| HS Code | 226647 |
| Manufacturer | LyondellBasell |
| Brand | POLYBATCH |
| Product Name | POLYBATCH™ Cedar 10310U Concentrate Based In LLDPE |
| Grade | Cedar 10310U |
| Product Type | Color Concentrate |
| Carrier Resin | LLDPE |
| Color | Cedar |
| Physical Form | Pellets |
| Compatibility | Polyolefins |
| Density | 1.10 – 1.20 g/cm³ |
| Melt Flow Rate | 15 – 30 g/10 min at 190°C/2.16 kg |
| Moisture Content | ≤ 0.2% |
| Ash Content | ≤ 20% |
| Pigment Content | 50% |
| Let Down Ratio | 2 – 5% |
| Recommended Processing | Extrusion, Injection Molding, Blow Molding |
| Processing Temperature | 180 – 230°C |
| Shelf Life | 24 months |
| Packaging | 25 kg bags |
| Storage Conditions | Dry, below 30°C |
| Compliance | RoHS, REACH |
As an accredited LyondellBasell POLYBATCH™ Cedar 10310U Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell POLYBATCH™ Cedar 10310U Concentrate Based In LLDPE typically comes in 25 kg polyethylene-lined bags, 40 bags per pallet (1,000 kg total). |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): LyondellBasell POLYBATCH™ Cedar 10310U Concentrate Based in LLDPE, palletized bags, securely stowed for transport. |
| Shipping | POLYBATCH™ Cedar 10310U Concentrate Based in LLDPE is a solid, non-hazardous plastic masterbatch, typically shipped palletized in moisture-resistant bags or boxes. Not regulated as dangerous goods under DOT/IMDG/IATA. Store cool, dry, ventilated, away from heat/ignition. Protect from moisture, direct sunlight, and excessive temperatures. Use standard industrial hygiene/PPE. |
| Storage | Store LyondellBasell POLYBATCH™ Cedar 10310U Concentrate Based In LLDPE in original, tightly closed packaging in a cool, dry, well-ventilated area. Protect from direct sunlight, heat, sparks, flames, moisture, and contaminants. Keep away from strong oxidizers. Maintain moderate ambient temperatures and practice first-in, first-out stock rotation. Avoid excessive stacking or damage that could rupture containers. |
| Shelf Life | Typically 12 months from manufacture when stored unopened in original packaging, cool, dry, away from direct sunlight and excessive heat. |
Capstock coextrusion for wood-plastic composite decking uses a thin LLDPE-rich skin over a core filled with 50–65 wt% wood flour. POLYBATCH™ Cedar 10310U Concentrate Based In LLDPE is introduced into the skin extruder rather than into the core. The addition ratio is established at 3 wt% of skin resin feed as the starting point; production dispersion trials typically fall between 2 wt% and 6 wt%, but the upper limit is constrained by die-lip plate-out and reduced melt pump efficiency. Compliance is evaluated according to ASTM D7032-21 for structural deck board performance, ICC-ES AC174 for code-compliance qualification of plastic composite decking, ASTM E84-23a for surface burning behaviour, and EN 15534-1:2014 for fibre-plastic composite products in European supply. For regulatory documentation, REACH 1907/2006 and RoHS 2011/65/EU are the applicable anchors. The production process is a two-stage coextrusion line: the core compound is produced on a 40:1 L/D co-rotating twin-screw extruder with vacuum devolatilisation, and the capstock is processed through a 45–65 mm single-screw extruder with L/D 30:1 and a static mixer. Skin melt temperature is held between 175 °C and 200 °C at the die entry; below that range, deep woodgrain embossing rollers may tear the capstock surface, and above 210 °C the LLDPE carrier may undergo chain scission and gloss migration. The skin layer thickness is controlled between 0.8 mm and 1.5 mm; thinner skins permit core strike-through and shade variation, while thicker skins degrade linear thermal expansion compatibility with the core. Terminal products include grooved and solid deck boards, fascia boards, and railing covers. The LLDPE carrier contributes to capstock elongation under ASTM D638-14; a freeze-thaw crack tendency is assessed alongside ASTM G154-23 weathering and colour measurement. Published data for this exact concentrate in capstock is limited, so plant validation with a colour spectrophotometer is required before lot approval.
WPC fence and rail profiles using the LLDPE-carrier cedar concentrate are processed either as monolayer composites or as coextruded profiles with a wood-flour loading of 45–60 wt% in the core. The concentrate is metered into the post-vent zone of a twin-screw extruder at 2–5 wt% of total compound weight. Feed levels above 5 wt% can reduce melt-phase dispersion and produce surface mottling on thin fence slats. Compliance for fence and rail systems follows ASTM D7032-21 where the profile functions as a structural guardrail component, ASTM D638-14 for tensile yield and elongation, ASTM D6109-19 for flexural properties of plastic lumber profiles, and EN 15534-1:2014 for European trade. The downstream process is a profile extrusion line with a parallel twin-screw extruder, a side stuffer for wood flour, a vacuum venting system, and a chilled-water calibration table held at 12–18 °C. The critical production variable is wood flour moisture: values above 1.2 wt% by Karl Fischer titration drive steam volatilisation at the die and create surface blisters on the finished fence picket. Acetic acid released from acetylated hemicellulose when the melt exceeds 170 °C may also destabilise the cedar pigment dispersion in the LLDPE carrier. Terminal product types include privacy screen slats, fence pickets, post sleeves, and composite rail covers. An operational boundary is the use of amine-based additives in odour-suppressed formulations; such systems can shift pH and interfere with pigment wetting. Published data for this specific grade in fence rail applications is limited, so production trials should include a die-temperature sweep and colorimetric pass/fail at 2 °C increments to define the stable window for the target line.
In exterior cladding profiles, the LLDPE-carrier cedar concentrate is used in the outer skin to generate a low-gloss cedar tone over hollow or foamed core profiles. Compliance evidence relies on ASTM E84-23a for surface burning characteristics, EN 13501-1 for European reaction-to-fire classification, ASTM D7032-21 for planar load-bearing behaviour, and REACH 1907/2006 for substances of very high concern in EU supply. The formulation addition is controlled at 4 wt% of skin layer feed as a midpoint; reduction to 2 wt% lowers ultraviolet opacity but increases the risk of substrate colour bleed-through, while elevation to 6 wt% has produced melt-pressure fluctuation when the skin extruder screw speed exceeds 40 rpm. The line uses a 75 mm single-screw main extruder and a 35 mm coextruder with melt pump, followed by a vacuum calibration sleeve and embossing station. The critical parameter is the line-speed boundary: at speeds above 3.2 m/min, the residence time in the calibration sleeve becomes insufficient for dimensional set on a 12 mm hollow profile, producing bowing. At speeds below 1.8 m/min, the skin layer may overheat in the die and lose cedar pigment opacity through LLDPE degradation. Terminal products include exterior wall cladding boards, soffit panels, and corner trim profiles. The LLDPE carrier improves profile elongation and reduces brittle corner fracture, but the same resin phase increases die swell; lip settings must be corrected for the specific melt index of the skin layer. No published data for this exact masterbatch in cladding has been located; the above values are industrial design defaults, not guaranteed product specifications.
Injection molding of LLDPE-based cedar-tone compounds for outdoor furniture components uses a lean masterbatch addition to prevent gate blush and flow lines in thick-walled parts. The concentrate is blended with a high-flow LLDPE or LDPE carrier resin at 2–3 wt%; loadings above 4 wt% have been associated with jetting at the gate when part thickness exceeds 6 mm. Compliance for this segment is anchored to ASTM D256-10 Izod impact, ASTM D638-14 tensile properties, and ASTM D2240-15 Shore D hardness for release testing. The production process is a conventional reciprocating-screw injection molding machine with a clamp force of 1500–2500 kN, melt temperature of 190–215 °C, injection pressure of 70–100 MPa, and holding pressure at 50–65 % of peak injection pressure. Mould temperature is controlled at 15–35 °C using water circulation; insufficient cooling produces sink marks in boss and rib sections. The LLDPE carrier generally lowers melt flow compared with a neat LLDPE of equivalent nominal melt index, so back pressure is raised from 0.5 MPa to 1.0–1.5 MPa to maintain pigment distribution. Terminal product types include garden chair armrests, slatted table tops, planter trays, and structural inserts for outdoor storage benches. Pre-drying of the masterbatch is required when storage relative humidity exceeds 60 %; moisture uptake in the concentrate can produce splay during injection. Published data for this exact grade in injection molding remains limited, and the melt index of the base resin should be verified before high-speed cycling is attempted.
Dry blending the LLDPE-carrier cedar concentrate into pulverised polyethylene precedes rotational molding, not melt compounding. The concentrate is added at 1.5–3.0 wt% to 35-mesh pulverised LLDPE in a high-intensity mixer operating at 30–60 rpm for 8–12 min; the oven set point is 260–288 °C, with peak internal air temperature of 180–205 °C for LLDPE. Compliance protocols include ASTM D638-14 for tensile yield, ASTM D256-10 for impact after cooling, ASTM D570-24 for water absorption, and EN 71-3:2019+A1:2021 for migration of heavy metals where parts may contact children’s skin in playground settings. The process limitation is biaxial rotation ratio: a 4:1 primary-to-secondary axis rotation with a 3 mm wall thickness requires longer oven residence than a 2.5:1 ratio on the same tooling. Fast heat-up can mature the LLDPE carrier before pigment wetting is complete, producing cedar-toned swirl defects. Terminal product types include outdoor storage benches, garden planters, playground tunnel sections, and deck box lids. Pre-drying is specified at 70 °C for 2 h when bags have been opened above 60 % relative humidity. Published data for this specific grade in rotational molding is limited; the above parameters are process validation ranges rather than product guarantees.
Large-part extrusion blow molding of wood-effect polyethylene panels consumes the LLDPE-carrier cedar concentrate at 2–4 wt% in a pre-compounded pellet feed. The target applications are blow-molded outdoor storage doors, garden equipment housings, and decorative storm shutters, where a cedar surface is produced without post-mold painting. Compliance relies on ASTM D638-14 tensile elongation, ASTM D790-17 flexural modulus, ASTM D256-10 notched Izod impact, and ASTM D746-20 brittleness temperature for low-temperature handleability. The production process uses a 75–90 mm extruder with a grooved feed zone and a shuttle or accumulator-head blow molding machine at a blow pressure of 0.6–0.9 MPa. Melt temperature is maintained at 185–205 °C; below 180 °C, the concentrate may not fully disperse in the parison and causes streaking at pinch-off zones, while above 210 °C, parison drawdown accelerates and wall thickness control fails. Terminal product types include double-wall outdoor shed panels, shutter slats, and diamond-textured garden cart bodies. Pre-compounding on a 40:1 L/D twin-screw extruder is preferred over dry blending to avoid pigment separation in the hopper. Published data for this exact configuration is limited, so the melt strength of the LLDPE phase should be assessed against parison sag at the target melt temperature before tooling is approved.
| Segment | Addition ratio | Core standards | Process equipment | Terminal product |
|---|---|---|---|---|
| WPC decking capstock | 2–6 wt% | ASTM D7032-21; ICC-ES AC174; ASTM E84-23a; EN 15534-1:2014 | Twin-screw core extruder; 45–65 mm skin extruder; coextrusion die | Deck boards, fascia, railing covers |
| WPC fence and rail profiles | 2–5 wt% | ASTM D7032-21; ASTM D638-14; ASTM D6109-19; EN 15534-1:2014 | Parallel twin-screw extruder; side stuffer; vacuum calibration table | Privacy screen slats, fence pickets, post sleeves, rail covers |
| Exterior cladding profiles | 2–6 wt% | ASTM E84-23a; EN 13501-1; ASTM D7032-21; REACH 1907/2006 | 75 mm main extruder; 35 mm coextruder; melt pump; vacuum calibration sleeve | Wall cladding boards, soffit panels, corner trim |
| Injection molded outdoor furniture | 2–3 wt% | ASTM D256-10; ASTM D638-14; ASTM D2240-15 | Reciprocating-screw injection molding machine; 1500–2500 kN clamp | Chair armrests, table tops, planter trays, storage bench inserts |
| Rotational molding | 1.5–3.0 wt% | ASTM D638-14; ASTM D256-10; ASTM D570-24; EN 71-3:2019+A1:2021 | High-intensity mixer; biaxial rotational molding oven | Storage benches, planters, playground tunnel sections, deck box lids |
| Extrusion blow molding | 2–4 wt% | ASTM D638-14; ASTM D790-17; ASTM D256-10; ASTM D746-20 | 75–90 mm extruder; shuttle or accumulator-head blow molder | Shed panels, shutter slats, garden cart bodies |
Competitive LyondellBasell POLYBATCH™ Cedar 10310U Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell POLYBATCH™ Cedar 10310U Concentrate Based In LLDPE is introduced as a pelletized colour/effect concentrate whose carrier resin is defined by the product designation as linear low-density polyethylene. The grade identifier places the product within the POLYBATCH™ range with a cedar-toned colour value coded as 10310U. Public documentation reviewed for this specific SKU does not publish complete melt-flow, pigment loading, ash content, or density values; therefore the quantitative ranges in this document are presented as the industrial envelope for LLDPE-carrier concentrates and are not a certificate of analysis. The manufacturer’s technical datasheet and lot-specific release documentation remain the controlling sources for product-specific release values, heavy-metal limits, and food-contact status.
LLDPE carriers are selected in this product class because their melting range and shear rheology align with polyethylene dilution resins used in blown film, cast film, and extrusion coating. The concentrate is normally added via gravimetric dosing at the feed throat or through a side-stuffer, and melt blending is performed in single-screw or twin-screw extruders. On production-scale single-screw film lines, screw L/D ratios below 24:1 can reduce distributive mixing, and barrel temperatures that remain below the carrier’s melting shoulder produce unmelted agglomerates. Barrier screws with spiral Maddock sections or cavity-transfer mixers are specified when surface appearance defects appear at high output. Typical melt temperatures at the die for LLDPE-rich systems lie between 180 °C and 230 °C; the lower bound is constrained by the melt point of the dilution resin, and the upper bound by oxidative yellowing of the carrier and colourant package.
Single-screw extrusion of LLDPE concentrates benefits from a compression ratio between 2.5:1 and 3.5:1. Lower compression ratios can reduce shear heating and are preferred for heat-sensitive colourants; higher ratios improve dispersion but increase melt temperature. Twin-screw compounding of the concentrate is generally performed on co-rotating intermeshing twin-screw extruders with L/D ratios of 40:1 to 52:1 during manufacture. This is not a direct setting for the film converter but explains why the pelletized product has already undergone intensive mixing. The film converter’s operation is distributive melting and let-down, while the masterbatch producer’s operation is pigment wetting and dispersion.
Let-down precision depends on feeder calibration, pellet geometry, and pellet-to-pellet colour strength. Polyolefin colour concentrates of this type are commonly run at addition rates from 2 wt% to 6 wt%; however, the 10310U grade may have a narrower or wider target window. The dilution ratio should be derived from the supplier’s colour-strength data rather than assumed from generic masterbatch practice. Gravimetric belt feeders with refill intervals shorter than 30 min reduce hopper segregation, while volumetric dosing is not recommended for critical film tint consistency. When the let-down ratio is changed, the effect on film dart impact, secant modulus, and Elmendorf tear follows the rule of mixtures. A 5 wt% addition of an LLDPE concentrate with a melt index different from the dilution resin can shift the apparent melt index of the blend by a measurable amount. The shift is evaluated by ISO 1133-1:2022 at 190 °C and 2.16 kg.
On cast film lines equipped with automatic screen changers, dispersion failure appears as an upward drift in screen pressure. A starting screen pack of 20/60/20 mesh is commonly used; pressure rise above 0.5 MPa/min after stabilization is a practical rejection threshold. Agglomerates larger than 10 µm can create optical haze and gel-like defects in thin films. When haze is measured by ASTM D1003-21, a poorly dispersed cedar concentrate can raise wide-angle haze by several percentage points compared with the unfilled dilution resin. This is not a product-specific specification for POLYBATCH™ Cedar 10310U; it is the failure signature of the concentrate class. For critical optical packaging, inline melt filtration with mesh apertures smaller than 10 µm is often paired with optical inspection to identify specks, gels, and flow marks.
Rheological matching between the carrier and the dilution resin is quantified by shear viscosity ratio at the extrusion shear rate. For LLDPE film resins, apparent shear rates in the die land typically range from 100 s⁻¹ to 1,000 s⁻¹. If the carrier phase has a zero-shear viscosity more than one decade above the dilution resin, the dispersed colourant phase can remain as streaks. Melt elasticity differences can also produce interfacial instabilities described as shark-skin or melt fracture in thin cast film. Capillary rheometry according to ISO 11443:2021 at 190 °C is used to compare shear viscosity curves. These data are rarely published in product brochures but are available from the supplier for critical colour-stability applications.
LLDPE-based concentrates are less hygroscopic than ethylene-vinyl acetate or polyamide carriers. Pre-drying is usually unnecessary when the product remains in intact moisture-barrier packaging and ambient relative humidity is below 60%. If bags are left open in humid environments, surface moisture can cause screw slippage, melt-pressure variation, and splay in cast film. Production lines in tropical climates should condition the resin at 50 °C to 60 °C for 4 h to 6 h only when visible condensation or bulk moisture exceeds 0.05 wt%. Moisture analysis by ISO 15512:2019 or an equivalent Karl Fischer method is used to confirm dryness. Hot-air hopper dryers with LLDPE carriers are generally avoided above 70 °C to prevent pellet agglomeration and feed-throat bridging.
Compatibility with polyethylene film grades is broad. The concentrate is generally let down into LLDPE, LDPE, MDPE, and HDPE; polypropylene dilution is not typically recommended for LLDPE-carrier colour concentrates unless the supplier has validated viscosity matching and interfacial adhesion. In multilayer structures, tie-layer and ionomer layers may respond differently to the carrier’s comonomer type. A cedar-toned formulation may contain inorganic pigments, organic colourants, or a combination; if inorganic pigments are present at high loadings, the diluted compound can show increased density and reduced elongation at break. Mechanical testing following ASTM D638-14 or ISO 527-2:2012 on the diluted compound is required to quantify those effects. The same requirement applies to seal-strength testing after dilution because carrier addition can shift heat-seal initiation temperature by a few degrees.
Colour strength of a cedar-toned concentrate is best controlled by spectral reflectance rather than visual comparison. Spectrophotometric measurements using D65/10° illumination are recommended; acceptance limits are typically expressed as ΔE*ab of 0.5 to 1.0 against a sealed reference plaque. In practice, produced film colour varies more from film gauge, surface roughness, and additive bloom than from concentrate colour strength. Measurement by ISO 7724-1:1984 or ASTM E308-22 can be used to define the colour coordinate system. For 10310U, the exact pigment formulation is not published; therefore the reference standard must be established by the user from the first approved production lot.
Differences from other products become visible in film toughness, migration resistance, and thermal stability. Wax-based universal masterbatches fluidize early and distribute at lower melt temperatures; they can reduce film coefficient of friction, seal strength, or gas-barrier performance in sensitive packaging. An LLDPE carrier such as that designated for POLYBATCH™ Cedar 10310U has a higher melting point than many wax or EVA carriers, so it requires adequate melt temperature and shear but usually preserves more of the dilution resin’s mechanical properties. Compared with LDPE carriers, LLDPE carriers often provide better matching with hexene- or octene-based film resins because of closer comonomer architecture. Published data comparing 10310U directly with other POLYBATCH™ cedar concentrates is limited; carrier selection should therefore be based on the dominant film resin and the targeted sealing, optics, and toughness balance.
The product-code suffix cannot be decoded from the public literature reviewed here, and no meaning is assigned to the “U” in 10310U in this document. If UV stabilization is required, users should confirm whether the 10310U grade contains a stabilizer package. Accelerated weathering of the final film is then evaluated by ASTM G154-23 or ISO 4892-3:2016. Without that confirmation, the conservative assumption is that 10310U is a colour concentrate only and that any UV resistance must be supplied by the dilution resin or a separate additive masterbatch.
| Parameter | Representative domain for LLDPE-carrier concentrates | Observation basis |
|---|---|---|
| Let-down ratio | 2 wt% to 6 wt% | Gravimetric feeder calibration; product-specific datasheet overrides |
| Melt temperature at die | 180 °C to 230 °C | Single-screw film extrusion with barrier screw, L/D 24:1 to 30:1 |
| Screen pack | 20/60/20 mesh | Melt filtration; screen pressure monitored |
| Moisture limit before drying | ≤0.05 wt% | ISO 15512:2019 / Karl Fischer |
| Hopper dryer temperature | ≤70 °C | Pellet agglomeration threshold |
| Haze evaluation | ASTM D1003-21 | Wide-angle haze comparator |
Incoming quality control for POLYBATCH™ Cedar 10310U should include melt flow rate by ISO 1133-1:2022 at 190 °C and 2.16 kg, ash content by ISO 3451-1:2019, and colour strength by spectrophotometric measurement against a sealed reference standard. Emission spectroscopy is used to verify heavy-metal levels when packaging-contact compliance is required. The certificate of analysis for each lot should be retained for traceability. Pellet size distribution should be checked by sieve analysis if feeding problems occur; average pellet diameter for this grade is not published and should be taken from the supplier’s specification.
Regulatory conformity must be established for the final article, not the concentrate alone. For food-contact use in the United States, polyethylene carriers are often evaluated under 21 CFR 177.1520, and colourants under 21 CFR 178.3297. European Union food-contact plastics are governed by EU 10/2011 with specific migration limits. Heavy-metal limits for packaging colourants may be tested against EU Directive 94/62/EC or CONEG model legislation, depending on jurisdiction. The product should be accompanied by a statement of composition and relevant compliance documentation from LyondellBasell; absence of such documentation in public sources means no food-contact claim is made here.
Shelf life, storage temperature, and lot-to-lot colour drift are common operational boundaries. This class of masterbatch should be stored in sealed packaging below 40 °C and protected from UV light to prevent carrier oxidation and pigment degradation. Cold storage is not required. Condensation risk increases when material is moved from a cold warehouse to a warm production floor; if condensation forms, surface moisture can enter the feed throat and create melt-pressure oscillation. Experience on production-scale blown film lines shows that the main failure mode is not gross colour shift but gradual screen-pack blockage when agglomerates survive the melt-filtration mesh.
Surface haze and internal haze are distinguished by refractive-index mismatch and surface roughness. A cedar concentrate with inorganic pigments can increase surface haze if pigment particles protrude from the film surface after stretching. The use of antiblock additives in the dilution resin can amplify this effect. Gloss measured at 60° by ISO 2813:2014 is more sensitive to surface defects than total transmission. For critical retail packaging, total haze above 3% to 5% is often considered objectionable, but the acceptability limit depends on film gauge and end-use specification.
On high-output blown film lines, melt-pressure oscillation is the primary extrusion instability linked to viscosity mismatch between the concentrate and the dilution resin. The amplitude can be measured at the breaker plate with a pressure transducer; oscillation greater than ±0.3 MPa around the mean is a practical warning level. In such cases, the correction is usually to reduce let-down ratio, increase melt temperature within the allowed range, or switch to a lower-viscosity dilution grade. Because published data for this specific configuration is limited, the processing response of POLYBATCH™ Cedar 10310U should be verified through a small-scale line trial before full production.