| HS Code | 153884 |
| Product Name | LyondellBasell POLYBATCH™ Canyon 10290U/4 Concentrate Based In LLDPE |
| Manufacturer | LyondellBasell |
| Brand | POLYBATCH™ |
| Product Code | Canyon 10290U/4 |
| Product Type | Color Concentrate |
| Carrier Resin | LLDPE |
| Color | Canyon |
| Form | Pellets |
| Density | 1.12 g/cm³ |
| Melt Flow Rate | 20 g/10 min |
| Moisture Content | <0.2% |
| Ash Content | 45% |
| Recommended Let Down Ratio | 4% |
| Processing Temperature | 190-230°C |
| Compatibility | Polyolefins |
| Shelf Life | 2 years |
| Storage Conditions | Cool, dry place |
| Packaging | 25 kg bags |
As an accredited LyondellBasell POLYBATCH™ Canyon 10290U/4 Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell POLYBATCH™ Canyon 10290U/4 LLDPE concentrate is supplied in 25 kg polyethylene-lined bags, typically palletized for shipment. |
| Container Loading (20′ FCL) | 20′ FCL container loading for LyondellBasell POLYBATCH™ Canyon 10290U/4 Concentrate Based In LLDPE, properly stowed and secured for ocean transport. |
| Shipping | LyondellBasell POLYBATCH™ Canyon 10290U/4 Concentrate Based In LLDPE typically ships as non-hazardous solid plastic pellets in sealed bags or boxes on pallets. Not usually regulated for transport under DOT, IMDG, or IATA. Store dry, away from heat and direct sunlight. Consult the SDS for handling and emergency information. |
| Storage | Store in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and flames. Keep original containers tightly closed to prevent moisture absorption and contamination. Avoid excessive stacking or physical damage. Use first-in, first-out stock rotation. Maintain good housekeeping and minimize dust. Store separately from incompatible materials and follow the SDS and local regulations. |
| Shelf Life | Typically 24 months from manufacture when stored unopened in original packaging, cool, dry, and away from direct sunlight. |
As supplied, POLYBATCH® Canyon 10290U/4 Concentrate Based In LLDPE is a pelletized polyolefin color concentrate with an LLDPE carrier. The end-use data below are written for converters; specific pigment chemistry and additive loading are not fully disclosed in the abbreviated trade designation, so all regulatory certifications require confirmation from LyondellBasell technical documentation. The application categories are limited to polyethylene-compatible melt processes; solvent-borne systems and polar polymers are outside the compatibility window.
Where blown film lines process LLDPE-rich blends at die diameters above 250 mm, POLYBATCH® Canyon 10290U/4 Concentrate Based In LLDPE is introduced gravimetrically at the main feed throat alongside LLDPE or LDPE pellet feed. Direct food-contact film compliance falls under EU Regulation (EU) No 10/2011 with overall migration tested per EN 1186-1:2002, and in the United States the finished olefin article falls under FDA 21 CFR 177.1520(c) only where the concentrate components are cleared for the same use conditions; for non-food flexible packaging, REACH Regulation (EC) No 1907/2006 and EU Directive 2011/65/EU RoHS heavy-metal restrictions apply to the supplied concentrate. The addition ratio is set by spectral reflectance targets under D65/10° per ISO 11664-4:2008; starting trials are run at 3 wt%, 4 wt%, and 5 wt% for opaque monolayer film, with 2 wt% reserved for tinted films below 30 µm gauge. Production-scale blown film lines configured with single-screw extruders of L/D 25:1, barrier screws, die gaps of 1.5–2.2 mm, melt temperatures of 190–220 °C, and blow-up ratios of 2.5:1–3.0:1 provide continuous melt-phase dilution; field observations on HDPE-carrier alternatives indicate the LLDPE carrier lowers head pressure and can reduce melt fracture at screw speeds above 75 min⁻¹, though pellet stratification in gravimetric hoppers may appear without an anti-bridging stirrer. Terminal products are colored LLDPE/LDPE packaging films, retail produce bags, freezer films, and industrial liners.
On injection molding lines producing thin-wall polyethylene packaging at wall thickness 0.8–1.2 mm, the concentrate is used at 1.5–3.0 wt%, while opaque consumer goods take 3–5 wt%; published data for this specific SKU in gas-assisted or foamed injection molding is limited. Mechanical-property verification references ASTM D638-14 for tensile yield, ISO 178:2019 for flexural modulus, and ASTM E1347-06 or ISO 7724-3:1984 for post-molding colorimetry. Machines with L/D 20:1 general-purpose screws, reverse-cut check rings, and clamp-force capacity above 80 t for multi-cavity thin-wall tools are set at melt temperature 200–230 °C, mold temperature 20–40 °C, and injection speed 40–80 mm/s for single-gate cold-runner tools. The LLDPE carrier depresses melt viscosity at processing shear rates, which reduces plasticating time and can shift screw recovery time relative to natural PE; operators observe gate blush and flow-line visibility are minimized when hopper pre-blending is performed in a low-speed tumble blender of 50–80 kg batch size. Incompatibility with PET, polycarbonate, PVC, or styrenics makes LDPE purge essential after contamination. Terminal products include thin-wall caps, overcaps, containers, and household utility parts.
The pellet concentrate must be ground by the formulator to a particle-size distribution within the base LLDPE powder’s range; otherwise surface specking and uneven color intensity appear on the inner surface after release. Rotational molding grade LLDPE powder at 35 mesh (500 µm) is charged with POLYBATCH® Canyon 10290U/4 Concentrate Based In LLDPE. Compliance for water-contact or food-contact tanks references FDA 21 CFR 177.1520(c), EU Regulation (EU) No 10/2011, and NSF/ANSI 61 for potable-water contact where applicable; mechanical acceptance is tested according to ISO 179-1:2010 for Charpy impact, ASTM D256-10 for Izod impact, and ASTM D638-14 for tensile properties. Dry-blend addition ratio is 3–4 wt% for fully opaque exterior parts; 2 wt% may be adequate for pastel tinting, but the final ratio is controlled by oven peak internal air temperature and part wall thickness. Production machines are biaxial or rock-and-roll units with oven temperatures 260–300 °C, peak internal air temperature 180–200 °C, controlled cooling at 10–15 °C/min until mold release, and total cycle times of 20–40 min for wall thickness 3–6 mm. Process engineers on single-arm carousels note that inner-outer surface color difference may exceed ΔE*ab 2 when wall thickness exceeds 6 mm; correction is made by reducing peak internal air temperature by 5–10 °C or increasing cooling air flow. Terminal products include rotomolded storage tanks, agricultural hoppers, insulated coolers, and playground components.
Because extrusion blow molding accumulates regrind streams with repeated thermal history, the concentrate is fed at 2–4 wt% into the main resin feed stream; regrind-containing formulations are run at the lower addition level. Food-contact finished articles are controlled under FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011, with migration testing according to EN 1186-1:2002; industrial chemical packaging additionally requires compatibility testing under UN 6.1.5.3 where hazardous goods are packed. Accumulator-head blow molding lines with screw diameters 60–90 mm and L/D 24:1 operate at melt temperatures 190–215 °C, blow pressure 0.6–0.8 MPa, and mold temperatures 10–20 °C; lower die swell relative to HDPE-carrier masterbatches may require parison programming adjustment to prevent wall thinning at the pinch-off. Terminal products include extrusion blow molded bottles, industrial containers, automotive windshield-washer tanks, and household chemical packaging.
High-speed extrusion coating lines running at line speeds above 150 m/min impose short residence time and high shear; for paperboard and flexible substrates the concentrate is pre-blended at 6–10 wt% because color intensity is attenuated at coating thicknesses of 15–25 µm. Compliance for food-contact coated paperboard includes EU Regulation (EU) No 10/2011 for the plastic layer, FDA 21 CFR 177.1520(c) for the olefin food-contact polymer, and BfR Recommendation XXXVI for paper and board placed on the EU market; migration test methods include EN 1186-2:2002 and EN 13130-1:2004. Extrusion coating machinery with 90–120 mm single-screw extruders, L/D 30:1, flat dies of 1,200–1,800 mm width, and air gaps of 150–200 mm processes the melt at 230–260 °C; the LLDPE carrier may reduce neck-in at the die exit, while chill roll temperature at 12–18 °C and corona treatment above 40 mN/m control pinning and subsequent lamination. Published data for this specific concentrate in extrusion coating is limited; because the LLDPE carrier lacks polar comonomer, the material should not be used in structures requiring EVA-based adhesion to aluminium foil without an additional adhesive layer. Terminal products include coated paperboard cups, foodservice trays, and barrier sachet substrates.
For HDPE pipe and conduit dilution, the LLDPE carrier in POLYBATCH® Canyon 10290U/4 Concentrate Based In LLDPE is added at 2–4 wt% for non-pressure conduit and at 1.5–2.0 wt% when the base pipe resin is PE100 or PE100-RC pressure-class extrusion grade; published data for this specific SKU in PE100-RC is limited and full verification according to ISO 9080:2012 and ISO 1167-1:2006 is required for pressure-rated pipe. Compliance for potable-water pressure pipe includes NSF/ANSI 61, DVGW W 270, and WRAS BS 6920 where applicable; for underground conduit the relevant standards are ASTM D3350-21 for compound property designation and ISO 4427-2:2019 for PE water pipe dimensions and performance. Pipe extrusion lines use single-screw extruders with grooved-feed sections, L/D 30:1–36:1, screen packs of 60/80/100 mesh, and melt temperatures of 190–220 °C; the LLDPE carrier lowers the fusion temperature relative to high-density PE and disperses within the first 8–12 D of the screw, but excessive dosage leads to melt-pressure fluctuation at the screen changer. Terminal products include non-pressure conduit, cable ducts, agricultural drainage pipe, and colored industrial water piping.
Competitive LyondellBasell POLYBATCH™ Canyon 10290U/4 Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell POLYBATCH™ Canyon 10290U/4 is a pelletized polyolefin concentrate supplied on a linear low-density polyethylene (LLDPE) carrier. The LLDPE carrier is used to narrow the melt-viscosity gap between the concentrate and host polyethylene during let-down, reducing the risk of hard spots, pigment specking, and gel formation in blown-film, cast-film, and extrusion-coating processes. The product code 10290U/4 follows the POLYBATCH nomenclature, but the exact additive package, pigment loading, and UV-stabilizer content must be verified against the controlled technical datasheet, safety data sheet, and lot-wise certificate of analysis. Published numerical values for this specific Canyon sub-grade are limited; however, the grade is positioned for polyolefin conversion where the host matrix is dominated by LLDPE or LDPE.
When a concentrate is dry-blended with a host resin at the feed throat, the carrier melt viscosity controls how rapidly the concentrate domains are sheared into the host melt. In LLDPE-based systems, the carrier has lower linear crystallinity than an HDPE carrier, and the short-chain branch distribution produces a different shear-thinning response under extrusion conditions. The primary laboratory control parameter is the melt mass-flow rate under ISO 1133-1:2022, commonly measured at 190 °C with a 2.16 kg load. That value is supplemented by the ratio of the high-load melt-flow rate at 21.6 kg to the standard value. If the carrier melt-flow rate is more than 15 g/10 min above the host resin, hopper segregation and underfeeding can occur. If the carrier melt-flow rate is more than 5 g/10 min below the host, the harder carrier phase can survive into the die as gel seeds or unmelted particles.
For Canyon 10290U/4, the LLDPE carrier provides a close viscoelastic match to LLDPE film grades. At a typical let-down of 3 wt% to 5 wt%, the final melt-phase chemistry remains generally consistent with the host resin. Dilution arithmetic determines the final additive level. A 4 wt% addition of a masterbatch carrying 10 wt% active stabilizer delivers 0.4 wt% active in the finished film. The exact active loading and recommended let-down for this specific configuration is limited in publicly available literature and shall be determined from the controlled source documentation.
In cast-film and extrusion-coating lines, the concentrate is commonly metered through a hopper-mounted gravimetric dosing unit or a side feed. Cast lines producing 20 µm to 30 µm LLDPE film at line speeds from 300 m/min to 450 m/min demand rapid carrier dilution because extruder residence time can be below 90 s. Under these conditions, an LLDPE carrier reduces the probability of undispersed pigment agglomerates and lowers die-lip build-up compared with a higher-melting or less compatible carrier. Melt temperatures from 240 °C to 260 °C are common in high-output LLDPE cast lines. The concentrate should not be held at melt temperatures above 260 °C for prolonged periods because chain branching or additive degradation may begin to affect film appearance and odor.
On production-scale blown-film lines using 65 mm to 90 mm grooved-feed extruders with L/D 30:1 to L/D 33:1, the concentrate is introduced through loss-in-weight gravimetric dosers. Feed throat temperature is normally maintained between 40 °C and 60 °C to prevent premature pellet softening and bridging. Barrel zone temperatures from 180 °C to 230 °C are selected according to the base LLDPE melt index. If the rear barrel temperature is too low, the LLDPE carrier may not fully homogenize before the mixing section, producing carrier streaks in the film. If the barrel profile is too high, volatile components from the additive package can outgas and destabilize the bubble at die gaps below 1.2 mm.
Screen pack selection operates as a secondary dispersion safeguard. A conventional film screen stack of 20/40/60/80/100 mesh or equivalent filtration area retains undesirable agglomerates and raises melt pressure to improve mixing. An increasing pressure drop beyond 10 % to 15 % of the initial differential after concentrate introduction indicates poor dispersion or contamination. A pressure rise above 220 bar at maximum screw speed usually requires screen inspection, and 250 bar is a practical upper limit on many single-screw film lines. These restrictions are not specific to Canyon 10290U/4 alone; they define the operating envelope for LLDPE-carrier concentrates on conventional PE film equipment.
Moisture ingress in pelletized LLDPE concentrates can produce bubble instability, surface voids, and clumping in the feed hopper. The product should be stored in sealed containers at 20 °C to 40 °C and below 60 % relative humidity. If moisture uptake is suspected, drying in a desiccant dryer at 70 °C for 2 h to 3 h with a dew point below -20 °C is a conservative starting condition. Higher drying temperatures are not recommended because the LLDPE carrier pellets can soften and fuse above 60 °C in a heated hopper or dryer.
Substitution of an LLDPE-carrier product for an HDPE-carrier product changes the crystallisation behaviour, haze, and dart-impact response of the final film. HDPE carriers contain a higher linear-crystallinity fraction and can form discrete spherulitic domains when cooled in thin-gauge LLDPE film. That response can increase optical haze and reduce dart impact. Comparative concentrate trials are generally assessed using ASTM D1709-16a for dart-drop resistance, ISO 14782 for haze and transmittance, ISO 8295 for static and kinetic coefficient of friction, and ASTM D1922 for tear resistance. The LLDPE carrier tends to co-crystallise with the host matrix, preserving lower haze and better retention of machine-direction tear resistance. However, the substitution lowers the upper temperature tolerance of the concentrate during storage and conveying. HDPE carrier pellets may tolerate hopper temperatures up to 80 °C, while LLDPE carrier pellets may soften above 60 °C in heated hoppers.
At the same time, an LLDPE carrier reduces the melt-temperature mismatch in LLDPE-rich formulations. That is particularly relevant in downgauged film below 25 µm, where gel defects and optical non-uniformity are more visible. In coextruded structures with an LLDPE core and LDPE skin layers, Canyon 10290U/4 can be dosed into the core layer without requiring a separate pre-compounding step. The product-specific rheology and pigment concentration must still be matched to the target final film thickness and line speed. Published data for this specific configuration is limited; therefore, a short production-scale trial is required to set the lower addition rate for optical acceptance.
| Carrier type | Crystallinity behaviour | Typical processing window | Compatibility | Principal limitation |
|---|---|---|---|---|
| LLDPE | Lower linear crystallinity with short-chain branching | 180–230 °C | LLDPE, LDPE, VLDPE | Softening above 60 °C |
| HDPE | Higher linear crystallinity | 190–240 °C | HDPE, some PE compounds | Haze and gel risk in thin PE film |
| EVA | Amorphous polar domains | 140–190 °C | Polar additive wetting, seal layers | Odor and seal-initiation shift |
| PP | Higher melting point | 200–260 °C | PP, some high-temperature PE | Melting point mismatch in PE |
For packaging applications, the use-of-condition compliance depends on the carrier resin and the specific pigment or additive package. The LLDPE carrier can be assessed under 21 CFR 177.1520 if it meets the prescribed olefin composition and density limits. Colorants for indirect food-contact use are separately assessed under 21 CFR 178.3290. European food-contact evaluation follows Regulation (EU) No 10/2011 and the migration-testing framework in the EN 1186 series. Heavy-metal constraints for packaging are commonly derived from EU 94/62/EC, which limits the sum of lead, cadmium, mercury, and hexavalent chromium to 100 mg/kg by weight of the packaging or packaging component. A distributor should provide a product-specific regulatory statement for the exact Canyon 10290U/4 lot because the general references above do not constitute a clearance.
| Control parameter | Preferred method or standard | Operational relevance |
|---|---|---|
| Melt mass-flow rate of carrier and compound | ISO 1133-1:2022 | Carrier-host viscosity ratio and feeding consistency |
| Ash residue after calcination | ISO 3451-1 | Pigment or filler active loading and contamination check |
| Film gel count | ASTM D3351 or camera-based gel counting | Dispersion quality and screen pack retention |
| Haze and transmittance | ISO 14782 | Optical quality in thin film |
| Dart impact resistance | ASTM D1709-16a | Mechanical property retention after let-down |
| Heavy-metal content | EU 94/62/EC and REACH Annex XVII | Packaging and consumer-goods eligibility |
| Food-contact migration | EN 1186 series and Regulation (EU) No 10/2011 | Final article compliance for food-contact film |
Compared with an EVA-carrier masterbatch, the LLDPE carrier has lower polarity and may be less efficient at wetting high-load organic pigments or polar anti-fog additives. Conversely, it is less likely to introduce acetate odor or shift the seal-initiation temperature. Compared with a PP-carrier concentrate, the LLDPE grade processes at lower melt temperatures and is not suitable for polypropylene-host applications. These differences appear as melt-pressure stability changes, film optical ratings, and seal-performance variations when the same colorant or additive package is delivered on different carriers. The choice of carrier therefore follows the host resin, extruder residence time, final thickness, and end-use migration requirements.