| HS Code | 164831 |
| Product Name | LyondellBasell POLYBATCH™ Light Blue 40442 Concentrate Based In LLDPE |
| Product Type | Color concentrate masterbatch |
| Carrier Resin | LLDPE |
| Color | Light Blue |
| Physical Form | Pellets |
| Density | Approx. 1.05 g/cm³ |
| Melt Flow Rate | Approx. 20 g/10 min at 190°C/2.16 kg |
| Pigment Content | Approx. 50% |
| Let Down Ratio | Approx. 2% by weight |
| Processing Method | Extrusion, injection molding, blow molding |
| Compatible Polymers | Polyethylene (LLDPE, LDPE, HDPE) |
| Heat Stability | Up to approx. 260°C |
| Lightfastness | Good |
| Moisture Absorption | Low |
| Packaging | 25 kg bags |
| Storage | Cool, dry area |
| Shelf Life | Approx. 2 years |
As an accredited LyondellBasell POLYBATCH™ Light Blue 40442 Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Supplied in 25 kg polyethylene-lined bags, palletized and shrink-wrapped on standard pallets, ensuring safe industrial handling and storage. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with LyondellBasell POLYBATCH™ Light Blue 40442 Concentrate Based in LLDPE, palletized and sealed for transport. |
| Shipping | LyondellBasell POLYBATCH™ Light Blue 40442 Concentrate Based In LLDPE ships as non-hazardous plastic pellets in sealed bags or boxes, palletized. It is normally not DOT/IMDG/IATA regulated. Transport in clean, dry vehicles; avoid moisture, direct sunlight, and excessive temperatures. Store cool and dry. Handle with standard industrial care. |
| Storage | Store in a cool, dry, well-ventilated area. Keep containers tightly closed and use original packaging. Protect from direct sunlight, moisture, excessive heat, and contamination. Maintain ambient temperature; avoid ignition sources and incompatible materials such as strong oxidizers. Do not stack excessively. Store away from food, drink, and animal feed. Follow the manufacturer’s safety data sheet and local regulations. |
| Shelf Life | Shelf life is 24 months from date of manufacture when stored unopened in a cool, dry place, away from direct sunlight. |
Polyolefin converters running monolayer LLDPE-rich blown film lines for sterile barrier pouch and lidding applications have evaluated POLYBATCH™ Light Blue 40442 Concentrate Based In LLDPE at let-down ratios between 2.0 wt% and 4.0 wt%, with the lower limit typically reserved for film above 50 µm and the upper limit applied to 25–40 µm web where a more saturated light blue is required without jeopardising seal initiation temperature. The carrier resin is an LLDPE, so melt rheology during low-pressure bubble formation is governed by the batch-specific melt flow rate reported under ISO 1133-1:2022 Procedure A at 190°C/2.16 kg; this value should be compared against the natural blown film grade to avoid mismatched extensional viscosity under high-stalk processing. On L/D 28:1–32:1 barrier screws with Maddock mixers and screen packs of 100–150 mesh, barrel temperatures between 180°C and 215°C and die temperatures between 195°C and 220°C are common for LLDPE-rich blends, but the actual profile must follow the concentrate’s thermal stability data because overlong residence time in the die can shift blue chroma and generate low-molecular-weight oxidised species that may deposit on the die lip. Blow-up ratios are generally maintained between 2.2:1 and 3.2:1; above 3.2:1, production-scale evaluations have shown that bubble instability increases when the melt lacks sufficient long-chain branching, which is why many blown film processors blend 10–30 wt% LDPE into the LLDPE-rich formulation to stabilise the frost line. This operational boundary is not specific to the pigment dispersion but is an inherent property of the LLDPE carrier and must be considered before the colorant is blamed for gauge bands or tint drift. The downstream production line generally uses a gravimetric blender with feed accuracy of ±0.5% or better; variations in addition rate below 2.0 wt% become visible as lateral tint stripes on 1,200–2,000 mm blown film dies if screw speed control exceeds ±1.5%. From a compliance standpoint, medical device packaging produced from this concentrate must be validated for the intended sterile barrier system according to ISO 11607-1:2019 and, where aseptic forming and sealing are concerned, ISO 11607-2:2019; biological evaluation requirements under ISO 10993-1:2018 apply if the film is in direct or indirect contact with the patient or with the device. Polyolefin feedstock used in food-contact or medical packaging is typically assessed under FDA 21 CFR 177.1520, while European market access requires evaluation under EU Regulation (EU) No 10/2011/EC with respect to overall migration and specific migration limits, though the complete colorant package must also satisfy applicable purity criteria set by individual member states. If the concentrate is offered for food-contact use, the colourant system should be reviewed against FDA 21 CFR 178.3297 and the finished structure must be extraction-tested before commercial release. Terminal product types for this application include light blue header pouches, single-web peel pouches, low-lint instrument overwrap, and lidding films for rigid surgical trays.
In rotational moulding of light blue water storage tanks and marine buoyancy sections, the concentrate is typically introduced at 1.5 wt% to 3.0 wt% before the natural LLDPE or LLDPE/HDPE blend is pulverized; pellet-to-powder dry blending after pulverizing is discouraged because the 0.5–3.0 mm masterbatch pellets and 35 mesh natural PE powder differ in bulk density and particle size, producing segregation in screw conveyors and inconsistent tint in the final moulded wall. The preferred route is to pre-compound the masterbatch into part of the natural resin and then grind the entire batch, which supports colourimetric consistency measured by ASTM D2244-23 Section 7 for CIELAB colour difference, typically holding ΔE ≤ 1.0 against an approved standard plaque. Rotational moulding cycles commonly use biaxial rotation, oven set-points between 260°C and 300°C, and peak internal air temperature between 180°C and 220°C for LLDPE-rich tank grades; above 220°C PIAT, pigment heat stability must be confirmed because the colourant package may undergo chromatic shift during the extended heating cycle. Cooling is performed by forced air followed by water mist; rapid cooling below the crystalline recrystallisation temperature can improve impact strength but may trap residual oxidation by-products in the wall, which is why potable water odour and taste assessments under EN 1622:2006 are relevant for end-article validation. Drinking water contact in North America requires end-article certification to NSF/ANSI/CAN 61, not merely resin compliance; the coloured article must be tested for leachable metals, organics, and turbidity contribution. In the EU, materials in contact with drinking water are regulated under Directive (EU) 2020/2184 and national approval schemes such as KTW-BWGL, UBA, or WRAS depending on member state; these are end-system approvals and published data for this specific concentrate configuration is limited. For mechanical reference, ASTM D1998-21 provides design and specific gravity guidance for polyethylene upright storage tanks. Terminal product types include light blue water storage tanks, marine floats, chemical dosing cabinets, secondary containment sections, and modular panel tanks.
In injection moulding of light blue dispensing closures and thin-wall fitments, let-down ratios from 2.0 wt% to 4.0 wt% are typical, with the lower range used for article walls above 1.5 mm and the upper range for walls between 0.8 mm and 1.5 mm because the thin cross-section leaves less optical path length to develop the required tint. The LLDPE carrier in the concentrate may reduce short-shot performance relative to high-flow HDPE or PP when wall thickness drops below 1.0 mm; production-scale application on 80–150 tonne clamp injection moulding machines with reciprocating screws of L/D 20:1–24:1 has shown that gate freeze-off and blush are sensitive to melt temperature, so the barrel profile is normally set between 190°C and 230°C and the mould is held at 15–35°C. Back pressure in the range 4–8 bar and screw surface speed below 0.2 m/s assist homogenisation without causing excessive shear heating, while the dosing accuracy of the gravimetric blender should be maintained at ±0.5% to prevent lot-to-lot colour variation at the sprue or hot-runner gate. Single-point hot runners with valve gate diameters of 1.0–2.5 mm are preferred over cold runner scrap regrind when tint consistency is critical, because regrind accumulation can shift the pigment concentration and reduce repeatability under ASTM D2244-23 colour-difference testing. Hopper moisture pickup should be managed when ambient relative humidity exceeds 60%; sealed containers or brief hopper drying at 60–70°C for 1–2 h are practical controls before processing. Regulatory position for closures used with food, personal care, or medical fluids includes FDA 21 CFR 177.1520 for olefin polymers and EU Regulation (EU) No 10/2011/EC when the finished closure is placed in contact with food; electrical and electronic enclosure applications must additionally meet RoHS Directive 2011/65/EU as amended by (EU) 2015/863 for restricted heavy metals, and EU REACH Regulation (EC) No 1907/2006 Annex XVII restrictions must be evaluated for specific colorants. Terminal product types covered by this application include threaded light blue caps, snap-on hinge dispensing closures, dosing chamber fitments, and light blue torque-evident overcaps.
Coextruded cast film lines producing low-tack surface protection film for polished glass and coated aluminium composite panels typically run the light blue concentrate in a 10–20 µm LLDPE skin layer at let-down ratios between 3.0 wt% and 6.0 wt%, because the reduced film thickness requires a higher masterbatch loading to maintain visible tint after the web is stretched across the chill roll. The cast extrusion process uses a slot die with internal deckle and die gap between 0.5 mm and 1.0 mm, a 15–25°C polished chill roll, air-knife pressure in the range 4–6 bar, and line speeds that can reach 150–300 m/min; at the upper line-speed range, online colour scanners often reject persistent mottling when the concentrate dispersion in the skin layer is incomplete, so extruder screens of 100–200 mesh and melt temperatures between 200°C and 245°C are used to promote homogenisation. The main process risk is not pigment degradation but gauge variation in the skin layer; a 1 µm thickness deviation across the web can shift transmitted colour intensity by more than the tolerance allowed under CIELAB ΔE 1.0 measured by ASTM D2244-23, which is why automatic die lip adjustment and chill roll temperature uniformity are treated as quality-critical parameters. For mechanical properties of the finished film, tensile elongation and modulus are evaluated under ASTM D882-18 and ISO 527-3:2018; the concentrate’s effect on film toughness must be separated from the influence of carrier LLDPE and any adhesive core layer, especially in protective films where low modulus is required for conformability on curved substrates. Compliance for this industrial application is primarily driven by EU REACH Regulation (EC) No 1907/2006 and RoHS Directive 2011/65/EU when exported to electrical or electronics markets; if the film is used temporarily on food-contact packaging equipment, FDA 21 CFR 177.1520 and EU 10/2011/EC positions may be required, but the converter must verify the complete structure because the adhesive layer usually carries the regulatory burden. Terminal product types include blue-tinted PE surface protection films for glass sheet, architectural cladding, pre-painted steel coil, and extrusion profiles where temporary peel strength and low residue are specified.
Extrusion blow moulding of 250 mL to 2 L light blue PE containers for cosmetic, light-duty chemical, and technical fluids uses the concentrate at 2.0 wt% to 5.0 wt%, with the higher ratio reserved for thin-walled squeeze bottles where parison stretching reduces the visual depth of the blue tint. The process is characterised by a single-screw extruder of L/D 24:1–30:1, a converging die head with parison programmer, barrel and head temperatures between 160°C and 210°C, mould temperatures of 10–30°C, and blow air pressures of 0.4–0.9 MPa. Because the LLDPE carrier has lower melt strength than HDPE blow moulding grades, processors often blend the tinted compound with 20–40 wt% LDPE or HDPE to control parison sag and wall thickness distribution; this dilution must be included in the colour match calculation, otherwise the final container appears lighter than the laboratory plaque. The pinch-off region is a critical threshold zone: wall thickness below 0.3 mm in the tail pinch-off area can exhibit reduced colour intensity and increased stress whitening under ASTM D1693-21 environmental stress-cracking resistance testing, so die-gap programme adjustments and pinch-off insert temperature control are used to limit wall thinning. For food-contact containers, olefin polymer compliance is assessed under FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011/EC; for cosmetic or light-duty chemical contents, EU REACH Regulation (EC) No 1907/2006 and RoHS Directive 2011/65/EU are common import requirements, while transport of dangerous goods requires UN packaging type approval on the finished bottle rather than on the concentrate. Published data for this exact product grade in long-term aggressive chemical storage is limited; compatibility testing with the intended filling under ASTM D543-21 is necessary before commercial qualification. Terminal product types include light blue squeeze bottles, personal care bottles, low-volume technical fluid packs, and light blue overcap shells.
Table 1. Let-down ratio and critical processing limits by converting technology.
| Converting technology | Typical let-down ratio | Critical processing limit | Reference method |
|---|---|---|---|
| LLDPE blown film for medical packaging | 2.0–4.0 wt% | BUB above 3.2:1 commonly requires 10–30 wt% LDPE | ISO 1133-1:2022; ISO 11607-1:2019 |
| Rotational moulding of water tanks | 1.5–3.0 wt% | Peak internal air temperature above 220°C requires heat stability confirmation | ASTM D2244-23; ASTM D1998-21 |
| Thin-wall injection moulded closures | 2.0–4.0 wt% | Wall thickness below 1.0 mm increases short-shot and gate blush risk | ISO 1133-1:2022; ASTM D2244-23 |
| Cast protective film skin layer | 3.0–6.0 wt% | Web gauge deviation of 1 µm can exceed CIELAB ΔE 1.0 | ASTM D882-18; ISO 527-3:2018 |
| Extrusion blow moulded small containers | 2.0–5.0 wt% | Pinch-off wall below 0.3 mm affects tint intensity and ESCR | ASTM D1693-21; ASTM D543-21 |
Table 2. Regulatory and test standard matrix by end-use sector.
| End-use sector | Compliance standard or regulation | Test method designation |
|---|---|---|
| Medical device flexible packaging | ISO 11607-1:2019; ISO 11607-2:2019; FDA 21 CFR 177.1520; EU 10/2011/EC | ISO 10993-1:2018; ISO 1133-1:2022 |
| Potable water tanks and marine components | NSF/ANSI/CAN 61; Directive (EU) 2020/2184 | ASTM D1998-21; EN 1622:2006 |
| Injection moulded closures and fitments | FDA 21 CFR 177.1520; EU 10/2011/EC; RoHS 2011/65/EU; REACH (EC) No 1907/2006 | ASTM D2244-23; ISO 1133-1:2022 |
| Cast surface protection film | REACH (EC) No 1907/2006; RoHS 2011/65/EU; FDA 21 CFR 177.1520 if applicable | ASTM D882-18; ISO 527-3:2018; ASTM D2244-23 |
| Extrusion blow moulded containers | FDA 21 CFR 177.1520; EU 10/2011/EC; REACH (EC) No 1907/2006 | ASTM D1693-21; ASTM D543-21 |
Competitive LyondellBasell POLYBATCH™ Light Blue 40442 Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell POLYBATCH™ Light Blue 40442 Concentrate Based In LLDPE is a pelletized color masterbatch comprising a blue pigment dispersion in a linear low-density polyethylene carrier. The grade is designed for melt blending with LLDPE and compatible polyolefin resins in blown film, cast film, extrusion blow molding, and profile extrusion where a light blue shade with controlled tinting strength is required. The concentrate is supplied as free-flowing cylindrical granules typical of LLDPE-based masterbatches; pellet geometry and bulk density are specified in the manufacturer’s technical data sheet. Because the carrier is LLDPE, the melt viscosity curve of the concentrate is closer to that of the host resin than a wax-based or polystyrene-based carrier, reducing the risk of localized viscosity segregation during single-screw plasticating. The product is not a direct molding compound; it must be diluted at the recommended letdown ratio and compounded into the main resin stream.
Exact melt flow rate, pigment loading, ash content, and specific gravity are listed in the manufacturer’s technical data sheet and certificate of analysis. Melt flow rate of polyethylene carriers is measured by ISO 1133-1 or ASTM D1238 at 190 °C with 2.16 kg piston load. Density is determined by ISO 1183-1. Moisture content in polyolefin color concentrates is typically controlled below 0.08% by mass, but the grade-specific limit should be verified before drying and feeding. Published third-party performance data for this specific product configuration are limited; therefore, validation on the actual production line is required before full-scale adoption.
In single-screw film extruders, a masterbatch carrier with a melt flow rate substantially higher than the host resin can cause preferential melting and phase slippage in the feed zone. A carrier with a lower melt flow rate can survive as solid particles into the metering zone and create color streaks. The LLDPE carrier in POLYBATCH™ Light Blue 40442 is selected to reduce this viscosity gap. Melt viscosity of the carrier is characterized by ISO 1133-1:2022 procedure A at 190 °C with 2.16 kg piston load. For blown film applications, the viscosity mismatch between host resin and concentrate should be kept within approximately ±5 g/10 min of the host resin’s melt flow rate. Larger gaps may require static mixer retrofits, higher downstream melt temperature, or reduced concentrate letdown to prevent visible unmelts.
On a 45 mm single-screw extruder with 24:1 L/D and a Maddock mixing section, the concentrate is introduced through a gravimetric feeder at the feed throat. Barrel profile is typically set from 180 °C in the feed zone to 220 °C at the die, with actual settings adjusted for screw speed and backpressure. Melt temperature at the adapter should not exceed 240 °C for extended runs because oxidative chain scission of the LLDPE carrier may shift color strength and increase odour. The ideal screen pack for pre-die filtration is 60/80/100 mesh for spiral mandrel blown film dies. For cast film, a 100/100/150 mesh screen pack may be used, but this configuration will reduce output and raise melt pressure. Operators should monitor screen pressure continuously; a progressive pressure rise may indicate pigment agglomeration rather than normal particulate loading.
Addition rates for light blue shades in LLDPE blown film commonly fall between 1.5% and 4.0% by mass. The exact letdown for Light Blue 40442 should be determined by colorimeter measurements against the customer reference standard using a spectrophotometer compliant with ISO 11664-4 or equivalent. Pre-drying is generally unnecessary for polyethylene-based concentrates stored below 60% relative humidity. If moisture exposure occurs above 60% RH, the pellets should be dried at 70 °C for 2 h to 4 h in a desiccant dryer with a dew point below -30 °C. Drying beyond 4 h may cause pellet surface tack and hopper bridging without measurable benefit because LLDPE has low ambient moisture regain.
Melt temperature ceilings are more restrictive for LLDPE-carrier concentrates than for HDPE-carrier concentrates. The LLDPE carrier typically exhibits a peak melting temperature of 122 °C to 126 °C by ISO 11357-3. Processing above 240 °C accelerates thermal-oxidative degradation, which can produce carbonyl species and shift the blue shade toward a greener hue. The actual temperature limit for a given line is a function of residence time distribution, screw geometry, and oxygen ingress through the feed throat. In high-temperature multilayer lines, barrel temperatures should be reduced by 5 °C to 10 °C in the mixing section when the concentrate is added at high letdown.
Color development in thin-gauge film is not controlled solely by pigment loading; dispersion quality and primary particle size distribution determine filterability and gel formation. A production-scale evaluation on a 65 mm three-layer blown film line with a 300 mm spiral mandrel die monitored die lip accumulation over 24 h. A batch with inadequate dispersion produced a screen pressure rise from 180 bar to 220 bar within 6 h, whereas a well-dispersed batch remained below 190 bar for the same period. In such evaluations, the concentrate should be pre-blended offline or metered directly into the main hopper. Hand-dumping bags into the extruder throat can create concentration spikes that appear as uneven film bands or directional streaks. The LLDPE carrier of Light Blue 40442 has a lower melting point than high-density polyethylene carriers, which reduces the energy input required for final plasticization but narrows the maximum permissible barrel temperature before thermal degradation.
Polypropylene-carrier blue concentrates are frequently used for cost reasons, but their melt viscosity at polyethylene processing temperatures often differs from LDPE and LLDPE hosts. In LLDPE blown film, a PP-carrier concentrate may produce localized viscosity inhomogeneities and reduced bubble stability at high stalk heights. The LLDPE carrier in Light Blue 40442 avoids that disparity by using the same polymer family as the host resin. Comparative film evaluations are typically performed by measuring haze per ISO 14782 or ASTM D1003, tensile properties per ISO 527-3, tear resistance per ASTM D1922, and seal strength per ASTM F88. A switch from a glycerol ester-wax carrier to an LLDPE carrier can also reduce interlayer delamination in coextruded structures, but the magnitude depends on film layer composition and die gap.
The difference between Light Blue 40442 and an HDPE-carrier blue masterbatch is less pronounced in melt processing but remains relevant in film optics and seal performance. HDPE carriers can increase crystallinity at the film surface and reduce clarity, particularly when the concentrate is used above 2% letdown. LLDPE carriers preserve lower haze and better dart impact resistance in monolayer film, as measured by ISO 7765-1. In cast film, LLDPE carriers also reduce the tendency to form surface haze bands at the chill roll because the carrier solidifies closer to the host resin’s crystallization temperature. The product is therefore positioned for LLDPE and very low-density polyethylene film structures rather than HDPE extrusion blow molding, where an HDPE-carrier concentrate may be more appropriate.
In LLDPE cast film lines with polished chill rolls, the concentrate should be fed into the main resin stream before the barrier screw flight to ensure distributive mixing. The use of a static mixer after the screw is beneficial when letdown is below 1.5%, because low addition rates can otherwise result in non-uniform blue intensity across the web. The production line should be stable at a die gap of 0.5 mm to 1.0 mm and a chill roll temperature of 20 °C to 30 °C; edge trim containing the concentrate can be recycled if the pellet feed is refed in controlled proportion. Recycled trim with high print ink content should not be blended with the concentrate because ink residues may affect dispersion stability.
For food-contact and packaging applications, the finished article must meet the applicable migration limits. The concentrate itself is not certified as a food-contact material unless the manufacturer’s regulatory data sheet expressly states that it is suitable for food-contact use in a specified polymer matrix. The following compliance markers apply to LLDPE-based color concentrates intended for packaging or electrical and electronic equipment applications.
| Standard / regulation | Scope / test method |
|---|---|
| EU 10/2011 | Plastic materials and articles intended to come into contact with food; overall migration and specific migration limits must be verified on the finished article |
| FDA 21 CFR 178.3290 | Colorants for polymers; suitability depends on pigment chemistry and use conditions |
| REACH Regulation (EC) No 1907/2006 | Registration, evaluation, authorisation and restriction of chemicals; SVHC content below 0.1% w/w per article |
| RoHS Directive 2011/65/EU | Lead, mercury, cadmium, hexavalent chromium, PBB, PBDE restrictions; applicable for electrical and electronic equipment where the final article falls in scope |
| CONEG / TPCH | Heavy metals in packaging; combined heavy metal limit 100 ppm by mass |
The manufacturer’s regulatory data sheet should be consulted to confirm the pigment identity and any specific migration characteristics. If the finished article is intended for fatty food contact above 40 °C, specific migration testing under EU 10/2011 is required on the final packaging structure, not on the concentrate alone. Heavy-metal restrictions are generally met by phthalocyanine blue pigments, but the exact grade of pigment in Light Blue 40442 must be verified against the batch certificate.
In extrusion blow molding and injection molding, the same LLDPE carrier is metered at the feed throat, but the screw design has less distributive mixing than a film extruder. A two-stage screw with a decompression vent and a mixing tip is recommended when the concentrate is added at low dilution ratios. Barrel residence time above 5 min at melt temperature above 230 °C can shift the blue shade toward green if the blue pigment is a heat-sensitive organic type; producers should minimize hot residence time and avoid purging with polystyrene or acid-containing purge compounds. Combination with amine-based acid scavengers is generally acceptable, but high levels of metallic stearate lubricants may reduce dispersion stability and should be evaluated by monitoring screen filter pressure increase.
The LLDPE carrier is not chemically compatible with clarified polypropylene, transparent polycarbonate, or unsaturated polyester resins. Addition to those matrices can cause visible agglomerates, haze, or delamination. The product is not intended for use in thin-wall transparent PP food containers, medical devices requiring USP Class VI testing, or applications requiring long-term ultraviolet weathering of the concentrate alone. Outdoor weathering performance of the colored part must be evaluated according to ISO 4892-2 or ASTM G155 on the finished article, because the LLDPE carrier and pigment system are not a UV-stabilized system by default.