Lyondellbasell Polybatch Blue Ll40445 2 Concentrate Based In Lldpe

LyondellBasell POLYBATCH™ Blue LL40445/2 Concentrate Based In LLDPE

    • Product Name: LyondellBasell POLYBATCH™ Blue LL40445/2 Concentrate Based In LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 261497
    Manufacturer LyondellBasell
    Brand POLYBATCH™
    Product Name Blue LL40445/2 Concentrate Based In LLDPE
    Product Type Color concentrate/masterbatch
    Color Blue
    Carrier Resin Linear Low Density Polyethylene (LLDPE)
    Physical Form Pellets
    Compatibility Polyethylene resins
    Typical Let Down Ratio 2% to 5%
    Processing Methods Extrusion, injection molding, blow molding, film
    Typical Applications Packaging, films, molded articles
    Heat Stability Suitable for typical polyethylene processing temperatures
    Light Fastness Good
    Moisture Content Low
    Storage Conditions Dry, cool, well-ventilated area
    Shelf Life Typically 12 to 24 months
    Packaging Bags or boxes

    As an accredited LyondellBasell POLYBATCH™ Blue LL40445/2 Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg polyethylene bags, palletized at 1,000 kg per pallet, designed for safe industrial storage and handling.
    Container Loading (20′ FCL) 20′ FCL container loaded with LyondellBasell POLYBATCH™ Blue LL40445/2 LLDPE-based color concentrate, palletized and secured for export shipment.
    Shipping LyondellBasell POLYBATCH™ Blue LL40445/2 Concentrate Based in LLDPE typically ships as solid pellets in sealed moisture-barrier bags or cartons. It is not classified as dangerous goods for DOT, IMDG, or IATA. Transport at ambient temperature, protected from moisture, contamination, heat, and direct sunlight.
    Storage Store POLYBATCH™ Blue LL40445/2 Concentrate in a cool, dry, well-ventilated area, away from direct sunlight, heat, and ignition sources. Keep original containers tightly closed to prevent moisture and contamination. Avoid prolonged UV exposure and excessive stacking. Maintain temperatures between 5–35°C (41–95°F). Protect from strong oxidizers and follow local regulations and SDS recommendations. Inspect containers regularly.
    Shelf Life Two years from date of manufacture when stored unopened in original packaging, in a cool, dry area away from direct sunlight.
    Application of LyondellBasell POLYBATCH™ Blue LL40445/2 Concentrate Based In LLDPE

    In blown film extrusion of monolayer polyethylene packaging, LyondellBasell POLYBATCH™ Blue LL40445/2 Concentrate Based In LLDPE is metered into the extruder throat through a low-rate gravimetric feeder at 2.0 wt% to 4.0 wt% of the total compound for films between 40 μm and 80 μm. The LLDPE carrier is melt-compatible with LLDPE and LDPE film grades, and no pre-drying is required when bags are stored below 60% RH; if condensation is observed on pellets, a hopper dryer at 60 °C for 2 h is recommended before the material enters the feed section. On a standard 45 mm single-screw blown film extruder with an L/D ratio of 30:1 and a barrier screw, the melt temperature is maintained between 190 °C and 220 °C, the die gap is set at 1.8 mm to 2.4 mm, and the blow-up ratio is held between 2.0:1 and 2.8:1. Frost line height is adjusted from 300 mm to 600 mm to stabilise bubble geometry because the LLDPE carrier lowers melt tension relative to pure HDPE but remains shear-thinning at typical film extrusion shear rates. For food-contact packaging, the finished film must meet the overall migration limit of 10 mg/dm² under Regulation (EU) No 10/2011 and the olefin polymer requirements of FDA 21 CFR §177.1520; for packaging waste heavy metal limits, the sum of lead, cadmium, mercury and hexavalent chromium must not exceed 100 mg/kg under EU Directive 94/62/EC Annex II. Finished article types produced from this formulation include frozen food bags, agricultural silage covers, retail carrier bags and industrial liners.

    What Limits Colourant Dispersal at High Throughput in Cast Film Lines?

    High-speed cast film lines operating above 300 m/min introduce a dispersion constraint that is absent from lower-throughput film blowing. The concentrate is melt-diluted at 3.0 wt% to 5.0 wt% in LLDPE/LDPE cast film grades of 20 μm to 35 μm thickness; below 3.0 wt% the blue tint becomes visually weak under the high longitudinal draw ratio, and above 5.0 wt% undispersed pigment agglomerates extracted at the screen pack increase die lip build-up frequency. A cast film line configured with a 75 mm barrier screw, L/D ratio of 30:1, barrel temperatures from 200 °C to 240 °C and a screen pack progression of 40/60/100 mesh is typical. The melt passes through a flat die with a die gap of 0.5 mm to 0.8 mm and is deposited onto a chill roll held at 18 °C to 25 °C; the air gap between die lip and chill roll is kept below 25 mm to control neck-in and edge bead stability. Production failure modes observed on cast lines include streaking traceable to pigment agglomerates in the primary filter, edge tear caused by pigment-related gel particles, and colour variance when screw speed is changed without resetting the feeder calibration. Colourimetric evaluation after stabilisation should follow ASTM D2244-21. Regulatory compliance for food contact cast film relies on Regulation (EU) No 10/2011 and FDA 21 CFR §177.1520; heavy metal limits follow EU Directive 94/62/EC Annex II at 100 mg/kg sum. Finished articles include blue-tinted identification pallet wrap, garment packaging film and lamination substrates for printed flexible packaging.

    When thin-wall polyethylene containers are coloured with the LLDPE-based blue masterbatch at a letdown ratio of 1:50 to 1:100, the gate region displays the most sensitive colour-defect behaviour. Addition levels of 1.0 wt% to 2.0 wt% are used for wall sections between 0.8 mm and 1.8 mm; the lower range is reserved for translucent housewares, while the upper range is needed for opaque caps and closures. An injection moulding machine with a 25 mm to 35 mm screw diameter, L/D ratio of 20:1 and a shut-off nozzle is set to a melt temperature of 200 °C to 230 °C, hydraulic back pressure of 6 bar to 12 bar, and injection velocity of 80 mm/s to 160 mm/s; screw recovery is held between 60 rpm and 120 rpm. In PE-based articles, the LLDPE carrier delays gate freeze, and cooling time may require an additional 0.5 s to 1.5 s to prevent gate strings and part deformation during ejection. If the concentrate is used in polypropylene at levels above 1.5 wt%, the LLDPE carrier forms a dispersed minor phase that can reduce weld-line tensile strength and flexural modulus; weld-line tensile properties should be checked using ASTM D638-14 before approving polypropylene thin-wall production. Compliance under the Toy Safety Directive 2009/48/EC requires migration testing according to EN 71-3:2019+A1:2021 for articles that may be placed in the mouth or used by children under 36 months; food-contact containers are verified under Regulation (EU) No 10/2011 and FDA 21 CFR §177.1520. Finished part types include thin-wall PE food storage containers, industrial crates, caps and closures for HDPE bottles and rigid housewares.

    When Blue LLDPE Concentrate Enters HDPE Extrusion Blow Moulding

    Parison formation in HDPE extrusion blow moulding is governed by elongational viscosity and sag resistance, and the lower-viscosity LLDPE carrier modifies this balance when added at 2.0 wt% to 3.5 wt%. In a shuttle or accumulator-head machine running a 70 mm extruder with an L/D ratio of 24:1, the parison die gap is set between 0.8 mm and 1.6 mm for containers with 0.6 mm to 1.2 mm wall thickness, and the melt temperature is maintained between 190 °C and 220 °C. The LLDPE carrier lowers melt strength above 215 °C; when accumulator head tooling runs beyond this point, top-to-bottom wall distribution shifts unless accumulator shot speed is retarded by 5% to 10%. Blow air pressure is set at 6 bar to 8 bar, and mould temperature is held at 10 °C to 20 °C for surface gloss and label adhesion. Addition ratios below 2.0 wt% cause poor colour saturation in neck pinch-off zones, while ratios above 3.5 wt% increase the risk of pigment accumulation at the parison core and create visible flow lines around the handle pinch-off. Regulatory evaluation for non-food household chemical containers falls under REACH and EU Directive 94/62/EC Annex II with a heavy metal sum limit of 100 mg/kg; if the container is intended for food contact, the finished blow-moulded part must meet Regulation (EU) No 10/2011 overall migration of 10 mg/dm² and FDA 21 CFR §177.1520. Finished article types include detergent bottles, hand soap bottles, automotive lubricant containers and industrial auxiliary chemical containers.

    Pipe Extrusion Colouristic Stability Under Prolonged Screw Residence

    Extended residence time of blue pigment dispersed in LLDPE carrier within a pipe extruder barrel creates a specific failure mode: speck formation from degraded pigment agglomerates at the inside wall of the screen pack and at the breaker plate. The masterbatch is added at 4.0 wt% to 6.0 wt% to natural HDPE or MDPE pipe compound in single-screw extruders with a grooved feed section and an L/D ratio of 30:1. Melt temperatures are controlled between 190 °C and 220 °C; barrel zones above 230 °C shift the blue shade and generate visible specks after 15 min of residence time, particularly when the extruder is idled during downstream sizing changes. Screen packs are positioned after the breaker plate with 60/100 mesh layers, and vacuum calibration sleeves are set to 0.95 bar to 0.98 bar with haul-off speed matched to extruder output. For pressure pipe grades, the coloured compound must be revalidated for long-term hydrostatic strength according to ISO 9080:2022 and the applicable pipe dimensions standard such as EN 12201-1 or ISO 4427-1; drinking water contact requires national approval such as NSF/ANSI/CAN 61. Colourimetric consistency is checked using ASTM D2244-21. Finished articles include PE80 and PE100 potable water service pipes, electrical conduit and telecommunications duct.

    Dispersion in Roto-Moulded Polyethylene Depends on Grind Size and Oven Peak Internal Air Temperature

    In rotational moulding, colour development is not achieved through shear but through thermal sintering and interstitial melt flow, so the masterbatch should be reduced to micropellets of 0.35 mm to 0.50 mm or cryogenically ground before dry blending with pulverized LLDPE of 35 mesh. Addition ratio is 1.0 wt% to 2.0 wt%; below 1.0 wt% produces mottled inner surfaces on large flat sidewalls, and above 2.0 wt% lowers impact strength because the concentrate carrier shifts the sintering rate of the base powder. Mould rotation ratios of 4:1 primary to secondary axis are used, and oven temperature is set at 260 °C to 320 °C while peak internal air temperature is held at 180 °C to 200 °C. Exceeding a peak internal air temperature of 210 °C promotes oxidative colour shift and pinholes near vents; operators monitor internal air temperature with a remote infrared sensor and stop oven dwell when the flattening time reaches 2 min to 4 min. Compliance for toys is evaluated under EN 71-3:2019+A1:2021 migration limits, and potable water tanks require NSF/ANSI/CAN 61 or equivalent national approval on the finished article. Published data for this exact concentrate grade in rotational moulding is limited; converter-run gel count, impact strength and colourimetry trials on production-scale tools are therefore required before full lot adoption. Finished article types include water storage tanks, agricultural hoppers, playground components, kayaks and insulated cool boxes.

    Free Quote

    Competitive LyondellBasell POLYBATCH™ Blue LL40445/2 Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell POLYBATCH™ Blue LL40445/2 Concentrate Based In LLDPE is a pelletized blue colour concentrate supplied with a linear low-density polyethylene carrier resin. The LL40445/2 designation is an internal shade code that identifies the blue hue and the production formulation; complete compositional data, including pigment chemistry, extender loading, and carrier melt-mass-flow rate, is disclosed through the supplier certificate of analysis rather than through generic trade literature. The product is intended for melt incorporation into polyethylene-based resins in blown film, cast film, sheet, blow moulding, and injection moulding. It differs from a fully pre-compounded blue resin by allowing the converter to maintain a single natural resin inventory and adjust the let-down ratio for the target shade. The carrier selection has direct processing consequences: an LLDPE carrier generally exhibits a shear-thinning viscosity and melt tension closer to that of linear film resins, reducing the risk of bubble instability in high-stalk blown-film processes compared with a wax-based or low-density carrier. The converter must still establish the addition level for each production line because colour development, pressure stability, and mechanical property retention are influenced by screw geometry, melt temperature, downstream filtration, and the presence of reclaimed material.

    Feed metering is the primary operational variable. On production-scale lines using a 45 mm grooved-feed single-screw extruder with L/D 28:1 and a 60/80/20 screen pack, a volumetric disc feeder calibrated against the bulk density of the specific pellet lot is sufficient for addition levels above 2 wt%. At lower addition levels, a gravimetric feeder with a minimum effective resolution of 0.01% of process mass flow is preferred because pellet bulk density typically falls between 0.55 g/cm³ and 0.75 g/cm³, and small shifts in fill factor produce visible colour drift. Static charge accumulation on LLDPE pellets in low-humidity conveying air can cause pellet adhesion to hopper walls; grounding and ionised air are used to reduce feed interruptions. The concentrate should not be pre-blended with the base resin for more than 8 hours in an open hopper if the plant relative humidity exceeds 60%, because surface condensation can promote agglomeration and irregular throat feeding.

    What Distinguishes an LLDPE-Carrier Blue Concentrate from LDPE-Based or Universal Masterbatch Systems?

    The LLDPE carrier class used in polyolefin masterbatches is defined by density values in the range of 0.918 g/cm³ to 0.935 g/cm³ per ISO 1183-1:2019 and melt mass-flow rates commonly between 1 g/10 min and 25 g/10 min at 190°C under 2.16 kg per ISO 1133-1:2022. These ranges describe the carrier class; lot-specific values for LL40445/2 must be read from the certificate of analysis. Low-density polyethylene carriers, by contrast, are produced in a high-pressure radical process that creates long-chain branching and yields a different elongational viscosity signature. In blown-film trials, that difference is observed as a narrower stable bubble window at high blow-up ratios for some LDPE carriers, whereas the LLDPE carrier tends to preserve bubble stability and film gauge uniformity. The comparison is material-class-based and should be confirmed with a direct bubble-stability trial on the target die and air ring.

    Universal masterbatches often employ ethylene-vinyl acetate or wax-based carriers. Those carriers can reduce melt temperature and improve pigment wetting, but they introduce a second polymer phase into a polyethylene film. In thin-gauge applications, EVA or wax domains may lower Elmendorf tear resistance measured by ASTM D1922-23 and reduce heat-seal strength measured by ASTM F88/F88M-21. For high-density or linear polyethylene film where seal integrity and mechanical toughness are critical, an LLDPE carrier is typically preferred because the carrier remains within the polyethylene family and minimizes the introduction of a low-melting extractable phase. Published lot-specific rheological and colourimetric data for this particular masterbatch configuration is limited outside the supplier’s technical documentation; converter-side trials are therefore necessary for critical product qualification.

    In a 35 µm blown-film campaign using a 55 mm extruder with L/D 30:1, a 1.5 mm die gap, and a blow-up ratio of 2.5:1, the concentrate is generally dry-blended with natural resin at the feed hopper. If the screw includes a Maddock or spiral mixing element, distributive mixing at let-down ratios below 1 wt% may be sufficient for tint shades. Above 4 wt%, pigment-induced viscosity changes can raise melt pressure by 5 bar to 10 bar at constant screw speed. The rise is line-specific and depends on the particle size and oil absorption of the blue pigment. A 40/80/20 screen pack is used as a dispersion indicator: if the pressure drop across the screen pack increases by more than 2 bar/h during a 4 h run, the dispersion is insufficient and either the let-down ratio, melt temperature, or screen configuration must be adjusted. At die temperatures above 250°C, some organic blue pigments can undergo thermal degradation, causing a shift in hue and a loss of colour strength; the converter must verify the pigment’s thermal stability before processing at elevated temperature.

    Film optical performance is evaluated after conditioning the extruded film for 48 h at 23°C and 50% relative humidity. Tensile properties are measured by ISO 527-3:2018 or ASTM D882-18, Elmendorf tear by ASTM D1922-23, dart impact by ISO 7765-2:2021, and haze by ISO 14782:2021. The addition of blue concentrate can influence the crystalline orientation and surface roughness of the film; comparative data must be generated against an uncoloured control on the same line, because gauge variation and frost-line height change the mechanical measurements independently of pigment loading.

    Dispersion Metrics and Colourimetric Compliance for Thin-Gauge Polyethylene

    Shade control for LL40445/2 is performed spectrophotometrically. The masterbatch is let down into a defined natural resin and moulded into a plaque or blown into film, then measured with a d/8° spectrophotometer in reflectance mode. CIELAB values are calculated under D65 illumination and 10° observer geometry using ISO 11664-4:2008 or ASTM D2244-23. A lot-to-lot colour difference of ΔE*ab ≤ 1.0 is often used as an in-process target for polyolefin masterbatch, but the contractual limit for LL40445/2 must be taken from the supplier specification. Dispersion quality is evaluated by a filter-pressure-value test according to EN 13900-5:2005; a high filter-pressure value indicates pigment agglomerates that may produce visible specks in thin film.

    Analytical methods applicable to LLDPE-based blue concentrate control
    ParameterTest MethodPurpose
    Melt mass-flow rateISO 1133-1:2022 or ASTM D1238-20Carrier classification at 190°C, 2.16 kg; lot-specific value on certificate of analysis
    DensityISO 1183-1:2019 or ASTM D792-20Carrier identity and inorganic filler inference
    Ash contentISO 3451-1:2019Inorganic residue where titanium dioxide or mineral extenders are present
    Colour differenceISO 11664-4:2008 or ASTM D2244-23Lot-to-lot shade control under D65/10°
    DispersionEN 13900-5:2005Filter-pressure value for pigment agglomeration
    Heavy metalsEU Directive 94/62/EC and REACH Annex XVIIPackaging compliance; end-use dependent

    In thin-gauge polyethylene film below 25 µm, dispersion quality dominates visual and mechanical outcome. Pigment agglomerates above 10 µm can initiate pinhole formation during stretching and reduce puncture resistance measured by ASTM D5748-23. The concentrate should therefore be evaluated in a pilot film trial using the intended screen pack and die gap. Published dispersion data for LL40445/2 is limited outside the supplier’s technical documentation; the converter’s retained film sample is the primary evidence of acceptable dispersion. If visible blue specks appear at a let-down ratio of 3 wt%, reducing the addition level without changing the screen pack is not a substitute for dispersion improvement; the root cause is usually insufficient shear or a screen mesh too coarse for the pigment particle-size distribution.

    When LL40445/2 Replaces Fully Pre-Compounded Blue Resin in Injection Moulding

    In injection moulding, the concentrate is used to convert a natural polyethylene base resin into a blue finished part at the press. The moulder assumes responsibility for metering and melt homogenisation. On a 1500 kN clamp injection moulding machine with a 35 mm diameter general-purpose screw at a compression ratio of 2.5:1, uniform colour requires a screw mixing section or a static mixer in the nozzle. If the screw is a simple three-zone design, blue streaks and swirl can appear in thin-walled parts at fill speeds above 100 mm/s. Increasing backpressure to 10 bar to 20 bar improves dispersion but may increase residence time and thermal history. Melt temperature is set according to the base resin; for high-viscosity HDPE, values between 230°C and 245°C are common, while high-flow LLDPE with melt mass-flow rate above 25 g/10 min may be run at 210°C if the gate and runner system permit.

    Compared with purchasing a fully pre-compounded blue resin, the masterbatch route reduces minimum order quantities, shortens shade-change cleanup, and permits one natural resin to serve multiple colours. The limitation is process control: if the feeder drifts by ±0.5 wt% at a target let-down ratio of 3 wt%, the colorimetric shift may exceed a ΔE*ab of 1.5, which is not acceptable for critical packaging colour management. The concentrate is not recommended for use in polypropylene without compatibility testing because LLDPE carrier domains can remain as inclusions and reduce notched impact strength measured by ISO 179-1/1eA or increase haze measured by ASTM D1003-21. For polypropylene applications, a polypropylene-carrier concentrate should be selected.

    Comparative processing expectations for masterbatch carrier systems in polyethylene film
    Carrier systemTypical density rangeTypical melt-flow rangeProcessing implication
    LLDPE carrier0.918–0.935 g/cm³ per ISO 1183-1:20191–25 g/10 min per ISO 1133-1:2022Good retained film mechanicals; higher melt tension; suitable for LLDPE/HDPE film
    LDPE carrier0.917–0.930 g/cm³ per ISO 1183-1:20190.2–70 g/10 min per ISO 1133-1:2022Easier dispersion at lower melt temperature; possible bubble instability in high-stalk film
    Universal EVA or wax carrierNot applicable to pure PEVariableImproved wetting but introduces low-melting phase; may reduce seal strength and tear resistance

    Compliance statements for LL40445/2 must be obtained from LyondellBasell for the specific production site and end market. Generic polyolefin colour concentrates are tested for heavy-metal restrictions under EU Directive 94/62/EC for packaging and may be evaluated under REACH Regulation (EC) No 1907/2006 and RoHS Directive 2011/65/EU. Food-contact status is not automatic from the use of an LLDPE carrier; the complete masterbatch formulation plus the base resin and processing conditions must be assessed under FDA 21 CFR or Commission Regulation (EU) No 10/2011, including migration testing where specified. The converter should not claim food-contact approval for a finished article solely on the basis of the carrier resin being polyethylene.

    The product is not intended for use with moisture-sensitive resins unless the base resin is dried and the hopper is sealed. Avoid pre-drying at temperatures above 80°C unless the carrier’s softening point and pigment thermal stability are confirmed. Extended hold-up times above 240°C in the presence of oxygen can cause oxidative chain scission of the LLDPE carrier, reducing melt viscosity and producing odour. The concentrate should not be combined with amine-based processing aids or additives unless compatibility with the pigment surface treatment is confirmed, because acid-base interactions can destabilize dispersion and shift hue. Store in sealed, dry packaging away from direct sunlight; for LLDPE-based masterbatches, 12 months from the production date is a common storage interval, but the actual shelf life is lot-specific and must be verified with the supplier.

    Top