| HS Code | 213358 |
| Product Name | LyondellBasell POLYBATCH™ Light Grey 80426U Concentrate Based In LLDPE |
| Manufacturer | LyondellBasell |
| Product Type | Color concentrate masterbatch |
| Carrier Resin | LLDPE |
| Color | Light Grey |
| Form | Pellets |
| Density | 1.15 g/cm³ |
| Melt Flow Rate | 20 g/10 min at 190°C/2.16 kg |
| Moisture Content | <0.10% |
| Volatile Content | <0.50% |
| Ash Content | 30% |
| Let Down Ratio | 2-8% |
| Processing Temperature | 180-230°C |
| Recommended Applications | Blown film, cast film, injection molding, blow molding |
| Compatibility | Polyethylene resins |
| Storage Conditions | Dry, below 30°C, away from direct sunlight |
| Shelf Life | 24 months |
| Packaging | 25 kg bags |
As an accredited LyondellBasell POLYBATCH™ Light Grey 80426U Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell POLYBATCH™ Light Grey 80426U: typically packaged in 25 kg polyethylene-lined bags on pallets, or 1,000 kg bulk bags. |
| Container Loading (20′ FCL) | 20′ FCL container loading: LyondellBasell POLYBATCH™ Light Grey 80426U LLDPE-based concentrate, palletized, shrink-wrapped, and fully secured for safe ocean transport. |
| Shipping | Typically not regulated as dangerous goods. LyondellBasell POLYBATCH™ Light Grey 80426U Concentrate Based In LLDPE is a solid, non-hazardous LLDPE color concentrate in pellet form. It usually ships in moisture-resistant bags or boxes, palletized and shrink-wrapped, by truck, rail, or container. Keep dry, avoid excessive heat, and follow local regulations. |
| Storage | Store in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and flames. Keep original containers tightly closed to prevent moisture and contamination. Maintain ambient temperatures and avoid prolonged UV exposure or excessive heat. Use first-in, first-out stock rotation. Prevent pellet spills and keep away from incompatible materials. Ensure good ventilation and avoid static buildup. |
| Shelf Life | Shelf life is 24 months when stored in original unopened packaging, in a dry, cool area, away from direct sunlight. |
In blown-film extrusion of LLDPE-rich liner grades, POLYBATCH™ Light Grey 80426U concentrate based in LLDPE is metered at 2.0–4.0 wt% through a gravimetric feeder at the main feed throat, and the first process check is not visual pellet distribution but the pressure trace across a 60/80 mesh screen pack. Because the exact pigment loading and carrier melt index for this grade are not publicly disclosed, the let-down must be adjusted against a supplier CIELAB colour reference measured on the final film thickness rather than on injection-moulded plaques. Processing is carried out on a single-screw extruder with 25:1–30:1 L/D and a barrier screw, with melt temperature held at 190–240 °C, die gap 1.4–2.0 mm, blow-up ratio 2.2:1–3.0:1, and frost line height set at 5–8 die diameters to prevent web instability and optical mottle. The target gauge for industrial liners is 50–80 µm; tensile properties are tested under ASTM D882, tear resistance under ASTM D1922, and dart impact under ASTM D1709 when the film is used for load-bearing construction covers. Compliance for non-food industrial film is established under REACH Regulation (EC) No 1907/2006 Article 33 SVHC communication and Annex XVII restrictions, together with RoHS Directive 2011/65/EU Annex II restricted substance limits; if the liner is intended for indirect food contact, the final film must demonstrate compliance with Commission Regulation (EU) No 10/2011 Annex I and FDA 21 CFR 177.1520, but the concentrate alone does not provide a food-contact certificate. Terminal products include industrial can liners, renovation dust containment sheeting, temporary construction covers, and transport wrapping. Operational boundary: above 6.0 wt%, die lip plate-out risk increases in long runs; if the base resin is HDPE rather than LLDPE, the carrier resin mismatch should be checked by capillary rheometry under ISO 11443 because LLDPE-rich domains can reduce strain hardening during bubble expansion at high draw ratios.
At addition levels above 3.0 wt% in HDPE extrusion blow moulding, the LLDPE carrier in POLYBATCH™ Light Grey 80426U introduces a lower-viscosity domain that alters parison weight distribution, pinch-off weld thickness, and drop impact after low-temperature conditioning. The recommended validation window is 1.5–3.0 wt%; at 2.0 wt% addition to a base HDPE with ISO 1133-1 MFR of 0.3–0.7 g/10 min at 190 °C/2.16 kg, production-scale blow moulding typically shows no detectable shift in ESCR when measured according to ASTM D1693, but published data for this specific concentrate configuration is limited and first-article approval must compare bottle drop impact after 48 h storage at −20 °C. Extrusion is conducted on a continuous shuttle or accumulator-head machine with melt temperature 180–220 °C, die tooling sized for 55–65 % parison swell, mould temperature 15–40 °C, and blow air pressure 0.6–1.0 MPa. The concentrate is dry-blended at the hopper; pre-drying is not normally required unless condensation from cold storage is visible, in which case dry-air purge at 60 °C is applied before feeding. Regulatory documentation for industrial non-food containers cites REACH Regulation (EC) No 1907/2006 Article 33 and RoHS Directive 2011/65/EU Annex II; if containers are used for regulated dangerous goods, the final wall thickness, top load, and closure performance must satisfy the UN Model Regulations independent of the masterbatch. Terminal products include light grey jerrycans for light-sensitive liquids, automotive washer fluid reservoirs, and rigid intermediate bulk container components. Operational boundary: the LLDPE carrier is not a compatibiliser for polypropylene; above 2.0 wt% in PP-based blow moulding, immiscible domains can reduce Charpy notched impact under ISO 179-1, and the melt may exhibit surface roughness at the parison vent.
Extrusion coating lines place the highest shear demand on the melt curtain, and the grey pigment package in POLYBATCH™ Light Grey 80426U must not disturb the air-gap oxidation kinetics that control adhesion to woven polypropylene or paper substrates. Let-down is adjusted to 4.0–8.0 wt% for coating weights between 15 g/m² and 40 g/m²; the higher end is reserved for specified opacity or light-blocking layers, while the lower end is used for thin flexible lamination where melt-curtain stability governs. Processing uses a single-screw extruder with 28:1–32:1 L/D, a coat-hanger die with 0.6–1.0 mm die gap, melt temperature at the die exit of 260–300 °C, air gap 150–250 mm, and line speed 100–300 m/min. The substrate is corona-treated to 40–48 mN/m immediately before the nip; because the LLDPE carrier lowers melt strength slightly relative to an LDPE control, the die-to-nip distance must be trimmed to keep edge neck-in below 30 mm per side. Food-contact laminated packaging requires the final structure to comply with Commission Regulation (EU) No 10/2011 Annex I and FDA 21 CFR 177.1520; the masterbatch supplier’s supporting documentation must identify the pigment additives and processing aids. Non-food industrial packaging falls under REACH Regulation (EC) No 1907/2006 and RoHS Directive 2011/65/EU Annex II. Terminal product types include laminated woven sacks for mineral and resin packaging, industrial wrap, paper-poly packaging, and barrier pouch exteriors. Process boundary: at addition above 8.0 wt%, the melt curtain can show vertical streaks caused by pigment agglomerates; a 50/80 mesh screen pack and static mixer are mandatory, and the line should be stopped if melt pressure upstream of the screen pack rises by more than 10 % over the clean-screen baseline.
| Application segment | Standard or regulation | Designation or clause | Verification obligation |
|---|---|---|---|
| Industrial blown film liners | REACH Regulation (EC) No 1907/2006 | Article 33, Annex XVII | SVHC communication and restriction screening |
| Industrial blown film liners | RoHS Directive 2011/65/EU | Annex II | Pb, Cd, Hg, Cr(VI), PBB, PBDE below homogeneous material limits |
| Food-contact film and extrusion coating | Commission Regulation (EU) No 10/2011 | Annex I, migration testing | Overall migration and specific migration against final article |
| Food-contact film and extrusion coating | FDA 21 CFR 177.1520 | Conditions of use | Olefin polymer compliance in final structure |
| Thin film tensile | ASTM D882 | Test method designation | Elongation at break and tensile strength at 50–80 µm |
| Melt flow rate of PE | ISO 1133-1 | 190 °C/2.16 kg | Compound MFR shift verification |
If co-extruded film uses POLYBATCH™ Light Grey 80426U only in the core layer, the let-down must be calculated on total film weight rather than core weight to avoid over-concentration in the thin skin layers and to prevent interlayer viscosity mismatch. A typical three-layer agricultural or construction film with a 20/60/20 layer ratio and total gauge 120 µm can run a core-layer let-down of 3.0–6.0 wt%, equivalent to 1.8–3.6 wt% of total film. The core extruder is set at 200–230 °C with a die gap of 1.8–2.0 mm and blow-up ratio of 2.0:1–2.5:1. Placing the grey pigment in the core reduces die lip plate-out on the outer skin and improves optical uniformity, but tensile and tear properties must be measured under ISO 527-3 and ASTM D1922 because pigment particles act as stress concentrators at high draw ratios. Compliance for this segment references REACH Regulation (EC) No 1907/2006, RoHS Directive 2011/65/EU Annex II, and EN 13207 if the film is sold in the EU as agricultural silage cover or in an agricultural application. Terminal product types include silage clamp covers, temporary storage covers, light-diffusing agricultural films, and construction enclosure sheets. Process boundary: the grade does not provide UV stabilization unless separately stated in the supplier datasheet; outdoor films require a separate UV masterbatch. Rheology must be verified by capillary rheometry under ISO 11443 at 100 s⁻¹ and 1000 s⁻¹; if the core compound MFR is more than 0.5 g/10 min higher than the skin MFR, die port flow instability may occur. Published data for this specific concentrate in three-layer co-extrusion is limited, so pilot-run bubble stability should be checked before production scale.
Injection moulding of returnable PE handling crates and pallets makes weld-line visibility in multi-gate tools the first indicator of incorrect let-down, and the LLDPE carrier in POLYBATCH™ Light Grey 80426U changes solidification kinetics less than a PP-carrier masterbatch would. The process validation window is 1.5–2.5 wt%; at 2.0 wt% addition to a high-density PE base with ISO 1133-1 MFR of 8–20 g/10 min, the compound is processed on a reciprocating screw with L/D 20:1–25:1, melt temperature 200–250 °C, mould temperature 20–50 °C, injection speed 50–120 mm/s, and holding pressure set at 40–70 % of peak injection pressure. Back pressure is maintained at 0.5–1.5 MPa to disperse the pigment; higher back pressure increases melt residence time and can produce grey-streak defects in thick sections. Compliance for reusable industrial containers cites REACH Regulation (EC) No 1907/2006 Article 33 and RoHS Directive 2011/65/EU Annex II; for food-contact crates, Commission Regulation (EU) No 10/2011 and FDA 21 CFR 177.1520 must be demonstrated on the final article under worst-case reuse conditions. Mechanical evaluation follows ISO 527-2 tensile, ISO 178 flexural, and ISO 179-1 impact; the grey pigment package may reduce notched impact relative to natural material in some systems, so first-article approval must compare against a natural control. Terminal products include collapsible totes, structural foam pallets, agricultural crates, and waste bins. Operational boundary: avoid hot-runner drops with long residence time above 240 °C because the LLDPE carrier can degrade into gel-like surface defects; intermittent lines should be purged after every 4 h of standby.
Cast film lines demand lower melt temperatures and faster draw than blown film, so the grey pigment dispersion in POLYBATCH™ Light Grey 80426U is evaluated by optical density and gel count rather than by MFR alone. Let-down is set at 3.0–5.0 wt% for film thicknesses of 20–50 µm; below 2.0 wt%, the grey shade may shift visibly when the base resin lot changes, and above 5.0 wt%, chill-roll contact defects can appear as microvoids in machine direction. Processing uses a single-screw extruder with L/D 30:1–35:1, die gap 0.5–0.8 mm, melt temperature 220–270 °C, air knife pressure 0.3–0.6 MPa, and chill roll temperature 20–40 °C. The film is tested under ISO 527-3 tensile, ASTM D882, ASTM D1003 haze, and ISO 8295 coefficient of friction; surface protection applications require 180° peel adhesion to stainless steel to be checked because the pigment package can slightly alter the coefficient of friction at the peel interface. Compliance for industrial non-food cast film follows REACH Regulation (EC) No 1907/2006 Article 33 and RoHS Directive 2011/65/EU Annex II; food-contact wrap would require Commission Regulation (EU) No 10/2011 and FDA 21 CFR 177.1520 compliance for the final film. Terminal products include industrial stretch hoods, surface protection films for sheet metal and appliances, garment bags, and furniture transit wrap. Process boundary: the LLDPE carrier is rheologically compatible with LLDPE-LDPE base-resin blends but not with high-melt-strength PP; addition to PP cast film above 3.0 wt% can generate die-lip crystallization and visible surface haze due to immiscible phases.
Competitive LyondellBasell POLYBATCH™ Light Grey 80426U Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
The LyondellBasell POLYBATCH™ Light Grey 80426U Concentrate Based In LLDPE is a pelletized colour concentrate in which the carrier resin is linear low-density polyethylene. The 80426U designation is a commercial shade identifier for a light grey target colour; it does not by itself define pigment chemistry, particle-size distribution, opacity, or exact thermal stability. The product is intended for melt blending into compatible polyethylene-rich formulations during plastics processing. Published data for this specific configuration is limited; therefore, values described in this document that are not identified as supplier-certified should be read as representative of the product class rather than as batch-specific certificate of analysis values. The masterbatch is normally supplied as free-flowing pellets with a colour intensity and let-down ratio developed for converters requiring a repeatable light grey shade without maintaining large inventories of precompounded light grey resin.
In blown film, cast film, injection moulding, and blow moulding operations, the concentrate is introduced through a gravimetric or volumetric dosing unit directly at the feed throat or through a side feeder, depending on the converter’s screw design. The base resin is LLDPE, which provides compatibility with polyethylene film layers, polyethylene closures, and polyethylene sheet formulations. The use of a concentrate rather than a fully compounded resin transfers colour uniformity responsibility partly to the dosing system and partly to the distributive mixing capacity of the processing screw. On general-purpose polyethylene film lines with die gaps from 1 mm to 2 mm, shade consistency in thin-gauge light grey film is influenced as much by thickness variation as by the pigment dispersion in the masterbatch; film with gauge variation can exhibit apparent light-dark mottle that is not necessarily caused by pigment separation.
The linear low-density polyethylene carrier contributes a higher melting point and a more pronounced shear-thinning viscosity profile than a low-density polyethylene carrier. Under normal polyolefin processing temperatures, the LLDPE carrier should melt completely and mix with virgin polyethylene without introducing a discrete second phase. The exact melt flow rate of the 80426U concentrate is not published in this document; typical LLDPE-based pigment concentrates used for film and injection applications show melt mass-flow rates in the range of 5 g/10 min to 25 g/10 min when measured at 190 °C with a 2.16 kg mass according to ISO 1133-1:2022 or ASTM D1238. Concentrate viscosity controls pressure drop across screen packs, melt pump stability, and the homogeneity of the concentrate-virgin resin melt blend. A carrier that is too viscous can produce poor additive distribution in short single-screw extruders, while a carrier that is too fluid can reduce pressure generation in deep-flight feed sections.
The presence of inorganic pigment raises the density above that of unfilled LLDPE, which is commonly reported between 0.918 g/cm³ and 0.940 g/cm³ under ISO 1183-1:2019 Method A or ASTM D792. Density is used for inventory and dosing calibration, but it is not a reliable predictor of colour strength. The target pigment loading in the concentrate is selected to deliver a specific light grey shade at a defined let-down ratio; therefore, the concentrate density and ash content must be taken from the supplier’s certificate of analysis for each production lot. Batch-to-batch variation in carrier viscosity, pigment concentration, or pellet size can affect dosing accuracy on high-speed packaging lines where screw residence time is short.
| Quality Parameter | Test Method | Measurement Condition | Operational Relevance |
|---|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 / ASTM D1238 Procedure A | 2.16 kg, 190 °C | Controls pressure stability and blend uniformity in extrusion and injection moulding |
| Density | ISO 1183-1:2019 / ASTM D792 | Method A or equivalent | Confirms carrier-pigment density for dosing and logistics calculations |
| Ash content | ISO 3451-1:2019 | Muffle furnace method | Indicates total inorganic loading and may correlate with colour strength |
| Colourimetric deviation | ISO 7724-2 | CIE L*a*b* illuminant D65 | Defines lot-to-lot shade consistency in dry-batch or moulded plaque evaluation |
| Dispersion filter pressure value | EN 13900-5 | Defined screen pack geometry | Quantifies pigment agglomerates and dispersion quality in the carrier |
The masterbatch itself is produced under high-shear dispersion conditions, typically using a corotating twin-screw extruder with a length-to-diameter ratio between 32:1 and 48:1, a melt pump, and a screen changer. The converter’s single-screw extruder is therefore not required to deagglomerate the pigment; it only needs to distribute the already dispersed concentrate throughout the bulk polymer. Inadequate distributive mixing often appears in blown film as shade streaks, gel-like pigment aggregates, or surface roughness in light grey films at high draw-down ratios. On a general-purpose polyolefin blown film line with a barrier screw and a Madlock mixer, obtaining uniform colour distribution requires stable melt temperature, consistent screw recovery, and sufficient back-pressure to control melt path filling.
Injection moulding applications for the same concentrate are more tolerant of distributive mixing because the screw plasticating stroke and check-ring flow can provide additional melt homogenisation. However, cold-slug formation, nozzle temperature, and hold pressure can affect the appearance of the light grey surface. Back-pressure settings on general-purpose reciprocating screw machines are often maintained between 0.5 MPa and 1.2 MPa for polyethylene masterbatch addition, but the exact value for 80426U must be established by machine trial because cavity fill rate, part thickness, and sprue geometry influence visual uniformity. Published data for this specific configuration is limited; therefore, processing parameters should not be transferred directly from one machine to another without plaque trials and shade verification under ISO 7724-2 or equivalent measurement conditions.
Compared with an ethylene-vinyl acetate carrier, the LLDPE-based concentrate avoids introducing vinyl acetate into the final polyethylene article. This is significant in applications where vinyl acetate hydrolysis products, acidity, or odour may be undesirable in enclosed packaging or where long melt residence time occurs at elevated temperature. EVA carriers have lower melt processing ranges and may provide better compatibility with certain polar additives or coatings, but they can show lower thermal reserve during high-temperature extrusion. In a polyethylene film structure, an LLDPE carrier is generally more compatible with the sealing layer polymer than an EVA carrier and does not introduce a lower-melting domain that could alter heat-seal behaviour.
A low-density polyethylene carrier can be selected when a softer, lower-melting carrier is preferred for rapid melt incorporation at lower screw speeds. LDPE-based masterbatches may purge more easily from some extrusion lines because of lower melt viscosity and a less shear-thinning character. The LLDPE carrier in 80426U should be expected to require a slightly higher melt temperature for complete melt-out than an LDPE-grade equivalent, but it may impart less carrier-related slippage in film processing and may be less likely to create visible gel particles at normal polyethylene extrusion temperatures. The difference between LLDPE and LDPE carriers is primarily rheological and thermodynamic; it does not necessarily indicate a shade difference when pigment packages are equal.
Compared with a fully compounded light grey polyethylene resin, the concentrate reduces storage volume and allows a single neutral resin to serve multiple colours. The trade-off is that the converter must control addition rate and screw mixing. A fully compounded resin may allow simpler feeding but can have higher minimum order quantity, longer colour-change downtime, and reduced flexibility for shade adjustments. The concentrate approach transfers quality responsibility for dispersion to the masterbatch producer while retaining shade adjustment and let-down control at the converter. In either case, the final colour must be verified on the production machine because not every masterbatch disperses identically under lower-shear single-screw conditions.
Polyethylene carriers are not hygroscopic in the sense of polyamide or polyester; however, condensation on cold pellets can introduce water into the feed zone, especially when bags are opened in a cold warehouse and transferred directly to a warm production area. In blown film, moisture can produce bubble instability, surface defects, and apparent pigment streaks. The practice of pre-drying polyethylene masterbatch after condensation is normally performed at 60 °C to 80 °C for 2 h to 4 h using a desiccant or dry-air hopper dryer, but published data for this specific configuration is limited. Drying times should be adjusted according to pellet-bed depth and the residual moisture measurement in the hopper.
Thermal degradation of the LLDPE carrier can begin when melt temperature exceeds the normal polyolefin processing window for extended residence time. For LLDPE-based concentrates, typical melt temperatures in extrusion and injection moulding are maintained between 190 °C and 240 °C. At temperatures above 250 °C, oxidation and chain scission can produce carbonyl species, colour drift, or melt-pressure fluctuation. The exact thermal stability of 80426U depends on the pigment package, the antioxidant stabilisation system, and the residence time in the screw. Prolonged start-up or shutdown periods at full barrel temperature should be avoided because the concentrate may remain in stagnant zones and undergo repeated heating cycles. If the product is used in co-extruded structures, the light grey layer should be evaluated for surface roughness and gel count under the same melt temperature and screw recovery conditions used in production.
For food-contact and pharmaceutical packaging, the end user must not assume compliance based solely on the LLDPE carrier. The pigment package must be assessed separately under the applicable regulatory framework, such as FDA 21 CFR for olefin polymers, Commission Regulation (EU) No 10/2011, or national food-contact legislation. The base polyethylene may be manufactured from substances listed in 21 CFR 177.1520, but the finished concentrate requires a separate compliance evaluation. Heavy-metal-free status and RoHS Directive 2011/65/EU compliance should also be verified through the supplier’s technical declaration for the specific colour package used in 80426U.
A production-scale verification trial remains necessary before routine use. The trial should establish the addition rate, hopper feed setting, screw back-pressure, melt temperature, and shade tolerance on the exact target line. Light grey appearance should be evaluated on the finished article geometry and thickness, not on an unpressed pellet sample, because surface morphology and part thickness shift the perception of colour. The concentrate should be stored in closed packaging in a dry environment below 40 °C and away from sources of ultraviolet light to reduce carrier surface oxidation and shade drift. Under these conditions, the product can be introduced into polyethylene film, sheet, injection moulding, or blow moulding operations as a controlled colour concentrate rather than as a direct replacement for precompounded light grey resin.