    Specifications
    HS Code 600789
    Productname LyondellBasell POLYBATCH™ Dark Blue Oil LL40350/4 Concentrate Based In LLDPE
    Brand LyondellBasell
    Productcode LL40350/4
    Carrierresin Linear Low Density Polyethylene (LLDPE)
    Color Dark Blue
    Form Pellets
    Density Approximately 1.0 g/cm³
    Meltflowrate Approximately 20 g/10 min (190°C/2.16 kg)
    Moisturecontent Less than 0.2%
    Pigmentcontent Approximately 50%
    Letdownratio 2% to 5%
    Processingtemperature 180°C to 260°C
    Thermalstability Up to 260°C
    Bulkdensity 0.55 to 0.65 g/cm³
    Pelletsize 2 to 3 mm
    Compatibility Polyolefins
    Typicalapplications Blow molding, injection molding, extrusion
    Packaging 25 kg bags
    Shelflife 24 months
    Storageconditions Dry, below 30°C

    As an accredited LyondellBasell POLYBATCH™ Dark Blue Oil LL40350/4 Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Typically supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for secure transport and storage.
    Container Loading (20′ FCL) 20′ FCL container loaded with LyondellBasell POLYBATCH™ Dark Blue Oil LL40350/4, LLDPE-based concentrate, palletized bags, securely stowed for ocean freight.
    Shipping Non-hazardous plastic color concentrate in LLDPE carrier. Not regulated for transport by DOT, IMDG, or IATA. Supplied in sealed bags or boxes on pallets. Store cool, dry, away from heat and sunlight. Keep containers closed. Use standard industrial hygiene. No special shipping labels required.
    Storage Store LyondellBasell POLYBATCH™ Dark Blue Oil LL40350/4 Concentrate Based in LLDPE in a cool, dry, well-ventilated area away from sunlight, heat, sparks, and flames. Keep containers closed, upright, and labeled. Protect from moisture, contamination, freezing, and overheating. Separate from oxidizers and incompatible materials. Use secondary containment where required. Avoid dust generation and static discharge. Follow the SDS and local regulations.
    Shelf Life The shelf life is typically 24 months when stored unopened in original packaging, dry, below 30°C, away from direct sunlight.
    Application of LyondellBasell POLYBATCH™ Dark Blue Oil LL40350/4 Concentrate Based In LLDPE

    In monolayer and coextruded blown film used for consumer and industrial packaging, POLYBATCH™ Dark Blue Oil LL40350/4 Concentrate Based In LLDPE is metered at the feed throat with gravimetric dosing units calibrated to ±0.2% accuracy. Standard commercial practice for LLDPE-based color concentrates places the addition between 2 wt% and 4 wt% for films of 20–80 µm; on three-layer coex lines, adding the concentrate to a skin layer representing 20–30% of total thickness generally requires dropping the letdown to 1.0–1.5 wt% to avoid excessive color saturation and die-lip deposit formation. Processing on 50–75 mm grooved-feed extruders with L/D 25–30 at melt temperatures between 180°C and 220°C provides acceptable carrier viscosity match with LLDPE film resins having melt flow rates of 0.8–1.2 g/10 min at 190°C/2.16 kg according to ISO 1133-1:2022. Screen packs of 20/40/60 mesh are fitted before the breaker plate; an increase in screen-pack differential pressure above 1.0 MPa within an 8 h run signals agglomerate retention or carrier incompatibility and requires reducing barrel zone temperatures by 5–10°C before increasing screen surface area. Dispersion quality is checked according to ISO 18553:2002; for film thinner than 50 µm, pigment agglomerates above 50 µm produce visible fisheyes and reduce dart impact. Finished products include printed carrier bags, freezer film, produce bags, and industrial liners. Food-contact articles require finished-article compliance under EU 10/2011 Annex I and II and FDA 21 CFR 178.3290; heavy-metal limits under RoHS Directive 2011/65/EU Annex II must also be confirmed for the pigment package.

    What Limits Letdown Ratio in High-Speed Cast Film Extrusion?

    Cast film extrusion of LL40350/4 into 15–25 µm stretch film and 25–60 µm hygiene backsheet runs at line speeds from 180–300 m/min, which places a higher shear and thermal history demand on the concentrate than blown film. Letdown is normally reduced to 2–3 wt% because higher addition rates increase surface haze and lower specular gloss, a measurable effect under ASTM D2457-21 at 20° and 60° incidence. On a 45 mm single-screw extruder with L/D 30, barrel zone settings from feed to adapter are typically 180°C, 210°C, 220°C, 230°C, 240°C; melt at the flat die is held at 235–250°C. The LLDPE carrier contributes a small density increase of approximately 0.02–0.05 g/cm³ at 3 wt%, measured by ISO 1183-1:2019, but the main process conflict is quenching rate variation across the web. Chill roll temperature is set at 15–25°C with an air knife and vacuum box to eliminate air entrainment; insufficient contact produces printability defects and uneven pigment distribution in the amorphous surface layer. Published data for LL40350/4 in this specific high-line-speed configuration is limited, so commissioning should include a 24 h screen-pack delta-P trial at the 100–150 kg/h output range, with the upper limit determined by torque rather than melt temperature. Tensile and tear properties are judged by ASTM D882-18 and ASTM D1922-23; final products include hand stretch wrap, machine wrap, construction film, and medical nonwoven backsheet laminates.

    Thin-wall closures and containers injection moulded from LLDPE-rich blends with LL40350/4 use LLDPE or LLDPE/HDPE base resins with melt flow rates between 20–40 g/10 min at 190°C/2.16 kg per ISO 1133-1:2022. The concentrate is added at 2–4 wt%; below 2 wt% color intensity varies with screw recovery time and dosage accuracy, while above 4 wt% the LLDPE carrier can reduce injection pressure requirements but increase gate freeze time and shrinkage anisotropy. Reciprocating screws of 20–25 mm diameter with L/D 20–22 and general-purpose metering profiles are used, with injection pressures from 80–110 MPa and hold pressures of 50–70 MPa for 0.5–1.5 s per mm of wall thickness. Barrel temperatures from feed to nozzle are set to 180°C, 200°C, 215°C, 225°C; mold temperatures of 15–30°C allow cycle times of 8–15 s for 1.2–2.0 mm walls. Dimensional stability is checked after 24 h conditioning according to ASTM D955-21; LLDPE-rich formulations usually show shrinkage of 1.5–2.2%, with higher values in the flow direction. Finished parts include overcaps, push-pull closures, thin-wall food containers, and cosmetic packaging. For food-contact grades, compliance must be established on the final article under EU 10/2011 and FDA 21 CFR 178.3290; the concentrate itself is not a food-contact certification and phthalocyanine pigments may be subject to specific migration limits.

    When Blow Moulded Containers Require Low-Temperature Impact Retention

    Extrusion blow moulding of HDPE containers coloured with LL40350/4 creates a rheological mismatch between the LLDPE carrier and the HDPE matrix that affects parison sag and die swell. In monolayer HDPE bottles, the concentrate is dosed at 2–4 wt%, displacing an equivalent mass of HDPE; at 4 wt% the final article exhibits lower density and flexural modulus, measurable by ISO 1183-1:2019 and ISO 178:2019, but often gains environmental stress crack resistance when tested under ASTM D1693-21 Condition B. Processing on 50–80 mm extruders with L/D 24 uses melt temperatures of 170–200°C and parison temperatures of 190–210°C; die head tooling is set to a die-to-pin diameter ratio of 0.6–0.9 to control parison diameter. Blow air pressure is maintained at 0.5–0.8 MPa, and mould temperatures of 10–20°C prevent surface fold lines. Containers are produced for automotive chemicals, household detergents, and personal care fluids. Low-temperature impact retention at -20°C is typically evaluated by drop tests according to internal protocol; if the part must meet ASTM D2463-15, the HDPE grade and concentrate addition should be fixed before tooling is cut because parison geometry changes with melt elasticity. Regulatory compliance for hazardous goods packaging must be demonstrated on the finished container under applicable transport regulations, and food-contact use requires further verification under EU 10/2011.

    ApplicationRegulatory/standard referenceMeasured parameterPractical control requirement
    Blown film food packagingEU 10/2011 Annex I/II, FDA 21 CFR 178.3290Overall migration, specific migrationFinished-article testing required; no blanket approval
    Injection moulded closuresEU 10/2011, FDA 21 CFR 178.3290Specific migration of pigmentsOnly approved pigment grades; traceability to positive list
    Blow moulded containersASTM D1693-21, ISO 178:2019ESCR, flexural modulusValidate at 4 wt% letdown in HDPE
    Rotomoulded water tanksNSF/ANSI/CAN 61, EU 10/2011Extraction of metals and organicsFinal-part certification mandatory
    Cable jacketingRoHS Directive 2011/65/EU Annex IIHeavy metalsCd <0.01 wt%, Pb/Hg/Cr(VI) <0.1 wt%

    For rotational moulding of large LLDPE parts, LL40350/4 is dry blended with ground LLDPE powder at 2–4 wt% before charging to the mould. The LLDPE carrier melts during the heating cycle, but dispersive mixing is not provided by the rotating mould; therefore the concentrate must be pulverized to a particle size distribution matching the base powder, typically 35 mesh or finer, to prevent colour streaks and surface pinholes. Oven temperatures are set at 260–300°C for 20–40 min, with peak internal air temperature maintained between 180–220°C depending on part thickness and resin supplier protocol. The process is inherently low-shear, so pigment dispersion and heat ageing are evaluated by ISO 18553:2002 and by measuring melt flow shift per ISO 1133-1:2022 after the cycle; a shift above 0.4 g/10 min from the specified resin baseline indicates carrier degradation or incomplete homogenization. Finished parts include storage tanks, agricultural hoppers, marine floats, and playground panels. For potable water contact in North America, the final rotomoulded article is subject to NSF/ANSI/CAN 61 and in the EU, EU 10/2011; published data for LL40350/4 in potable water rotomoulding is limited, so certification on the finished article is mandatory before specifying this concentrate.

    Melt Filtration and Pressure Build-Up Behaviour on 40 L/D Single-Screw Lines

    On 90–120 mm single-screw sheet extrusion lines with L/D 35–40, LL40350/4 is added at 2–4 wt% into monolayer LLDPE or LLDPE/HDPE sheet from 2–6 mm thickness. Melt temperatures are controlled at 200–230°C and three-roll polishing stack temperatures at 60–90°C. The main production bottleneck is melt filtration: the LLDPE carrier has a broader molecular weight distribution than the base HDPE, and screen packs of 40/60/80 mesh can accumulate pigment agglomerates and gelled carrier fragments. A differential pressure above 2.5 MPa across the screen changer signals a need for back-flush or mechanical screen change; failure to monitor this leads to pressure fluctuation at the die lip and thickness variation in the sheet. Thermoformed parts include reusable transit trays, equipment covers, and automotive trunk liners. Automotive interior applications require fogging and odour testing under DIN 75201:2011-04 and VDA 270:2018; volatile organic compounds from the pigment carrier or processing aids may affect results, so pre-production validation is required. Mechanical properties of the formed sheet are tested according to ISO 527-2:2012 and ISO 178:2019; published data for this specific product in 6 mm thermoformed sheet is limited, so corner radius thinning and wall thickness distribution should be mapped during pilot runs.

    ProcessEquipment configurationMelt temperature/control parameterLetdown rangeCritical operational limit
    Blown film50–75 mm grooved-feed, L/D 25–30, 20/40/60 mesh180–220°C2–4 wt%Screen delta-P <1.0 MPa/8 h
    Cast film45 mm, L/D 30, flat die235–250°C2–3 wt%Line speed 180–300 m/min
    Injection moulding20–25 mm, L/D 20–22180–225°C2–4 wt%Injection pressure 80–110 MPa
    Blow moulding50–80 mm, L/D 24170–200°C2–4 wt%Parison 190–210°C
    Sheet extrusion90–120 mm, L/D 35–40200–230°C2–4 wt%Screen delta-P <2.5 MPa

    Dark Blue Jacketing Compounds for Low-Voltage Cable Extrusion

    Coloration of polyethylene cable jackets with LL40350/4 is carried out on crosshead extruders of 60–90 mm screw diameter and L/D 25, with melt temperatures from 180°C to 220°C. The concentrate is dosed at 2–4 wt% into LLDPE or LDPE jacket compounds; because cable extrusion runs at line speeds of 50–200 m/min and uses crosshead dies with screen packs of 40/60 mesh, any agglomerate above 50 µm can create a surface protrusion detected by in-line spark testing at 3–6 kV AC depending on insulation thickness. The LLDPE carrier affects elongation at break and cold bend behaviour; jacket compounds are tested according to IEC 60502-1 for low-voltage cables and ISO 527-2:2012 for tensile properties. Dark blue pigments must be selected to avoid heavy-metal content above the maximum concentration values in RoHS Directive 2011/65/EU Annex II; lead, mercury, and hexavalent chromium each have a limit of 0.1 wt%, with cadmium at 0.01 wt%. Final products include low-voltage power cable jackets, data cable sheaths, and underground conduit. When flame-retardant jackets are required, the additive package must be evaluated for interaction with dark blue pigments because some metal hydrate flame retardants can shift the shade and increase plate-out; published data for LL40350/4 in filled FR jackets is limited, and plant-scale color matching is required.

    Free Quote

    Competitive LyondellBasell POLYBATCH™ Dark Blue Oil LL40350/4 Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell POLYBATCH™ Dark Blue Oil LL40350/4 is a pelletized colour concentrate supplied in a linear low-density polyethylene carrier. The product is intended for melt dilution into polyethylene-based streams where a dark blue oil shade is required in blown film, cast film, extrusion blow moulding, or injection moulding. The use of an LLDPE carrier places the masterbatch closer in melt rheology and crystallization behaviour to LLDPE-rich host resins than concentrates carried in polypropylene, EVA, or low-density polyethylene. Published numerical data for this specific product code are limited in the abbreviated technical literature; batch-specific values for melt-flow rate, density, ash content, and pigment assay should be read from the supplier’s certificate of analysis rather than inferred from generic carrier-resin values.

    Routine specification tests for an LLDPE-carrier colour concentrate are performed under ISO 1133-1:2022 for melt mass-flow rate at 190 °C and 2.16 kg, ISO 1183-1:2019 for compounded density, and ISO 3451-1:2019 for ash or pigment residue. Colour coordinates are determined from CIE L*a*b* measurements under ISO 7724-2 or ASTM D2244. Because the product contains a dark blue organic colourant, the compounded density cannot be compared directly with neat LLDPE. The carrier polyethylene absorption bands near 718 cm⁻¹ and 730 cm⁻¹ remain visible in infrared analysis, while the colourant contributes spectral response in the visible range.

    What Limits the Letdown Ratio in Dark Blue PE Film Applications?

    The lower practical letdown threshold is governed by colour saturation, opacity, and final film thickness. For a 50 µm monolayer LLDPE blown film, a starting point of 3–5 wt% is common for dark blue polyolefin concentrates, but this is not a product specification. The upper practical letdown is constrained by rheological disturbance, die-lip deposit formation, and loss of mechanical properties. At letdown ratios above approximately 6–8 wt%, the pigment-carrier package can increase low-shear melt viscosity and require higher screw torque or elevated melt temperature. Tensile elongation at break of the diluted compound should be retested under ISO 527-3 or ASTM D882 after formulation changes because pigment agglomerates introduced at excessive letdown can act as stress concentrators.

    On a typical 50 mm grooved-feed blown film extruder with an L/D ratio of 30:1 and a 200 mm spiral mandrel die, the concentrate is metered through a gravimetric feeder. Pellet bulk density differences between natural LLDPE and the colour concentrate can produce feeding offset of approximately ±0.5 wt% if the feeder is not recalibrated. Melt temperature at the die is generally maintained between 190 °C and 240 °C for LLDPE-based systems. Residence time above 260 °C may decompose the organic blue colourant and create colour drift, odour, or sudden screen-pack pressure rise.

    Screen-pack response is more sensitive to pigment dispersion than to carrier melt-flow rate alone. A typical blown film screen arrangement uses 80/100/200 mesh packs. A differential pressure increase above 0.5 MPa within the first 10 min of running may indicate pigment agglomeration, incorrect screen placement, or insufficient melt homogenization. Dispersion quality in the finished film is assessed by transmitted-light microscopy at 100× magnification or by ISO 18553 for pigment agglomerates. Agglomerates above 50 µm are generally visible in films thinner than 25 µm and may require higher shear or a twin-screw pre-dispersion step.

    Polyethylene injection moulding grades can be coloured with the concentrate when the base resin is LLDPE, LDPE, MDPE, or HDPE. Clamp force requirements are determined by the base resin and part geometry rather than by the concentrate. Addition of the masterbatch at 2–4 wt% can shift melt viscosity slightly, and barrel zone profiling from 180 °C at the feed throat to 230 °C at the nozzle is normally sufficient. Spiral-flow testing under ISO 16790 provides a direct comparison of flow length between natural and coloured compound on a given injection machine.

    Dispersion, Screen Pack Loading, and Extrusion Backpressure

    High-shear dispersion is necessary because the dark blue oil colourant must be distributed uniformly without creating visible specks in thin-gauge polyethylene. In a co-rotating twin-screw extruder with an L/D ratio of 40:1, the masterbatch is typically fed downstream into a side feeder when additional pigment extension is performed. Screw speed, throughput, and melt temperature are balanced so that the specific mechanical energy input does not exceed the thermal stability limit of the colourant. If the concentrated product is simply dry-blended with natural LLDPE at the film extruder, distributive mixing may be insufficient at low screw speeds, producing colour streaks in the machine direction.

    In cast film production, the shorter residence time and higher line speed place a greater demand on rapid melting of the concentrate. A 75 mm barrier-screw extruder with a melt pump ahead of the flat die is commonly used. Poor dispersion can appear as transverse colour streaks or as dark-blue die-lip deposit accumulating on the inner lip of a 2,000 mm cast die. Monitoring the melt pump inlet pressure and comparing it with the natural resin baseline at constant throughput is a practical method for detecting concentrate-induced backpressure drift.

    Differences from other dark blue products are most apparent when a PP-carrier or LDPE-carrier concentrate is substituted. The LLDPE carrier can retain a higher fraction of the base film’s dart impact resistance, but the optimum letdown ratio may shift because the viscosity profile of the compound changes. In a 25 µm LLDPE blown film, dart impact is measured under ISO 7765-1, tear strength under ISO 6383-2, and haze under ASTM D1003. Replacement of a PP-carrier dark blue concentrate should be tested at the same die gap, blow-up ratio, and frost-line height, followed by adjustment of letdown in 0.5–1.5 wt% increments.

    Comparative carrier characteristics for dark blue concentrate letdown into polyethylene
    Carrier Typical processing window Melt-flow test method Primary advantage in PE film Observed limitation at high letdown
    LLDPE 190–240 °C ISO 1133-1:2022 at 190 °C/2.16 kg Compatibility with LLDPE-rich film; improved dart impact retention relative to PP carrier Higher low-shear viscosity; possible bubble instability if melt fracture is not controlled
    LDPE 170–210 °C ISO 1133-1:2022 at 190 °C/2.16 kg Lower melt viscosity and easier drawdown Dilutes LLDPE toughness; limited benefit in high-dart-drop film
    PP 200–250 °C ISO 1133-1:2022 at 230 °C/2.16 kg Higher thermal stability in high-heat applications Risk of immiscible PP domains, haze, and reduced tear resistance in PE films
    EVA 150–200 °C ISO 1133-1:2022 at 190 °C/2.16 kg Improved adhesion and flexibility Lower thermal stability, potential odour, and altered seal performance

    Regulatory acceptability of the dark blue LLDPE-carrier concentrate depends on the final packaged article and food-contact status. Where indirect food contact is claimed, the supplier may provide a compliance statement under FDA 21 CFR 178.3290 for colourants used in polymers, or migration testing under EU Regulation 10/2011 may be required for the finished article. Heavy metals are typically quantified by IEC 62321-5 or by acid digestion with ICP-OES. The product is not automatically suitable for medical device use; converters must verify the finished component under ISO 10993 when required. These are application-specific verification obligations rather than intrinsic product properties.

    Analytical and compliance references for dark blue LLDPE-carrier colour concentrates
    Control point Standard or method Reporting metric
    Melt mass-flow rate ISO 1133-1:2022 g/10 min at 190 °C/2.16 kg
    Density ISO 1183-1:2019 g/cm³
    Ash or pigment residue ISO 3451-1:2019 wt%
    Colour difference ISO 7724-2 / ASTM D2244 ΔE*
    Heavy metals IEC 62321-5 mg/kg
    Food-contact migration EU 10/2011 or FDA 21 CFR 178.3290 mg/kg or compliance statement

    When PP-Carrier or LDPE-Carrier Dark Blue Concentrates Are Substituted

    Substitution of a PP-carrier dark blue concentrate with LL40350/4 in a polyethylene film line changes the melt-viscosity balance and the bubble cooling requirement. PP carriers require higher melt temperature and exhibit a different elongational viscosity. LLDPE carriers eliminate the immiscible PP phase but may increase low-shear viscosity enough to alter bubble stability on a 70 mm blown film line. A trial replacement should be conducted at the same letdown ratio first, then adjusted by measuring film haze under ASTM D1003, dart impact under ISO 7765-1, and tear strength under ISO 6383-2. The LLDPE carrier may preserve more puncture resistance, but the optimum letdown often differs from that of the PP-carrier formulation.

    Compared with an LDPE-carrier dark blue concentrate, the LLDPE-carrier product introduces a polymer backbone with short-chain branches and a higher neat tensile modulus. At 2 wt% letdown, the effect on the diluted compound is typically small; at 5 wt%, the effect can become measurable in machine-direction tensile modulus under ASTM D882. However, the exact value depends on the base resin, film gauge, and frost-line height. The product should not be presumed interchangeable with a wax-based or EVA-based dark blue concentrate because those carriers can reduce film stiffness and alter heat-seal initiation temperature.

    The designation “Dark Blue Oil” may indicate a colourant preparation or shade distinct from standard dark blue grades. In some production comparisons, oil-formulated blue concentrates can produce different die-lip deposit behaviour, melt viscosity, or colour strength than dry-pigment dark blue masterbatches. The only reliable comparative method is to run the two candidates on the same extrusion line with the same base resin and letdown ratio, then measure pressure drop, colour coordinates, and film defect counts. Without such a trial, published property tables are insufficient for substitution decisions.

    Storage of the LLDPE-carrier masterbatch follows the same moisture-control procedures used for the host polyethylene resin. Although LLDPE is not hygroscopic, surface condensation can occur after transfer from a cold warehouse to a warm production hall at relative humidity above 60 % RH. Pellets should remain sealed in original packaging until feeding. If surface moisture is suspected, drying with desiccant air at 70–80 °C for 2 h is generally sufficient for this product class. Overdrying above 90 °C may soften the pellets and cause bridging in the hopper or feeder screw slippage.

    Optical properties of dark blue polyethylene films are best evaluated with a spectrophotometer rather than by visual inspection alone. Total luminous transmittance is measured under ISO 13468-2, while surface scattering from melt fracture or die-lip deposit is separated from pigment opacity by transmission haze under ASTM D1003. Colour strength can be checked against a pressed plaque standard using K/S values at the reflectance minimum between 550 nm and 650 nm. When the film gauge is reduced below 25 µm, the letdown ratio required to maintain the same visual hiding generally increases, and dispersion defects become more visible.

    Dosing accuracy on production lines should be verified gravimetrically because the bulk density of the concentrate may differ from the natural resin. A feeder calibration with 1 kg sample collection over 10 min at the intended throughput provides better control than a volumetric setting. If the masterbatch is preblended with natural LLDPE by tumble mixing, pellet segregation during hopper discharge can produce colour drift over the extrusion run. Transfer equipment and hopper geometry should be checked to ensure that fine particles or broken pellets do not accumulate in dead zones, where prolonged heat history can generate black specks.

    In extrusion blow moulding of dark blue polyethylene bottles and containers, the concentrate is used at the same class of letdown ratios as in film, but the parison swell and melt strength should be monitored. Addition of the masterbatch at 2–4 wt% may alter parison sag in large containers. A comparison against the natural base resin on the same shuttle blow moulder with a 1.5 kg shot provides direct evidence of viscosity change. Wall thickness distribution and drop resistance under ASTM D2463 should be measured after the colourant is introduced because dark blue pigmentation can mask visual defects such as gels, voided welds, or thin spots.

    The suffix /4 in LL40350/4 is best interpreted as a formulation or production designation rather than a publicly disclosed pigment concentration. Converter records should therefore include the full product code and batch number for traceability. Colour acceptance limits should be defined against a physical standard or CIELAB coordinates, not against a generic colour name. Because pigment strength can vary between production campaigns, lot-to-lot verification under ASTM D2244 is recommended when the product is used in thin films or in multi-layer structures where the dark blue layer is visible through a clear skin layer.

    Top