Lyondellbasell Polybatch Fta 50 P Concentrate Based In Lldpe

LyondellBasell POLYBATCH™ FTA-50-P Concentrate Based In LLDPE

    • Product Name: LyondellBasell POLYBATCH™ FTA-50-P Concentrate Based In LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 646601
    Product Name LyondellBasell POLYBATCH™ FTA-50-P Concentrate Based In LLDPE
    Carrier Resin LLDPE
    Antiblock Agent Talc
    Active Content 50%
    Form Pellets
    Color White
    Specific Gravity 1.5
    Melt Flow Rate 10 g/10 min
    Moisture Content <0.1%
    Bulk Density 0.8 g/cm³
    Pellet Size 2-4 mm
    Processing Temperature 180-240 °C
    Recommended Let Down Ratio 1-5%

    As an accredited LyondellBasell POLYBATCH™ FTA-50-P Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell POLYBATCH™ FTA-50-P Concentrate Based In LLDPE typically comes in 25 kg (55 lb) polyethylene-lined bags, 40 bags per pallet.
    Container Loading (20′ FCL) 20′ FCL: LyondellBasell POLYBATCH™ FTA-50-P LLDPE-based concentrate, palletized 25 kg bags, shrink-wrapped, secured in dry container for ambient ocean shipment.
    Shipping POLYBATCH™ FTA-50-P, an LLDPE-based concentrate, typically ships as non-hazardous free-flowing pellets in 25 kg bags or octabins, palletized and stretch-wrapped. It is not usually classified as dangerous goods for DOT/IMDG/IATA. Store/transport dry, away from excessive heat, moisture, and sunlight; follow SDS/TDS. Maintain package integrity.
    Storage Store POLYBATCH™ FTA-50-P concentrate in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and flames. Keep original containers tightly closed to prevent moisture pickup, contamination, and dust. Avoid excessive stacking or physical damage. Maintain ambient storage temperatures, practice good housekeeping, and rotate stock using oldest material first. Do not store near food, feed, or drinking water.
    Shelf Life Shelf life: 24 months from date of manufacture, stored in original, unopened packaging under dry, cool conditions, away from sunlight.
    Application of LyondellBasell POLYBATCH™ FTA-50-P Concentrate Based In LLDPE
    In monolayer LLDPE blown film extrusion, the practical upper shear rate is limited by sharkskin and stick-slip flow instability at the annular die exit. LyondellBasell POLYBATCH™ FTA-50-P Concentrate Based In LLDPE is introduced at 0.5 wt% to 2.0 wt% of extruder throughput; a maintenance dose of 0.8 wt% to 1.2 wt% is typically used for 1-butene and 1-hexene LLDPE film grades with melt indices from 0.8 g/10 min to 2.0 g/10 min determined under ASTM D1238-20 at 190 °C and 2.16 kg. Conditioning on a 60 mm to 90 mm single-screw extruder with 30:1 to 40:1 L/D and a grooved feed section requires 20 min to 45 min before die pressure readings stabilize; where die-lip accumulation has already formed, a temporary purge at 2.0 wt% to 3.0 wt% for 30 min is applied before returning to the maintenance dose. Downstream production process parameters include barrier screw geometry, annular die gap 1.6 mm to 2.4 mm, blow-up ratio 2.0:1 to 3.0:1, and frost-line height controlled by chilled-air ring velocity. Industry compliance for food-contact can liners or seal layers is predicated on the olefin polymer resin meeting FDA 21 CFR 177.1520(c) and EU No 10/2011 positive-list migration limits; the fluoropolymer component requires end-use verification against FDA 21 CFR 177.1550 where applicable. Terminal product types include industrial can liners, heavy-duty shipping sacks, frozen-food packaging, and medium-duty agricultural mulching film in which surface smoothness and gauge uniformity are measured by ISO 4591 rather than by post-extrusion surface treatments.

    Why Does Extrusion Blow Molding of HDPE Containers Generate Die Drool at High Clamp-Frequency Cycles?

    Accumulator-head and continuous shuttle presses running high-molecular-weight HDPE for blow-molded containers encounter die-lip build-up when shear stress at the die land exceeds the critical slip threshold of the melt. The LLDPE carrier in FTA-50-P does not depress bottle Environmental Stress Crack Resistance when added at 0.5 wt% to 1.5 wt%; blow molders using post-consumer HDPE blends often operate at 1.5 wt% to 2.0 wt% to control parison surface roughness and reduce the interval between die-lip cleaning cycles. The downstream production process includes grooved-feed single-screw plastication with 24:1 to 30:1 L/D, parison die gap programming from 1.0 mm to 2.2 mm, melt temperatures between 180 °C and 210 °C, and mold clamping force normally from 50 t to 500 t depending on container volume. Industry compliance standards for HDPE bottles intended for food service or household chemicals include FDA 21 CFR 177.1520, EU No 10/2011, and stress-crack testing per ASTM D1693-21 where ESCR retention in the finished article is a release criterion. Terminal product types include 250 mL to 5 L dairy and juice containers, health-care reagent bottles, agricultural chemical containers, and household detergent packaging; where UN certification is required, the finished container must pass UN 3H1 or UN 3H2 packaging tests based on closure configuration.

    Cast Film Edge Neck-In, Chill-Roll Release, and Fluoropolymer Slip Chemistries

    Cast film extrusion of LLDPE and metallocene LLDPE at line speeds above 250 m/min is constrained by edge neck-in and unstable melt curtain draw resonance. Addition of FTA-50-P at 0.5 wt% to 1.0 wt% is used to lower apparent die-wall adhesion and stabilize the melt curtain before contact with the chill roll. The downstream production process uses a coat-hanger slot die with lip gap 0.4 mm to 0.8 mm, chill-roll temperatures from 15 °C to 35 °C, air-knife or vacuum-box pinning, and corona treatment at 38 mN/m to 44 mN/m for downstream lamination. The additive functions primarily at the die metal interface; therefore optical haze measured by ASTM D1003-21 and tensile properties measured by ASTM D882-18 are used to verify that the masterbatch is not interfering with bulk film optical or mechanical performance. Industry compliance for direct food-contact cast film follows FDA 21 CFR 177.1520 and EU No 10/2011 overall migration limits; for industrial stretch film, REACH SVHC screening under EC 1907/2006 and chlorinated-organic-free certifications are the relevant compliance boundaries. Terminal product types include machine-wrap stretch film, hand stretch film, lamination film for flexible packaging, and breathable backsheet films where a uniform melt curtain and reduced die deposit formation are critical for obtaining defect-free roll stock.

    When Post-Consumer Recycled PE Feedstocks Enter Thin-Wall Irrigation Tubing Extrusion

    Thin-wall drip irrigation laterals extruded from post-consumer recycled polyethylene contain gels, paper fines, and metal-oxide pigments that raise screen-pack differential pressure and create localized die-lip buildup. FTA-50-P is introduced at 1.0 wt% to 3.0 wt% in recycled PE irrigation tubing because the fluoropolymer slip layer reduces the frequency of die-face accumulation that can form pinholes and weak weld lines in 0.6 mm to 1.2 mm wall sections. The downstream production process involves single-screw extrusion with a 30:1 L/D barrier screw, screen packs from 60 mesh to 120 mesh, vacuum-sizing calibration, and in-line perforation or emitter insertion. Published dose-response data for highly contaminated post-consumer recycled PE with this specific masterbatch configuration are limited; line trials should therefore monitor screen-pack differential pressure, die pressure, and finished tube burst strength rather than relying solely on masterbatch addition rate. Industry compliance for agricultural irrigation laterals includes dimensional tolerance verification under ISO 9261:2004 for emitting pipes and emitters, with additional potable-contact certification conducted only under NSF/ANSI 61 or equivalent where required. Terminal product types include pressure-compensating drip laterals, micro-sprinkler distribution lines, and recycled-content agricultural drainage tubing.At line speeds above 300 m/min, wire and cable jacketing operations running linear polyethylene and HDPE compounds often convert to FTA-50-P when surface roughness from melt fracture becomes visible as periodic ridges at the crosshead die exit. The masterbatch is added at 0.3 wt% to 1.0 wt% in natural or carbon-black-loaded jacketing compounds; the LLDPE carrier is compatible with HDPE and MDPE cable insulation shields, but formulators should verify the effect of the fluoropolymer on printing adhesion after spark testing and surface treatment. The downstream production process uses a 45 mm to 120 mm single-screw extruder coupled to a crosshead and pressure die, melt temperature 190 °C to 230 °C, water trough cooling from 40 °C to 80 °C, and on-line diameter measurement. Compliance for low-voltage power cable jackets under IEC 60502-1:2021 and for optical fiber duct under IEC 60794 requires that the finished compound pass aging, shrinkage, and low-temperature bending tests before the processing aid is approved; the PPA is not a substitute for proper carbon black dispersion or antioxidant packages. Terminal product types include low-voltage power cable jackets, fiber-optic microducts, and HDPE conduit for buried telecommunication cable, where surface smoothness and dimensional control are the primary process acceptance criteria.

    High-Draw Monofilament and Slit-Tape Extrusion Runs Into Sharkskin at the Die Land

    High-draw orientation of LLDPE monofilaments and slit tapes creates a narrow processing window between die exit swell and the first godet stand, where melt fracture defects generate filament breaks during orientation. FTA-50-P is added at 0.3 wt% to 1.0 wt% for LLDPE tape extrusion; onset of sharkskin is typically suppressed at draw ratios from 6:1 to 10:1 when the masterbatch has been conditioned for at least 20 min on the extrusion line. The downstream production process involves a slit die or spinneret, water bath quenching at 25 °C to 45 °C, hot-air orientation oven, and annealing rolls; for slit tapes, fibrillation needles and winding tension are adjusted based on elongation at break measured under ISO 527-3 or ASTM D882-18. Industry compliance for agricultural twine and woven sack tape focuses on UV stabilization protocols under ISO 4892-2 and REACH reporting under EC 1907/2006; food-contact woven sacks for bulk packaging require FDA 21 CFR 177.1520 and EU No 10/2011 compliance for the polyolefin substrate. Terminal product types include high-strength agricultural tying twine, woven polyethylene sack fabric, turf reinforcement netting, and geotextile filament; the PPA does not contribute to fiber strength but reduces surface defects that otherwise initiate premature orientation failure.
    Free Quote

    Competitive LyondellBasell POLYBATCH™ FTA-50-P Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    POLYBATCH™ FTA-50-P is a pelletized fluoropolymer processing aid concentrate supplied in a linear low density polyethylene carrier resin. The grade designation encodes product structure: FTA identifies the fluoropolymer processing aid chemistry, 50 indicates 50 wt% active fluoropolymer, and P designates pelletized delivery. The concentrate is added to polyolefin extrusion lines—principally blown and cast film lines—to delay the onset of sharkskin melt fracture, reduce die lip build-up, stabilize die pressure, and shorten purging time after resin or color changes. The product is not an antiblock masterbatch, a slip masterbatch, or a coefficient-of-friction control system. It does not intentionally create surface roughness or bloom a low molecular weight amide to the film surface.

    Because the carrier resin is LLDPE, the concentrate is mechanically compatible with polyethylene-rich formulations. At the normal letdown range for processing aid masterbatches, the mass of LLDPE carrier added to the final film is small enough that standard tensile and tear property changes are generally below routine measurement variability. The pellets are designed for gravimetric or volumetric metering through standard additive feeders.

    Fluoropolymer Migration and Die Wall Coating in Polyolefin Extrusion

    In single-screw extrusion of unfilled LLDPE, sharkskin melt fracture appears when wall shear stress at the die exit exceeds a critical value. For linear polyethylenes, the onset is commonly reported between 0.1 MPa and 0.3 MPa, depending on molecular weight distribution, melt temperature, and die land geometry. A fluoropolymer processing aid is a low-surface-energy material that is immiscible with the polyolefin matrix. During extrusion, the active fluoropolymer phase migrates to the metal die surface and forms a thin, stable coating. The coated die wall reduces polymer-metal friction and suppresses the stick-slip cycle that appears as sharkskin. As conditioning proceeds, the external melt layer slips at the coating interface instead of adhering to the die land. The visible result is a progressive clearing of surface melt fracture, typically beginning at the film edges and moving inward across the web.

    The conditioning period is an operational boundary. On blown film lines with 40 mm to 90 mm single-screw extruders, commercial PPA conditioning periods typically range from 20 min to 60 min, but the exact time depends on die surface condition, output rate, melt temperature, screw design, and the presence of oxidized polymer or inorganic deposits. During conditioning, sharkskin may persist for longer than expected if the die has heavy residue from previous production. A temporary increase in letdown, commonly 2 to 3 times the steady-state level, is used in some plants to shorten this interval. Once the die coating is established, the letdown is reduced to the maintenance level.

    Why Is a 50 wt% Active Fluoropolymer Concentrate Less Sensitive to Feed Throat Starvation?

    Steady-state use of fluoropolymer processing aids generally requires a final active concentration of 200 mg/kg to 1000 mg/kg in the polymer melt. For a concentrate with 50 wt% active fluoropolymer, this corresponds to a masterbatch letdown of 0.04 wt% to 0.2 wt%. Lower-activity PPA masterbatches containing 3 wt% to 5 wt% active require proportionally higher letdowns. The higher active content of POLYBATCH FTA-50-P reduces the mass of LLDPE carrier introduced into the final product by a factor of approximately 10 to 17 compared with a 3–5 wt% active masterbatch. That arithmetic matters in thin-gauge film extrusion, where carrier resin contributions can affect gauge uniformity if the letdown is high or the feeder is unstable.

    Feed systems remain the limiting parameter. At 0.04 wt% letdown on a line producing 300 kg/h, the required masterbatch feed rate is 0.12 kg/h. Gravimetric batch feeders with narrow screw diameters may require recalibration at such low rates. The pellet form of FTA-50-P reduces bridging compared with fine powders or microbeads in some hopper geometries, but periodic feeder checks are still necessary. Feeder instability produces cyclic melt fracture because the active fluoropolymer concentration at the die fluctuates below the critical level needed to maintain the die coating.

    Dispersion of the concentrate in the base resin follows conventional single-screw mixing behavior. Because the active fluoropolymer functions by die-wall deposition rather than by molecular dispersion, submicron distributive mixing is not required; pellet melting and sufficient shear to interrupt the fluoropolymer domain are adequate. The product should be introduced before the compression zone rather than side-stuffed after plasticating is complete.

    When the LLDPE Carrier Is Introduced Into Polypropylene Cast Film Lines

    The LLDPE carrier in FTA-50-P is part of the product design because it matches the base resin in polyethylene film extrusion. In polypropylene cast film or extrusion coating, the carrier is a minor but distinct second phase. At a letdown of 0.2 wt%, the LLDPE carrier contribution is 0.2 g per 100 g of polymer. In pigmented or opaque PP film, this level is generally undetectable in standard tensile or tear tests. In high-clarity PP film, however, even low levels of a semicrystalline polyethylene phase can create optical defects if melting and dispersion are incomplete. Melt temperatures should remain above the crystalline melting point of LLDPE, normally above 120 °C, and the additive should be introduced early enough in the screw to allow complete melting. If a polypropylene-carrier processing aid masterbatch is available, it may be preferred for optical PP applications; published data for the specific FTA-50-P configuration in high-clarity PP film is limited.

    No predrying is typically required under normal storage conditions because LLDPE and fluoropolymer processing aids are not hygroscopic. Surface condensation from cold warehouse storage should nevertheless be avoided because water droplets entering the feed throat can produce steam-induced melt disturbances and localized die pressure fluctuations.

    Die lip build-up in high-speed cast film lines is commonly associated with low molecular weight oligomers, oxidized gels, and polymer degradation products accumulating at the die exit. A fluoropolymer coating reduces the adhesion of these residues to the die lip. When FTA-50-P is introduced at the lower end of its use range, the coating forms preferentially on the metal surface and reduces the rate of deposit accumulation. In practice, the product is often combined with a separate antiblock masterbatch; the processing aid addresses melt fracture and die build-up, while the antiblock concentrate provides film separation and winding performance. These functions do not overlap. Substitution of one for the other leads to unresolved melt fracture or blocking depending on the direction of the error.

    Because the fluoropolymer processing aid acts at the die wall, it should not be expected to reduce blocking force between film layers during storage. The surface of the film does not receive the same continuous fluoropolymer layer that forms on the die land. If a film requires reduced coefficient of friction, an erucamide or oleamide slip masterbatch is a separate addition. The processing aid is not a purging compound; it does not remove existing carbon deposits quickly. A dedicated mechanical or chemical purging compound is required for severe die lip contamination. Using FTA-50-P as a maintenance additive after cleanup helps extend the interval between die cleanings, but the actual interval is line-dependent and cannot be predicted from masterbatch data alone.

    Compared with conventional fluoroelastomer PPA masterbatches at 3–5 wt% active content, POLYBATCH FTA-50-P reduces the amount of masterbatch that must be stored, transported, and metered for a given final active concentration. The trade-off is that low letdown rates demand more accurate feeders. For example, achieving a final active concentration of 500 mg/kg requires 0.10 wt% of a 50 wt% active masterbatch but 1.0 wt% of a 5 wt% active masterbatch. The result is a 10-fold difference in masterbatch letdown for the same active dose. Within the POLYBATCH processing aid range, the 50 wt% active level sits above low-concentration masterbatches and below compounded fluoropolymer concentrates used in cable jacketing. The pellet form, rather than powder or microbead form, affects feeder calibration and dust exposure on the production floor.

    Functional distinctions between processing aid and surface-effect masterbatches
    Masterbatch class Active chemistry Representative function Typical final active concentration range
    POLYBATCH FTA-50-P Fluoropolymer processing aid at 50 wt% in LLDPE Delays sharkskin melt fracture; reduces die lip build-up 200–1000 mg/kg active fluoropolymer
    Conventional fluoroelastomer PPA Fluoroelastomer at 3–5 wt% in polyolefin carrier Delays sharkskin melt fracture; higher masterbatch letdown 200–1000 mg/kg active fluoropolymer
    Synthetic silica antiblock Silica in polyolefin carrier Creates surface micro-roughness for film separation 1000–5000 mg/kg silica in final film
    Primary amide slip Erucamide or oleamide in polyolefin carrier Reduces coefficient of friction by surface bloom 300–1500 mg/kg amide in final film
    Typical material characterization parameters and relevant standards
    Parameter Standard method Relevance to this concentrate
    Melt mass-flow rate of LLDPE carrier ISO 1133-1:2022 / ASTM D1238 Controls carrier viscosity and feed behavior
    Density of LLDPE carrier ISO 1183-1:2019 Confirms carrier polymer identity
    Fluoropolymer active content Internal QC / thermogravimetric analysis Verifies grade designation 50 wt% content
    Pellet dimensions and bulk density Internal QC Affects gravimetric feeder accuracy

    Food-contact status is not determined by the LLDPE carrier alone.

    For food-contact applications in the United States, the LLDPE carrier resin is generally assessed under FDA 21 CFR 177.1520 for olefin polymers. In the European Union, the carrier resin may be assessed under Commission Regulation (EU) No 10/2011 on plastic materials intended to contact food. However, the active fluoropolymer component requires separate verification through a food-contact substance notification, a positive national list entry, or a specific migration limit assessment. A statement of composition and regulatory data sheet should be requested from LyondellBasell for the exact grade, because the overall compliance status of a masterbatch cannot be inferred from the carrier resin alone.

    For general industrial applications in the EU, REACH obligations under Regulation (EC) No 1907/2006 apply to the supplied preparation. Users should verify that the product is covered by a safety data sheet and that any substances of very high concern are not present above applicable reporting thresholds. Where electrical and electronic equipment is involved, RoHS Directive 2011/65/EU restrictions apply to the finished article rather than separately to the masterbatch. Standard mechanical test methods such as ASTM D638 and ISO 527 can be used to verify that the low letdown of this concentrate does not introduce measurable film property changes. For medical packaging or pharmaceutical contact, additional extractables testing according to ISO 10993 or regional pharmacopoeia methods may be required, and the processor should obtain a specific regulatory statement from LyondellBasell for those end uses.

    Operational boundary conditions are defined by the feeder and the extruder rather than by the concentrate chemistry alone. At letdowns below 0.03 wt% product, feeder accuracy becomes the dominant source of variation. At letdowns above 0.4 wt%, the LLDPE carrier may influence film stiffness or haze in non-polyethylene matrices, and excess fluoropolymer may accumulate in screen packs or static mixers rather than improving die performance. Combination with silicone-based external lubricants may delay the formation of a complete fluoropolymer die coating because competitive coating of the die wall can occur. If both are present, the conditioning period may increase. Processors should verify the certificate of analysis for melt flow rate, density, and fluoropolymer content before qualifying the product. Published numeric data for this specific configuration is limited; therefore, incoming lot release values should be compared against internally derived baselines rather than literature values.

    Top