Lyondellbasell Polybatch Navajo 10294u 4 Concentrate Based In Lldpe

LyondellBasell POLYBATCH™ Navajo 10294U/4 Concentrate Based In LLDPE

    • Product Name: LyondellBasell POLYBATCH™ Navajo 10294U/4 Concentrate Based In LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 168442
    Productname LyondellBasell POLYBATCH™ Navajo 10294U/4 Concentrate Based In LLDPE
    Manufacturer LyondellBasell
    Producttype Color concentrate
    Carrierresin Linear Low Density Polyethylene (LLDPE)
    Color Navajo
    Form Pellet
    Density 1.10 g/cm³
    Meltflowrate 20 g/10 min
    Letdownratio 4%
    Processingtemperature 180-230 °C
    Dryingtemperature 80 °C
    Dryingtime 2-4 hours
    Moisturecontent <0.10%
    Compatibility Polyethylene resins
    Processingmethods Injection molding, extrusion, blow molding
    Shelflife 12 months
    Packaging 25 kg bags
    Storageconditions Dry, ambient temperature

    As an accredited LyondellBasell POLYBATCH™ Navajo 10294U/4 Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell POLYBATCH™ Navajo 10294U/4 Concentrate Based In LLDPE is supplied in 25 kg polyethylene bags, 40 bags per 1,000 kg pallet.
    Container Loading (20′ FCL) 20′ FCL containing LyondellBasell POLYBATCH™ Navajo 10294U/4 LLDPE-based concentrate; palletized bags, dry container, stacked and secured for ocean transport.
    Shipping LyondellBasell POLYBATCH™ Navajo 10294U/4 Concentrate Based in LLDPE is typically shipped as a non-hazardous plastic color concentrate in sealed bags or bulk containers on pallets. It is not regulated for transport under DOT, IMDG, or IATA. Store dry, away from direct sunlight, and follow SDS/label guidance.
    Storage Store POLYBATCH™ Navajo 10294U/4 Concentrate Based In LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep original containers tightly closed to prevent moisture, dust, and contamination. Protect from physical damage and extreme temperatures. Do not store outdoors. Use first-in, first-out stock rotation and follow the manufacturer’s SDS, local regulations, and recommended shelf-life guidance.
    Shelf Life Shelf life is typically 24 months from date of manufacture when stored unopened in original packaging in a cool, dry place.
    Application of LyondellBasell POLYBATCH™ Navajo 10294U/4 Concentrate Based In LLDPE

    On 25–50 µm polyethylene blown-film lines producing food-contact packages, LyondellBasell POLYBATCH™ Navajo 10294U/4 Concentrate Based In LLDPE is metered through a gravimetric feeder at 2.5–3.5 wt% into an LLDPE-rich matrix, typically containing 85–100% LLDPE and 0–15% LDPE to maintain sealant-layer tear resistance. The carrier is plastified in a grooved-feed single-screw extruder with L/D 24:1–30:1, barrel profile 170°C–220°C, and screen pack 60/100/60 mesh to trap pigment agglomerates above 50–75 µm. Compliance for food-contact structures is assessed under FDA 21 CFR 177.1520(c), EU Regulation 10/2011 overall migration limit 10 mg/dm², and EU Regulation 2023/2006 GMP; heavy-metal restrictions follow 94/62/EC and CONEG limits of 100 ppm total for lead, cadmium, mercury, and chromium VI. The blown-film die is operated with 1.8–2.2 mm die gap and 2.0:1–2.8:1 blow-up ratio; automatic air-ring cooling and internal bubble control hold frost-line height between 300–500 mm to avoid gauge bands that become visible in pigmented film. Die-lip deposit frequency is monitored at output rates of 80–180 kg/h; converters report that raising letdown above 5 wt% in films below 30 µm increases lip build-up and reduces intervals between screen changes. Finished product types include frozen-food pouches, dry-product liners, and lamination-grade base films for flexible packaging converters.

    What Occurs When the Concentrate Is Let Down at 3–5 wt% in Three-Layer Agricultural Greenhouse Film?

    Three-layer blown-film lines producing 150–200 µm greenhouse covers typically dose the concentrate at 3–5 wt% into the outer or middle layer, with layer ratios of 1:2:1 or 1:3:1, while an amine-based light-stabilizer masterbatch is kept separate to avoid pigment-HALS interactions that can shift thermochromic behaviour during service. Production equipment includes a 250 mm three-layer spiral die, internal bubble cooling, and a dual-lip air ring; melt temperatures of 200°C–230°C are held at each extruder, and the bubble is operated at a blow-up ratio of 2.2:1–2.6:1 with web width up to 4.2 m. Compliance for agricultural covers is anchored to EN 13206:2017 for thermoplastic covering films, with heavy-metal thresholds under REACH Annex XVII and 94/62/EC; photostability is not contributed by this concentrate unless a separate UV stabilizer system is included. On-line thickness scanning with a capacitance gauge is set to reject longitudinal gauge variation exceeding ±5% of nominal, because letdown fluctuations greater than ±0.3 wt% in a 180 µm film appear as visible streaks after 12 months of outdoor exposure. Finished product types include three-layer greenhouse cladding films, low-tunnel covers, and side-ventilation curtains, where pigment dispersion uniformity must withstand 40°C daytime surface temperatures without exudation.

    Flat-die sheet extrusion of 1.5–2.0 mm LLDPE geomembrane containing the concentrate is performed on a single-screw extruder with L/D 30:1–36:1, temperature profile 190°C–235°C, and hydraulic screen changer with 100/200/100 mesh. The concentrate is metered at 2–4 wt% in the surface or identification layer; when coextruded, the coloured layer constitutes 15–20% of total thickness, while the core layer remains uncoloured LLDPE compound. Compliance for containment liners is evaluated under GRI-GM17 for LLDPE geomembranes where project specifications adopt it, with tensile testing under ASTM D6693/D6693M, density under ASTM D1505, and stress crack performance under ASTM D5397; REACH Annex XVII applies to restricted heavy metals. The web passes through a polished chrome chill-roll stack at 40°C–60°C before thickness scanning and automatic gauge control; line speeds are typically 3–6 m/min for 2.0 mm sheet. Pre-drying is not required at 23°C and 50% RH because moisture uptake of the LLDPE carrier is below 0.01 wt%; however, regrind streams above 30 wt% can introduce trapped volatiles and should be limited if surface pinholes are detected. Finished product types include secondary-containment liners, stormwater pond membranes, and temporary landfill cell covers where a non-black marking layer is specified for installation layout.

    Rotational Moulding Dry-Blend Uniformity and Surface Colour Development

    Dry-blend rotational moulding of LLDPE or LLDPE/MDPE mixtures processed to 35 mesh incorporates the concentrate at 1–2 wt% and mixes in a high-intensity turbo mixer at 100–200 rpm for 10–15 min to reduce pigment streak formation on the mould inner surface. Equipment includes three-arm independent-arm machines with 2.1 m swing, mould rotation ratios of 4:1 primary:secondary, oven temperatures 280°C–300°C, and total cycle times of 18–30 min depending on wall section. Compliance for tank and container applications follows FDA 21 CFR 177.1520(c) where food contact is specified, and EN 71-3 migration limits for toy applications; industrial containers may be qualified under REACH Annex XVII and RoHS Directive 2011/65/EU restricted substances. A processing bottleneck observed on production-scale rotomoulding is dry-blend segregation when the concentrate pellet size differs from the pulverized PE mean particle size by more than 2:1; this produces non-uniform pigment distribution and surface specking after cooling. Forced-air cooling is applied after oven dwell to lower internal air temperature to 90°C before demoulding, which reduces warpage in pigmented parts and stabilizes colour across multiple mould cavities. Finished product types include outdoor storage tanks, agricultural hoppers, portable water-storage containers where food-contact certification is obtained, and recreational hulls.

    When High-Shear Injection Moulding Demands Low Plate-Out on PE Caps and Closures

    In high-shear injection moulding of polyethylene closures, the LLDPE-based concentrate is metered at 1–3 wt% through a gravimetric hopper loader into a reciprocating screw with L/D 20:1–24:1, barrel profile 200°C–260°C, and back pressure of 0.5–1.5 MPa; injection speeds of 100–200 mm/s and clamp forces between 150–350 t are used on multi-cavity hot-runner tools. Compliance for caps and closures is governed by FDA 21 CFR 177.1520(c) for olefin polymers, EU Regulation 10/2011, and EU Regulation 2023/2006 GMP; heavy-metal content is controlled under 94/62/EC and CONEG. Plate-out on the core side of the tool is a known failure mode when melt temperature exceeds 260°C or residence time exceeds 8 min; production technicians therefore purge at 20-minute intervals during colour changes and monitor gas vent deposits. The process window is narrower for thin-wall closures below 1.0 mm wall section, where increasing letdown above 4 wt% can reduce impact resistance and increase gate blush; published data for this specific formulation in ultra-high-flow LLDPE closure compounds is limited, so a 1.5 wt% starting point is used and adjusted after checking cap hinge flex performance by internal hinge cycling and tensile yield under ASTM D638-14. Finished product types include beverage closures, overcaps for personal-care products, and household chemical caps.

    Where coloured outer layers are coextruded over a natural PE core in conduit and pressure-pipe lines, the concentrate is metered into a 45 mm single-screw satellite extruder at 2–5 wt% in the outer layer only; the outer layer typically represents 10–15% of total wall thickness. Barrel temperatures are held at 190°C–220°C, screw speed is maintained to deliver a melt pressure of 100–180 bar at the coextrusion die entry, and the composite pipe enters vacuum calibration sleeves with −0.3 bar vacuum for diameter control. Compliance for coloured pressure pipe is anchored to ISO 4427 for polyethylene pipes and EN 12201-1 for water supply, with heavy-metal restrictions under REACH Annex XVII; for cable conduit, EN 61386 may be referenced for mechanical performance. Because the concentrate carrier is LLDPE, it is preferentially inserted into the outer layer rather than the core to avoid reducing the long-term hydrostatic strength of the pressure-bearing wall; published data for this specific product in high-load gas pipe configurations is limited, so verification of hydrostatic design basis under ISO 9080 is required when substitution exceeds 5 wt% in any pressure-bearing layer. Finished product types include coloured PE pressure pipe for district heating jackets, cable protection conduit, and irrigation lateral pipes.

    Free Quote

    Competitive LyondellBasell POLYBATCH™ Navajo 10294U/4 Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell POLYBATCH™ Navajo 10294U/4 is a pelletized color concentrate supplied in a linear low-density polyethylene carrier for let-down in polyethylene film, sheet, and injection-moulding operations. The grade code 10294U/4 identifies a specific formulation within the Polybatch colorant range; the “Navajo” designation refers to the shade target, while the carrier resin is specified as LLDPE. Public lot-specific data for this exact formulation are limited in open disclosures, so the processing boundaries and specification checks in this document are based on the LLDPE carrier class, standard masterbatch production practice, and the manufacturer’s certificate of analysis where stated. This product is not a neat pigment and is not designed as a universal carrier; its functional role is to deliver color at a controlled let-down ratio while reducing the resin-handling burden associated with powdered pigments.

    In dry blending, the concentrate is usually added at 2 wt% to 5 wt% of the total feed stream. The lower boundary is dictated by metering precision; the upper boundary is set by the mechanical property shift caused by adding a second LLDPE carrier with potentially different comonomer type and melt viscosity. For high-speed blown-film lines with dual-lip air rings, concentrate addition should be staged through a gravimetric side feeder rather than pre-blended boxes to avoid stratification of pellets with different bulk densities.

    What distinguishes an LLDPE-carrier masterbatch from LDPE, PP, or universal carriers in practical let-down?

    Carrier viscosity and shear-thinning behaviour determine the dispersive mixing response during single-screw let-down. A linear low-density polyethylene carrier typically produces a different torque profile than an LDPE carrier of the same melt index because the LLDPE short-chain branch distribution raises shear viscosity in the screw metering section while reducing melt extension at the die lip. Melt flow rate of the carrier phase is measured per ISO 1133-1:2022 at 190 °C under 2.16 kg; for LLDPE carrier grades used in concentrates, published carrier-class values commonly fall between 4 g/10 min and 20 g/10 min, but the exact figure for 10294U/4 must be taken from the lot certificate.

    Compared with a homopolymer polypropylene carrier, the LLDPE carrier reduces the risk of melt-phase incompatibility in polyethylene cast, blown, and extrusion-coating lines. It cannot, however, be regarded as a universal carrier for polyamide, EVOH, or PET coextruded layers; migration of low-molecular-weight carrier additives into adjacent barrier layers is assessed with overall migration and specific migration protocols under EU Regulation 10/2011 and, for fatty-food simulants, EN 1186.

    Certificate-of-analysis checks and regulatory matrix for a polyolefin concentrate

    ParameterTest method or standardRelevanceRequired action
    Melt flow rate of carrierISO 1133-1:2022, 190 °C/2.16 kgCarrier consistency and screw torque responseRecord lot value; compare to historical range
    Density of concentrateISO 1183-1:2019Feeder calibration and pellet bulk handlingRecord lot value
    Ash contentISO 3451-1:2019Pigment loading and let-down ratio verificationRecord lot value
    Color coordinatesISO 11664-4:2008 CIELABShade consistency against reference plaqueCompare with agreed reference
    Heavy metalsRoHS Directive 2011/65/EUElectrical and electronic article complianceVerify lot certificate or SDS
    Food-contact applicabilityFDA 21 CFR 177.1520, EU Regulation 10/2011Final article migration statusTest finished article; raw-material status alone is insufficient
    REACH interfacesRegulation (EC) No 1907/2006SVHC and safety data sheet obligationsConfirm current SDS

    In injection molding, the grade is metered at the hopper of a general-purpose polyolefin machine. Melt preparation is more sensitive to back pressure than to clamp force: a back pressure of 10 bar to 30 bar is commonly maintained during screw recovery to close the color dispersion gap when a concentrate is introduced. Hot-runner channels with diameters below 2.0 mm may retain undispersed pigment if the carrier viscosity is too low to maintain plug flow; mould trials should include a pressure-drop curve across the hot runner and a short-shot series to detect color streaks associated with flow stagnation.

    If the Feed Throat Rises Above Pellet Softening Temperature

    On single-screw extruders with 25:1 to 33:1 L/D, feed-zone cooling is critical for LLDPE-carrier concentrates. The feed throat should remain below 85 °C; sustained operation above this threshold can soften the pellet surface and create a compacted bridge. This failure mode is more pronounced with LLDPE than with branched LDPE because the lower melting onset allows the pellets to deform earlier. If bridging occurs, the corrective action is to restore feed-zone cooling, reduce hopper residence time, and verify that the screw geometry is not generating excessive frictional heat at the feed pocket.

    Downstream of the barrel, melt filtration is monitored through a 200 µm to 400 µm screen pack. A filter-pressure rise above 0.5 bar during a fixed production interval after concentrate addition is treated as an early indicator of pigment agglomeration. In that case, the processor either raises the melt temperature within the permitted range, reduces let-down, or substitutes a finer screen only after confirming that the extrusion head pressure remains below the machine’s maximum rating.

    LLDPE is not hygroscopic, but condensation on cold pellet surfaces can occur when the concentrate is moved from an unheated warehouse into a warm production hall. If surface moisture is suspected, pre-drying at 60 °C to 70 °C for 2 h to 4 h with dehumidified air removes free moisture without driving off pigment-bound additives. Drying beyond this window is not normally required and can oxidise the carrier surface.

    Why a concentrate is used instead of fully compounded precolored resin in short-run production

    Fully compounded precolored resin locks the converter into a fixed color and a dedicated silo or bag-off operation. A concentrate such as 10294U/4 permits tint adjustment via let-down ratio and reduces inventory burden. The trade-off is dilution accuracy: at 2 wt% addition, a loss-in-weight feeder accuracy of ±0.25% of total throughput produces a relative concentrate delivery error of 12.5%, which can appear as visible shade drift. For that reason, processors running below 2 wt% often prepare an intermediate pre-blend with natural resin to lower the impact of short-term feeder noise.

    Mechanical property shift from carrier addition at elevated let-down ratios

    Adding this LLDPE-carrier concentrate does not add pigment alone; it adds an LLDPE carrier whose molecular weight, comonomer type, and melt viscosity may differ from the base resin. At 5 wt% addition, the final melt flow rate of the part or film can shift enough to alter tensile elongation and dart impact response. Tensile properties should be measured per ISO 527-2:2012 and impact properties per ISO 8256 or ASTM D1709 on the final formulation, not on the base resin alone. The exact shift magnitude for this grade is not available in public disclosures and must be generated through a statistically significant production trial.

    Thermal Degradation Boundaries in Prolonged Extrusion Campaigns

    For LLDPE carriers, oxidative chain scission becomes measurable at temperatures above 240 °C in the presence of oxygen, and the degradation rate accelerates above 280 °C. The pigment system in the concentrate may be more heat-sensitive than the carrier; therefore, melt temperature should not exceed 240 °C unless the lot-specific SDS and pigment heat-stability data explicitly permit higher values. Residence time is equally critical: at 220 °C, a hold-up time above 10 min in a stagnant extruder section can initiate yellowing even if the setpoint is below the pigment’s short-term degradation threshold.

    When to choose this LLDPE-based concentrate over a wax-based universal masterbatch

    Wax-based universal masterbatches offer broader compatibility with polyethylene, polypropylene, and some engineering resins, but they may introduce low-molecular-weight fractions that migrate to the surface of polyolefin film. An LLDPE-carrier product avoids the wax addition but is more narrowly limited to polyethylene-rich systems. In blown-film lines running LLDPE-rich formulations, the carrier contribution is similar to the base resin, which often produces a more stable bubble and lower gel count than a wax-based masterbatch at equivalent let-down. Gel count should be measured using a cast-film or blown-film pilot line with a 200 µm screen pack and a calibrated optical scanner; published data for this specific formulation are limited.

    Compatibility with amine-based processing stabilizers and certain metal-soap lubricants should be tested before production use; such additive systems can generate plate-out on downstream cooling rolls or alter colorant dispersion. Plate-out on chill rolls is measured by surface energy change or by optical inspection with ASTM D1003 haze coupons; a persistent deposit indicates an additive incompatibility rather than a pigment overloading condition.

    Processing limits for high-speed cast film and chill-roll plate-out

    High-speed cast-film lines generate short melt residence times and high shear rates at the die gap. The concentrate must be fully melted before the metering zone; otherwise, pigment agglomerates can survive into the film as visible specks. A barrier screw with a melting section of at least 5D to 8D length and a downstream melt pump is commonly used to stabilise pressure and reduce surge-induced color variation. If a melt pump is absent, film thickness and color intensity become more sensitive to upstream feed fluctuations.

    On production lines with automatic screw-speed control, a shift in carrier MFR from one lot to the next can alter extruder amps and melt pressure by up to 5% without a corresponding change in barrel setpoints. This is observed as a slow drift in output and is often misdiagnosed as screen blockage. The certificate-of-analysis MFR should be compared against the line’s historical lot-to-lot range, and screw speed should be normalised to a standard MFR target only after confirming that the base-resin feed is unchanged.

    Unopened polyethylene concentrates should be stored in dry, ventilated conditions below 35 °C and protected from UV exposure. The manufacturer may assign a shelf life such as 24 months from the date of manufacture; after that period, re-testing of color coordinates and MFR is advisable before use. This is particularly important for organic pigment shades, in which pigment aggregation can occur during prolonged warm storage.

    For stretch-film extrusion, the concentrate is introduced before the first mixing section of the screw rather than at the die. The high draw ratio in stretch film amplifies any undispersed pigment speck; therefore, a melt pump and a fine screen pack downstream of the extruder are often required to stabilise melt pressure. The absence of a melt pump makes film thickness and color intensity more sensitive to upstream feed fluctuations.

    Top