| HS Code | 755075 |
| Carrier Resin | LLDPE |
| Color | Red |
| Form | Pellets |
| Density | 1.05 g/cm³ |
| Melt Flow Rate | 20 g/10 min (190°C/2.16 kg) |
| Pigment Content | 50% |
| Moisture Content | <0.2% |
| Processing Temperature | 180-230°C |
| Let Down Ratio | 24:1 (4% addition) |
| Compatibility | Polyolefins |
| Lightfastness | 7 (Blue Wool Scale) |
| Heat Stability | 260°C |
As an accredited LyondellBasell POLYBATCH™ House Red 50311U/4 Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Typically packaged in 25 kg polyethylene-lined bags, palletized; standard pallet quantity is 1,000 kg (40 bags) for safe handling. |
| Container Loading (20′ FCL) | 20′ FCL loaded with LyondellBasell POLYBATCH™ House Red 50311U/4 concentrate based in LLDPE, palletized in sealed bags, secured for transport. |
| Shipping | POLYBATCH™ House Red 50311U/4, a non-hazardous LLDPE-based color concentrate, ships as non-regulated cargo. It is typically packaged in bags or boxes, palletized and stretch-wrapped. No UN number, hazard class, or marine pollutant designation applies. Keep dry, avoid excessive heat, and consult the SDS. |
| Storage | Store in a cool, dry, well-ventilated area in original, tightly closed containers. Protect from direct sunlight, heat, moisture, and ignition sources. Keep away from incompatible materials and contaminants. Maintain ambient storage temperatures; avoid freezing or excessive heat. Use adequate ventilation and follow local regulations. Do not stack excessively. |
| Shelf Life | Typically two years from date of manufacture when stored in original unopened packaging, dry, below 30°C, away from direct sunlight. |
During single-screw blown film extrusion of LLDPE/LDPE blends incorporating LyondellBasell POLYBATCH™ House Red 50311U/4 Concentrate Based In LLDPE, the carrier resin's comparatively high melt flow index—typically 20–30 g/10 min when determined per ISO 1133-1:2022 at 190 °C with 2.16 kg load—necessitates screw configurations with a minimum L/D ratio of 24:1 and a downstream mixing element to achieve adequate distributive dispersion before the melt reaches the annular die. Instances of pigment agglomerate deposition at the die lip, documented on production lines operating with die gaps below 1.2 mm and let-down ratios exceeding 4.5 wt%, have been attributed to insufficient shear history in shallow-metering feed sections; the condition manifests as intermittent red streak defects detectable under ASTM D6290 colorimetric evaluation with ΔE values exceeding 1.5 CIE units relative to laboratory pressed plaques. Blow-up ratios between 2.2:1 and 3.0:1 with frost line heights between 300 mm and 450 mm above the die face have been documented to produce acceptable gauge uniformity in the 18–45 μm film thickness range; increasing BUR beyond 3.5:1 introduces pigment orientation effects and gauge variation that produce visible streaking in formulations containing this concentrate at loadings near the upper bound.
Industry compliance for refuse sack and can liner applications is anchored to EU Directive 94/62/EC Article 11, which restricts the combined concentration of lead, cadmium, mercury, and hexavalent chromium to 100 mg/kg in packaging or packaging components; heavy metal verification is executed by acid digestion followed by ICP-OES in accordance with EPA Method 3050B/6010D. For North American markets, the Coalition of Northeastern Governors (CONEG) Model Toxics in Packaging Legislation imposes the identical 100 ppm total limit for the four regulated metals. The formulation addition ratio for standard refuse sack production in virgin LLDPE/LDPE blends—typically 70 wt% LLDPE (MFI 1.0–2.0 g/10 min, density 0.918–0.925 g/cm³ per ASTM D792) and 30 wt% LDPE—is 2.0–4.0 wt%, achieving sufficient opacity for 20–40 μm films. Let-down rates below 1.5 wt% produce perceptible translucency in film thicknesses above 30 μm, while loading above 5.0 wt% introduces the risk of melt fracture at output rates exceeding 450 kg/h on 80 mm screw diameter extruders. Downstream production equipment for this scenario consists of single-screw extruders with 65–90 mm screw diameters, spiral mandrel dies of 200–350 mm diameter, and oscillating haul-offs for flat-width winding; output speeds of 60–90 m/min are standard for 25 μm films. Terminal products include high-density commercial can liners at ≥38 μm, municipal refuse sacks spanning 25–60 μm, and industrial waste bags requiring color-coded waste stream identification under ISO 14021 environmental labeling practices.
Because high-cavitation injection molding of thin-walled closures (0.6–1.2 mm wall section) exposes the melt to shear rates exceeding 10³ s⁻¹ in sub-gates and hot runner drops, the carrier resin's viscosity profile and pigment dispersion stability are governed by plastication conditions rather than die geometry. The recommended let-down ratio is 1.5–3.0 wt% when the base resin is HDPE with MFI 8–20 g/10 min (per ISO 1133-1:2022 at 190 °C, 2.16 kg) and 2.0–3.5 wt% when polypropylene homopolymer or random copolymer with MFI 12–25 g/10 min (per ISO 1133-1:2022 at 230 °C, 2.16 kg) is used. Processing at melt temperatures of 210–230 °C for HDPE closures and 220–240 °C for PP closures, with barrel residence times not exceeding 5 minutes and back pressures of 10–20 bar (hydraulic) during plastication, maintains color consistency; extended residence times above 8 minutes produce measurable yellowing in the red shade as quantified by a b* value shift exceeding 1.2 CIE units. Industry compliance for food-contact closures follows US FDA 21 CFR 178.3290 (Colorants for polymers), which lists colorants approved for use in food-contact polymer applications subject to extractives limitations; parallel European compliance requires affirmation under EU Regulation 10/2011 for plastic materials and articles intended to come into contact with food. For non-food applications, RoHS Directive 2011/65/EU restricts cadmium, lead, mercury, and hexavalent chromium in homogeneous materials. Downstream production is executed on hydraulic or hybrid injection molding machines with clamp forces of 150–400 tonnes, typically configured with 32–64 cavity hot runner tooling and valve-gated drop tips; cycle times of 8–15 seconds are characteristic for closure molding at thin-wall sections. Terminal products include beverage closure shells, cosmetic cap bases, and dairy container lids where the colorant must survive chilled logistics conditions without bleed or migration into package contents.
| Application Segment | Base Resin System | Let-Down Ratio (wt%) | Melt Temperature (°C) | Primary Processing Equipment | Terminal Product Dimension |
|---|---|---|---|---|---|
| Blown film refuse sacks | LLDPE/LDPE 70/30 blend | 2.0–4.0 | 205–220 metering zone | Single-screw extruder 65–90 mm, spiral mandrel die 200–350 mm | 18–45 μm film |
| Injection molded closures | HDPE (MFI 8–20) or PP (MFI 12–25) | 1.5–3.0 HDPE; 2.0–3.5 PP | 210–240 depending on base | Hydraulic/hybrid IMM 150–400 t, hot runner 32–64 cavity | 0.6–1.2 mm wall |
| Agricultural mulch film | LLDPE (MFI 1.0–2.0) | 3.0–5.0 | 200–215 die set point | Blown film with IBC, L/D 30:1, die 250–450 mm | 12–50 μm film |
| Rotational molding | LLDPE powder (MFI 3–6) | 1.0–2.0 | 260–290 oven; PIAT 180–200 | Carousel/shuttle rotomolding machine | 3–6 mm wall |
| Wire and cable jacketing | LLDPE or EVA (VA 9–19 wt%) | 2.5–4.0 | 190–220 | Cable extrusion line, crosshead die 24–40 mm, screw 60–90 mm | 0.2–1.5 mm jacket |
| Extrusion blow molding | HDPE (MFI 0.3–1.0) | 2.0–3.0 | 180–210 | Shuttle/continuous rotary, 50–120 mm, 6–12 parison heads | 250 mL–5 L |
Subjecting agricultural LLDPE mulch film to UV irradiation for extended field deployment periods imposes demands on colorant photostability that differ fundamentally from interior packaging applications. Films extruded with LyondellBasell POLYBATCH™ House Red 50311U/4 Concentrate Based In LLDPE at let-down ratios of 3.0–5.0 wt%—co-extruded with a 15–20 μm clear LLDPE outer layer to reduce direct pigment surface exposure—have demonstrated acceptable color retention under ISO 4892-3 weathering regimens (xenon arc, 102 min light/18 min spray cycles) with ΔE values below 3.0 CIE units at 2000 hours exposure. For field service lives exceeding 24 months, additional UV stabilizer masterbatch at 0.5–1.5 wt% (HALS-based, molecular weight 3000–4000 g/mol) is required, because the red organic pigments in this color class do not provide sufficient photoprotection to prevent LLDPE chain scission; unstabilized systems exhibit tensile elongation losses below 200% when measured per ASTM D882 after 3000 hours of accelerated weathering. Compliance for agricultural films is framed by EN 13655:2018 (Plastics—Thermoplastic mulch films recoverable after use, for use in agriculture and horticulture), which specifies requirements for thickness, mechanical properties, and degradation behavior; films intended for organic farming systems additionally require review under EU Regulation 2018/848 for soil-contact input non-toxicity. Production is carried out on blown film lines with LLDPE-specific barrier screws (L/D 30:1, barrier flights 25–30 mm), die diameters of 250–450 mm, and internal bubble cooling (IBC) systems maintaining bubble stability at BUR 2.0:1–3.0:1; terminal film gauges range from 12–50 μm in widths up to 6 m using rotating dies or oscillating haul-off equipment. Terminal products include red-pigmented mulch films for select horticultural crops where spectral reflectance management supports early-season soil warming (documented in peer-reviewed USDA field trials for tomato production systems), silage cover stretch films at 80–150 μm requiring high-opacity color for UV shielding of ensiled feedstock, and greenhouse repair films where red color coding distinguishes replacement panels per grower lot-tracking requirements.
At peak internal air temperatures of 180–200 °C and oven residence times spanning 20–45 minutes, rotational molding subjects polymer powders and the dispersed colorant to a cumulative thermal load that exceeds typical injection molding or extrusion exposure by an order of magnitude. The recommended let-down ratio for House Red 50311U/4 in rotomolding-grade LLDPE powder (MFI 3–6 g/10 min, bulk density 0.30–0.40 g/cm³) is 1.0–2.0 wt%; the lower bound is preferred for large-surface-area parts exceeding 300 L cavity volume where dry-blend uniformity depends on electrostatic adhesion between the concentrate and base resin powder. Industry compliance for rotomolded articles in potable water contact is governed by NSF/ANSI 61 with specified extraction test protocols; for general-purpose storage applications, EU Directive 94/62/EC Article 11 heavy metal restrictions apply. Downstream production occurs in carousel-type or shuttle-type rotational molding machines with oven temperatures of 260–290 °C and total cycle times of 20–45 minutes depending on wall thickness (3–6 mm); the concentrate is added during dry-blending prior to mold charging. Terminal products include red-pigmented water storage tanks, agricultural chemical dispensing enclosures, and playground structures requiring safety identification coloring.
| Application Scenario | Regulatory/Compliance Standard | Specific Threshold/Requirement | Verification Method |
|---|---|---|---|
| Blown film refuse sacks (EU) | EU 94/62/EC Art. 11 | Pb+Hg+Cd+Cr(VI) ≤ 100 mg/kg combined | Acid digestion + ICP-OES per EPA 3050B/6010D |
| Blown film refuse sacks (NA) | CONEG Model Toxics | Pb+Hg+Cd+Cr(VI) ≤ 100 ppm combined | Acid digestion + ICP-OES per EPA 3050B/6010D |
| Injection molded closures (US food) | FDA 21 CFR 178.3290 | Positive list colorants with extractives limits | Migration testing per FDA protocols |
| Injection molded closures (EU food) | EU Regulation 10/2011 | Specific Migration Limits (SML) | EN 1186 series or equivalent |
| Agricultural mulch film | EN 13655:2018 | Thickness, mechanical, degradation requirements | ISO 4892-3 weathering; ASTM D882 tensile |
| Rotational molding (potable water) | NSF/ANSI 61 | Extraction test protocols | NSF/ANSI 61 extraction testing |
| Wire and cable jacketing | RoHS 2011/65/EU Annex II | Pb, Hg, Cd, Cr(VI) ≤ 0.1 wt% each | XRF screening + ICP confirmation |
| Wire and cable jacketing (Cd) | REACH Annex XVII Entry 23 | Cd ≤ 100 ppm | ICP-OES quantification |
| Extrusion blow molding (food) | FDA 21 CFR 178.3290 / EU 10/2011 | Positive list + SML compliance | Migration testing per applicable protocols |
In cable jacketing compounds where red color coding serves phase identification or functional differentiation, chromaticity coordinates and color consistency become acceptance criteria on the same level as mechanical properties. The concentrate is incorporated into jacketing compounds based on LLDPE or EVA (vinyl acetate content 9–19 wt%) at let-down ratios of 2.5–4.0 wt%, achieving target CIELAB values (L* 45–55, a* 25–35, b* 15–25) measured per ISO 7724-2; batch-to-batch ΔE variation below 0.8 CIE units is considered acceptable for cable color lot traceability per IEC 60304. Compliance for this segment is anchored to RoHS Directive 2011/65/EU Annex II, where lead, mercury, cadmium, hexavalent chromium, and brominated flame retardants are each restricted to ≤1000 ppm (0.1 wt%) for electrical and electronic equipment; additional compliance under REACH Annex XVII Entry 23 restricts cadmium content to ≤100 ppm in the compound. Processing is executed on cable extrusion lines with crosshead dies (crosshead orifice 24–40 mm) and screw diameters of 60–90 mm with L/D ratios of 24:1–30:1; melt temperatures of 190–220 °C and line speeds of 200–800 m/min are typical for LLDPE-based jacketing compounds. Terminal products include phase-identified power cable jackets per IEC 60445:2021, automotive primary wire insulation per SAE J1128, and telecommunication conduit color-coded for service differentiation. Published data for the specific chromaticity retention of this concentrate under extended thermal cycling in cable service conditions is limited; qualified color stability should be validated on the target production line using the intended jacketing compound.
The processing of monolayer HDPE bottles through continuous extrusion blow molding requires colorant concentrates that tolerate continuous parison extrusion at melt temperatures of 180–210 °C without inducing parison instability or melt fracture at the die exit. The LLDPE carrier's low crystallinity produces parison swell characteristics intermediate between pure HDPE and LDPE behavior; for monolayer HDPE bottles (MFI 0.3–1.0 g/10 min, density 0.950–0.960 g/cm³), the recommended let-down ratio is 2.0–3.0 wt%, adjusted upward to 3.5 wt% when post-consumer HDPE recyclate forms 25–50 wt% of the bottle composition to mask inherent grey discoloration. Industry compliance follows US FDA 21 CFR 178.3290 for food-contact applications and EU Regulation 10/2011; for household chemical products packaged in HDPE, classification under the UN Globally Harmonized System labeling framework does not impose additional colorant restrictions, but compatibility testing with bottle contents (acidic detergents at pH 3–5, hypochlorite solutions, hydrocarbon-based cleaners) is required to rule out pigment extraction. Downstream production on shuttle or continuous rotary blow molding machines with 50–120 mm extruder diameters and 6–12 parison heads operates at cycle times of 12–30 seconds per bottle depending on container volume (250 mL–5 L); terminal products include colored bottles for automotive detergent concentrates, residential cleaning product packaging, and industrial chemical containers where red coding denotes hazardous content per ANSI Z535.1 safety color communication.
Competitive LyondellBasell POLYBATCH™ House Red 50311U/4 Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell POLYBATCH™ House Red 50311U/4 Concentrate Based In LLDPE is a pelletized color masterbatch in which a red pigment preparation is dispersed in a linear low-density polyethylene carrier resin. The product code 50311U/4 functions as a manufacturer identifier; it does not disclose pigment chemistry, pigment loading, or carrier melt index. Those values are controlled by lot-specific certificate of analysis and the current technical data sheet. In industrial practice, medium-strength red concentrates for polyethylene are often screened at addition levels between 2 wt% and 5 wt% by total blend weight, but the optimum for this grade must be set by pigment strength, target color coordinates, and finished-article thickness. The material is supplied as free-flowing pellets; pellet dimensions and bulk density vary by production campaign and are not fixed by the product designation.
The controlling specifications are batch-specific. A full certificate of analysis typically reports carrier melt flow rate by ISO 1133-1:2022, bulk density, moisture content, pigment loading, and heavy-metal content. Published data for this specific configuration is limited; processors should not assume values from other POLYBATCH grades. The designation “House Red” indicates a standard shade but does not define the exact pigment chemistry. For color-critical work, the finished article should be measured in the intended polymer system after letdown, because the carrier alone does not determine final color coordinates.
In blown film extrusion, the concentrate is normally metered into the main feed throat with a gravimetric feeder. LLDPE film grades processed on single-screw extruders with L/D ratios of 24:1 to 30:1 are commonly run with barrel temperature profiles from 170°C to 200°C and die temperatures from 190°C to 230°C. When 50311U/4 is added at 2 wt% to 5 wt%, the LLDPE carrier melts within the same thermal window as the dilution resin, reducing the probability of unmelted pellets reaching the die lip. The limiting factor is often distributive mixing rather than pigment dispersion. A single-screw extruder without a barrier screw or static mixer may exhibit longitudinal striping at letdown ratios above 4 wt% if screw speed exceeds the melting capacity of the mixing section. Filtration through a 60/100/60 mesh screen pack is common; finer filtration below 100 mesh can increase backpressure and shear heating. In such cases, melt temperature measured at the adapter should be maintained below 240°C to avoid thermal shift of the red pigment system. Lot-specific heat stability data must confirm the exact limit.
Carrier viscosity influences color uniformity more than pigment loading alone. A carrier with a melt index of 20 g/10 min at 190°C and 2.16 kg per ISO 1133-1:2022 will flow more readily than a film-grade LLDPE with a melt index of 1.0 g/10 min under the same conditions. This differential can generate streaks if the concentrate enters the melt stream late or if the screw has a short compounding section. The exact carrier melt index for 50311U/4 is not published in this document and must be read from the certificate of analysis. In co-rotating twin-screw extruders used to pre-disperse the concentrate, pigments are milled into the carrier at specific energy inputs of 0.15 kWh/kg to 0.35 kWh/kg depending on pigment hardness and aggregate size. Dispersive mixing is often checked by pressing a 50 µm film and counting undispersed pigment particles under 100× transmitted light. A typical acceptance criterion for high-quality film concentrate is fewer than 5 undispersed particles larger than 10 µm per 100 cm². Published data for this specific product is limited; the figure is a general industrial benchmark.
On production lines, the concentrate should be added at the beginning of the screw with the main resin, not through a downstream side feeder. Direct addition at the throat allows the LLDPE carrier and the pigment to traverse the full barrel residence time. For single-screw extruders with a three-zone screw, residence time distributions may range from 2 min to 5 min at screw speeds of 60 rpm to 120 rpm. Early melting is improved if the feed throat is water-cooled and the compression zone remains partially filled. If the concentrate is pre-blended by tumble mixing instead of metered separately, the blend should be mixed for 10 min to 15 min in a low-shear tumbler. Longer mixing times can stratify pellets by density and produce color drift.
Cast film lines and extrusion coating lines operate with different residence times and melt temperatures than blown film. In extrusion coating, LLDPE-rich formulations are often processed at melt temperatures of 260°C to 310°C to improve adhesion to paper, board, or foil. This thermal environment requires a red pigment with sufficient heat stability; the LLDPE carrier itself does not protect a heat-sensitive pigment. The use of 50311U/4 in this setting should be confirmed with heat stability data generated on the target line because published data for this specific configuration is limited. In cast film, the melt film is quenched rapidly on a chill roll held at 15°C to 30°C. Fast quenching reduces crystalline growth and can change apparent color strength relative to slower-cooled blown film. Therefore, color match certificates generated in blown film are not automatically transferable to cast film.
Red organic pigments vary widely in lightfastness and migration resistance. Before 50311U/4 is used in consumer goods, outdoor furniture, or food-contact packaging, the final part should be tested under the intended use conditions. Lightfastness can be assessed by ISO 4892-2 xenon-arc exposure with a total radiant exposure of 1 200 kJ/m² at 300 nm to 400 nm and a blue wool reference comparison. Migration into food simulants is evaluated per EU No 10/2011 using 10 days at 40°C in 10% ethanol, 3% acetic acid, and olive oil or 95% ethanol substitutes, depending on the food type. The supplier’s documentation should state whether the pigment system is covered by a positive list; if not, the processor must obtain a declaration of compliance. Published data for this specific grade is limited, so regulatory certificates are the controlling documents.
In applications with high humidity and long storage times, moisture pickup by the LLDPE carrier can create surface splay or bubbles. Polyethylene is not hygroscopic; however, surface condensation on cold pellets brought into a warm plant can introduce moisture. If wet pellets are suspected, pre-drying at 70°C to 80°C for 2 h to 4 h in a desiccant or hot-air dryer is usually sufficient. Drying beyond 4 h is unnecessary and can increase energy cost without improving dispersion. The concentrate should be stored in sealed containers below 40°C and out of direct sunlight to reduce pigment exposure to UV and heat.
The carrier resin in a color concentrate governs compatibility with the letdown resin, melt temperature window, and final-article optical properties. An LLDPE carrier is selected for this grade because it matches the melt temperature and viscosity of polyethylene film and molding resins more closely than a polypropylene or wax-based carrier would. The table below summarizes general differences among carrier systems used in polyolefin colorants. The values are typical literature ranges, not lot-specific data for 50311U/4.
| Carrier type | Typical peak melting range | Typical melt index or MFR | Compatibility with LLDPE | Processing consequence |
|---|---|---|---|---|
| LLDPE | 120–125°C | 0.5–30 g/10 min at 190°C/2.16 kg | High | Lower interfacial haze in thin film; best carrier match for LLDPE-rich lines |
| LDPE | 105–115°C | 0.2–70 g/10 min at 190°C/2.16 kg | Good | Softens earlier; may alter bubble stability in blown film |
| PP homopolymer | 160–165°C | 1–35 g/10 min at 230°C/2.16 kg | Poor | Can form visible specks or delamination in polyethylene |
| Polyethylene wax | 95–110°C | High melt flow; not measured by standard MI | Moderate | Aids pigment dispersion but can reduce melt strength at high addition |
In injection molding of LLDPE or LDPE parts, addition levels of 2 wt% to 4 wt% are common for red concentrates. The barrel temperature profile is normally set between 200°C and 240°C from feed to nozzle. Screws with L/D ratios of 20:1 or higher and a general-purpose check ring provide adequate melt homogeneity for solid colors. For thin-wall parts with wall thickness below 1 mm, the concentrate should be pre-mixed or metered consistently because short cycle times leave little residence time for distributive mixing. Clamp force requirements depend on part area and not on the concentrate; the LLDPE carrier does not significantly alter injection pressure. If the press has a hot runner, the manifold temperature should be kept below 250°C and dead spots should be avoided to prevent long residence times. Red pigments can show visible streak defects when flow passes around sharp corners or through small gates; raising the gate size or reducing injection speed often resolves these flow-induced color streaks more effectively than increasing concentrate level.
Rotational molding is another application where LLDPE-based colorants are dry-blended with LLDPE powder. On single-layer machines, 3 wt% to 5 wt% of 50311U/4 may be tumble-mixed for 10 min to 15 min before charging the mold. Oven temperatures of 260°C to 290°C and cycle times of 20 min to 40 min impose a long thermal history on the pigment. The concentrate must have adequate heat stability for the full cycle; otherwise the red shade can shift toward orange or brown. Because published data for this specific product in rotational molding is limited, a trial at the target oven temperature and peak internal air temperature is required.
For regulated applications, the concentrate must be evaluated as part of the finished article rather than in isolation. The LLDPE carrier and the pigment system may be subject to positive lists, migration limits, and heavy-metal restrictions. The table below lists the standards most commonly referenced for polyolefin color concentrates. A declaration of compliance from LyondellBasell should be obtained for each production campaign because raw material substitutions and batch-specific variations can change regulatory status.
| Standard or regulation | Scope | Typical data required |
|---|---|---|
| EU No 10/2011 | Plastic food contact materials and articles | Overall migration and specific migration limits in food simulants |
| FDA 21 CFR 178.3290 | Colorants for polymers used in food contact | Conditions of use and extractables data |
| RoHS Directive 2011/65/EU | Restriction of hazardous substances in electrical and electronic equipment | Lead, cadmium, mercury, hexavalent chromium, PBB, PBDE |
| REACH Regulation (EC) No 1907/2006 | Substance registration and safety data sheets | Registration status and safe-use information |
Line cleaning after red concentrate use is handled with the same purge discipline used for other polyolefin colorants. A purge resin with slightly lower melt index than the production resin is introduced at the running temperature until the extrudate is free of visible pigment. For hot runner systems, purging should include short high-pressure shots rather than continuous low-pressure extrusion, because red pigment can collect in low-flow zones. The concentrate does not require aggressive chemical purges; mechanical purging with LLDPE is usually adequate if performed before the pigment bed can carbonize at high temperature.