| HS Code | 200070 |
| Productname | LyondellBasell POLYBATCH™ Blue LL40348/4 Concentrate Based In LLDPE |
| Producttype | Blue color concentrate |
| Color | Blue |
| Carrierresin | LLDPE (Linear Low Density Polyethylene) |
| Physicalform | Pellets |
| Density | Approximately 1.10 g/cm³ |
| Meltflowrate | Approximately 20 g/10 min at 190°C/2.16 kg |
| Moisturecontent | ≤0.2% |
| Recommendedletdownratio | 4% |
| Processingtemperature | 180–230°C |
| Shelflife | 24 months |
| Storageconditions | Dry, below 30°C |
| Packaging | 25 kg bags |
| Compatibility | Polyolefins |
As an accredited LyondellBasell POLYBATCH™ Blue LL40348/4 Concentrate Based In LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell POLYBATCH™ Blue LL40348/4 Concentrate is packaged in 25 kg (55 lb) polyethylene-lined bags on pallets, shrink-wrapped. |
| Container Loading (20′ FCL) | 20′ FCL container loading of LyondellBasell POLYBATCH™ Blue LL40348/4, an LLDPE-based concentrate, palletized and secured for safe ocean transport. |
| Shipping | LyondellBasell POLYBATCH™ Blue LL40348/4 Concentrate Based in LLDPE is normally shipped as non-hazardous plastic pellets in 25 kg bags or octabins, palletized and stretch-wrapped. No UN number, hazard class, or placards required. Store cool and dry, away from moisture, heat, and direct sunlight. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed when not in use to prevent moisture and contamination. Do not stack excessively. Use first-in, first-out rotation. Avoid prolonged storage above recommended temperatures. Store in original packaging, protected from physical damage. Keep away from incompatible materials and ensure spill containment. |
| Shelf Life | Shelf life is approximately two years when stored unopened in original packaging under cool, dry conditions away from direct sunlight. |
In blown-film extrusion of industrial refuse sacks and heavy-duty can liners on 70 mm grooved-barrel single-screw extruders with 30:1 L/D screws, 250–400 mm spiral-mandrel dies, and die gaps between 1.6 mm and 2.0 mm, POLYBATCH™ Blue LL40348/4 Concentrate Based In LLDPE is dry-blended with neat LLDPE or an LLDPE/LDPE mixture and fed through gravimetric dosing hoppers at 2.0–4.0 wt%, with the 4.0 wt% figure read from the product suffix /4 as a standard let-down reference rather than a fixed value; melt temperatures of 195–220°C, blow-up ratios of 2.2:1 to 3.0:1, and frost-line heights of 600–900 mm are maintained because the LLDPE carrier can reduce bubble stability when the concentrate is dosed above 4.0 wt% in film gauges below 50 µm. The relevant compliance baseline for non-food sacks is EU Directive 94/62/EC on packaging and packaging waste and, from 12 August 2026, Regulation (EU) 2025/40, with CONEG Model Toxics in Packaging limits for the sum of lead, cadmium, mercury and hexavalent chromium at 100 ppm; if a can liner is intended for short-term contact with dry food, the final film must be verified under Regulation (EU) 10/2011 Annex I with an overall migration limit of 10 mg/dm², and the olefin polymer must satisfy FDA 21 CFR §177.1520(c). Downstream converting includes inline perforation, gusseting, and heat-sealed side welds on bag-making machines, with seal settings of 130–150°C and 0.5–1.0 s dwell. Terminal finished products are heavy-duty refuse sacks in 40–80 µm thickness, contractor cleanup bags, can liners for food-service and institutional waste, and coloured recycling collection bags.
The same concentrate, let down at lower loadings of 2.0–3.0 wt% for 25 µm silage stretch film and 2.5–3.5 wt% for 150–200 µm greenhouse cover film, is processed on three-layer blown-film coextrusion lines with 1.8–2.2 mm die gaps, product blow-up ratios of 3.0:1, and frost-line heights between 700 mm and 950 mm; the masterbatch is preferably metered into the middle or outer layer using layer ratios of 20/60/20 or 15/70/15 to preserve total film dart impact and interlayer adhesion while maintaining visual tint. Compliance for bale-wrap films is assessed under EN 13206:2017 for thermoplastic stretch films used for wrapping bales, including tensile strain retention and dart impact; where silage covers and greenhouse films are placed in contact with animal feed or food-producing crops, the finished film is evaluated against Regulation (EU) 10/2011 and relevant national feed-chain requirements. Colour strength is controlled by CIE L*a*b* measurement under D65/10° according to ISO 11664-4, with a batch-to-batch ΔE of 0.8 or less across the roll width at 3.0 wt% dose; full-width scanning on the bubble is required because blue pigmentation can obscure visual gel detection. Terminal products include silage bale wrap, silage pit covers, low-tunnel greenhouse films, and light-diffusing agricultural covers.
If the concentrate is metered into thin-wall polyolefin closure compounds at let-down ratios above 3.5–4.0 wt%, stock temperature uniformity and pigment dispersion at weld lines become critical; high-speed injection moulding machines with 150–250 t clamping force, 0.8–1.2 mm nominal wall thickness, melt temperatures of 220–240°C, injection velocities of 40–90 mm/s, and hydraulic back pressures of 60–100 bar are used, with a screw L/D of 20:1 to 24:1 and a sliding-ring non-return valve clearance maintained below 0.05 mm to avoid blue streaks. The compliance framework for food-contact closures includes FDA 21 CFR §177.1520(c) for the polyolefin base polymer, FDA 21 CFR §178.3297 for colourants used in polymers, and Regulation (EU) 10/2011 Annex I for overall migration; for non-food detergent or lubricant closures, EU Directive 94/62/EC or its successor Regulation (EU) 2025/40 and CONEG heavy-metal limits at 100 ppm operate as the minimum regulatory baseline. Process limits arise from the LLDPE carrier, which can alter the heat distortion performance of the final HDPE or polypropylene compound when over-dosed; validation under ISO 75-2 is therefore required, and screw recovery time below 1.5 s has been associated with unmelted masterbatch particles and flow-line marking on the closure outer surface. Terminal products include tamper-evident closures for non-carbonated beverages, dispensing caps, sport caps, flip-top closures, and thin-wall containers for cosmetics and household chemicals.
Because parison melt strength and colour dispersion are both sensitive to die-head temperature, extrusion blow-moulding of HDPE/LLDPE bottles using POLYBATCH Blue LL40348/4 is run on shuttle or continuous wheel machines with 50–90 mm extruders at 24:1 L/D, die-head temperatures of 190–210°C, and parison drop times of 1.2–2.0 s; the masterbatch is pre-mixed with HDPE pellets and metered at 2.5–4.5 wt%, with the upper boundary set by visual flow lines in the bottle wall rather than by pigment dispersion failure. Compliance for household chemical and agrochemical packaging starts with REACH Regulation (EC) No 1907/2006 for the polymer and colourant substances and CLP Regulation (EC) No 1272/2008 for classification, while packaging placed on the EU market must meet Directive 94/62/EC or Regulation (EU) 2025/40; if the bottle is used as dangerous-goods packaging, the design and construction are tested under UN Model Regulations Chapter 6.1 for drop, leakproofness and stacking, independent of colour masterbatch. In production, die-head pressure fluctuations below ±0.3 MPa across a 4-hour run indicate stable masterbatch feed; larger fluctuations have been linked to bridging in the hopper when dosing above 4.5 wt% in humid environments above 60% RH, and pre-drying at 70°C for 2 h may be required. Terminal finished products are detergent bottles, agrochemical containers, automotive washer-fluid bottles, and light-industrial chemical packs in 0.7–1.5 mm wall thickness.
Extrusion coating lines running at 200–350 m/min impose a much shorter thermal history and a thinner final colour layer than blown-film extrusion, so POLYBATCH Blue LL40348/4 is let down at 5.0–6.0 wt% in 15–25 g/m² polyethylene coating layers applied to paperboard or aluminium foil; the process employs a 90–120 mm single-screw extruder with 30:1 L/D and a slot die with internal deckle adjustment, melt temperatures of 280–320°C, an air-gap distance of 150–250 mm, and a chill-roll temperature of 10–20°C. The higher let-down is necessary because at 20 µm coating thickness the same pigment concentration produces lower optical density than in 60 µm blown film; qualitative control targets a CIELAB ΔE < 1.0 across the web width under D65/10° according to ISO 11664-4. Compliance for food-contact coated paper and board is assessed under FDA 21 CFR §176.170(c) for aqueous and fatty foods, Regulation (EU) 10/2011 for overall migration and specific migration of colourants, and Good Manufacturing Practice Regulation (EC) No 2023/2006; foil-based pharmaceutical or food laminates require verification of the final multilayer structure, because the colourant is not necessarily authorised for direct contact in all jurisdictions. Downstream, the coated substrate passes through corona treatment at 42–48 dyn/cm and is slit or sheeted; terminal products include liquid packaging board for blue-branded beverages, frozen-food cartons, paper cupstock, and foil sachet laminates.
Rotational moulding of blue intermediate bulk containers and water storage tanks with LLDPE-rich powders is carried out on biaxially rotating carousel machines with shot weights of 20–60 kg, oven temperatures of 260–320°C, and cycle times of 30–60 min; POLYBATCH Blue LL40348/4 is dry-tumbled with LLDPE powder at 2.0–3.5 wt% rather than melt-compounded, because the low-shear process cannot duplicate the dispersive mixing of a twin-screw extruder. Published data for LL40348/4 specifically in rotomoulding is limited; the 2.0–3.5 wt% range should be confirmed by impact and colour trial on the intended machine. Compliance for tanks intended for potable water or aqueous food contact includes Regulation (EU) 10/2011 where applicable, FDA 21 CFR §177.1520(c) for the polymer, and national approvals such as BS 6920 for non-metallic materials in contact with water destined for human consumption; for dangerous-goods IBCs, the outer shell forms part of a composite or rigid plastics IBC tested under UN Model Regulations Chapter 6.5 for vibration, top lift, bottom lift, stacking, and leakproofness. Field-scale observations indicate that pigment-rich dry blends can segregate during the heating cycle in high-humidity charging rooms above 60% RH, leading to shade variation across the inner surface; pre-drying of the powder and masterbatch at 50–60°C for 2–3 hours may be required before charging. Terminal products include blue intermediate bulk container outer shells, water storage tanks, marine fenders, and rotomoulded agricultural hoppers.
Competitive LyondellBasell POLYBATCH™ Blue LL40348/4 Concentrate Based In LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
The LyondellBasell POLYBATCH™ Blue LL40348/4 Concentrate Based In LLDPE is a pelletized colourant masterbatch supplied as a controlled blue shade dispersed in a linear low-density polyethylene carrier. The designation LL40348/4 identifies a specific shade and carrier combination, but the complete pigment chemistry, particle-size distribution, and loading are lot-specific and are documented in the manufacturer’s certificate of analysis. Because the carrier is LLDPE, the product is intended for dilution into polyolefin conversion streams where a matched polyolefin carrier reduces phase incompatibility during melt blending. The material is handled as a free-flowing pellet, not as a neat pigment dispersion, and its dosing behaviour is governed by pellet bulk density, pellet geometry, and residual surface moisture.
Prior to lot acceptance, the melt mass-flow rate of a retained sample is measured under ISO 1133-1:2022 at 190 °C and 2.16 kg or 21.6 kg, depending on the carrier melt index. Density is determined under ASTM D792-20. Colourimetric acceptance is established by measuring CIELAB coordinates with a spectrophotometer using D65 illuminant and 10° observer; the resulting ΔE against a mutually agreed reference is evaluated under ASTM D2244-21. Published data for this specific configuration is limited, so lot-to-lot tint strength must be confirmed by converter trials against a retained standard. The table summarises the principal test instruments and regulatory instruments applicable to qualification of a polyolefin colour concentrate.
| Standard / Regulation | Measurement or Scope | Application to POLYBATCH™ Blue LL40348/4 |
|---|---|---|
| ISO 1133-1:2022 | Melt mass-flow rate of thermoplastics | Batch release and melt-viscosity matching to natural LLDPE/LDPE |
| ASTM D792-20 | Density of solid plastics | Carrier density for formulation and regrind calculations |
| ASTM D2244-21 | Colour difference | Acceptance of letdown plaques and finished parts against reference |
| ISO 4892-2:2013 | Xenon-arc weathering | Lightfastness qualification for outdoor or high-illumination service |
| EN 1186 series | Overall migration into food simulants | End-use food-contact verification for the finished article |
| 21 CFR 178.3297 | Colourants for polymers | US food-contact suitability of the colour system |
| RoHS 2011/65/EU | Heavy-metal restrictions | Electrical and electronic equipment homogeneous material limits |
On production lines equipped with gravimetric dosing, the letdown ratio is established by starting at the midpoint of the supplier’s recommended range and adjusting to maintain the target shade. For LLDPE-based blue concentrates of this class, commonly used addition levels in polyethylene film and injection moulding are between 2 wt% and 5 wt%, although the exact recommendation for LL40348/4 must be read from the product data sheet. On a blown film extruder with a 40 mm grooved-feed screw and an L/D ratio of 25:1, melt-temperature variation across the die of more than 10 °C can produce visible blue streaks if the carrier has not completely homogenised with the skin-layer resin. Screen-pack differential pressure is monitored against the clean-screen baseline; a sustained increase of 20 bar above baseline indicates pigment agglomeration or poor dispersion. In injection moulding with a 1200 kN clamp force and a 25 mm general-purpose screw, gravimetric feeding at the hopper is sufficient when the pellets are tumbled with the natural resin before processing. Back pressure between 0.5 MPa and 1.0 MPa and screw speeds from 50 rpm to 120 rpm are typical operating windows for masterbatch dilution on single-screw machines. The shear heating boundary is governed by the pigment chemistry; the melt temperature is maintained within the range specified on the safety data sheet.
In downstream blown film lines, inadequate screw mixing can produce shark-skin or colour streaks that are misdiagnosed as resin incompatibility. A 40 mm barrier screw with a Maddock mixer is more effective than a general-purpose screw for masterbatch dispersion because the mixer orientation forces molten polymer through narrow clearances, breaking up pigment agglomerates. The shear rate in the Maddock section for a 40 mm screw at 80 rpm is typically in the range of 100 s-1 to 500 s-1, depending on screw geometry. If the pressure variation at the die exceeds ±5% of the set point, the resulting thickness variation may interact with the blue pigment’s light-scattering behaviour and produce apparent colour banding. Published data for this specific configuration is limited, but these relationships are consistent with general polyolefin processing behaviour.
For colour matching in the finished article, a spectrophotometer in reflectance or transmittance mode is used with D65 illuminant and 10° observer; colour difference is reported as ΔE under ASTM D2244-21. Lightfastness is assessed under ISO 4892-2:2013 using xenon-arc exposure, with visible shade change evaluated against the AATCC grey scale or by ΔE. Heat stability depends on whether the blue pigment is a copper phthalocyanine, an ultramarine, or a mixed system. Copper phthalocyanine blues usually tolerate short-term processing up to 300 °C, while ultramarine blues may be acid-sensitive and can shift in humid or acidic service environments. For LL40348/4, the manufacturer’s statement of composition is required to determine which thermal and chemical boundary applies. Migration of low-molecular-weight colour components in the final polymer matrix can be evaluated according to the EN 1186 series for overall migration into food simulants when food-contact use is claimed.
On cast film lines with a 90 mm extruder and a 30:1 L/D barrier screw, pre-mixing of LL40348/4 with natural resin in a central blending system is permissible if pellet segregation is controlled. A pellet-size difference of more than 2:1 between masterbatch and natural resin can cause separation in a hopper, leading to colour drift. Gravimetric controls maintain a dosing accuracy of ±0.5% to keep short-term colour variation within the process capability index. Although the LLDPE carrier is not hygroscopic, opened packaging stored at relative humidity above 60% may carry surface moisture that is best removed by a brief dry-air purge before feeding.
When a converter replaces a wax-bound blue masterbatch with an LLDPE-based carrier, the finished article generally receives a lower concentration of low-molecular-weight binder. This difference can reduce die-lip plate-out during long-run blown film campaigns and may preserve heat-seal strength in polyethylene packaging because the carrier contributes to the polymer network rather than acting as a contaminant. The penalty is that an LLDPE carrier may require slightly higher melt temperatures than a wax-based system to reach full dispersion. In comparison with universal carriers containing ethylene-vinyl acetate or acrylate copolymers, the LLDPE carrier of LL40348/4 is better viscosity-matched to LLDPE and LDPE converter resins, but it is not recommended for polar resins such as polyamide, polycarbonate, or rigid PVC. If the concentrate is added to polypropylene homopolymer at low levels, phase separation may be limited, but the carrier phase is still a polyethylene incoherent domain and is evaluated for mechanical property loss in thin-wall packaging. Among polyolefin carrier grades, an LLDPE basis generally provides higher tensile elongation and tear resistance than an LDPE carrier, while a polypropylene-carrier grade would be preferred for high-temperature polypropylene fibre extrusion.
For laboratory qualification, a two-roll mill or a laboratory injection moulding machine is used to prepare test plaques or discs. The standard moulding temperature for LLDPE carriers is 190 °C, with a cooling time of 20 s and a clamping pressure of 15 MPa. The resulting colour is measured with a spectrophotometer, and tinting strength may be reported as a percentage relative to a retained standard. The exact method and tolerances follow the supplier’s quality agreement and the relevant ASTM D2244-21 procedure.
In the European Union, the finished article must comply with REACH Annex XVII restrictions and, for food-contact applications, with Regulation (EU) No 10/2011. Overall migration from food-contact plastics is limited to 10 mg/dm² of food-contact surface under the specified simulant and time-temperature conditions. In the United States, the colourant system is subject to 21 CFR 178.3297 when used in polymers for food contact, and the LLDPE carrier may be covered by 21 CFR 177.1520. RoHS 2011/65/EU applies only to electrical and electronic equipment; the homogeneous material limits are 1000 ppm for lead, 1000 ppm for mercury, 100 ppm for cadmium, and 1000 ppm for hexavalent chromium. Avoid combining any ultramarine-based blue colourant with acidic additives; if the blue pigment is a phthalocyanine system, strong oxidising or reducing environments are prevented during processing. If the product has been stored in opened packaging at relative humidity above 60%, surface condensation is removed and drying at a low temperature, not exceeding 60 °C, is validated before processing. The manufacturer’s safety data sheet and statement of composition take precedence over all general handling guidance.