Lyondellbasell Polybatch Light Grey Ll803366 4 Concentrate Based In Lldpe

LyondellBasell POLYBATCH™ Light Grey LL803366/4 Concentrate Based In LLDPE

    • Product Name: LyondellBasell POLYBATCH™ Light Grey LL803366/4 Concentrate Based In LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 224438
    Product Name LyondellBasell POLYBATCH™ Light Grey LL803366/4 Concentrate Based In LLDPE
    Manufacturer LyondellBasell
    Brand POLYBATCH™
    Product Code LL803366/4
    Product Type Color Concentrate
    Carrier Resin LLDPE
    Color Light Grey
    Form Pellets
    Density 1.05 g/cm³
    Melt Flow Rate 20 g/10 min (190°C/2.16 kg)
    Moisture Content <0.10%
    Pigment Content 50%
    Let Down Ratio 4%
    Processing Temperature 180-230°C
    Shelf Life 12 months
    Storage Conditions Dry, below 30°C

    As an accredited LyondellBasell POLYBATCH™ Light Grey LL803366/4 Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg polyethylene bags, palletized, for LyondellBasell POLYBATCH™ Light Grey LL803366/4 Concentrate Based In LLDPE.
    Container Loading (20′ FCL) 20′ FCL loading of LyondellBasell POLYBATCH™ Light Grey LL803366/4 concentrate based in LLDPE, palletized, shrink-wrapped, and secured for transport.
    Shipping LyondellBasell POLYBATCH™ Light Grey LL803366/4 Concentrate Based in LLDPE ships as a non-hazardous, non-regulated solid in sealed polyethylene bags or boxes, palletized and stretch-wrapped. Keep dry and away from direct sunlight, excessive heat, moisture, and contamination. Use standard industrial handling; no special transport classification is normally required.
    Storage Store LyondellBasell POLYBATCH™ Light Grey LL803366/4 Concentrate Based in LLDPE in original, tightly closed containers in a cool, dry, well-ventilated area. Protect from direct sunlight, moisture, heat, and ignition sources. Avoid excessive stacking and container damage. Keep away from incompatible materials, oxidizers, and contaminants. Follow local regulations and the manufacturer’s SDS storage guidance. Use first-in, first-out stock rotation.
    Shelf Life Shelf life is typically 24 months when stored in original unopened packaging under dry, ambient conditions, away from direct sunlight.
    Application of LyondellBasell POLYBATCH™ Light Grey LL803366/4 Concentrate Based In LLDPE

    In blown-film extrusion of light grey refuse sacks and industrial liners produced on single-screw lines with screw L/D between 28:1 and 32:1, LyondellBasell POLYBATCH™ Light Grey LL803366/4 Concentrate Based In LLDPE is gravimetrically metered into a natural LLDPE/LDPE let-down resin at 2.0–3.5 wt%; this addition range normally gives a final film thickness of 45–70 µm with sufficient opacity for light-duty containment. The LLDPE carrier is not an inert pigment paste and can shift the let-down melt-flow rate measured under ISO 1133-1:2022 at 190 °C/2.16 kg; barrel profiles are therefore set from 180–195 °C in the feed zone to 210–220 °C at the die to keep bubble contact and haul-off tension stable. Die gap settings of 1.8–2.2 mm and a blow-up ratio between 2.5:1 and 3.2:1 are used on lines running above 60 m/min, but recycled LDPE fractions with a melt-flow-rate spread above 0.5 g/10 min can destabilise the frost line when the concentrate is added at the upper limit. Screen packs of 80/100/120 mesh downstream of the breaker plate remove agglomerates larger than approximately 150 µm; haze is measured on final film according to ASTM D1003-21, and colour is quantified by ASTM D2244 using D65 illuminant and 10-degree observer geometry. Terminal articles from this processing window include grey refuse sacks, wheelie-bin liners, e-commerce mailer film, and light-duty protection shrouds.

    What Processing Windows Govern LL803366/4 Let-Down in Thin-Wall Injection Moulding?

    A gravimetric dosing system with shot-to-shot repeatability better than ±0.2% is specified for thin-wall polyolefin parts with nominal wall sections from 0.6 mm to 1.2 mm; melt-flow variation caused by uneven masterbatch feeding appears as short-shot defects and weld-line flow marks before the part reaches the ejection station. LL803366/4 is typically metered at 2.0–4.0 wt% into natural HDPE, LLDPE, or HDPE/LLDPE moulding compounds. Because the concentrate uses an LLDPE carrier, the diluted blend has a slightly lower viscosity than a comparative HDPE-only natural resin; this shift can be logged with ISO 1133-1:2022 at 190 °C/2.16 kg and compared against the natural resin baseline before modifying sprue or gate dimensions. Forced-air drying is not normally required because the LLDPE carrier is non-hygroscopic, but hopper fogging from cold warehouse storage indicates condensed surface moisture and should be eliminated before start-up. Barrel temperatures are normally set between 210 °C and 245 °C, with nozzle temperature held 5–10 °C below the front zone to reduce stringing; hydraulic back pressure between 5 bar and 15 bar is maintained, but dead spots in worn screw tip and check ring regions can produce yellow shift measured as a CIELAB b* increase above 1.5 against the control under ASTM D2244. Pigment dispersion is checked on polished plaques according to ISO 18553, and mould temperature is kept between 20 °C and 40 °C for thin-wall caps and food-service containers. Terminal products include thin-wall caps, closures, stackable totes, and disposable takeaway containers; the light grey masterbatch should not be combined with brass inserts or amine-based antioxidant packages where premature pigment/polymer interaction produces pink-grey discolouration.

    Compliance matrix applicable to final articles, not the masterbatch alone
    ReferenceScopeCriterionTest method
    EU Regulation (EC) No 10/2011Food-contact plasticsOverall migration 10 mg/dm²EN 1186 series
    FDA 21 CFR 177.1520Olefin polymers in repeat-use food-contact articlesEnd-use extraction under 21 CFR 176.170Exposure conditions specified in reference
    RoHS Directive 2011/65/EULead and mercury in homogeneous material1000 mg/kgIEC 62321 series
    RoHS Directive 2011/65/EUCadmium in homogeneous material100 mg/kgIEC 62321 series
    REACH Regulation (EC) No 1907/2006SVHC content in article0.1% w/w notification thresholdCandidate List verification
    EN 71-3Migration of certain elements from toy materialsCategory-dependent migration limitsEN 71-3

    Particle-Size Parity Limits Rotational Moulding Use

    Rotational moulding of outdoor PE storage tanks and agricultural water butts with wall sections above 4 mm does not accept pelletised LL803366/4 as a direct dry-blend; the pelletised carrier must first be pulverised to pass a 500 µm US Standard 35 mesh screen. Otherwise the pelletised masterbatch segregates from the PE powder, migrates to the inner wall, and produces grey streaks and pinholes at the weld line of the final moulding. The ground masterbatch is introduced at 2.0–4.0 wt% into LLDPE or MDPE powders and mixed in a low-speed helical mixer for 10–20 min; mixing beyond 30 min can create electrostatically bound fines that do not coalesce uniformly. Internal air temperature in the mould is held between 260 °C and 300 °C during the coalescence phase, but light grey colour should not be regarded as a long-term UV stabiliser for PE tanks exposed outdoors; a separate hindered amine light stabiliser and antioxidant masterbatch must be qualified for the intended service life. Published data for this specific pelletised concentrate in food-contact rotomoulded tanks is limited, so final-article migration testing according to EU Regulation (EC) No 10/2011 or FDA 21 CFR 177.1520 is required before such use. Terminal products are grey chemical storage tanks, underground utility chambers, and agricultural water-holding cells.

    HDPE Sheet Melt Strength and LLDPE Carrier Dilution Effects

    In flat-die sheet extrusion from 0.5 mm to 6 mm thickness, LL803366/4 is metered at 1.5–3.0 wt% into natural HDPE or LLDPE/HDPE blends, and the three-roll stack is operated with middle roll surface temperature 60–90 °C to avoid embossed surface defects. The LLDPE carrier broadens the melting range of the diluted resin, which can reduce melt strength at the die lip; this is observed as edge sag and non-uniform draw after the sheet exits the calendar stack, particularly when die temperature exceeds 200 °C. In polypropylene sheet, the same concentrate is not fully miscible: differential scanning calorimetry on blended samples commonly shows a separate low-temperature melting endotherm from the LLDPE carrier, and flexural modulus tested according to ISO 178 or ASTM D790-17 may fall with increasing masterbatch addition. Let-down above 2.5 wt% in PP should be preceded by a notched impact test and a low-temperature instrumented falling-weight test on the actual part because the dispersed LLDPE phase can act as a stress concentrator at service temperatures below −10 °C. Terminal grey sheet products include industrial dunnage trays, reusable transit sheets, appliance back panels, and thermoformed automobile trunk floor liners.

    Under High Line Speeds, Melt-Pressure Oscillation Governs Drip Tube Colour Uniformity

    Light grey drip irrigation laterals and HDPE ducts extruded above 30 m/min require a gravimetric feeder with repeatability better than ±0.3%; LL803366/4 is fed into a natural PE80 or PE100 compound at 1.5–3.0 wt%, and the small tube diameter of 12–20 mm plus thin wall leaves a short residence time to homogenise masterbatch streaks. Screw L/D ratios of 24:1 to 30:1 are common on these lines, and pressure transducers ahead of the breaker plate should hold a melt-pressure band within ±10 bar; longer-period oscillations indicate feed surging or a carrier melt-flow mismatch and correspond with longitudinal light/dark grey banding on the extrudate surface. Dispersion is assessed on microtomed cross-sections by ISO 18553. Light grey pigmentation does not replace carbon black for UV blocking; pipes intended for multiyear above-ground solar exposure should be coextruded with a carbon black outer layer or formulated with a separate UV stabiliser masterbatch. For potable water contact, final system compliance with NSF/ANSI 61, AS/NZS 4020, or equivalent national standards must be demonstrated on the finished pipe and fittings. Terminal products are grey drip laterals, grey HDPE ducts, and low-pressure irrigation headers.

    When low-voltage power, signal, or instrumentation cable outer jacketing is specified in light grey, the formulation is more demanding than black jacketing because the absence of carbon black removes a natural UV-screening pigment; LL803366/4 is incorporated at 2.0–3.0 wt% only after the jacket compound has been qualified for thermal and UV endurance with a separate stabiliser package. The concentrate is added using a hopper or side gravimetric feeder on a single-screw cable extruder with L/D 24:1–30:1; melt temperatures are normally kept between 160 °C and 210 °C for EVA-rich sheath formulations, and screw speed is trimmed to keep die-head pressure stable because pigment agglomerates can accumulate on breaker plates after runs longer than 8 h. Final jackets are tested for tensile strength and elongation at break before and after thermal ageing according to IEC 60811-501, and the light grey shade is assessed against a customer-approved CIELAB reference using ASTM D2244. LL803366/4 is not recommended for primary insulation layers unless the complete insulation system passes the applicable electrical property tests, because the masterbatch is intended for sheath colouration only. Terminal products include grey sheathing for control cables, instrumentation lines, and low-voltage power distribution cables.

    Free Quote

    Competitive LyondellBasell POLYBATCH™ Light Grey LL803366/4 Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell POLYBATCH™ Light Grey LL803366/4 is a pelletized colour concentrate supplied with a linear low-density polyethylene carrier resin. The grade is designated for let-down in LLDPE and LLDPE-rich polyethylene streams, principally in film extrusion, pipe coating, and injection moulding. The light grey pigment system is dispersed in the LLDPE carrier; the product is a masterbatch rather than a pre-coloured compound. Published numerical specifications for this specific product are limited, and the following technical description therefore distinguishes between values documented for the LLDPE carrier class and properties that must be confirmed from the supplier’s certificate of analysis.

    The suffix 803366/4 is an internal formulation identifier. Public technical literature does not define the pigment-to-carrier ratio, the exact pigment composition, or the let-down tolerance. The term “light grey” is a qualitative colour description rather than an instrumental colour coordinate. Batch-to-batch colour tolerance should be obtained from the manufacturer as CIELAB ΔE* values under defined illuminant and observer conditions.

    Carrier-Resin Identity and Physical Form

    Because the concentrate is based in LLDPE, the carrier melt behaviour is expected to resemble that of linear low-density polyethylene film resins. Typical LLDPE carrier values fall within a density range of 0.918–0.922 g/cm³ when tested according to ISO 1183-1:2019 and a melt flow rate of 1.0–2.0 g/10 min at 190 °C under 2.16 kg load according to ISO 1133-1:2022. These are not product-specific limits for LL803366/4 and may be altered by the pigment loading. The melting peak temperature of an unfilled LLDPE carrier in this class is generally recorded between 119 °C and 124 °C using ISO 11357-3:2018. In the finished light grey concentrate, inorganic pigments or mixed metal oxides may broaden the crystallization exotherm and increase thermal conductivity relative to unfilled polymer.

    The material is supplied as pellets. Typical bulk density for LLDPE-based colour concentrates is approximately 0.55–0.65 g/cm³, but the vendor’s packaging or safety data sheet should be consulted. Pellet hardness, pellet size distribution, and dust content are controlled to allow continuous gravimetric feeding. Breakage and angel hair during pneumatic conveying can occur when pellet temperatures exceed 60 °C or when line velocities exceed 25 m/s. Slow, dense-phase conveying with radius bends is the standard practice for preserving pellet integrity on production lines.

    In blown-film extrusion, the concentrate is metered at the throat of a single-screw extruder or into the main feed stream upstream of the mixing section. Uniform colour development depends on the concentrate’s ability to be dispersed under the shear history of the primary film screw. A grooved-feed extruder with an L/D ratio of 30:1 and a barrier screw with a Maddock mixing element provides sufficient shear for polyolefin-based concentrates. Colour streaks can persist if the concentrate is added to a starved feed zone because reduced pressure generation and short residence time limit pigment dispersion. At a melt temperature of 193–232 °C at the die, typical LLDPE-rich film formulations maintain thermal stability during continuous operation. The light grey concentrate should not be exposed to die temperatures above 260 °C for extended runs, because organic components may degrade and produce yellowing, which is measurable as a shift in CIELAB b* value. Film opacity, haze, and gloss are evaluated using ASTM D1003, ASTM D2457, and ASTM D6290; however, published data for LL803366/4 in a defined film gauge is limited.

    What Let-Down Ratio Should Be Selected for LL803366/4 in Polyethylene Film?

    No universal let-down ratio is assigned to LL803366/4 in public documentation. Industrial formulation practice for LLDPE-based light grey concentrates commonly begins at 3 wt% for monolayer film and adjusts within a range of 2 wt% to 5 wt% based on final colour coordinates. At ratios below 1 wt%, gravimetric feeder resolution and hopper segregation may produce visible lot-to-lot variation, especially on lines with short mixing screws. At ratios above 5 wt%, the inorganic pigments can shift the melt rheology and may reduce tensile properties if dispersion is incomplete. The degree of dispersion is inspected by compression-moulding a thin film and examining it under polarized light microscopy; a quantitative accept/reject threshold for LL803366/4 is not published, so internal limits should be established on the target reduction ratio.

    Transitioning from dark-colour to light grey runs requires purging. A commercial purging compound with a melt flow rate above 10 g/10 min at 190 °C and 2.16 kg is used to shorten colour changeover. The screw and die should be cleaned until no visible carbonized specks or previous-colour streaks remain before introducing LL803366/4. Purging temperature should not exceed 230 °C for typical LLDPE carriers to avoid formation of black specks.

    When LL803366/4 Replaces a Universal Wax-Based Grey Concentrate in LLDPE Blown Film

    A switch from a wax-carrier universal concentrate to an LLDPE-based concentrate changes both dilution resin compatibility and film surface behaviour. The LLDPE carrier has a higher molecular weight and a higher melt viscosity than low-molecular-weight wax carriers. Low-molecular-weight wax carriers can migrate to the film surface, increasing coefficient of friction and altering heat-seal performance. Because the LLDPE carrier remains miscible with LLDPE film resin and does not introduce a separate low-melting phase, seal initiation temperature is primarily governed by the base film resin. The complete formulation must still be evaluated according to ASTM F88 for seal strength and ASTM F1921 for hot tack. Kinetic coefficient of friction is evaluated with ASTM D1894 and blocking with ASTM D3354. The absence of wax bloom may improve blocking resistance but may also reduce slip performance if external slip additives are not adjusted.

    Compared with a PP-carrier grey concentrate, LL803366/4 avoids the melting point mismatch between polypropylene carrier and polyethylene base resin. PP carrier domains may remain as discrete inclusions in LLDPE film produced at melt temperatures below 200 °C, creating visible gel-like defects or localised haze. The LLDPE carrier melts in the same temperature interval as the dilution resin, reducing the risk of hard pigments being carried by an unmelted carrier particle. This distinction is critical in thin-gauge film below 40 µm, where unmelted PP domains are more apparent and may reduce dart impact strength under ASTM D1709.

    Carrier Technology Melt Compatibility with LLDPE Observed Film or Moulding Defect Risk Relevant Test Method
    LLDPE carrier High; similar melting interval and rheology Streaks from inconsistent feeding or low shear ISO 1133-1:2022, ASTM D1003
    Low-molecular-weight wax carrier Limited; may bloom to surface Slip change, seal interference, coefficient of friction increase ASTM D1894, ASTM F88
    PP carrier Low; immiscible domains in PE melt Gel-like inclusions, localised haze, reduced dart impact ASTM D1709, ASTM D1003
    Pre-coloured compound No separate carrier phase No let-down variation, but higher inventory volume Supplier-specific CIE ΔE* data

    Assessing Regulatory Compliance for Polyolefin Color Concentrates

    Compliance documentation for LL803366/4 should be requested from LyondellBasell before use in food-contact, medical, or toy applications. Many polyolefin colour concentrates are evaluated against FDA 21 CFR 178.3290 for colourants for polymers and against EU Regulation 10/2011 for plastic materials intended to come into contact with food, but the specific status of LL803366/4 is not publicly confirmed. Absence of confirmation means the processor must obtain a written statement rather than infer compliance from the general POLYBATCH™ product line.

    The inorganic pigments in a light grey concentrate may be subject to heavy-metal restrictions. Under Directive 2011/65/EU for the restriction of hazardous substances, cadmium, lead, mercury, and hexavalent chromium are controlled. Standard analytical methods include EN 62321-5:2014 for cadmium and lead and EN 62321-4:2014 for mercury. For REACH obligations, a supplier statement is required if any substance of very high concern is present above 0.1% w/w by article weight. Inorganic pigment incompatibilities should also be considered; strongly acidic or oxidative process additives may destabilise certain mixed metal oxides, and the concentrate should not be premixed with oxidising chemical blowing agents without trial.

    Compliance Area Standard or Regulation Typical Data Required
    Heavy metals in plastics Directive 2011/65/EU Cd, Pb, Hg, Cr(VI) by EN 62321 series
    SVHC communication REACH Article 33 Supplier declaration at 0.1% w/w threshold
    Colourants for polymers FDA 21 CFR 178.3290 Supplier-specific compliance letter
    Food-contact migration EU Regulation 10/2011 Overall migration and specific migration limits
    Inorganic pigment loading ISO 3451-1:2019 Ash content of concentrate

    On production-scale extrusion lines with loss-in-weight gravimetric dosing, the predominant failure mode is concentrate segregation in the hopper. LLDPE-based pellets can stratify if the feeder hopper is refilled with excessive free-fall height or if regrind is mixed at the feed throat. Hopper agitation and low-level refill are used to preserve colour uniformity. When injection moulding, screw recovery time and shot-to-shot colour stability should be monitored because a higher-viscosity LLDPE carrier can alter plastication rates compared with low-molecular-weight universal concentrates. If pellets have been stored at temperatures below 10 °C and relative humidity above 60 %, they should be pre-dried at 60–80 °C for 2–4 h before feeding to prevent surface moisture defects. LLDPE is not hygroscopic, but surface condensation from cold storage can generate visible splay or silver streaking in film and moulded parts.

    Top