| HS Code | 498484 |
| Manufacturer | LyondellBasell |
| Brand | POLYBATCH™ |
| Product Name | Canyon 10277U/4 Concentrate Based In LLDPE |
| Product Type | Color Concentrate |
| Carrier Resin | LLDPE |
| Color | Canyon |
| Physical Form | Pellets |
| Compatible Polymers | Polyethylene (PE) |
| Processing Method | Extrusion, Blow Molding, Injection Molding |
| Let Down Ratio | 4% |
| Density | 1.13 g/cm³ |
| Melt Flow Rate | 20 g/10 min |
| Moisture Content | <0.2% |
| Ash Content | 30% |
| Processing Temperature | 180-230°C |
| Shelf Life | 2 years |
| Storage Conditions | Dry, cool, ventilated area |
| Packaging | 25 kg bags |
| Application | Coloring of polyethylene articles |
| Industry | Plastics |
As an accredited LyondellBasell POLYBATCH™ Canyon 10277U/4 Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell POLYBATCH™ Canyon 10277U/4 Concentrate Based In LLDPE is supplied in 25 kg polyethylene bags, 40 bags per 1,000 kg pallet. |
| Container Loading (20′ FCL) | 20′ FCL container loading: LyondellBasell POLYBATCH™ Canyon 10277U/4 Concentrate Based in LLDPE, standard palletized bags, dry, secure, under ambient conditions. |
| Shipping | LyondellBasell POLYBATCH™ Canyon 10277U/4 Concentrate Based in LLDPE is generally a non-hazardous polymer concentrate. Ship in original sealed bags, boxes, or drums on pallets. Protect from moisture, heat, direct sunlight, and physical damage. Store cool, dry, ventilated; handle per SDS. |
| Storage | Store LyondellBasell POLYBATCH™ Canyon 10277U/4 Concentrate Based in LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original containers closed, palletized, and protected from moisture, dust, and physical damage. Use FIFO rotation, inspect for leaks, and follow local regulations. Avoid storing near food, drink, or animal feed. |
| Shelf Life | Shelf life is 12 months from date of manufacture when stored unopened in original packaging in a cool, dry place. |
On mono-layer blown-film lines running LLDPE-rich flexible packaging structures at 250–450 kg/h, LyondellBasell Polybatch Canyon 10277U/4 is introduced through a gravimetric feeder at 2–5 wt% into the main feed throat, preferably after pre-blending with natural LLDPE in a low-shear tumble mixer for 10–15 min. The LLDPE-based carrier reduces the viscosity mismatch with film-grade LLDPE having a melt mass-flow rate of 0.8–1.2 g/10 min under ISO 1133-1:2022, but a barrier screw of 24–30 L/D with a Maddock mixing section is still required to disperse pigment agglomerates before the film exits an 1.8–2.2 mm die gap. Melt temperature on the extruder is maintained at 190–210°C, while the die temperature should not exceed 215°C because the low-molecular-weight fraction of the LLDPE carrier may form volatile condensation products at extended residence time. Blow-up ratio is typically 2.0–2.5:1, with frost-line height held between 2 and 4 die diameters; a frost-line deviation greater than ±50 mm has been observed on production lines to produce visible colour-intensity bands even when the overall film gauge remains within specification. Finished food-contact film must comply with FDA 21 CFR 177.1520 for olefin polymers and EU Regulation 10/2011, including an overall migration limit of 10 mg/dm² using the appropriate food simulant; the masterbatch itself is not a direct food additive. Mechanical and optical verification of the letdown film is performed according to ASTM D1709 for dart impact, ASTM D882 for tensile properties, and ASTM D1003 for haze. In a 50 µm film, haze above 6% is usually not attributable to the pigment alone unless die-lip build-up or poor masterbatch dispersion is confirmed by microscopic examination.
Cast film conversion of a 20–30 µm LLDPE web at 80–150 m/min imposes a shorter thermal history than blown film, so 2–4 wt% 10277U/4 is metered into a reverse temperature profile ranging from 180°C at the feed throat to 230°C at the die. At screw speeds above 90 rpm, melt residence time may fall below 30 s, which is often insufficient for complete pigment wetting if the masterbatch pellet is not fully melted before the compression zone. Undispersed pigment specks are detected on the chill-roll side as light-transmitting microvoids, especially in thin-gauge cast film used for high-clarity lamination webs. The extruder is equipped with a vacuum box maintained at −0.04 to −0.06 MPa and an air-knife gap of 2–5 mm from the die exit to pin the melt curtain to a polished chill roll held at 20–28°C. Surface appearance is evaluated with ASTM D2457 20° gloss, ASTM D1003 haze, and ASTM D1922 tear; haze below 2.0% should be interpreted only after controlling die-lip oxidation deposits, because pigment oxidation products can form a low-molecular-weight wet film on the die lips. When line output exceeds 350 kg/h, a static mixer installed before the die is recommended; without it, optical density variation measured by ISO 5-3:2009 has been recorded across the web at more than ±15% in some high-output cast film campaigns.
Representative process windows for a LLDPE-based concentrate of this class are shown below; exact letdown and temperature settings must be confirmed against the product technical data sheet.
| Conversion process | Letdown range | Melt temperature | Critical control variable | Reference method |
|---|---|---|---|---|
| Blown film | 2–5 wt% | 190–210°C | Frost-line height ±50 mm | ASTM D1709 |
| Cast film | 2–4 wt% | 215–240°C | Chill-roll pinning vacuum | ASTM D1003 |
| Extrusion coating | 3–5 wt% | 260–310°C | Neck-in and back pressure | ISO 1133-1:2022 |
| Injection moulding | 2–4 wt% | 190–230°C | Cushion 3–6 mm | ASTM D1238 |
| Rotational moulding | 0.5–1.5 wt% | 260–290°C internal air | Powder mesh 35–60 | ASTM D1921 |
On tandem extrusion coating lines applying 10–25 g/m² LLDPE-based layers to paper, aluminium foil, or polyethylene terephthalate film, 10277U/4 is dosed at 3–5 wt% into the coating resin. Melt temperatures of 260–310°C are required for adequate adhesion to foil and for low neck-in; the LLDPE carrier contributes to a broader molecular weight distribution than a wax-based concentrate and may reduce edge-bead severity. If moisture content of the masterbatch exceeds 0.05 wt% after storage at relative humidity above 60%, pre-drying at 70–80°C for 2–4 h in a desiccant dryer with a dew point of −30°C or lower prevents microbubble formation in the melt curtain. The die-to-substrate gap is maintained at 100–250 mm, corresponding to an air-gap time of 30–80 ms; a change above ±10 ms alters melt oxidation and can produce colour variation along the coating edge. For food-contact laminates, the complete laminate is assessed under EU Regulation 10/2011 and FDA 21 CFR 177.1395 for foil-containing structures, with overall migration not exceeding 10 mg/dm². Adhesion of the coated sealant layer is evaluated using ASTM F88 or ASTM D1876 T-peel; a peel value below 150 N/m on aluminium foil is generally associated with insufficient melt oxidation rather than pigment concentration.
Injection moulding of unfilled LLDPE-based thin-wall containers, pails, and caps in multi-cavity tools requires a colour concentrate whose carrier does not create a visible weld-line colour shift at knit lines. 10277U/4 is fed at 2–4 wt% by a separate gravimetric or volumetric feeder mounted over the machine throat; screw speed is set at 60–100 rpm, and back pressure is held between 4–8 bar to prevent colour slugs from entering the metering zone. A general-purpose screw of 18–20 L/D produces lower dispersion than a barrier screw; therefore, colour streaks at the gate or linear marks on the sidewall are corrected first by increasing back pressure rather than raising melt temperature above 230°C. The melt cushion is kept at 3–6 mm to maintain shot-weight stability; cushion deviations greater than ±1 mm create batch-to-batch colour intensity drift, particularly in cycles below 12 s. For direct food-contact packaging, the moulded article is evaluated according to FDA 21 CFR 177.1520 and EU Regulation 10/2011, while pigment dispersion in high-purity closures may be checked by ASTM D6642 microscopy. Published data for this specific concentrate in highly pigmented closure formulations is limited; verification on the target tool is necessary because gate geometry and shear-induced pigment depletion at weld lines are tool-dependent.
In rotational moulding of cross-linked PE tanks, playground components, or industrial containers, LLDPE-based micro-pellet concentrates are not dry-blended directly into 35–60 mesh ground polyethylene powder unless the concentrate is pulverised to the same particle-size range. Processing 10277U/4 at 0.5–1.5 wt% requires cryogenic or ambient grinding of the concentrate pellets to below 500 µm, followed by low-intensity mixing for 15–20 min to avoid pigment segregation. The peak internal air temperature is typically 260–290°C for LLDPE rotational moulding grades; above 300°C, the LLDPE carrier may release low-level degradation products that reduce surface gloss and promote pinholing at mould parting lines. Heating rate between 100°C and 220°C should be controlled to 4–8°C/min, because a temperature ramp above 10°C/min can melt the carrier before the powder bed has densified, generating pigment-rich islands on the inner surface. Final part density is tested by ASTM D792, and wall-thickness distribution is verified by ultrasonic measurement because colour uniformity cannot be separated from wall-thickness uniformity in rotomoulded parts. For outdoor tanks, the converter must separately establish UV stability of the finished compound because the concentrate does not automatically provide weathering performance unless the base resin already contains the required stabiliser package.
| End-use sector | Regulation/standard | Measurement condition or limit | Test method |
|---|---|---|---|
| Food-contact PE film | FDA 21 CFR 177.1520; EU 10/2011 | Overall migration ≤10 mg/dm²; OM2 simulant | EN 1186 |
| Toys or childcare articles | EN 71-3; ASTM F963 | Soluble element limits by element | ICP-OES after acid extraction |
| Electrical/electronic housings | RoHS 2011/65/EU; REACH Annex XVII | Pb ≤1000 mg/kg; Cd ≤100 mg/kg; CrVI ≤1000 mg/kg | IEC 62321 |
| Packaging and packaging waste | EU Directive 94/62/EC | Sum of heavy metals ≤100 mg/kg | ISO 11885 |
Post-industrial LLDPE film scrap containing 20–30 wt% printed or unprinted recyclate is re-pelletised with 2–5 wt% 10277U/4 on a co-rotating twin-screw extruder with 26–40 L/D, atmospheric and vacuum degassing, and a gear pump. The screw configuration is assembled with two or three kneading blocks at 30–45° staggering angle and a dispersive mixing section near the vent; melt temperature is held between 190°C and 220°C, and vacuum is set below −0.06 MPa to remove printing-ink degradation products. A screen changer with 100/120/100 mesh screens protects the pelletiser die; a pressure increase above 8 MPa across the screen indicates pigment agglomerates or undispersed recycled gel loading and requires filtration adjustment only after melt pump stability is confirmed. The compounded pellets are tested for melt mass-flow rate by ISO 1133-1:2022, density by ASTM D792, and colour consistency by CIE L*a*b* spectrophotometry under D65/10° conditions; a colour difference above ΔE*ab 1.0 between production lots is detectable in unpigmented film, so automotive or building-panel applications require tighter lot acceptance. Restriction of hazardous substances for the recyclate-containing compound is verified by REACH Annex XVII and RoHS Directive 2011/65/EU when the final part is supplied to electrical or electronic equipment; published data for this specific concentrate in recycled electronic housing grades is limited.
Competitive LyondellBasell POLYBATCH™ Canyon 10277U/4 Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell POLYBATCH™ Canyon 10277U/4 is a pelletized masterbatch concentrate carried in linear low-density polyethylene. It is not supplied as a finished molding or extrusion compound; it is intended for melt dilution into a host polyolefin at a controlled addition level. The product code includes a formulation-specific suffix, and published data specific to the 10277U/4 composition are limited. Until a certificate of analysis is available, processing parameters can be established only from the known behaviour of LLDPE carriers and from the supplier’s recommended letdown ratio. LLDPE carrier grades commonly exhibit a melt flow rate of 8–30 g/10 min when determined by ISO 1133-1:2022 at 190 °C and 2.16 kg. The active pigment or additive loading may reduce the apparent melt flow rate below that of the neat carrier, especially in high-loading concentrates. The product is therefore best characterized as a high-solids dispersion system rather than as a simple polyethylene resin.
No public certificate of analysis for 10277U/4 is available in the task-defined information set. The following sections therefore use LLDPE carrier reference ranges and process-engineering boundaries, not product-specific values. Exact specifications for pigment or additive loading, ash content, moisture content, heavy-metal concentration, and food-contact status must be obtained from the supplier or from a lot-specific quality sheet before production release. The concentrate should be evaluated on the actual host resin and converting line because laboratory-scale data do not capture film bubble shear, die residence time distribution, or die pressure stability.
Because the carrier is LLDPE, the concentrate is positioned for polyethylene blown film, cast film, extrusion coating, pipe, and injection molding applications where melt compatibility with linear polyethylene grades is required. Gravimetric feeding is recommended over volumetric feeding for low addition levels, and feeder accuracy should be within ±0.2 wt% of setpoint for a letdown ratio below 5 wt%. Calibration against belt or weigh-belt data should be repeated whenever a new lot is introduced, because pellet bulk density and pellet geometry can shift with particle size changes. Bulk density for LLDPE-based concentrates typically falls in the range of 500–650 kg/m³ when measured by ISO 60; the exact value should be confirmed for silo or hopper design.
The selection of LLDPE as the carrier resin changes both thermal response and melt compatibility in polyolefin conversion. Linear low-density polyethylene grades used in masterbatch carriers typically show a density range of 0.915–0.925 g/cm³ by ASTM D1505, compared with 0.917–0.930 g/cm³ for many LDPE carriers. The thermal peak for LLDPE carriers is commonly observed between 119 °C and 124 °C by differential scanning calorimetry following ASTM D3418, which is close to LDPE but sufficiently different in crystallization kinetics to affect bubble stability in blown film. In contrast, EVA-based concentrates are used when polarity, adhesion, or lower melt viscosity is needed, while PP carriers require processing above the polypropylene melting range of approximately 160–165 °C and are unsuited to polyethylene film lines operating below 230 °C. The LLDPE carrier therefore offers a narrower compatibility window within polyethylene applications, but provides improved drawdown and a stronger dilution match with modern hexene- and octene-based film resins. Differences from other POLYBATCH products should be assessed primarily by carrier resin identity, additive loading, and the target letdown ratio, because each code within the same product family may contain a different pigment or processing package.
| Property | Test method | LLDPE carrier reference range | Comparative note |
|---|---|---|---|
| Melt flow rate | ISO 1133-1:2022 | 8–30 g/10 min at 190 °C/2.16 kg | LDPE carriers may be higher; PP carriers require 230 °C |
| Density | ASTM D1505 | 0.915–0.925 g/cm³ | LDPE carriers often fall between 0.917 g/cm³ and 0.930 g/cm³ |
| Melting peak | ASTM D3418 | 119–124 °C | EVA carriers broaden below 100 °C; PP carriers melt near 160–165 °C |
| Carrier polarity | Not applicable | Nonpolar | EVA carriers are polar and can improve adhesion to polar substrates |
| Melt processing window | Extrusion trial | 190–230 °C | PP carriers typically require 220–250 °C |
The final melt flow rate after letdown can be estimated from the logarithmic mixing rule for melt flow index, but this rule often fails when the concentrate contains structured pigments or mineral fillers. A more reliable procedure is to prepare capillary rheometry samples from dry blends at the intended letdown ratio and measure viscosity at 100 s⁻¹ and 210 °C by ISO 11443:2021. If the final viscosity deviates from the host resin by more than 15–20%, the screw speed, temperature profile, or letdown ratio should be adjusted before the concentrate is released to production.
On a production-scale blown film line, the concentrate is introduced at the feed throat as a dry blend with the host polyethylene. A starting letdown ratio of 2–5 wt% is typical for high-loading concentrates, but the exact ratio must be derived from the 10277U/4 formulation and the downstream specification. Melt temperature should not exceed 230 °C for LLDPE-rich systems unless the line is designed for high-temperature operation; sustained temperatures above 240 °C can decompose additives, generate crosslinked gel particles, or shift colour strength. A barrier screw with 25:1 to 30:1 L/D and a mixing section is normally the minimum mechanical prerequisite. A simple three-zone screw will not distribute a high-hardness concentrate into a low-viscosity host melt. If the host resin is a fractional-melt LLDPE with apparent melt viscosity above 1,200 Pa·s at 100 s⁻¹, a two-stage screw or static mixer before the die may be required.
Dispersion of pigment agglomerates and additive particles in the LLDPE carrier is governed by shear stress, not by melt temperature alone. For film-grade masterbatches, undispersed particles larger than 25 µm can appear as specks or gel-like defects. A screen pack combination of 100–250 µm mesh or equivalent depth filtration media is often used to capture residual agglomerates that survive screw shear. On a 75 mm single-screw extruder running 150–250 kg/h, a pressure rise from clean-screen baseline to +20–40 bar over 4–8 h is normal for a well-dispersed concentrate; a faster pressure climb indicates hard agglomerates, incompatibility, or excessive concentrate addition. Because LLDPE is more shear-sensitive than LDPE, barrel temperatures in the compression zone should be monitored closely. Local overheating above 210 °C before the mixing section may create low-viscosity streaks and reduce the stress transfer needed to break agglomerates.
In blown film applications, dispersion should also be assessed optically. A film sample of 50 µm thickness can be scanned with a camera-based gel counter. Acceptance criteria for high-clarity film may be set at fewer than 10 visible particles per 100 cm², but the threshold is application-specific. Haze and clarity are measured by ASTM D1003, and colour coordinates can be determined by spectrophotometry following ISO 7724 or an equivalent method. Mechanical film properties should be verified before continuous use, particularly Elmendorf tear by ASTM D1922, dart impact by ASTM D1709, and puncture resistance by ASTM D5748. These tests are necessary because the carrier contributes to the amorphous and crystalline structure of the final film, and even a small carrier mismatch can alter tear propagation.
At letdown ratios above 5 wt%, the contribution of the LLDPE carrier to final melt rheology is no longer negligible. The carrier’s molecular architecture, comonomer type, and stabilizer package may reduce equilibrium melt strength or alter the bubble expansion ratio. On high-stalk blown film lines, die pressure and frost line height can shift because the average melt elasticity changes; bubble instability and gauge variation may appear even when the letdown ratio is still within the supplier’s maximum recommendation. If the host resin is an autoclave LDPE with long-chain branching, diluting it with 5–10 wt% of an LLDPE-carrier concentrate can reduce the strain-hardening behaviour measured by extensional rheometry. The practical response is to reduce concentrate addition to the minimum level that achieves the required colour or additive loading, and to raise the die temperature by 5–10 °C only if gauge variation remains outside ±5% of nominal thickness. In applications where the host resin is already a highly linear metallocene LLDPE, this carrier is less likely to alter bubble stability but may still affect blocking and coefficient of friction through its additive surface.
Blown film, cast film, and extrusion coating operations can use this concentrate when the target additive is acceptable in the final article and when the LLDPE carrier does not create a density or melting mismatch. For injection molding, the concentrate may be used in polyethylene grades processed below 230 °C, but high-shear injection screws with check valves are recommended to avoid carrier-rich material accumulating in the metering zone. The product is not automatically suitable for polypropylene, polyamide, or polycarbonate compounds; those hosts require polar or higher-temperature carriers such as PP, EVA, or polyolefin elastomers. If food-contact status is required, confirmation from the supplier against 21 CFR 177.1520 for the carrier and the relevant colorant or additive regulation is mandatory, because the LLDPE designation alone does not establish compliance.
Polyethylene compounds containing a masterbatch are at risk of thermal stabilizer depletion because the carrier has already experienced one compounding heat history. Regrind of film produced with 10277U/4 should be reintroduced at no more than 20 wt% of the total feed unless a production trial demonstrates that yellowness index, melt viscosity, and film appearance remain stable. Yellowness index can be tracked by ASTM E313, and melt flow rate by ISO 1133-1:2022. Additive migration from the concentrate to film surfaces can influence blocking, coefficient of friction, and print adhesion; the coefficient of friction should be tested by ISO 8295:1995. In ethylene-vinyl acetate or low-melt-temperature hosts, migration tendency may increase and reduce seal initiation temperature. Seal strength should be evaluated by ASTM F88/F88M if the film enters a flexible packaging line.
Product changeovers from coloured concentrates to natural resin require a purging protocol. LLDPE-based masterbatches can leave residual colour in screw flights, screen changers, and die lips, especially when the concentrate contains hard pigments. Purging should be performed with a commercial polyethylene-based purging compound or natural LLDPE with a melt flow rate below 1 g/10 min. The purge resin should be run at 200–220 °C until the extrudate is visually clear. For critical colour changes, dismantling of the screen pack and die assembly may be required because surface-bound pigment on the die lip cannot be removed by melt flow alone.
Storage conditions for LLDPE-based concentrates do not require intimate handling, but thermal and moisture limits remain relevant. Bags should be kept sealed below 40 °C and away from direct sunlight to limit thermal aging of the carrier stabilizer system. If storage occurs in an unheated warehouse where condensation risk exceeds 60% relative humidity, a pre-drying step at 60–70 °C for 2–4 h is prudent for film lines with vacuum venting or tight moisture limits. The necessity should be determined by moisture measurement rather than by fixed schedule, because overdrying can introduce handling static and dusting. Residual moisture levels below 0.05 wt% are generally acceptable for polyolefin extrusion, and the measurement can be performed by ISO 15512:2019.