| HS Code | 304537 |
| Productname | LyondellBasell POLYBATCH™ Dark Grey LL80362/4 Concentrate Based In LLDPE |
| Brand | POLYBATCH™ |
| Supplier | LyondellBasell |
| Producttype | Color concentrate (masterbatch) |
| Color | Dark Grey |
| Carrierresin | Linear Low Density Polyethylene (LLDPE) |
| Form | Pellets |
| Compatibility | Polyethylene (PE) homopolymers and copolymers |
| Recommendedletdownratio | 4% (typical) |
| Processingtemperature | 180–230°C |
| Density | 1.10 g/cm³ (typical) |
| Meltflowrate | 5–20 g/10 min at 190°C/2.16 kg (typical) |
| Moisturecontent | <0.20% (typical) |
| Storageconditions | Dry, below 30°C |
| Shelflife | 24 months (typical) |
As an accredited LyondellBasell POLYBATCH™ Dark Grey LL80362/4 Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell POLYBATCH™ Dark Grey LL80362/4 Concentrate is supplied in 25 kg polyethylene bags, 40 bags per 1,000 kg pallet. |
| Container Loading (20′ FCL) | 20′ FCL loading of LyondellBasell POLYBATCH™ Dark Grey LL80362/4 LLDPE-based concentrate: properly palletized bags, evenly distributed, secured, moisture-protected dry container. |
| Shipping | LyondellBasell POLYBATCH™ Dark Grey LL80362/4 Concentrate Based in LLDPE is a non-hazardous, solid plastic color concentrate. It ships as non-regulated cargo—no UN number, hazard class, or packing group—in polyethylene-lined bags or boxes, palletized and shrink-wrapped. Store dry, away from excessive heat. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed and use original packaging to prevent moisture, dust, and contamination. Avoid extreme temperatures and prolonged UV exposure. Handle with good industrial hygiene. Follow local regulations and the supplier’s safety data sheet for additional storage precautions. |
| Shelf Life | Typically 24 months from production if stored in original, unopened packaging under cool, dry conditions away from direct sunlight. |
On blown-film lines converting LLDPE-rich formulations into agricultural mulch and silage-cover film, POLYBATCH™ Dark Grey LL80362/4 is metered into the main feed throat at a mass let-down ratio of 2–5 wt%, with the upper end of the range reserved for films below 15 µm and the lower end used when high calcium carbonate filler levels already contribute opacity. The concentrate carrier is LLDPE, which limits melt-viscosity mismatch when the base resin is a high-molecular-weight film grade with a melt mass-flow rate of 0.9–1.2 g/10 min under ISO 1133-1:2022 at 190 °C and 2.16 kg. A barrier screw with a length-to-diameter ratio of 25:1–30:1 and a feed-throat temperature of 35–50 °C is recommended, because premature softening of the concentrate at the feed opening can create intermittent feed slugs and visible grey bands in the layflat. A graduated screen pack of 60/80/100 mesh retains undispersed pigment agglomerates larger than 100 µm, while a typical barrel profile from feed to die is 160 °C, 180 °C, 200 °C, 210 °C with adapter and die at 210–220 °C. The melt temperature measured at the die exit is kept below 240 °C to avoid oxidative chain scission in the LLDPE carrier, and the bubble is run at a blow-up ratio of 2.2:1–3.0:1 with a frost-line height of 4–8 die diameters. Raising the frost line beyond this range with dark grey formulations increases surface migration of low-molecular-weight pigment carrier fractions and can raise blocking forces on wound film. Tensile properties of 12–20 µm mulch film are evaluated under ASTM D882-18, and light transmission is checked by ASTM D1003-21; the concentrate is expected to reduce transmission progressively with addition level, but published data for this exact product configuration is limited, so end-use validation under ISO 4892-2 xenon-arc weathering is required before UV-screening performance is guaranteed. At 2 wt% addition the film may retain slight translucency in the thinnest gauges, while at 5 wt% the surface approaches full visual opacity but the bubble can become more sensitive to tower draughts and gauge variation. The concentrate should be pre-dried at 60–70 °C for 2–4 h when ambient storage humidity exceeds 60% RH; moisture carried into the melt through high-surface-area pigment particles otherwise forms fisheyes and pinholes that are difficult to remove without shutting down the tower.
In flat-die sheet extrusion for LLDPE-based geomembranes with thicknesses from 0.75 mm to 2.0 mm, the concentrate is usually compounded at 3–6 wt% into a medium-density or high-density polyethylene-rich matrix; the LLDPE carrier is miscible enough in polyolefin blends that it does not form visible weld-line boundaries, but its lower melt viscosity reduces the bulk melt strength of thick sheet at higher addition rates. A 90 mm single-screw extruder with a 30:1 L/D and a coat-hanger die opened to 1.0–1.5 mm is operated with a melt temperature of 195–230 °C, while the first polishing roll is held at 60–80 °C and the second at 40–55 °C; higher roll temperatures force low-molecular-weight pigment carrier fractions to deposit on the roll surface as plate-out, which subsequently transfers back to the sheet as dull grey streaks. Concentrate addition above 6 wt% increases the risk of edge waviness and transverse gauge variation across a 4 m web, and the increased pigment loading shifts the sheet coefficient of linear thermal expansion, making seam-weld alignment more sensitive to ambient temperature changes; this property is verified under ASTM D696-16 if the geomembrane is installed with welded seams. Dark grey sheet also absorbs more incident radiation during the polishing-stack cooling step, so the temperature difference between the sheet core and the sheet surface can widen if the polishing-roll water flow is not adjusted, resulting in residual stress that appears as curl at the cut edges. Oxidative induction time is tested under ISO 11357-6:2021 at 200 °C in oxygen, and the dark grey concentrate must not reduce the OIT of the formulated antioxidant package below project-specific minimums; high-surface-area carbon black can adsorb a fraction of the phenolic stabilizer during melt mixing, an effect that becomes measurable at addition levels above 5 wt% unless the base resin contains additional stabilizer. The concentrate should be pre-dried at 60 °C for 2 h if opened bags are stored at ambient humidity above 70% RH, and it must not be combined with amine-based antistatic masterbatches because such additives can react on the pigment surface and produce low-level organoleptic contaminants in confined installation environments.
Where gauge uniformity below 20 µm governs the conversion of refuse sacks and heavy-duty industrial liners, the dark grey concentrate is usually introduced into LLDPE by direct dosing at 2–4 wt%, with the carrier resin selected to match the melt mass-flow rate of the base polymer within 0.3 g/10 min under ISO 1133-1:2022. On a high-output blown-film line with an extruder L/D of 24:1–30:1 and a die diameter of 150–300 mm, the head pressure is monitored continuously; a pressure increase greater than 15% over the start-up value usually indicates pigment agglomerate build-up on the 60/80 mesh screen pack, which is then replaced every 6–12 h during prolonged runs. The blend is processed at 190–220 °C for film thicknesses of 15–25 µm, and dart-impact resistance is evaluated under ASTM D1709-22 method A or B depending on the expected service load; because dark pigment particles act as stress concentrators in thin sections, the let-down ratio is deliberately reduced toward 2 wt% when low-temperature impact resistance at -20 °C is required. A grooved-feed extruder section with forced cooling prevents pre-melting and slug feeding of the concentrate, which would otherwise create light grey streaks that are visible against a backlit inspection light table. The thickness profile is scanned by an oscillating capacitive gauge, and deviations outside ±2 µm are corrected by adjusting the internal bubble cooling airflow rather than altering the let-down ratio, because pigment distribution responds more slowly to screw-speed changes than the air ring. Compliance for refuse-sack waste-stream applications is generally assessed against REACH Article 33 and EU Directive 94/62/EC; if the dark grey concentrate is supplied with food-contact declarations, migration testing of the finished film under EU Regulation 10/2011 and FDA 21 CFR 178.3290 remains the responsibility of the converter because pigment purity and addition-rate limits are not universally food-grade across all packaging configurations.
For cast pallet-hood and silage-wrap constructions where line speeds above 120 m/min are typical, the dark grey concentrate is metered at 3–5 wt% into an LLDPE base with a melt mass-flow rate of 2.0–3.5 g/10 min under ISO 1133-1:2022. The cast-film process gives the concentrate a shorter thermal residence time than blown film, which can reduce pigment heat history, but it places a premium on rapid pigment wetting because the melt travels from die exit to chill roll in a fraction of a second. A slot die with a 0.4–0.6 mm die gap is held at 220–240 °C, and the melt curtain is pinned to a polished chill roll at 20–30 °C using a vacuum box or electrostatic edge-pinning system. Surface roughness from poorly dispersed pigment agglomerates larger than 50 µm can disturb the pinning edge and create periodic gauge bands across the web; these bands are not acceptable in stretch hoods because they convert into premature tearing under elongation. The resulting cast film is evaluated for elongation at break under ASTM D882-18; typical dark grey stretch-hood films require machine-direction elongation above 500% and transverse-direction elongation above 700%, although the actual values are set by the converter's base resin and not by the concentrate alone. Because the dark grey film absorbs more infrared radiation during the draw, the chill-roll surface temperature is controlled within ±2 °C; a higher roll temperature can cause blocking, while a lower temperature can increase transverse crystallinity gradients and reduce tear resistance. A gravimetric dosing unit with 0.1 wt% accuracy is used to avoid minor let-down fluctuations that would appear as visible dark streaks at these line speeds. Moisture pickup above 0.05% by weight in the pigment concentrate is sufficient to create moisture marks on the cast web, so closed hopper storage under nitrogen purge at 0.1–0.3 bar is applied in high-humidity production halls.
In polyethylene injection-moulding grades used for storage bins, agricultural clips, and material-handling components, POLYBATCH™ Dark Grey LL80362/4 is added at 2–4 wt%, and the converter confirms that the LLDPE carrier does not exceed 10 wt% of the total polymer matrix to avoid softening the part and reducing heat deflection temperature under ISO 75-2:2022 method A at 1.8 MPa. A general-purpose injection screw with a 20:1 L/D and a compression ratio of 2.5:1–3.0:1 is sufficient, but the screw back pressure is set to 0.5–1.5 MPa to improve dispersion homogeneity without generating excessive shear heat. Melt temperature at the nozzle is held at 200–230 °C for polyethylene-based parts, and the mould surface temperature is set at 20–40 °C; dark pigment systems respond poorly to excessively high injection speeds because the melt front can orient pigment particles along the filling path, leaving flow lines that are visible on the part surface. Weld-line regions such as hinge intersections or boss junctions are particularly sensitive because pigment particles accumulate at the melt front and can produce a lighter grey weld line that is structurally sound but aesthetically rejected. Tensile property verification on injected plaques is performed under ISO 527-2:2022 at 50 mm/min; if the part is intended for outdoor agricultural service, accelerated weathering under ISO 4892-2 with a xenon lamp and a black-standard temperature of 65 °C is used to quantify colour stability and surface chalking. The mould must not be pre-treated with silicone sprays because such sprays can alter the surface gloss of dark grey parts and create a non-uniform release profile that mimics pigment streaking. When the concentrate is stored in partially opened bags above 60% RH, pre-drying at 60–65 °C for 2 h is applied before injection to prevent moisture-induced silver streaks in thick sections; this is especially important when the component contains a flat closure face that is inspected under direct light.
In extrusion coating of dark grey tie layers or surface layers onto paper, board, or aluminium foil in industrial packaging, the concentrate is introduced at 4–7 wt% into an LLDPE or LDPE coating grade with a melt mass-flow rate of 7–15 g/10 min under ISO 1133-1:2022. A 90–120 mm single-screw extruder with a barrier screw feeds a slot die with a die gap of 0.8–1.2 mm, mounted above a chill roll and pressure roll arrangement. Melt temperature at the die is 250–280 °C to promote substrate wetting, but the concentrate is not held at this temperature for more than 5 min because the high pigment surface area accelerates thermal-oxidative degradation of the LLDPE carrier, leading to odour and pinholes in the thin coating. Coating weight is typically 15–30 g/m², and the pigment dispersion must be sufficiently fine that no visible specks above 25 µm appear on the coated surface; this is checked by light microscopy at 50× magnification under a halogen backlight. Adhesion to the substrate is tested by tape peel per ASTM D3359-23 method B, and pigment agglomerates that protrude through the thin coating layer can reduce adhesion ratings from 5B to 3B or lower. The dark grey colour in thin coating layers is sensitive to dilution; below 4 wt% there may be visible variation in optical density when the substrate colour is inhomogeneous, and above 7 wt% the melt curtain can lose stability at high line speeds because the particulate phase interferes with the extensional flow field. The coated surface temperature on the chill roll is maintained at 15–20 °C to prevent blocking, and the take-off speed is limited by the cooling capacity of the chill-roll diameter and the air-gap length rather than by a single published speed limit. If the concentrate is used in direct food-contact surface layers, the finished article must be tested for overall migration under EU Regulation 10/2011 and the pigment package must meet the purity requirements of FDA 21 CFR 178.3290; for non-food industrial packaging, REACH SVHC screening and RoHS Directive 2011/65/EU Annex II restrictions are the applicable baseline.
Because outdoor micro-irrigation tube and drip-tape formulations require a balance between UV opacity and dimensional stability, the concentrate is typically metered at 2–5 wt% into LLDPE-rich irrigation compounds, and the LLDPE carrier is not used as the sole carrier in high-pressure PE80 or PE100 pipe formulations unless the converter has verified long-term hydrostatic strength under ISO 9080:2022. A single-screw extruder with a 25:1–30:1 L/D and a pipe die with a land length ratio of 10:1–15:1 is operated at melt temperatures of 190–220 °C, with vacuum sizing controlled at -0.2 to -0.6 bar to maintain outer diameter tolerance. The concentrate is pre-dried at 60–70 °C for 2–3 h if exposed to ambient humidity above 60% RH, and the extruder head pressure is monitored so that an increase above 250 bar triggers screen-pack replacement for pigment agglomerates. Slow crack growth resistance of the final pipe is assessed by the ISO 13479-1:2022 notched-pipe test, and because dark grey concentrates contain carbon black, the dispersion quality directly influences brittle failure initiation; the let-down ratio is therefore limited to 5 wt% and the screw back pressure is set to 0.8–1.5 MPa to prevent undispersed pigment clusters larger than 50 µm. In agricultural drip tapes, the dark grey colour reduces visible algae growth when the tape is exposed to sunlight, but the addition must not reduce burst pressure; hydrostatic burst testing is conducted under ISO 1167-1:2022 at 20 °C and 60 °C depending on the application class. Published data for this specific grade in drip-tape extrusion is limited; start-up trials should begin at 2 wt% and increase only after extrusion pressure, dispersion screening, and burst-strength data are collected.
Competitive LyondellBasell POLYBATCH™ Dark Grey LL80362/4 Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell POLYBATCH™ Dark Grey LL80362/4 is a pelletized colour concentrate in which a dark grey pigment preparation is dispersed in a linear low-density polyethylene carrier. The LLDPE carrier is selected for melt-state compatibility with polyethylene-rich base resins in cast film, blown film, injection moulding, and profile extrusion. Incoming inspection for this grade is typically performed against the certificate of analysis because published data for this specific configuration is limited. Characterisation methods applicable to the concentrate include ISO 1133-1:2022 for melt mass-flow rate, ISO 1183-1:2019 or ASTM D792-20 for density, ISO 3451-1:2019 for residue after polymer pyrolysis, and EN 13900-5 for filter pressure value as a dispersion indicator. The product code structure LL80362/4 identifies the carrier class and the internal formulation revision, but it does not by itself define pigment loading or final let-down ratio.
In film extrusion lines, the concentrate is introduced through gravimetric dosing equipment at the main feed throat. Feed-throat temperature should remain below 40 °C to prevent pellet agglomeration and bridging; if hopper heating elements raise the metal temperature above the dew point, condensation can occur and increase the risk of screw slip. Let-down ratio cannot be fixed without colourimetric verification, because pigment dispersion quality in the final article is a function of base resin melt viscosity, screw geometry, and draw-down ratio rather than concentrate composition alone. Colour acceptance is commonly evaluated with a spectrophotometer using D65 illumination, 10° observer, specular-included geometry, and CIELAB coordinates under ASTM D2244. When a dark grey film must match a reference, ΔE*ab tolerances are normally set at or below 1.0 CIELAB unit; tighter ΔL*, Δa*, and Δb* split tolerances may be required for mono-layer packaging.
Dispersion quality is governed by the relationship between carrier melt viscosity and base resin melt viscosity, not solely by pigment particle size. In blown-film dilution, a concentrate with a polyethylene carrier enters the primary melt stream and must be homogenised within the residence time of a single-screw extruder. If the carrier melt mass-flow rate is significantly higher than that of the base LLDPE, the low-viscosity fraction can separate at the screw root and create visible streaks or tonal variation across the film width. On production-scale lines equipped with barrier screws and grooved feed sections, this condition is often corrected by increasing downstream mixing rather than by raising melt temperature, because excessive temperature increases the risk of oxidative shift in grey tone. Single-screw extruders with L/D ratios between 24:1 and 30:1 are generally adequate when a Maddock or Egan mixing section is positioned near the metering zone. Twin-screw extruders with L/D ratios near 40:1 are used for concentrate production, but downstream let-down rarely requires equivalent intensity unless the base resin is highly viscous or the film is thinner than 25 µm.
Screw speed and back pressure should be monitored. If a 75 mm single-screw extruder running at production rates above 150 kg/h shows pigment specking, reducing screw speed by 10 % to 15 % while maintaining the same die pressure can increase residence time enough to eliminate agglomerates without increasing melt temperature. The filtration pressure value obtained by EN 13900-5 is a relevant incoming-inspection control for such defects; a rising filter pressure during let-down indicates local pigment aggregation or screen packing. On cast film lines using screen packs of 100/60/20 mesh, pressure rises above the normal post-startup baseline by more than 50 bar over a shift should trigger inspection of the pack for concentrate-related residue.
Thermomechanical characterisation of LL80362/4 should be performed under the same conditions as polyolefin raw materials. Melt mass-flow rate is normally determined at 190 °C under 2.16 kg load using ISO 1133-1:2022 or ASTM D1238-20. Because the concentrate contains pigment particles, the measured value is a composite rheological expression rather than a pure resin melt flow. Density is measured on compression-moulded plaques by ISO 1183-1:2019 or a density gradient column under ASTM D792-20. The density of LLDPE-based grey concentrates typically lies above that of unfilled LLDPE but below that of high-carbon-black black concentrates; the exact value for LL80362/4 must be taken from the certificate of analysis, since published data for this specific configuration is limited.
Thermogravimetric analysis under nitrogen from 40 °C to 700 °C at a heating rate of 20 K/min can separate polymer decomposition from inorganic residue. ISO 11358-1:2014 provides the method framework, although pigment-specific decomposition behaviour may require method adjustment in the ramp profile to avoid overlaps between volatile additives and colourant degradation. For dark grey concentrates, residual ash is lower than for black concentrates at equal pigment dispersion level, because the colour adjustment relies on mixed pigments rather than a maximum carbon-black loading. Oxidative stability can be screened by differential scanning calorimetry under ISO 11357-6:2018 using an isothermal oxygen-induction-time protocol at 200 °C; antioxidant depletion in the carrier can alter the long-term ageing performance of the final article.
| Property | Method | Purpose | Acceptance basis |
|---|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 / ASTM D1238-20 | Carrier/base resin viscosity match | Certificate of analysis value only |
| Density | ISO 1183-1:2019 / ASTM D792-20 | Pigment loading indicator | Certificate of analysis value only |
| Ash residue | ISO 3451-1:2019 | Approximate inorganic content | Certificate of analysis value only |
| Filter pressure value | EN 13900-5 | Dispersion quality | Internal control limit |
| Colour coordinates | ASTM D2244 | L*a*b* match to reference | ΔE*ab tolerance |
The let-down ratio for LL80362/4 is not governed by a single number cited in literature. Industrial practice for LLDPE-carrier grey concentrates commonly requires pilot-scale evaluation at multiple let-down ratios using the same base resin and extrusion conditions as the production line. Colourimetric data from injection-moulded plaques rather than film can mask draw-down-related optical differences; therefore, final acceptance should be measured on film samples at the target thickness and gauge variation.
In injection moulding, replacement of an EVA-carrier concentrate with LL80362/4 shifts the additive phase from an ethylene-vinyl acetate copolymer to linear low-density polyethylene. This substitution reduces the concentration of polar vinyl acetate groups at the carrier/base interface, which can lower moisture sensitivity and reduce potential mould deposit in long-run production. EVA carriers are sometimes preferred when low melt temperature is mandated or when the base resin is a high-flow random copolymer. The LLDPE carrier in LL80362/4 may require a slightly higher melt temperature or slightly longer plastication time to reach the same dispersion quality in thin-wall moulding. Actual processing conditions should be established by instrumented cavity-pressure measurement and not by visual evaluation alone.
Compared with wax-based let-down systems, a polyethylene carrier has fewer volatile components and lower likelihood of screw slippage caused by molten wax films on the barrel wall. Wax carriers can reduce energy input and lower viscosity in the feed zone, but they can also affect seal initiation temperature and coefficient of friction in film. The LLDPE carrier typically has less effect on heat-seal performance than wax carriers, although final seal strength must be tested according to ASTM F88/F88M-21 or ISO 527-3 on the actual laminate structure. For injection-moulded parts, mechanical integrity after let-down is commonly checked by ISO 527-2:2012 tensile testing and ISO 180:2019 notched Izod impact; pigment concentrates can reduce impact strength at high addition levels, so post-moulding tests should be performed at the lowest intended manufacturing specification.
When LL80362/4 is used in polypropylene, the polyethylene carrier is not a perfect rheological match. In semi-crystalline PP matrices, PE domains can remain discrete at low let-down ratios and may slightly reduce stiffness; compatibility is screenable by melt-phase morphology examination under polarised optical microscopy or by ASTM D790-17 flexural modulus measurement. If a PP automaker specification is involved, the end user should request specific PP-carrier or universal-carrier alternatives rather than assuming direct drop-in behaviour.
Blown-film processors should monitor die lip plate-out, especially if the concentrate is added at feed throat levels above those validated for the line. A progressive loss of melt strength or increase in bubble instability after a masterbatch lot change can indicate a change in pigment dispersion or carrier-stabiliser balance, not necessarily a change in pigment colour. Pressure tracing around the die lip and measurement of film gauge profile using a capacitance gauge across the bubble circumference are objective methods to separate concentrate-related instability from air ring or cooling tower variation.
Storage of the concentrate should follow standard conditions for polyolefin masterbatches: ambient warehouse temperature below 40 °C, protection from direct UV exposure, and unopened packaging until use. If bags are exposed to high humidity above 60 % RH, pre-drying is not usually required for LLDPE-carrier colour concentrates; however, if surface condensation is observed after cold storage, drying in a desiccant or hot-air hopper dryer at 60 °C to 80 °C for 2 h to 4 h can restore free-flowing pellet behaviour. The exact bulk density, pellet count, and packaging format should appear in the certificate of analysis or shipping documentation.
Regulatory compliance of the concentrate is not determined solely by the carrier chemistry. The dark grey pigment preparation may contain carbon black, inorganic fillers, or organic colourants that carry different food-contact, heavy-metal, and waste-directive statuses. For food-contact applications, the finished article must be evaluated under the appropriate national or regional regulation; the concentrate may support compliance but does not by itself certify the final article.
Under US law, colourants for polymers used in food-contact applications are often evaluated under 21 CFR 178.3290. In the European Union, plastic food-contact materials are assessed under EU Regulation 10/2011 as amended by Regulation 2020/1245, with overall migration tested according to the EN 1186 series and specific migration methods as applicable. RoHS conformity for electrical and electronic equipment is evaluated against Directive 2011/65/EU for restricted substances such as lead, mercury, cadmium, and hexavalent chromium; a dark grey concentrate containing carbon black or mixed metal oxides should have raw-material declarations checked against EN 62321 analytical methods. REACH obligations apply to substances present above the defined concentration threshold, and a Safety Data Sheet should be consulted for hazard classification and safe handling.
| Regulatory area | Reference | Scope | Verification approach |
|---|---|---|---|
| US food contact | 21 CFR 178.3290 | Colourants for polymers | Pigment/carrier status review |
| EU food contact | EU Regulation 10/2011 / 2020/1245 | Plastic food-contact materials | Final article migration testing |
| RoHS | Directive 2011/65/EU | Restricted heavy metals | Raw-material declaration / EN 62321 |
| REACH | Regulation (EC) 1907/2006 | Registered substances and SVHCs | SDS and substance inventory review |
For industrial colour formulation, LL80362/4 differs from single-pigment black masterbatches because its tonal target is a dark grey with lower jetness and lower carbon-black loading. It should not be used as a black masterbatch substitute to achieve low L* values because increasing its let-down ratio to compensate for lightness may reduce mechanical properties and alter viscosity. Compared with white or additive masterbatches, the concentrate carries a light-absorbing pigment package; UV exposure of the tinted article under ISO 4892-2:2013 or ASTM D2565-16 is therefore relevant for exterior film and moulding specifications. No published long-term weathering data for this specific product configuration was available; end users should run comparative xenon-arc exposure against an unpigmented control and against a currently approved grey masterbatch.