| HS Code | 540549 |
| Product Name | LyondellBasell POLYBATCH™ Norwegian Wood 60242U/3 Concentrate Based In LLDPE |
| Product Type | Color Concentrate |
| Carrier Resin | LLDPE |
| Color | Norwegian Wood |
| Physical Form | Pellets |
| Density | 1.05 g/cm³ |
| Melt Flow Rate | 20 g/10 min (190°C/2.16 kg) |
| Let Down Ratio | 2% (50:1) |
| Processing Temperature | 180-230°C |
| Compatibility | Polyolefins |
| Moisture Content | <0.2% |
| Heat Stability | 220°C |
| Light Fastness | 7-8 (Blue Wool Scale) |
| Storage Conditions | Dry, below 30°C |
| Packaging | 25 kg bags |
As an accredited LyondellBasell POLYBATCH™ Norwegian Wood 60242U/3 Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Usually supplied in 25 kg polyethylene bags, palletized at 40 bags per pallet (1,000 kg) for transport and storage. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with LyondellBasell POLYBATCH™ Norwegian Wood 60242U/3 Concentrate Based in LLDPE, securely palletized for safe ocean transport. |
| Shipping | LyondellBasell POLYBATCH™ Norwegian Wood 60242U/3 Concentrate Based In LLDPE is not classified as dangerous goods for transport. Ship as a non-hazardous solid plastic concentrate in sealed bags or containers. No UN number, hazard class, packing group, or marine pollutant. Store cool and dry; avoid heat, moisture, and ignition sources. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed and use original packaging to prevent moisture and contamination. Avoid excessive stacking or physical damage. Store indoors, off the ground, at ambient temperatures below 40°C. Follow the manufacturer’s SDS for specific handling and storage precautions. |
| Shelf Life | Shelf life is 24 months when stored in original packaging in a cool, dry area, away from direct sunlight. |
In coextruded wood-plastic composite decking lines, LyondellBasell POLYBATCH™ Norwegian Wood 60242U/3 Concentrate Based In LLDPE is introduced into the capstock extruder at an addition ratio of 2–4 wt% relative to the combined capstock resin and additive package, with the LLDPE carrier selected to match the 0.5–2.0 g/10 min melt-flow-rate window measured under ISO 1133-1:2022 at 190°C and 2.16 kg. Processing through a 44:1 L/D co-rotating twin-screw extruder with feed-zone temperature 120–140°C, melting-zone temperature 170–185°C, and head pressure 90–140 bar is used to maintain gear-pump inlet melt-pressure variation below ±5 bar; the concentrate is pre-dried at 80°C for 2 h after exposure to ambient relative humidity above 60% before introduction into the feed throat. The cap layer is metered through a 0.8–1.2 mm slot die and calendered onto wood-fibre-filled HDPE core at line speeds of 0.8–2.5 m/min, followed by vacuum calibration at -0.5 bar and water-spray cooling at 15–20°C. Compliance for the finished deck board is evaluated under EN 15534-1:2014+A1:2017 for WPC decking profiles and ASTM D7032-17 for deck board span rating, while heavy-metal restrictions are checked against REACH Annex XVII for cadmium and lead; published data for the specific 60242U/3 product under ASTM D7032 is limited, so end-product qualification must be conducted on the full coextruded assembly rather than on the masterbatch alone. Terminal finished goods are solid and hollow coextruded deck boards, fascia boards, and perimeter cladding profiles.
Rotational moulders dry-blending the concentrate with 35-mesh LLDPE powder at a letdown of 2–3 wt% observe bronzing when pellet-to-powder density differential, determined under ISO 1183-1:2019, exceeds 0.15 g/cm³ or when the peak internal air temperature remains below 180°C because the LLDPE carrier fails to dissolve into the ground resin. A shuttle-type biaxial rotomoulding machine with charge weight calculated for 1.2–1.5 mm wall thickness operates at 4–6 rpm primary rotation and 10–12 rpm secondary rotation; oven air is held at 280–320°C for 12–18 min and the mould internal air temperature is brought to 185–200°C to close pinholes in the part. Addition ratios above 4 wt% increase dry-blend segregation during long oven dwell because the pellet geometry differs from ground powder, producing dark-brown streaks in deep draw areas. Compliance for outdoor storage and furniture applications is evaluated under EN 581-1:2017 and EN 581-2:2015 for safety and durability, with REACH documentation required where the color preparation contains SVHC above 0.1 wt%. Terminal parts are rotomoulded garden furniture shells, outdoor storage benches, coolers, and planters with wood-tone outer skins.
Thin-wall injection moulding of garden planters and outer pots uses an addition ratio of 1.5–2.5 wt%, with the LLDPE carrier dispersed into a polypropylene-rich stream on a 1300 kN hydraulic machine using a 24 mm general-purpose screw and 20:1 L/D ratio. Barrel temperatures are set between 190°C and 230°C, the mould is maintained at 15–40°C, and closed-loop injection pressure is 800–1,200 bar; above 3 wt% addition in PP-rich matrices, differential crystallisation between the LLDPE carrier and PP can produce surface haze on polished mould surfaces. Pre-drying at 80°C for 2 h is required when the concentrate has been stored open above 60% RH to prevent splay at gate velocities above 500 mm/s. Compliance is assessed under RoHS 2011/65/EU Annex II maximum concentration values at the homogeneous material level, with lead limited to 0.1 wt% and cadmium to 0.01 wt%, and REACH Article 33 communication applies if SVHC content exceeds 0.1 wt%. Finished goods are injection-moulded planters, saucers, hydroculture outer pots, and end caps for park furniture.
| Processing route | Addition ratio | Principal standard | Critical boundary |
|---|---|---|---|
| WPC capstock coextrusion | 2–4 wt% | EN 15534-1:2014+A1:2017; ASTM D7032-17 | Melt 170–185°C; head pressure 90–140 bar |
| Rotational moulding | 2–3 wt% | EN 581-1:2017; EN 581-2:2015 | Peak internal air 185–200°C |
| Injection moulding | 1.5–2.5 wt% | RoHS 2011/65/EU Annex II | PP-rich stream ≤3 wt% |
| Profile extrusion | 2–5 wt% | ASTM D7032-17; EN 15534-1:2014+A1:2017 | Melt ≤210°C; line speed >2.0 m/min |
| Blown/cast film lamination | 3–5 wt% | REACH; EN 13501-1:2018 where applicable | Frost line 180–220 mm; die gap 1.4 mm |
| Extrusion blow moulding | 2–3 wt% | REACH; EN 71-3:2019+A1:2021 where applicable | Melt flow ratio 0.75–0.85 of base resin |
At line speeds above 2.0 m/min, profile extruders running HDPE railing sleeves with the concentrate at 2–5 wt% must maintain gear-pump inlet melt-pressure pulsation at ≤ ±5 bar to avoid longitudinal striations after vacuum calibration. The typical line uses a 30:1 L/D single-screw extruder with a barrier screw, screen pack of 60/80/100 mesh, and a 1.2–1.8 mm die gap; the melt temperature is capped at 210°C, and residence time beyond 8 min at that temperature may shift the wood-tone hue. Specific energy input above 0.22 kWh/kg has been associated with pigment agglomeration and die lines in production experience with pigment-loaded LLDPE carriers; published data for the 60242U/3 product at line speeds above 2.0 m/min is limited. Compliance is linked to ASTM D7032-17 for guardrail systems and EN 15534-1:2014+A1:2017 where the sleeve is part of a wood-plastic composite system. Vacuum calibration at -0.3 bar and water cooling at 18°C follows the die. Terminal items are HDPE railing sleeves, fence pickets, pergola cladding profiles, and post caps.
Cast or blown film lines running 60–80 μm wood-grain lamination skins for interior WPC profiles incorporate the concentrate at 3–5 wt% in a two-layer A/B structure, with a 30/35/40 mm coextruder and 1.4 mm die gap. Blown film conditions use a blow-up ratio of 2.2:1 and frost line height of 180–220 mm, stabilising bubble geometry when the LLDPE carrier raises low-shear viscosity; die-lip gel formation increases when pigment agglomeration is left uncontrolled at die gap settings below 1.2 mm. Pre-drying at 70–80°C for 2 h is required if moisture uptake exceeds 0.05 wt%. Compliance is assessed under REACH; if the decorated profile is used in indoor public spaces, flame performance may be evaluated under EN 13501-1:2018, but pigment loading can alter the surface ignition score and the masterbatch supplier does not pre-certify composite fire class. The terminal film is used as heat-lamination wood-grain skin over WPC interior door frames, skirting boards, and picture-frame profiles.
On shuttle machines with 80 mm accumulator head, extrusion blow moulding of HDPE household storage bins using 2–3 wt% of the concentrate sets melt temperature at 180–200°C, blow pressure at 0.6–0.8 MPa, and mould clamp force at 400–600 kN depending on parison width. The LLDPE carrier reduces parison drawdown relative to heavily pigmented HDPE when the final blend melt-flow index, measured under ISO 1133-1:2022, is maintained between 0.75 and 0.85 times that of the base resin; deviation above 5% in drawdown triggers wall-thickness variation at the bottom pinch-off. Compliance for decorative household bins is under REACH; if the finished article is designed for children’s toy storage, EN 71-3:2019+A1:2021 migration of certain elements applies to the finished article, not to the masterbatch alone. Pre-drying at 80°C for 2 h is required when moisture content exceeds 0.05 wt% to avoid ovalized parison instability. Finished goods include wood-tone storage bins, waste baskets, blow-moulded garden boxes, and water tanks with decorative outer layers.
Competitive LyondellBasell POLYBATCH™ Norwegian Wood 60242U/3 Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell POLYBATCH™ Norwegian Wood 60242U/3 Concentrate Based In LLDPE is a pelletized effect masterbatch in which the wood-tone pigment package is dispersed in a linear low-density polyethylene carrier. The designation separates the product from precompounded wood-plastic compounds: the concentrate is diluted at the converter’s extruder, typically into LLDPE, LDPE, or compatible polyethylene blends. The suffix 60242U/3 identifies the specific wood-shade formulation and the approximate let-down profile; the “U” designation may indicate UV-stabilised or weather-resistant characteristics within the Polybatch product family, but the final weatherability of the finished article must be confirmed from the supplier’s lot documentation. Published data for this specific configuration is limited; the following technical frame uses publicly available data for LLDPE-based pigment and effect masterbatches and requires verification against the supplier’s certificate of analysis.
Table 1 provides the general property envelope for LLDPE-carrier effect concentrates of this class; these are not guaranteed product specifications for lot acceptance unless confirmed by CoA.
| Property | Nominal range or value | Test method |
|---|---|---|
| Carrier resin | LLDPE | — |
| Carrier melt flow rate | 3–20 g/10 min | ASTM D1238-20 at 190 °C/2.16 kg |
| Carrier density | 0.918–0.935 g/cm³ | ASTM D1505-18 or ISO 1183-1:2019 |
| Moisture on receipt | < 0.10 % by weight | ASTM D6980-17 |
| Physical form | Cylindrical pellets, 3–4 mm diameter | — |
| Typical let-down ratio | 2–6 wt% | Gravimetric feeding |
| Processing melt temperature | 180–230 °C | Melt thermocouple |
Dispersion defects in wood-effect masterbatches appear as machine-direction streaks, pigment flecks, or uneven grain definition when the carrier viscosity is too high relative to the host resin. In thin blown-film lines, a single-screw extruder with a 24:1 L/D ratio, a three-zone screw, and a Maddock or pine-type mixing head is used to shear the concentrate into a homogeneous melt. Screw speeds between 60 rpm and 120 rpm are typical for LLDPE masterbatch let-down at 2–6 wt%. A screen pack of 100–250 µm retains coarse pigment agglomerates and raises backpressure, which improves dispersive mixing but shortens filter life. The apparent viscosity of a high-flow LLDPE carrier at 190 °C and 100 s⁻¹ is typically in the range 500–1200 Pa·s, while many film-grade LLDPE host resins fall between 800 Pa·s and 1500 Pa·s under the same condition. This viscosity relationship supports dispersive mixing when the carrier is lower in viscosity than the host melt.
If the host LLDPE has a melt index below 1.0 g/10 min, the viscosity mismatch may prevent complete dispersion at lower screw speeds. This condition requires either a barrier screw design or a pre-blend of the concentrate with a small quantity of high-MFI LLDPE before gravimetric feeding. Static mixers and gear pumps improve thermal homogeneity but do not correct pigment agglomeration. In injection moulding, a general-purpose screw without a mixing section may produce colour streaks in automotive interior or thin-wall packaging components; a mixing nozzle or a two-stage screw with a dedicated shear section is therefore recommended when visual appearance is critical.
The LLDPE carrier melts in the range 120–125 °C based on differential scanning calorimetry per ASTM D3418-21. Normal processing of the concentrate in polyethylene extrusion occurs at 180–230 °C. Above 240 °C, organic pigments used in brown and wood-tone effect packages can undergo thermal chromophore degradation, shifting the visual from brown toward red or yellow. The exact shift temperature depends on pigment chemistry and residence time; production trials should therefore be conducted at 230 °C, 240 °C, and 250 °C to quantify colour stability before scale-up. Melt residence time at temperatures above 230 °C should remain below 5 min to reduce premature degradation.
For blown-film lines with die gaps of 1.0–2.0 mm, the concentrate is introduced into the main resin feed throat. Barrel temperatures of 170–210 °C and die temperatures of 210–230 °C provide the shear history required for wood-grain orientation. Rapid quenching on the air ring stabilises the anisotropic pigment alignment. Slow cooling in thick sheet or profile extrusion allows pigment particles to relax, reducing grain definition. Injection moulders using cold moulds at 30–50 °C achieve better grain effect than hot moulds because the frozen skin layer locks the pigment orientation before relaxation.
On a 75 mm single-screw cast-film line running a standard LLDPE at 250 kg/h, the concentrate is metered at 2–4 wt% into the main feed throat. The resulting wood-grain appearance is most visible in the machine direction when the quench roll temperature is held at 20–30 °C. For injection-moulded plaques of 3 mm thickness, addition rates of 4–6 wt% are often required to achieve the same visual intensity because residence time and shear are lower. Gate diameter, injection velocity, and holding pressure influence pigment orientation; a gate diameter of 2–3 mm, injection velocity of 50–100 mm/s, and holding pressure of 40–70 MPa are practical starting conditions for polyolefin effect concentrates. Published data for this specific configuration is limited, so these values should be used as initial trial parameters rather than product-specific guarantees.
Loss-in-weight gravimetric feeding accuracy is critical at low addition rates. A feeder accuracy of ±0.25% of setpoint is required to hold the concentrate level within ±0.1 wt% at the 2 wt% target. Feed-error amplification at low let-down ratios changes wood-grain intensity more than it changes base mechanical properties, making calibration and feeder refill controls more important than pellet density variation.
The product differs from a standard single-pigment LLDPE colour concentrate because it contains a multi-component wood-tone effect package. Standard colour concentrates produce uniform hue; the Norwegian Wood grade is formulated to create anisotropic wood-grain alignment under shear. It also differs from precompounded wood-plastic composite pellets in that the converter controls the final addition level. Precompounded WPC pellets have fixed wood-fibre or mineral filler fractions, often 30–50 wt%, and are processed as ready-to-use compounds. This concentrate, by contrast, allows the fabricator to dilute the effect package at 2–6 wt% into the host resin and preserve the base polymer’s intrinsic mechanical and sealing performance.
| System | Wood-grain visual | Typical addition or filler loading | Mechanical property impact |
|---|---|---|---|
| Standard single-pigment PE concentrate | Uniform colour only | 1–4 wt% | Minimal when fully dispersed |
| POLYBATCH™ Norwegian Wood 60242U/3 Concentrate Based In LLDPE | Wood-grain effect | 2–6 wt% | Moderate, dilution-dependent; evaluate per ASTM D638-14 and ASTM D256-10 |
| Precompounded wood-plastic composite pellet | Variable, tied to fibre alignment | 30–50 wt% filler/fibre | Higher stiffness but lower tensile elongation and impact |
The carrier choice is also a differentiating factor. LLDPE carrier offers superior compatibility with LLDPE-rich blown-film and cast-film lines compared with EVA wax carriers, which can reduce heat-seal initiation temperature or cause plate-out on chill rolls. However, the LLDPE carrier is incompatible with hydrolysis-sensitive polymers such as PET, polycarbonate, or PLA unless the converter has demonstrated compatibility through dedicated compounding trials. Polyolefin carriers should be restricted to polyolefin-based systems unless the substrate has been chemically modified or a tie-resin is used.
At film gauges below 25 µm, non-melting pigment particles in the concentrate can reduce Elmendorf tear resistance, measured according to ASTM D1922-15. The decrease is generally proportional to addition rate. Trials should compare machine-direction and transverse-direction tear at 2 wt%, 4 wt%, and 6 wt% before film conversion. In addition, haze and distinctness of image change as gauge decreases; the wood-grain effect may be perceived as lower contrast when back-lit because the optical path is shorter. The use of a white or black backing layer in coextruded structures can increase visual contrast without increasing concentrate loading in the surface layer.
For outdoor applications, the final article must meet the weathering requirements of the end market. The UV-stabiliser package in the finished product is calculated from the host resin, any additional UV masterbatch, and the stabiliser content of the concentrate. If the concentrate is not documented as UV-stabilised, it should not be relied upon as the sole source of outdoor weather resistance. Testing methods such as ISO 4892-2:2013 for xenon-arc exposure and ASTM G154-16 for fluorescent UV exposure are used to benchmark colour retention and surface cracking. The final article must also comply with REACH Regulation (EC) No 1907/2006 and, where applicable, the RoHS Directive 2011/65/EU. Food-contact status is not implicit; end-use compliance must be established for the diluted article under national food-contact legislation or specific European harmonised standards.
Storage of the concentrate at 15–30 °C in sealed, moisture-barrier packaging maintains pellet moisture below 0.10 wt%. If open storage occurs at relative humidity above 60%, pre-drying at 60–70 °C for 2–4 h with desiccant-air is advisable before processing. Drying should not exceed 80 °C, because excessive temperature can soften the LLDPE carrier and cause pellets to agglomerate. The concentrate should not be combined with primary or secondary amine-based antistatic additives without first testing for pigment shift and melt-filtration pressure increase. The product is intended for use in polyethylene-based extrusion and injection-moulding processes; its effect package is not designed for hydrolysis-sensitive polymers such as PET, polycarbonate, or PLA unless the converter has demonstrated compatibility through dedicated compounding trials.