | Pigment agglomerates and die-lip deposit |
| Cast film | 1.5–2.5 wt% | 200–240 °C | 0.5–0.8 mm die gap; chill roll 15–25 °C | Streaking and melt-pressure fluctuation |
| Injection moulding | 2.0–3.5 wt% | 200–230 °C | Hot-runner pressure transducer; gate diameter ≥ 1.0 mm | Gate blush and dimensional drift |
| Extrusion blow moulding | 2.0–4.0 wt% | 180–210 °C | Parison swell 20–35%; die 190–220 °C | Parison sag and drop impact reduction |
| Extrusion coating | 2.0–4.0 wt% | 280–320 °C | Adapter melt ≤ 320 °C; residence time <10 min | Hue shift and neck-in increase |
| Pipe extrusion | 2.0–5.0 wt% | 190–230 °C | 30:1–38:1 L/D grooved-feed extruder | Reduced OIT and streaking |
HDPE water and industrial pipe extrusion applies the concentrate at 2.0–5.0 wt% into PE100 or PE80 pipe grades; the LLDPE carrier is melt-compatible with pipe-grade HDPE but does not replace the stabilizer package. A single-screw extruder with 30:1–38:1 L/D and grooved feed section is operated at 190–230 °C, with melt temperature and head pressure monitored at the breaker plate; screen packs of 60/80/100 mesh are placed upstream of the die to remove undispersed solids. Vacuum calibration sleeves control outer diameter and wall thickness; blue pigmentation must remain uniform enough to avoid visible streaking at wall sections above 2.0 mm. The terminal product is blue HDPE cold-water service pipe, compressed-air line, and cable duct; potable-water contact requires extraction testing to NSF/ANSI/CAN 61 in North America or BS 6920 in the United Kingdom, while local drinking-water approvals must be obtained for the finished pipe. Thermal stability of the finished pipe is assessed by oxidation induction time per ISO 11357-6:2018 at 210 °C; dispersed pigment can reduce OIT if stabilizer demand is underestimated, so a comparative OIT test between unpigmented and pigmented pipe compound is necessary before long-term use. A limitation is that the LLDPE carrier has lower modulus than pipe-grade HDPE; at the upper letdown of 5.0 wt%, slow crack growth resistance measured by ISO 13479 may shift, and published data for this specific blue concentrate in pressure-pipe formulations is limited, so long-term hydrostatic testing at 20 °C / 50 yr per ISO 9080 is recommended for pressure-rated service.
Competitive LyondellBasell POLYBATCH™ Opaque Blue 40356 Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell POLYBATCH™ Opaque Blue 40356 Concentrate Based In LLDPE is a pelletized color masterbatch formulated with an opaque blue pigment system dispersed in a linear low-density polyethylene carrier. The designation “Based In LLDPE” identifies the carrier polymer, not the final article composition. Published data for this specific configuration is limited; therefore lot-specific melt flow rate, pigment loading, and recommended letdown ratio should be obtained from the certificate of analysis or technical data sheet rather than inferred from general grade literature. The carrier class, however, imposes a processing and compatibility envelope that can be described from publicly available LLDPE behavior. Linear low-density polyethylene typically exhibits a melting peak of 120–128 °C when measured by ASTM D3418 or ISO 11357-3, and a density from 0.918–0.935 g/cm³ when tested according to ASTM D792 or ISO 1183-1. These values overlap with the thermal profile of most polyethylene film, sheet, and molding lines, which supports the use of an LLDPE carrier in polyethylene applications.
The product is supplied as free-flowing pellets. Pellet hardness and size uniformity are relevant in pneumatic conveying systems because fines generated during transfer can segregate in hopper corners and create localized color spikes. On production lines, such spikes appear as blue streaking at the die lip or as pigment agglomerates after the screen pack. The pigment system is not a single colorant; opaque blue concentrates of this class typically contain rutile titanium dioxide as a scattering phase and a blue organic pigment for selective absorption in the red-to-green portion of the visible spectrum. Titanium dioxide raises opacity through refractive index contrast, while the blue organic component controls chroma. If the TiO₂ loading is reduced while the blue pigment concentration is held constant, opacity falls sharply when film gauge drops below 50 µm. The exact pigment ratio for 40356 is not specified in this summary.
In the carrier selection decision, LLDPE is not a neutral diluent. Its melt-viscosity curve, melting range, and mechanical properties transfer to the final article. A polyethylene-compatible carrier reduces the probability of interfacial voids around pigment particles, which is a known cause of optical haze in thin film and of dart impact loss in film applications. If the carrier were replaced by a PP-based universal masterbatch, the difference in surface energy and melt-phase immiscibility could create inclusions that act as stress concentrators. If the carrier were LDPE rather than LLDPE, long-chain branching would contribute higher melt strength but lower tensile elongation and puncture resistance after letdown. The opaque blue 40356 product, by specifying LLDPE as the carrier, therefore addresses conversion environments where retaining film toughness and low-temperature performance is as important as achieving a particular blue shade.
Rheological matching between the concentrate carrier and the dilution resin controls the visual uniformity of the final article. If the carrier melt flow rate is too far below the matrix MFI, the masterbatch melts later in the screw and produces blue streaks in the metering zone. If it is too far above, channeling occurs and dispersion is incomplete. In LLDPE-carried concentrates, the shear-thinning behavior of linear polyethylene improves distribution in barrier screws with grooved feed sections, provided the feed-zone temperature is kept below the melting range. On high-speed blown film lines, the lower melt strength of LLDPE relative to LDPE can reduce bubble stability when the carrier addition rate is high; this is a line-design constraint rather than an intrinsic defect of the colorant. Operators commonly adjust die gap, frost line height, or internal bubble air pressure to compensate.
Compared with an LDPE-carried blue concentrate, the LLDPE vehicle contributes higher tensile strength and puncture resistance to the finished film, but may require a slightly higher melt temperature to fully plasticate at high throughput. Compared with a PP-carried masterbatch, the LLDPE carrier prevents gross incompatibility in polyethylene processing. In a thin-gauge LLDPE blown film, a PP-carried blue concentrate can produce visible gel-like defects, lower dart impact resistance, and poor heat-seal integrity because the PP domains do not crystallize in phase with the polyethylene matrix. That defect mechanism is not present when 40356 is let down into polyethylene because carrier and matrix share the same polymer backbone.
Production-scale compounding of an LLDPE-carried masterbatch typically occurs on co-rotating twin-screw extruders with L/D 36:1 to 48:1. The screw should contain at least one dispersive mixing block followed by a distributive mixing section. High-shear dispersion reduces primary pigment agglomerates, but the temperature rise across the mixing block must be monitored. Organic blue pigments can undergo shade drift under excessive energy input or extended residence time; titanium dioxide is thermally robust but may abrade and promote wear in screw elements and barrel liners. Melt filtration before pelletizing is common, with screen packs from 60/80/100 mesh to 80/100/120 mesh being typical. Finer screens remove agglomerates and contamination but increase melt pressure and residence time; if pressure upstream of the screen pack rises beyond the extruder operating limit, back-flushing or screen changes become necessary.
On the converter side, letdown is usually performed on single-screw machines. The LLDPE carrier melts at normal polyethylene processing temperatures, but insufficient mixing in a low-compression screw can leave undispersed pigment even when the pellets are fully molten. A barrier screw with a Maddock mixing section and a pressure transducer before the screen pack is preferred for accurate diagnosis. When the pressure drop across the screen pack fluctuates by more than 20 % from baseline, the cause is usually partial melting, screen fouling, or pigment agglomeration. Raising all barrel temperatures is not the recommended first response; selective adjustment of rear and feed-zone temperatures, along with verification of color feeder accuracy, can be more effective. Color concentrates of this class are commonly let down at 2–5 wt%, but optimum dosage must be established against the target opacity and article thickness. The given range is a general industrial window and not a 40356-specific value.
Ambient moisture can influence the feeding behavior of polyolefin masterbatches. At relative humidity above 60 % RH, surface moisture on pellets can generate steam during extrusion, producing porosity or surface defects. A drying step of 70–80 °C for 2–4 h is frequently applied to polyolefin masterbatches under humid storage conditions, but the relevant 40356 handling instruction should be consulted. Bags should not be left open between shifts in non-climate-controlled warehouses.
In HDPE blow molding of blue containers, the addition of an LLDPE-carried blue concentrate can shift parison sag and die swell even if the color matches. The effect is not caused by the pigment but by the carrier contribution to the melt. Blow molders should verify part weight distribution and pinch-off integrity after color introduction. Injection molders working with blue crates, caps, or appliance parts should confirm that the color feeder delivers stable mass flow because pellet size and bulk density variations can change the addition rate. Regrind containing the color concentrate can be returned to the process at controlled percentages, but repeated heat histories can darken or shift the blue shade if process temperatures and residence time are high. Color measurements should be performed on conditioned samples, not at the press, because surface temperature and crystallinity change spectrophotometric readings.
Colorimetric acceptance is usually based on CIE L*a*b* coordinates under D65 illumination and 10° observer geometry. Haze and opacity are measured according to ASTM D1003 or ISO 14782. In opaque blue films, total luminous transmittance may be less informative than contrast ratio, which better correlates with visual hiding power.
High-speed cast or blown film lines have short residence time and high shear. Under these conditions, an LLDPE-carried concentrate must be fully molten before the die; otherwise, titanium dioxide agglomerates pass through screens and appear as optical defects. The processing window can be narrow because the blue organic pigment is more sensitive to melt temperature than TiO₂. If line speed is increased while the concentrate melting capacity of the extruder is unchanged, opacity may fall even though the addition rate remains constant. The failure mode is often misread as a color feeder error; in fact, it reflects incomplete dispersion and reduced residence time. Die-lip thermocouples, melt-pressure transducers before the filter, and light-box inspection of the web provide more diagnostic value than random pellet testing.
Frost line height affects color development in LLDPE film. At low frost line heights, smaller spherulites scatter more light and may reduce apparent color depth. At high frost line heights, freeze-line orientation and higher crystallinity can increase opacity but may lower dart impact and tear resistance. The same 40356 concentrate can therefore appear different on two blown film lines with identical letdown ratio. A sealed reference plaque and 24 h post-extrusion aging are recommended before final color approval because post-crystallization changes can shift L*, a*, and b* values. Spectrophotometric readings taken on warm film immediately after the nip are not comparable to conditioned laboratory measurements.
Regulatory status of a masterbatch is lot-specific and end-use-dependent. The checklist below is not a 40356 certification; it identifies the standards normally reviewed for olefinic color concentrates intended for packaging or consumer goods.
| Regulatory dimension | Standard or clause | Typical measured limit | Verification note |
|---|---|---|---|
| US food-contact olefin polymer | FDA 21 CFR 177.1520 | End-use extraction limits apply | Carrier PE may be covered; pigments and additives require separate status. |
| EU plastic food-contact materials | EU 10/2011 | Overall migration 10 mg/dm² or 60 mg/kg | Pigment-specific SMLs apply where listed. |
| RoHS hazardous substances | Directive 2011/65/EU, Annex II | Pb 1000 ppm, Cd 100 ppm, Hg 1000 ppm, Cr(VI) 1000 ppm | Raw material documentation must be maintained. |
| REACH SVHC communication | Regulation (EC) No 1907/2006, Article 33 | 0.1 wt% per article | Applies to articles, not the masterbatch as supplied. |
The safety data sheet and technical data sheet for POLYBATCH™ Opaque Blue 40356 should be consulted for the prevailing regulatory classification and any food-contact status of the specific lot.
An LLDPE-carried opaque blue concentrate has operational boundaries that are not visible in a simple color chip. It is intended for polyethylene and polyolefin-compatible matrices; it should not be used as a colorant for polyamide, PET, polycarbonate, or rigid PVC because the LLDPE carrier forms an immiscible phase and can reduce weld-line strength or create delamination. Additive compatibility should be checked when the formulation contains highly polar lubricants, antistatic amine compounds, or certain metal stearates, because these can alter pigment dispersion or increase plate-out on cooling rolls and die lips. Where such additives are required, production trials at the lowest feasible addition rate are warranted, with periodic checks of die-lip buildup and film haze.
Color strength and opacity should be evaluated against a sealed physical standard rather than against a printed Pantone reference. The standard should be produced on the same grade of polyethylene, at the same gauge, and with the same thermal history as the production article. If the standard is not chain-linked to the production line, lot-to-lot variation in carrier MFI, pellet size, or TiO₂ content may be interpreted as a color mismatch even when the colorant itself is within specification. The person responsible for color approval should record extruder head pressure, melt temperature, frost line height, and colorimetric readings together with lot number; without these records, a blue shift or opacity loss cannot be assigned to the concentrate, the process, or the base resin.